Nb 첨가에 따른 저탄소강의 충격 특성에 미치는 변태 온도의 영향 (Influence Nb Addition and Transformation Temperature on Impact Properties of Low-Carbon Steels)

  • 이상인;강준영;황병철
    • 한국재료학회지
    • /
    • 제26권11호
    • /
    • pp.590-597
    • /
    • 2016
  • In this study, six kinds of low-carbon steel specimens with different ferrite-pearlite microstructures were fabricated by varying the Nb content and the transformation temperature. The microstructural factors of ferrite grain size, pearlite fraction, interlamellar spacing, and cementite thickness were quantitatively measured based on optical and scanning electron micrographs; then, Charpy impact tests were conducted in order to investigate the correlation of the microstructural factors with the impact toughness and the ductile-brittle transition temperature (DBTT). The microstructural analysis results showed that the Nb4 specimens had ferrite grain size smaller than that of the Nb0 specimens due to the pinning effect resulting from the formation of carbonitrides. The pearlite interlamellar spacing and the cementite thickness also decreased as the transformation temperature decreased. The Charpy impact test results indicated that the impact-absorbed energy increased and the ductile-brittle transition temperature decreased with addition of Nb content and decreasing transformation temperature, although all specimens showed ductile-brittle transition behaviour.

선급용 고강도 극후물재의 취성파괴 정지 성능에 관한 연구 (Brittle Crack Arrestability of Thick Steel Plates for Shipbuilding)

  • 안규백;류강묵;박준식;정보영;김태수;이종섭
    • Journal of Welding and Joining
    • /
    • 제28권1호
    • /
    • pp.47-53
    • /
    • 2010
  • In recent time there is vigorous requirement for the use of thick steel plate in various industrial fields including shipbuilding industry. Especially, with the continual increases in marine transportation volumes on a global scale, the steel of container ships has become thicker and thicker with the increased size of ships. In addition, the brittle crack arrestability of heavy thick plates was big issue, in recently. In this study, crack arrest test were conducted in order to investigate the crack arrestability of thick plates for shipbuilding steels, where test plate thicknesses were 50mm and 80mm. This paper introduces the brittle crack arrestability of heavy thick plates with thickness effect for shipbuilding.

아공석강의 충격인성 및 연성-취성 천이온도에 미치는 펄라이트 층상간격의 영향 (Effect of Pearlite Interlamellar Spacing on Impact Toughness and Ductile-Brittle Transition Temperature of Hypoeutectoid Steels)

  • 이상인;강준영;황병철
    • 한국재료학회지
    • /
    • 제25권8호
    • /
    • pp.417-422
    • /
    • 2015
  • In this study, low-carbon hypoeutectoid steels with different ferrite-pearlite microstructures were fabricated by varying transformation temperature. The microstructural factors such as pearlite fraction and interlamellar spacing, and cementite thickness were quantitatively measured and then Charpy impact tests conducted on the specimens in order to investigate the correlation of the microstructural factors with impact toughness and ductile-brittle transition temperature. The microstructural analysis results showed that the pearlite interlamellar spacing and cementite thickness decreases while the pearlite fraction increases as the transformation temperature decreases. Although the specimens with higher pearlite fractions have low absorbed energy, on the other hand, the absorbed energy is higher in room temperature than in low temperature. The upper-shelf energy slightly increases with decreasing the pearlite interlamellar spacing. However, the ductile-brittle transition temperature is hardly affected by the pearlite interlamellar spacing because there is an optimum interlamellar spacing dependent on lamellar ferrite and cementite thickness and because the increase in pearlite fraction and the decrease in interlamellar spacing with decreasing transformation temperature have a contradictory role on absorbed energy.

Brittle Deformation History Based on the Analyses of Dikes and Faults within Sedimentary Rocks on Geoje Island, SE Korea

  • Hategekimana, Francois;Kim, Young-Seog
    • 지질공학
    • /
    • 제31권3호
    • /
    • pp.239-255
    • /
    • 2021
  • Kinematic analyses of magmatic intrusions and faults can provide useful information on stress conditions and chronological relationships between dike emplacement and brittle deformation events. We studied structures in rocks exposed on a coastal platform in Geoje Island off the southern Korean Peninsula because of its well-developed dikes and faults. The geology of the study area includes the Cretaceous Seongpo-ri Formation, which is composed mostly of shale, sandstone, and hornfels intruded by magmatic dikes. Most of the dikes are developed along pre-existing structural features (faults and fractures), indicating that their emplacements were structurally controlled. Because dikes commonly open along the direction of the minimum principal stress, the direction of this stress can be obtained from dike geometry and orientation through the matching of piercing points on either side of a dike. In addition, the deformed dikes can give information regarding later deformation. On the basis of the kinematic analyses, we identified five deformation events in the study area, which are kinematically related to changes of the regional maximum principal stress. Results indicate that the structures in the study area have been controlled predominantly by episodes of reactivation of the NNE-trending Yangsan strike-slip fault, located to the northeast of the study area, under different stress regimes. In a wider tectonic context, the brittle deformation of the rocks of Geoje Island was probably induced by interactions among the Philippine Sea, Pacific, and Eurasian plates, including changes in subduction parameters with respect to the latter two plates over time.

