고분자 절연재료의 트랙킹 열화에 미치는 오손액의 영향 (The Effect of Contaminants on Tracking Aging in Polymer Insulating Materials)

  • 조한구;박용관
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권8호
    • /
    • pp.770-777
    • /
    • 1997
  • Some polymer materials including epoxy resin are being instead of porcelain for outdoor insulating materials such as insulators bushings cable terminators and surge arrester housing. And the largest problem to be overcomed is the tracking and erosion of the outdoor polymer material brought about by dry band arcing during prolonged exposure to contaminations. In this paper the effect of surface tension wettability flow rate of contaminants with varying surfactant content and frequency of applied voltage on the tracking breakdown of epoxy insulating materials were investigated. As the flow rate of contaminant is increased the surface resistivity is decreased and the leakage current is increased the time to tracking breakdown is decreased. It is found that time to tracking breakdown depends on the surface tension of contaminant that is difference of wettability. And as the frequency of applied voltage is increased time to tracking breakdown decreased.

  • PDF

APPLICATION OF ALANINE/ESR SPECTRUM SHAPE CHANGE IN GAMMA DOSIMETRY

  • Choi, Hoon;Kim, Jeong-In;Lee, Byung-Ill;Lim, Young-Ki
    • Nuclear Engineering and Technology
    • /
    • 제42권3호
    • /
    • pp.313-318
    • /
    • 2010
  • Alnine pellets were installed in a nuclear power plant for one or two operation cycles and measured by electron spin resonance (ESR) spectrometers for dosimetry. Dose and "x/y ratio", i.e., satellite peak over main center peak ratio, were measured for the returned alanine dosimeters from the nuclear power plant and compared to the values of reference alanine dosimeters exposed only to gamma rays. The variation of the x/y ratio change depended on the population of radicals from each radiation component with different LET. The gamma dose in a mixed radiation field was estimated by an additive gamma ray irradiation experiment and the measured dose rate at specified locations in the containment building.

파괴수명예측을 통한 지중배전용 전력케이블의 열화 진단 (Aging Diagnosis of Underground Distribution Power Cables Using Breakdown Lifetime Prediction)

  • 김충배;이정빈;임장섭;장영학;이진;김태성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.222-225
    • /
    • 1999
  • Degradation diagnosis of XLPE insulated URD cables was accomplished through out new method. which was to be analyzed non-electrical experiments and synthesized by degradation points. To supplement this method, it was also carried out using several electrical analyses. Breakdown voltages were measured and breakdown lifetimes were Predicted appling for Weibull distribution function. As a result, breakdown lifetime in failure cables was shorted up to 1/3 times than that in general cables. It was very available to estimate cable degradation using above method, but it needs further study on XLPE insulated URD cables in order to improve reliability.

  • PDF

A critical comparison of reflectometry methods for location of wiring faults

  • Furse, Cynthia;Chung, You Chung;Lo, Chet;Pendayala, Praveen
    • Smart Structures and Systems
    • /
    • 제2권1호
    • /
    • pp.25-46
    • /
    • 2006
  • Aging wiring in buildings, aircraft and transportation systems, consumer products, industrial machinery, etc. is among the most significant potential causes of catastrophic failure and maintenance cost in these structures. Smart wire health monitoring can therefore have a substantial impact on the overall health monitoring of the system. Reflectometry is commonly used for locating faults on wire and cables. This paper compares Time domain reflectometry (TDR), frequency domain reflectometry (FDR), mixed signal reflectometry (MSR), sequence time domain reflectometry (STDR), spread spectrum time domain reflectometry (SSTDR) and capacitance sensors in terms of their accuracy, convenience, cost, size, and ease of use. Advantages and limitations of each method are outlined and evaluated for several types of aircraft cables. The results in this paper can be extrapolated to other types of wire and cable systems.

