  • In this study, a series of laboratory column test on Suction Drain Method which is one of the way to make an soft ground improvement were conducted in order to investigate the effect of the Hardening Zones and the ratio of improvements depending on periods of the improvements and various applied suction pressures. On this occasion, the experimental conditions are followings; in the case of the periods of effectiveness, 4 days, 8 days, 12 days, 16 days, 20 days and in the case of the applied pressures of the Suction are -20 kPa, -40 kPa, -60 kPa and -80 kPa were carried out. As a result of test, settlement increased with suction pressure and duration increase, and gradually converged. Also, as comparing permeability decrease ratio with which calculated back from water content and numerically predicted using Hansbo's radial consolidation theory, measured value was almost coincide with predicted value when permeability decrease ratio was assumed as 2~3. Furthermore, the hardening zone was appeared within 7~8 cm of whole radial (25 cm).

The Mechanical Properties of Porous Concrete using Recycled Asphalt Aggregate (아스팔트순환골재를 이용한 투수성 콘크리트의 역학적 특성)

  • Lee, Dong-Wook;Yun, Jung-Mann;Kim, Nam-Sik;Kang, Young-Min
    • Journal of the Korean Geosynthetics Society
    • /
    • v.10 no.1
    • /
    • pp.37-42
    • /
    • 2011
  • In this study, it is analyzed that mechanical properties and required strength of porous concrete according to the mixing ratio of cement, fine aggregate, and water/cement ratio in order to evaluate mechanical properties of porous concrete using recycled asphalt aggregate. Recycled asphalt aggregates of 13 mm were used without modification of aggregate grading to extend porous concrete application. The water/concrete ratio was poor mix and the range of compressive strength was 18.2 to 19.5 MPa. The average value of permeability showed 8.0E-02 cm/sec.

A Study on the Development of Geothermal Energy Using the Hydraulic Fracturing method (수압파쇄법을 이용한 지열에너지 개발에 관한 연구)

  • 이희근
    • Tunnel and Underground Space
    • /
    • v.5 no.4
    • /
    • pp.323-335
    • /
    • 1995
  • 지열에너지 개발의 기본적 개념은 지하 심부의 고온건조암체에 시추공을 이용한 수압파쇄를 실시하여 고온건조암체내에 인공파쇄대를 형성함으로써 유체의 유동회로를 구축하여 지열에너지의 회수를 도모하는 것이다. 본 논문에서는 수압파쇄균열의 발전방향 조절문제와 관련하여, 초고압수 절삭장치를 이용, 수압파쇄공 내에 인공슬롯을 형성하여 수압파쇄를 실시함으로써 균열의 발전방향을 조사하였으며, 수압파쇄에 의한 파쇄대내로의 유체순환실험을 통해 지열수의 유동특성을 규명하였다. 이를 위해 모델에 종균열과 횡균열을 형성시키고 균열내에 주입되는 물의 주입률, 정상류압력, 흐름저항을 조사하고, 이 결과를 이용하여 전산모델링을 수행하였다. 인공절리면에 대한 투수시험에서는 10$0^{\circ}C$까지의 온도변화에 따라 투수계수가 증가하였으며, 봉압 증가에 따라 증가율이 현저히 감소하였다.

  • PDF

A Study on Crushing and Engineering Characteristics Caused by Compaction of Recycled Aggregates (다짐으로 인한 순환골재의 파쇄 및 공학적 특성에 관한 연구)

  • Park, Sung-Sik;Chen, KeQiang;Lee, Young-Jae;Moon, Hong-Duk
    • Journal of the Korean Geotechnical Society
    • /
    • v.33 no.12
    • /
    • pp.35-44
    • /
    • 2017
  • A large amount of recycled aggregates was produced and crushed from old buildings and pavements. In this study, when these aggregates are re-used in subbase or subgrade materials in near construction sites, their engineering characteristics caused by crushing are investigated in terms of permeability and shear strength. Three different sizes of aggregates (31.5-45.0 mm, 19.0-31.5 mm, 9.5-19.0 mm) and their mixtures, a total of 7 types of aggregates were used in compaction tests (modified D and B methods). After compaction tests, aggregates were sieved and analyzed with four different breakage factors ($B_{15}$, $C_c$, $B_{10}$, $B_r$). The D compaction method gave 2.0-8.0 times more crushable than B compaction method. The breakage factors for the largest size aggregate was 1.4-3.0 times higher than those of the smallest size aggregate. For aggregates with 5.6-9.5 mm sizes, the samples were prepared with $B_{15}$ of 1, 3, 10, 20, 30, 50, 60, and 70 for permeability and direct shear tests. As $B_{15}$ increased, the hydraulic conductivity decreased up to 1/22 for $B_{15}=50$. As $B_{15}$ increased from 1 to 50, the peak friction angle increased from $46.1^{\circ}$ to $54.5^{\circ}$. On the other hand, the friction angle decreased after $B_{15}=60$.

