• Title/Summary/Keyword: Ceramic tile

Search Result 68, Processing Time 0.024 seconds

Study on the Growth of Monoclinic VO2 Phase Applicable for Thermochromic Ceramic Tile

  • Jung, DaeYong;Kim, Ungsoo;Cho, Wooseok
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.5
    • /
    • pp.361-365
    • /
    • 2015
  • Vanadium dioxide ($VO_2$) of monoclinic phase exhibits Metal Insulator Phase Transition (MIPT) phenomenon involving a sharp change in electrical and optical properties at $68^{\circ}C$. Solution-based process is applied to form uniform $VO_2$ coating layer on ceramic tiles. This can selectively block the near-infrared light to possibly reduce the energy loss and prevent dew condensation caused by the temperature difference. Heat treatment conditions including temperature and dwell time were examined to obtain a monoclinic $VO_2$ single phase. Both rutile and monoclinic $VO_2$ phases were observed from in the tiles post-annealed below $700^{\circ}C$. Desired monoclinic $VO_2$ single phase was grown in the tiles heat treated at $750^{\circ}C$. Nano facets of irregular size were observed in the monoclinic $VO_2$ phase involving the phase-transition. Grain growth of monoclinic $VO_2$ phase was observed as a function of dwell time at $750^{\circ}C$.

Performance of one-part alkali activated recycled ceramic tile/fine soil binders

  • Mawlod, Arass Omer
    • Advances in concrete construction
    • /
    • v.10 no.4
    • /
    • pp.311-317
    • /
    • 2020
  • Performance of Sustainable materials continues through using of recycled waste construction materials to minimize the utilization of the natural resources. The cement industry is a major source of CO2 in the atmosphere which is the main cause of global warming. Replacement of OPC with other sustainable cementitious materials has been the most interesting area of researches. This investigation focuses on the properties of alkali-activated mortar with the different replacement ratios of ceramic tile powder (CTP) by fine soil powder (FSP) (0 to 100)% and different molarities of sodium hydroxide concentrations. The experimental program was conducted by examining the compressive strength, water absorption, and water sorptivity. The results showed that the compressive strength of the specimens at age of (28, 56, and 90 days) increases with an increase in the amount of fine soil powder content and decreases at the age of 120 days. Also, minimum water absorption at the age of 90 days was found in the mixes containing 100% fine soil powder. However, fine soil powder replacement had a negative effect on the sorptivity and water absorption values at the age of 120 days. On the other hand, the 12M sodium hydroxide concentration was considered the optimum concentration compared to other concentrations.

Effect of microstructure of surface glaze on printability of ink-jet printing ceramic tile (표면 유약 미세구조가 잉크젯 프린팅 도자타일의 인쇄적성에 미치는 효과)

  • Lee, Ji-Hyeon;Hwang, Kwang-Taek;Han, Kyu-Sung;Kim, Jin-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.28 no.6
    • /
    • pp.243-249
    • /
    • 2018
  • Ceramic tiles, which were manufactured through high-temperature firing process at over $1000^{\circ}C$, are widely used as interior and exterior materials for building construction due to their excellent durability and aesthetic of surface glaze. In recent years, the introduction of digital ink-jet printing in ceramic tiles for architectural use has been rapidly proceeding, and studies on the materials such as ceramic ink, ceramic pigment, glaze have been actively conducted. In this study, the effect of microstructure change of surface glaze on the printing properties of ceramic inks was investigated by micronization of kaolin, which is the raw material of surface glaze. Black ceramic ink was used for ink-jet printing on the surface glaze of ceramic tile to evaluate the printability by measuring the size and roundness of the printed ink dot. The relationship between microstructure change of surface glaze and printability of ceramic ink was also investigated by analyzing the surface roughness and internal micropore distribution of surface glaze.

