Testing and evaluation of the corrosion behavior of Aluminum/Alumina bulk composites fabricated via combined stir casting and APB process

  • Abdalkareem Jasim;Ghassan Fadhil Smaisim;Abduladheem Turki Jalil;Surendar Aravindhan;Abdullah Hasan Jabbar;Shaymaa Abed Hussein;Muneam Hussein Ali;Muataz S. Alhassan;Yasser Fakri Mustafa
    • Advances in materials Research
    • /
    • v.12 no.4
    • /
    • pp.263-271
    • /
    • 2023
  • In this study, AA1060/Alumina composites were fabricated by combined stir casting and accumulative press bonding (APB). The APB process was repeated up to six press bonding steps at 300Ċ. As the novelty, potential dynamic polarization in 3.5Wt% NaCl solution was used to study the corrosion properties of these composites. The corrosion behavior of these samples was compared and studied with that of the annealed aluminum alloy 1060 and versus the number of APB steps. So, as a result of enhancing influence on the number of APB process, this experimental investigation showed a significant enhancement in the main electrochemical parameters and the inert character of the Alumina particles. Together with Reducing the active zones of the material surfaces could delay the corrosion process. Also, at higher number of steps, the corrosion resistance of composites improved. The sample produced after six number of steps had a low corrosion density in comparison with high corrosion density of annealed specimens. Also, the scanning electron microscopy (SEM), was used to study the corrosion surface of samples.

The Squeeze Casting and Its Structure of Mg-Al-Zn Alloy (Mg-Al-Zn합금에 있어서의 용탕단조와 그 조직)

  • Choi, J.C.;Choi, Y.D.
    • Journal of Korea Foundry Society
    • /
    • v.17 no.5
    • /
    • pp.419-425
    • /
    • 1997
  • 용탕단조방법에 의해 제조된 Mg-6Al-xZn(x=0, 1, 2)합금의 기계적 성질에 미치는 시효열처리의 영향을 조사한결과 아래와 같은 결론을 얻었다. (1) 주조조직을 관찰한 결과 미세한 수지상조직을 나타냈으며 초정${\alpha}$, 과포화 ${\alpha}$, ${\beta}$상 등 세가지 상으로 구성되어 있었다. (2) Mg-6Al-xZn합금은 시효경화성을 나타내었으며 Zn의 첨가량이 증가할수록 전시효구간에서 경도값이 높게 나타났다. (3) 시효조직을 관찰한 결과 $200^{\circ}C$의 시효시에는 불연속 석출물이 대부분 차지했으나 $240^{\circ}C$의 시효온도에서는 수지상 경계에서 시작되는 미세분산된 연속석출물이 대부분 이었다. (4) $240^{\circ}C$에서 시효열처리 한 시편은 연속석출물이 석출됨으로서 $200^{\circ}C$에서의 시효열처리된 시편에 비하여 과시효되는 경향이 작았다. (5) T6열처리 후 인장시험 결과 Zn 첨가량에 따라 강도가 증가하였는데 Mg-6Al-2Zn합금의 경우 인장강도는 248.4 MPa을 나타내었으며 Zn양에 따른 연신율의 감소는 나타나지 않았다.

  • PDF

Effect of Sn Addition on Microstructure of Al Alloy Powder for Brazing Process (브레이징용 Al 합금 분말의 미세조직에 미치는 Sn 함량의 영향)

  • Kim, Yong-Ho;Yoo, Hyo-Sang;Na, Sang-Su;Son, Hyeon-Taek
    • Journal of Powder Materials
    • /
    • v.27 no.2
    • /
    • pp.139-145
    • /
    • 2020
  • The powder manufacturing process using the gas atomizer process is easy for mass production, has a fine powder particle size, and has excellent mechanical properties compared to the existing casting process, so it can be applied to various industries such as automobiles, electronic devices, aviation, and 3D printers. In this study, a modified A4032-xSn (x = 0, 1, 3, 5, and 10 wt.%) alloy with low melting point properties is investigated. After maintaining an argon (Ar) gas atmosphere, the main crucible is tilted; containing molten metal at 1,000℃ by melting the master alloy at a high frequency, and Ar gas is sprayed at 10 bar gas pressure after the molten metal inflow to the tundish crucible, which is maintained at 800℃. The manufactured powder is measured using a particle size analyzer, and FESEM is used to observe the shape and surface of the alloy powder. DSC is performed to investigate the change in shape, according to the melting point and temperature change. The microstructure of added tin (Sn) was observed by heat treatment at 575℃ for 10 min. As the content of Sn increased, the volume fraction increased to 1.1, 3.1, 6.4, and 10.9%.