14주기 열화에 따른 22.9kV TR CNCV-W 전력케이블의 Lightning-Impulse 파괴전압 특성분석 (Lightning Impulse Breakdown Voltage Characteristics for 22.9kV TR CNCV-W Power Cable Before and After Cyclic Aging for 14days)

  • 김위영;허종철;박태곤
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 제37회 하계학술대회 논문집 C
    • /
    • pp.1505-1506
    • /
    • 2006
  • XLPE 절연 전력케이블의 제조과정에서 발생하는 가교부산물을 제거할 목적으로 14주기노화를 실시한다. 이 과정에서 가교부산물이 제거되는 효과도 있지만 열에 의한 구조적 결함도 생기게 되며, 이들 모두가 뇌충격파괴전압에 영향을 준다. 22.9kV 트리억제형(TR CNCV-W) 케이블에 대하여 14주기노화 전과 후의 파괴전압을 분석하였으며, 전반적으로 노화과정이 파괴전압을 감소시키는 결과를 보였으나 60 $mm^2$ 케이블은 상승효과와 감소효과가 비슷하게 작용하는 것으로 나타났다.

  • PDF

14주기 열화 및 AWTT에 따른 22.9kV TR CNCV-W 전력케이블의 교류파괴전압 특성분석 (AC Breakdown Voltage Characteristics of 22.9kV TR XLPE Power Cable Before and After 14days Cyclic Aging and AWTT)

  • 김위영;허종철;박태곤
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 제37회 하계학술대회 논문집 C
    • /
    • pp.1507-1508
    • /
    • 2006
  • XLPE 절연 전력케이블의 제조과정에서 발생하는 가교부산물을 제거할 목적으로 14주기노화를 실시하며, XLPE 절연체에 발생하는 수트리를 가속 발생 성장시킬 목적으로 가속수트리 열화를 실시한다. 22.9kV 트리억제형(TR CNCV-W) 케이블에 대하여 14주기노화 전과 후, 120, 240, 360일 가속수트리(AWTT) 후의 파괴전압을 분석하였다. 14주기노화는 상승효과와 감소효과가 비슷하게 작용하는 것으로 나타났으며, 240일 AWTT 이후에 노화가 가속되는 것으로 나타났다.

  • PDF

지중송전 편단접지개소에서의 병행지선 설치효과 검토 (Study on the Effect of Parallel Ground Conductor at the Single Point Bonding in Underground Transmission System)

  • 강지원;박흥석;윤형희;윤종건;배주호;석광현;오장만;김재승
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2007년도 제38회 하계학술대회
    • /
    • pp.736-737
    • /
    • 2007
  • The single point bonding in underground transmission system can induce high voltage on the sheath when ground fault, lightning serge and switching serge occurs, at that time underground cable systems cannot offer a return path of fault current. Accordingly if fault current, which cannot return to ground, flows at the single point bonding, high voltage can be induced in SVL and that voltage can cause aging and breakdown of SVL. Therefore this paper study on the effect of parallel ground conductor at the single point bonding when ground fault and lightning serge occurs by using ATPDraw.

  • PDF

가속열화 된 CSPE의 특성에 미치는 담수침지의 영향 (Effects of Freshwater Flooding on the Properties of the Accelerated Thermally Aged CSPE)