Combustion Characteristic and Stability of Flat Premixed Ceramic Burner with Different Porous Baffle Plates (평판 예혼합 세라믹 버너의 분포판 변화에 따른 연소화염특성과 안정성 분석)

  • Lee, Jae-Young;Lee, Pil-Hyong;Park, Chang-Soo;Park, Bong-Il;Hwang, Sang-Soon
    • Journal of the Korean Society of Combustion
    • /
    • v.14 no.4
    • /
    • pp.7-16
    • /
    • 2009
  • Porous metal plates (Metal fiber, muti-hole metal plate) using mainly in surface burner are known to have a corrosion and durability problem under high temperature condition. In this study, premixed flat flame with perforated ceramic tile of more durable cordierite material was examined with respect to combustion stability and emission. The flat premixed ceramic burner consists of perforated ceramic tile and various type of baffle plates to form stable surface flame. The results show that most stable flat flame is generated using baffle plate with open ratio of 0.193. In downward flat flame mode which is widely used in condensing boiler, CO is measured below 50ppm from equivalence ratio 0.755 to 0.765 and $NO_X$ is measured below 12ppm from equivalence ratio 0.75 to 0.79. It is also found that the range of blue flame in flame stability curve becomes wider with increasing heat capacity.

  • PDF

New Development of Eco-friendly cementitious Ceramic Tile Adhesive by Thick-Bed method for Polishing tile and Porcelain tile (폴리싱 및 포세린 타일 떠붙임용 시멘트계 친환경 타일접착제 개발)

  • Cho, Chang-Hwan;Lee, Duk-Yong;Lee, Jae-Min;Choi, Il-Joon;Eom, Joo-Il
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2019.11a
    • /
    • pp.62-63
    • /
    • 2019
  • Currently, polymer-based tile cement (Thin-bed method) and epoxy adhesive (Thick-bed method) are mainly used as tile adhesive for polishing and porcelain. In the case of epoxy adhesive, there is a low economic efficiency, there is a problem that the work efficiency is reduced by mixing the resin and the hardener. In particular, the epoxy contains a bisphenol A and amine component, there is a risk of workable disease when a worker is exposed to odor and harmful gases generated in the epoxy adhesive for a long time. Against this background, it is necessary to analyze the hazards of using epoxy adhesives indoors, and develop cementitious high performance tile adhesive products with significantly lower hazards than epoxy adhesives.

  • PDF

The Effect of Compressing ER Electrode on Electrorheological Properties of Anhydrous ER Fluids (ER 유체용 압축전극이 ER 유체의 전기유변학적 특성에 미치는 영향)

  • Ahn, Byeng-Gil
    • Tribology and Lubricants
    • /
    • v.18 no.1
    • /
    • pp.16-23
    • /
    • 2002
  • For increasing the yield stress of ER fluids, the compressing ER electrode was developed and the compressing electrorheological (ER) behavior of anhydrous ER fluids in silicone oil of phosphorous ester cellulose powder was investigated. Under constant electric field, not only the current density but also the yield stress of anhydrous ER fluids were studied as varying the compressing length of ER electrode distance. From the experimental results the compressing of ER electrode had a large influence to the ER properties of anhydrous ER fluids. The current density was proportional to the compressing length of ER electrode under constant electric field and volume fraction also tile compressing yield stress was proportional to the volume fraction of dispersed particles under constant electric field and compressing length. When the ER electrode was compressed with 150mm after charging the electric field, 4 kV, tile yield stress of phosphoric ester cellulose ER fluids increased to thirteen times comparing with the yield stress measured at normal electrode.

Experimental Examination of Nonslip Technique of Floors (바닥의 미끄럼 방지기술에 관한 실험적 검토)

  • Shin, Yoon-Ho;Baek, Koen-Hyuk;Choi, Soo-Kyung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2009.05b
    • /
    • pp.235-238
    • /
    • 2009
  • The study of our investigating and analyzing through experiments the performance on nonslip techniques, which has been nationally applied and represented, showed the following results. 1) In wearing shoes condition, regardless the shape of the surface and surface condition of the object, it satisfied the performance standard in cleaned and dried condition and the pulverulent body mixed liquid dispersed moisture condition. However, for the case of the non-slip agent treatment, not likely as the non-slip tape treatment case, the effect was not approved as it shows almost the same CSR as none treatment. 2) In bare foot condition, it satisfied the performance standard in most of the objects except for the Ceramic tile (A), Ceramic tile (B), pure and soapy water dispersed condition.