Development and Application of Modified SWMM to Simulate Permeable Pavement and Infiltration Trench (투수성 포장과 침투 트렌치를 고려한 수정 SWMM의 개발 및 적용)

  • Lee, Jung-Min;Lee, Sang-Ho;Park, Jae-Hyeon;Lee, Kil-Seong
    • Proceedings of the Korea Water Resources Association Conference
    • /
    • 2007.05a
    • /
    • pp.326-330
    • /
    • 2007
  • 도시화 면적이 증가하면 불투수 면적이 증가하고 그에 따라 도시 하천의 평상시 유출이 감소한다. 도시유역의 평상시 수량을 회복시키는 방법으로는 침투 증진시설(투수성 포장, 침투 트렌치, 침투 측구 등)의 설치, 하수의 고도처리 후 방류 저수지에 의한 유황 개선, 지하철 용출수 활용 등이 있다. 우리나라의 경우에 일부 도시하천의 수량 감소가 심각한 상황에 이르고 있으며 이를 해결하고자 하는 노력이 최근에 나타나고 있다. 수량을 회복하려면 유량 평가를 위한 현장조사, 수량회복 계획, 재원의 반영, 수량회복 시설의 설치 및 관리의 순서로 단계별 사업이 수행되어야 한다. 계획 단계의 과업에서 필요한 사항은 여러 가지 수량 회복 방법의 영향을 정량 평가하는 것이다. 이에 핵심이 되는 것은 수량 회복 요소를 포함하거나 추가한 수문순환 평가 도구이다. 침투시설 중 투수성 포장과 침투 트렌치를 모의하도록 기존의 SWMM 모형을 수정하였다. 그 과정에서 증발량 처리와 지하수 출력기능에 대한 오류도 수정되었다. 수정 개발된 SWMM을 침투시설 모형실험 결과와 비교하여 수정된 프로그램의 적합성을 검증하였다. 투수성 포장과 침투 트렌치를 고려하여 수정된 프로그램을 안양천의 지류인 학의천 유역에 적용하여 침투시설의 효과를 분석하였다. 만일 학의천 불투수 면적의 10%를 투수성 포장으로 교체하면 하류 비산교 지점의 저수량$(Q_{275})$이 3 %, 갈수량$(Q_{355})$이 17 % 증가하는 것으로 분석되었다. 침투 트렌치의 경우 학의천 소유역 별로 100m 트렌치를 $5{\sim}10$개 시공할 경우 저수량은 약 1 %, 갈수량은 약9 %가 증가하였다. 수정 개발된 SWMM을 사용하면 침투 트렌치와 투수성 포장 이 도시 유역의 건기 수량회복에 미치는 영향을 분석할 수 있다.해 경보발령 이전에 한계수위를 넘어서는 경우(case_3)로서 분석되었다. 이러한 실패한 경보발령의 경우에 대한 원인분석 결과, 기존의 모형화를 통해 고려되지 못하였던 해안도시 홍수의 특성 중 총강우량에 대한 고려, 선행강우 여부 및 강우 지속시간, 지속시간 내 강우집중도 그리고 선정지점 내 조위의 영향과 유역내 합류식 하수관거 시스템의 영향 등 자연유역과는 다른 다소 복잡한 요소를 고려한 해안도시홍수 경보발령 기준에 대한 개선이 필요함을 확인할 수 있었다.이 좋다고 고찰된다. 6. 우리 나라의 현행 수도작기로 본 기온 및 일조조건은 수도의 분얼전기에 대해서는 호조건하에 놓여 있으나, 분얼후기인 7월 중ㆍ하순 경의 일조부족과 고온다습조건은 병해, 특히 도열병의 유발원인이 되고 있다. 7. 우리 나라의 현행수도작기로 본 전국각지의 수도의 출수기는 모두 일조시간이 적은 부적당한 시기에 처해 있다. 8. 출수후 40일간의 평균기온에 의한 적산온도 88$0^{\circ}C$의 출현기일은 수원에서 8월 23일이었고, 년간편차를 고려한 안전출수기일은 8월 19일로서 적산온도면에서는 관행 출수기일은 약간 늦다고 보았다. 9. 등열기의 평균기온에 의한 적산온도는 현행 수도작기로서는 최종한계시기에 놓여 있으며, 평균기온의 년간편차와 우리 나라의 최저기온이 낮은 점을 고려할 때, 현행출수기는 다소 늦은 것으로 보았다. 10. 생육단계별의 수도체내의 질소함량은 영양생장기의 질소함량이 과다하였으며, 출수 이후에 영양조락을 여하히 방지하느냐가 문제된다고 보았다. 11. 수리불안전답 및 천수답이 차지하는 전답면적의 비율은 차차 감소되고 있는데, 이와 전체 10a당 수량의 증가율과의 상관계수를 산출하였는데, 수리불안전답과의 상관계수 (4)는 +0.525였으며, 천수답과는 r=+0.832, 그리고 수리불안전답과 천수답을 합계한 것과의