조선용 EH40 강판의 용접부 취성 균열전파정지에 관한 연구 (Study of Brittle Crack Propagation Welding for EH40 Steel Plate in Shipbuilding Steel)

  • 최경신;이상훈;정원지;황희건;홍석한;홍지웅
    • 한국기계가공학회지
    • /
    • 제18권5호
    • /
    • pp.9-16
    • /
    • 2019
  • Recent economic trends are worsening and becoming longer, and Korean shipbuilding is focused on high value added and high technology, especially for LNG carriers and large container ships. Both ship types increased in size in the 2010s but have requirements such as high strength, toughness at low temperatures and continuous weldability for preventing brittle fractures at service temperatures. In particular, as container ships become larger, the International Classification Society (IACS) has established a provision (IACS UR S33) that mandates the use of BCA (Brittle Crack Arrest) certified vessels for large container vessels contracted after 2014 to ensure safety. Therefore, studies on BCA 47Y.P are currently being undertaken, but BCA 40Y.P has not been actively studied yet. We will test BCA 40Y.P to verify why it can be applied to a large container ship and measure fatigue cracking.

컨테이너선의 후 물재 용접부 취성 균열 전파에 대한 FCAW와 SAW의 비교 특성에 관한 연구 (Comparison of the Characteristics of FCAW and SAW for the Brittle Crack Propagation of Welded Parts of BCA Steel in Container Ships)

  • 최경신;이상훈;최정주
    • 한국기계가공학회지
    • /
    • 제20권3호
    • /
    • pp.24-32
    • /
    • 2021
  • The size of container ships is increasing to increase the cargo loading capacity. However, container ships are limited in terms of the hull longitudinal strength. To overcome this limitation, brittle crack arrest steel can be used. This study was aimed at examining the influence of the heat input on the welding procedures of flux cored arc welding and submerged arc welding. In the experiment, the crack tip opening displacement test, which pertains to a parameter of fracture mechanics, was performed, and a 3-point bending tester was adopted. Based on the results, the crack measurement method was presented, and the stress expansion coefficient value for the pre-fatigue crack length was derived according to the heat input after the pre-cracking length was measured. It was noted that the heat input affected the crack tip opening displacement of brittle crack arrest steel.

STS429L 겹침 용접부의 파단 특성에 관한 연구 (A Study on Characteristic of Fracture in Lap Joint Welded STS429L)

  • 최동순;김재성;김현재;이보영
    • Journal of Welding and Joining
    • /
    • 제27권5호
    • /
    • pp.49-54
    • /
    • 2009
  • Recently, a demand of ferritic STS is increasing rapidly in automobile exhaust system. Exhaust manifolds are the part nearest to the engine so that the material is exposed to high temperature exhaust gas. Excellent heat resistant properties, especially high temperature strength, thermal fatigue resistance and high corrosion resistance are necessary for these parts. STS429L contains 15 weight percent of Cr and low Mo, so has good price competitive. And it has excellent high temperature strength and corrosion resistance, so receives attentions as material that applying to exhaust manifold. In tensile test of lap joint welded STS 429L, most of specimens are failed in base metal, but occurs brittle fracture in weld metals at some specimens in the face of good welding conditions. In the process of tensile test, lap joint welded STS429L specimens are transformed locally. The brittle fracture occurs that local transforming area exists in weld metals. But, butt welding specimens made by same materials showed ductile fracture in tensile test and bending test. In this study, suppose the reason of brittle fracture is in the combined local transform and tensile stress, through analysis of bead geometry, evaluate geometrical factor of brittle fracture in lap joint welded STS429L.