  • 강명균;이정훈;이승훈;전준수;김인용;신용덕
    • 전기학회논문지
    • /
    • 제63권3호
    • /
    • pp.367-370
    • /
    • 2014
  • The accelerated thermal aging of a CSPE were carried out for 0, 80.82, 161.63 days at $100^{\circ}C$, which are equal to 0, 40 and 80 years, respectively. The volume electrical resistivities of the non-accelerated thermally aged CSPE and the accelerated thermally aged CSPE for 40y and 80y were $9.620{\times}10^{12}{\sim}1.246{\times}10^{13}{\Omega}{\cdot}cm$, $5.066{\times}10^{12}{\sim}7.576{\times}10^{12}{\Omega}{\cdot}cm$ and $7.195{\times}10^{12}{\sim}9.208{\times}10^{12}{\Omega}{\cdot}cm$ at room temperature, respectively. The dielectric constant of the non-accelerated thermally aged CSPE and the accelerated thermally aged CSPE for 40y and 80y were 3.355~4.030, 2.996~3.963 and 3.020~4.776 at room temperature, respectively. After seawater and freshwater flooding, the volume electrical resistivity of the CSPE trend slightly upward according to drying day at room temperature. After seawater flooding, the dielectric constant of the accelerated thermally aged CSPE were not measured. After seawater flooding, bright open pores of the accelerated thermally aged CSPE were partly transferred to dark close pores due to salinity. After freshwater flooding, dark close pores of the accelerated thermally aged CSPE were partly transferred to bright open pores because salinity of them is decreased. An insulation property of a cable in NPPs was decreased because of the seawater flooding, and an insulation property of them was recovered through the freshwater flooding. As a result, it is considered that an insulation property of a contaminated cable through Tsunami can be recovered if it is cleaned quickly.

배전용 전력 케이블을 위한 비-가교 폴리올레핀 재질의 절연특성 연구 (A Study on the Dielectric Characteristics of Non-Cross Linked Polyolefin for Distribution Power Cables)

  • 김준일;이온유;방승민;강종오;이홍석;정영호;강형구
    • 전기학회논문지P
    • /
    • 제63권4호
    • /
    • pp.373-377
    • /
    • 2014
  • A cross linked polyethylene (XLPE) material has been widely used to develop a distribution power cable due to its excellent electrical characteristics and mechanical strength. However, several problems such as environmental disruption, electrical aging, thermosetting property, and impurities which cause degradation also arise. Therefore, a novel dielectric material should be developed to substitute for the XLPE. Several kinds of polyolefin materials to substitute for the conventional dielectric material, XLPE are developed and A cylindrical rod to cylindrical rod electrode system made with stainless steel is used to perform the experiments according to the ASTM D-149 protocol under an AC and Impulse input voltage condition. The experimental results are calculated by the Weibull distribution method and analyzed by an Finite Element Method(FEM). Finally, the dielectric characteristics of the conventional XLPE and novel polyolefin are experimented compared with each other in this study.

Structural evaluation of all-GFRP cable-stayed footbridge after 20 years of service life

  • Gorski, Piotr;Stankiewicz, Beata;Tatara, Marcin
    • Steel and Composite Structures
    • /
    • 제29권4호
    • /
    • pp.527-544
    • /
    • 2018
  • The paper presents the study on a change in modal parameters and structural stiffness of cable-stayed Fiberline Bridge made entirely of Glass Fiber Reinforced Polymer (GFRP) composite used for 20 years in the fjord area of Kolding, Denmark. Due to this specific location the bridge structure was subjected to natural aging in harsh environmental conditions. The flexural properties of the pultruded GFRP profiles acquired from the analyzed footbridge in 1997 and 2012 were determined through three-point bending tests. It was found that the Young's modulus increased by approximately 9%. Moreover, the influence of the temperature on the storage and loss modulus of GFRP material acquired from the Fiberline Bridge was studied by the dynamic mechanical analysis. The good thermal stability in potential real temperatures was found. The natural vibration frequencies and mode shapes of the bridge for its original state were evaluated through the application of the Finite Element (FE) method. The initial FE model was created using the real geometrical and material data obtained from both the design data and flexural test results performed in 1997 for the intact composite GFRP material. Full scale experimental investigations of the free-decay response under human jumping for the experimental state were carried out applying accelerometers. Seven natural frequencies, corresponding mode shapes and damping ratios were identified. The numerical and experimental results were compared. Based on the difference in the fundamental natural frequency it was again confirmed that the structural stiffness of the bridge increased by about 9% after 20 years of service life. Data collected from this study were used to validate the assumed FE model. It can be concluded that the updated FE model accurately reproduces the dynamic behavior of the bridge and can be used as a proper baseline model for the long-term monitoring to evaluate the overall structural response under service loads. The obtained results provided a relevant data for the structural health monitoring of all-GFRP bridge.