  • PDF

Determination of Solidified Material's Optimum Mixing Ratio for Reservoir Embankment Reinforcement (저수지 제체 보강을 위한 고화재 최적 배합비 결정)

  • Jaegeun Woo;Jungsoon Hwang;Seungwook Kim;Seungcheol Baek
    • Journal of the Korean GEO-environmental Society
    • /
    • v.25 no.6
    • /
    • pp.5-12
    • /
    • 2024
  • Currently, a grouting method that minimizes damage to the reservoir embankment by injecting solidification agent at low pressure is commonly used to ensure waterproofing and safety of the embankment, but the use of solidification agents can cause issues, such as a decrease in durability and a lack of clear method for determining the mixing ratio. In this study, when the base ground and solidification agent were stirred and mixed at various weight mixing ratios, the permeability coefficient and strength of the mixture were confirmed through laboratory tests, and the optimal mixing ratio was suggested through analysis of the test results. The specimen for the laboratory test was produced considering the mixing ratio of the solidification agent. The specimen for the permeability coefficient test was tested by producing one each of cohesionless and cohesive soil for a mixing amount of 1.5 kN/m3 of solidification agent, and the permeability test results confirmed that the water barrier performance was secured below the permeability coefficient value required by various design criteria. A total of 24 specimens for the strength test were produced, 3 for each of 5 mixing amounts for cohesive soil and 3 mixing amounts for cohesionless soil. The strength test results showed that the uniaxial compressive strength tends to increase linearly with increasing curing time for both cohesionless soil and cohesive soil when the mixing amount is less than 2.0 kN/m3. Therefore, the optimal mixing ratio applied to the site is determined to be mixing amount of 1.5 kN/m3 and 2.0 kN/m3. Finally, numerical analysis reflecting test results was conducted on design case for improvement projects for aging reservoirs embankment to verify the water barrier performance and safety improvement effects.

Permeability Evaluation in Cold Joint Concrete with Mineral Admixture under Compressive and Tensile Loading (혼화재료를 고려한 압축 및 인장상태에서 콜드조인트 콘크리트의 투수성 평가)

  • Choi, Se-Jin;Kim, Seong-Jun;Mun, Jin-Man;Kwon, Seung-Jun
    • The Journal of the Korea Contents Association
    • /
    • v.15 no.9
    • /
    • pp.576-587
    • /
    • 2015
  • This paper presents a quantitative evaluation of water permeability in concrete with cold joint considering mineral admixture and loading conditions. Concrete samples with OPC (Ordinary Portland Cement) and GGBFS(Ground Granulated Blast Furnace Slag) are prepared considering 0.6 of W/C ratio and 40% of replacement. 30% and 60% loading levels for compression and 60% loading level for tension are induced to concrete samples. In compression conditions, the permeability in control case shows $2.41{\times}10^{-11}m/s$ in OPC concrete, and it changes to $2.07{\times}10^{-11}m/s$ (30% of peak) and $2.36{\times}10^{-11}m/s$ (60% of peak). The results in GGBFS concrete shows the same trend, which yields $2.17{\times}10^{-11}m/s$ (control), $1.65{\times}10^{-11}m/s$ (30% of peak), and $1.96{\times}10^{-11}m/s$ (60% of peak), respectively. In tensile conditions, the permeability increases from $2.37{\times}10^{-11}m/s$ (control) to $2.67{\times}10^{-11}m/s$ (60% of peak) while that in GGBFS concrete increases from $2.17{\times}10^{-11}m/s$ (control) to $2.24{\times}10^{-11}m/s$ (60% of peak). Permeability coefficients decreases in 30% of compressive level but increases in 60% level, while results in tensile level increases rapidly. This shows pore structure in concrete is condensed and with loading and permeability increases due to micro-cracking. Permeability evaluation considering the effects of loading conditions, cold joint, and GGBFS is verified to be important since water permeability greatly changes due to their effects.