응력조건에 따른 원형터널 주변의 취성파괴범위와 파괴심도 (The extent and depth of brittle failure around circular tunnel with stress conditions)

  • 천대성;박철환;전석원;박찬
    • 터널과지하공간
    • /
    • 제17권4호
    • /
    • pp.311-321
    • /
    • 2007
  • 경암 내 암반구조물의 파괴는 현지응력의 크기, 무결암의 강도 그리고 암반 내에 존재하는 불연속면의 상태에 의해 결정되며, 특히 높은 현지응력이 작용하는 경우 유도응력에 의해 취성파괴가 발생할 수 있다. 취성 파괴의 특성은 파괴수준, 파괴개시시점, 파괴범위와 파괴심도 등으로 구분할 수 있으며, 암반구조물의 안정성을 확보하기 위해서는 응력조건에 따른 취성파괴의 특성을 규명하여야 한다. 본 연구에서는 취성파괴가 발생한 상태에서 응력조건에 따른 파괴범위와 파괴심도를 평가하고자 하였다. 이를 위해 진삼축 압축응력조건에서 모형실험을 수행하였으며, 취성파괴가 발생한 모형실험체에 대하여 육안관찰과 컴퓨터단층촬영을 수행하여 파괴심도와 파괴범위를 결정하였다. 파괴심도는 터널단면에 작용하는 축차응력의 크기에 영향을 받으나 파괴범위의 경우 응력조건에 따른 뚜렷한 경향성을 보이지 않는 것으로 나타났다.

FRACOD를 이용한 취성 암석의 손상 및 파괴에 대한 경계요소 해석 (A Boundary Element Analysis for Damage and Failure Process of Brittle Rock using ERACOD)

  • 이희석
    • 터널과지하공간
    • /
    • 제14권4호
    • /
    • pp.248-260
    • /
    • 2004
  • 응력 증가에 의한 취성 암석의 손상은 미세균열의 개시로부터 시작하여 각 개별 균열들의 전파 및 결합에 의해 거시적인 파괴면을 발생시킨다. 전통적으로 암반의 손상 및 파괴현상을 설명하기 위해 거시적인 파괴 기준이나 탄소성 모델과 같은 연속체적인 접근법이 주류를 이루어왔다. 하지만 개별적인 균열들의 개시와 전락 과정을 명시적으로 고려할 수 있다면 현상론적인 관점에서 보다 실제에 가까운 암석 손상 및 파괴 과정을 재현할 수 있을 것이다. 본 연구에서는 암석의 균열 진전 모델링을 위해 개발된 경계요소 코드인 FRACOD를 이용하여 암석의 손상 및 파괴 과정을 모사한 결과를 제시한다. 수치일축압축시험을 통해 개발된 모델의 적정성을 검증하고 암반의 치수효과를 고려한 현실적인 암석 파괴 과정을 재현하였다. 또한 이러한 접근법의 적용 사례로서, 실제 굴착이 진행중인 심부 수갱 암반 주변에서 심도와 암반 특성에 따라 균열 진전과 이에 따른 암반 손상의 범위를 예측한 결과를 제시하였다. 이 접근법은 취성도가 큰 암반에서 발생하는 안정성 문제에 대한 공학적인 해법을 찾는데 기여를 할 수 있을 것으로 기대된다.

Metastatic Inhibitory and Radical Scavenging Efficacies of Saponins Extracted from the Brittle Star (Ophiocoma erinaceus)

  • Amini, Elaheh;Nabiuni, Mohammad;Baharara, Javad;Parivar, Kazem;Asili, Javad
    • Asian Pacific Journal of Cancer Prevention
    • /
    • 제16권11호
    • /
    • pp.4751-4758
    • /
    • 2015
  • Echinodermata use saponins in chemical defense against pathogens and predators. The molecular mechanisms of antimetastatic effects of brittle star saponins are still unknown. The present study examined antioxidant capacity and invasive ability in HeLa carcinoma cells exposed to brittle star crude saponins. Discolorating methods with DPPH and ABTS and expression of SOD-2 with RT-PCR were used to estimate the antioxidant activity. The anti-invasive activity of extracted saponins was examined through adhesion of HeLa cells to extracellular matrix, wound healing and evaluation of the mRNA levels of MMP-2 and MMP-9 by real time-PCR. The results showed that extracted saponins had cytotoxicity against cervical cancer cells and ABTS and DPPH scavenging properties with $IC_{50}$ values of 604.5, $1012{\mu}g/ml$, respectively. Further, we found that, in wound healing assay, brittle star saponins could prevent invasion of HeLa cells in a concentration dependent manner. Furthermore, cell adhesion assay demonstrated blockage of cell attachment to extracellular matrix with an $IC_{50}$ concentration of $16.1{\mu}g/ml$. The significant dose dependent down regulation of MMP-2 and MMP-9 in treated cells demonstrated that isolated saponins can decline tumor metastasis in vitro. The brittle star saponins remarkably prevented cervical cancer invasion and migration associated with down regulation of matrix metalloproteinase expression. Therefore, saponins could be suggested as an anti-invasive candidate against cervical cancer and an antioxidant as well.