Fabrication of Metal Matrix Composites and Development of Forming System in Mashy State (반응고법에 의한 금속복합재료의 제조 및 성형 시스템의 개발)

  • 강충길;김현우;김영도
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.14 no.3
    • /
    • pp.581-593
    • /
    • 1990
  • A semi-solid alloy in which solid and liquid phase are co-existing is obtained by strirring of Al7075 molten metal. A semi-solid alloy is dependent on the corresponding temperature within the solid-liquid range, and the process parameters should be controlled accurately to obtain the homogeneous semi-solid alloy. The possibility o homogeneous fiber-reinforce aluminum alloy by addition of $Al_{2}$O$_{3}$ short fibers with vigorous agitation was investigated. The billet of composite materials was fabricated by squeeze casting, and homogeneous dipersion state of fibers in billet of fabricated metal matrix composites was observed. A slurry of semi-solid short fiber metal matrix composites is used in the direct rolling process, and this process showed the fabrication possibility of metal matrix composite sheets. The fabricated sheet was tested regarding vickers hardness, elongation and micro-structure. It has become clear that mashy state processing and working are very useful to obtain parts of composites material closed to near net shape.

High Temperature Deformation Behavior and Formability of Zr-Cu-Al-Ni Bulk Metallic Glass (Zr 계 비정질 합금의 고온 변형거동과 성형성 예측)

  • Jun, H.J.;Lee, K.S.;Chang, Y.W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.05a
    • /
    • pp.123-126
    • /
    • 2007
  • Deformation behavior of $Zr_{55}Cu_{30}Al_{10}Ni_5$ (at. %) bulk metallic glass (BMG) fabricated by suction casting method has been investigated at elevated temperatures in this study. The BMG was first verified to have an amorphous structure thru X-ray diffraction (XRD) and differential scanning calorimetry (DSC). A series of compression tests has consequently been performed in supercooled liquid temperature region to investigate the high temperature deformation behavior. A transition from Newtonian to non-Newtonian flow appeared to take place depending upon both the strain rate and test temperature. A processing map based on a dynamic materials model has been constructed to estimate a feasible forming condition for this BMG alloy.

  • PDF

ALLOY STRUCTURE AND ANODIC FILM GROWTH ON RAPIDLY SOLIDIFIED AL-SI-BASED ALLOYS

  • Kim, H.S.;Thompson, G.E.;Wood, G.C.;Wright, I.G.;Maringer, R.E.
    • Journal of the Korean institute of surface engineering
    • /
    • v.17 no.2
    • /
    • pp.29-40
    • /
    • 1984
  • The structure of rapidly solidified Al-Si-based alloys and its relationship to subsequent anodic film growth in near neutral and acid solutions have been investigated. Solidification of the alloys proceeds via pre-dendritic nuclei, associated with rugosity of the casting surface, from which cellular-type growth, comprised of aluminium-rich material surrounded by silicon-containing material, emanates. Observation of ultramicrotomed sections of the alloys and their anodic films reveals the local oxidation of the silicon-rich phase and its incorporation into the anodic alumina film, formed in near neutral solutions. Such incorporation occurs but resultant isolation of the silicon-rich phase is not possible for anodizing in phosphoric acid, and a three-dimensional network of the oxidized silicon-containing phase, with continuing development of porous anodic alumina, is observed.