The Compatibility of Slurry Wall Materials with Leachate for Cut -off of Contaminated Sites (오염지역 차폐용 슬러리월 재료와 침출수의 반응 특성)

  • 이용수;정하익
    • Geotechnical Engineering
    • /
    • v.13 no.2
    • /
    • pp.9-16
    • /
    • 1997
  • Cut-off methods of controlling leachate migration from waste landfills and contaminated sites are studied. Permeability and chemical compatibility tests are prrforlned on slurry wall materials including soil-bentonite, cement-bentonite, cement / fly ash-bentonite, plastic concrete. Hydraulic conductivity of soil-bentonite mixture is the lowest of these four bacuill materials. The leachate from municipal solid waste has little influence on the permeability of the backfill materials. The bentonite slurry becomes flocculated and aggregated when exposed to the leachate. The results of the permeability test showed that the hydraulic conductivities of the backfill materials are in the order soil-beiltonite, Plastic concrete, cement-bentonite. And the result c: the compatibility test showed increase in permeability due to the effects of leachate. Thus, in designing the slurry wall it is essential to check the behaviour of the bentonite slurry and backfill materials on the compatibility with the contaminants.

  • PDF

Effect of Acidic Leachate on the Cement-based Landfill Soil Liner System (고화토차수층에 대한 산성침출수의 영향과 대책방안 - 산업부산물(고로슬래그, 플라이애쉬) 재활용 방안 중심으로 -)

  • Cho, Jae-Beom;Hyun, Jae-Hyuk;Lee, Jong-Deuk;Park, Joung-Ku
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.28 no.3
    • /
    • pp.265-269
    • /
    • 2006
  • This study was to investigate the effect of acidic leachate on the landfill liner system and healing of cracks by using industrial by-products; BFS(Blast Furnace Slag) and FA(Fly Ash). From the results of pH measurement, for OPC(Ordinary Portland Cement) and DM(Dredged Mud) mixtures immersed acidic leachate, the initial pH($4.5{\sim}5.5$) was heavily increased to approximately 10 after 60 days experiment due to the production of 2 mole $OH^-$ which was occurred by hydrolysis of CaO and MgO etc.. Meanwhile, the initial pH of acidic leachate immersed DM mixtures with BFS and FA respectively was lasted for longer period as compared to the comparison. The reason was that production of low Ca C-S-H hydrates which stabilized in acidic liquid. The physical properties(compressive strength, hydraulic conductivity) of DM mixtures added BFS and FA was improved. It was concluded that the dissolution of hydrates was disturbed by high alkalinity of BFS and FA.

Field Tests and Analysis of Groundwater System for Stabilization of Slope in Large Open-Pit Coal Mine (대규모 노천 석탄광산의 사면 안정화를 위한 지하수 유동 체계 분석)

  • Ryu, D.W.;Kim, H.M.;Oh, J.H.;Sunwoo, C.;Jung, Y.B.
    • Tunnel and Underground Space
    • /
    • v.19 no.3
    • /
    • pp.248-260
    • /
    • 2009
  • With regard to oversea mineral resources development, recent trend has been changed from a simple capital investment to a direct development of the resources. In relation to the stability of a slope in large open-pit coal mine, groundwater system was investigated and the validity of horizontal drainage hole was evaluated in Pasir coal mine, Indonesia. In this work, various field tests were carried out for a characterization of groundwater system, which included in-situ permeability measurement, tracer test and monitoring of groundwater levels. Especially, the influence of SM river on the characteristics of the groundwater flow system was mainly inspected. For the permeability measurement, Guelph permeameter was employed, and was found that sandstone was more permeable than mudstone and coal seam. From a comparison of lithological structure and the results of groundwater level monitoring, sandstone and thin coal seam with fractures were found to be a main channel for groundwater flow. In the results of tracer tests, the effect of SM river on the groundwater system depends on the geological structure of its base. To identify the effect of horizontal drainage holes, 2-D groundwater modeling was performed. Four different cases were tested, which are different from the length of drainage hole and the existence of pond on top of the slope. To enhance the drainage effect and slope stability, the drainage hole should be drilled to the depth of coal seam layer, which provides a main pathway of groundwater flow and embedded by sandstone. For this purpose, correct identification of surrounding geology should be preceded.