  • PDF

Effects on extrusion ratio and temperature of shore fiber reinforcd metal matrix composites by rheo-compocating (반용융 가공법에 의한 단섬유 보강 급속복합재료의 강도에 미치는 압출비와 압출온도의 영향)

  • 윤한기;김석호;이상필
    • Journal of Ocean Engineering and Technology
    • /
    • v.11 no.2
    • /
    • pp.18-27
    • /
    • 1997
  • Al 6061 alloy reinforced with 10 vol.% ${\delta}-Al_2O_3$ short fiber was fabricated by Rheo-compocasting and squwwze cating. Extrusion processings were performed at temperatures from 40$0^{\circ}C$ to 55$0^{\circ}C$ with various extrusion ratio for curved shape dies. In proportion to the increase of extrusion ratios and temperatures, ultimate tensile strength for extruded materials improved. SEM observation of fractured surfsce was capcble oof accounting for fracture mechanism and bounding state of fiber and matrix.

  • PDF

High Temperature Deformation Behavior and Estimation for Formability of Zr55Cu30Al10Ni5 Bulk Metallic Glass (Zr계 비정질 합금의 고온 변형거동과 성형성 예측)

  • Jun, H.J.;Lee, K.S.;Chang, Y.W.
    • Transactions of Materials Processing
    • /
    • v.16 no.4 s.94
    • /
    • pp.309-312
    • /
    • 2007
  • Deformation behavior of $Zr_{55}Cu_{30}Al_{10}Ni_5$(at. %) bulk metallic glass(BMG) fabricated by suction casting method has been investigated at elevated temperatures in this study. The BMG was first verified to have an amorphous structure with the analysis of X-ray diffraction(XRD) and differential scanning calorimetry(DSC) data. A series of compression tests has consequently been performed in the region of supercooled liquid temperature to investigate the behavior of high temperature deformation. A transition from Newtonian to non-Newtonian flow appeared to take place depending upon both the strain rate and test temperature. A processing map based on a dynamic materials model has been constructed to estimate a feasible forming condition for this BMG alloy.

Characteristic Strength of $\delta$-Al$_2$O$_3$/Aluminum Composite by Rheo-compocasting (반용융 가공법에 의한 $\delta$-Al$_2$O$_3$/Aluminum 복합재료의 강도 특성)

  • 이상필;김만수;김석호;윤한기
    • Proceedings of the KWS Conference
    • /
    • 1995.04a
    • /
    • pp.155-159
    • /
    • 1995
  • A16061 alloy reinforced with 10 vol% $\delta$-A1$_2$O$_3$ short fiber have been fabricated by Rheo-compocasting and squeeze casting and extruded at high temperature using conical shape die and curved shape die with various extrusion ratios.. Tensile and hardness tests were carried out to examine mechanical properties of extruded materials and SEM observation of fractured surface was capable of accounting for fracture mechanism and bonding state of fiber and matrix.

  • PDF

Change in Corrosion Resistance of Solution-Treated AZ91-X%Sn Magnesium Alloys (용체화처리한 AZ91-X%Sn 마그네슘 합금의 부식 저항성 변화)

  • Moon, Jung-Hyun;Jun, Joong-Hwan
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.28 no.5
    • /
    • pp.229-238
    • /
    • 2015
  • The effects of Sn addition and solution treatment on corrosion behavior were studied in AZ91 magnesium casting alloy. The addition of 5%Sn contributed to the introduction of $Mg_2Sn$ phase, to the reduction in dendritic cell size and to the increase in the amount of secondary phases. After the solution treatment, trace amount of $Al_8Mn_5$ particles were observed in the ${\alpha}$-(Mg) matrix for the AZ91 alloy, while $Mg_2Sn$ phase with high thermal stability was additionally found in the AZ91-5%Sn alloy. Before the solution treatment, the AZ91-5%Sn alloy had better corrosion resistance than the Sn-free alloy, which is caused by the enhanced barrier effect of the (${\beta}+Mg_2Sn$) phases formed more continuously along the dendritic cell boundaries. It is interesting to note that after the solution treatment, the corrosion rate of both alloys became increased, but the Sn-added alloy showed higher corrosion rate than the Sn-free alloy. The microstructural examination on the corroded surfaces revealed that the remaining $Mg_2Sn$ particles in the solution-treated AZ91-5%Sn alloy play a role in accelerating corrosion by galvanic coupling with the ${\alpha}$-(Mg) matrix.