• 제목/요약/키워드: Boron addition

검색결과 200건 처리시간 0.024초

고탄소강의 흑연화거동에 미치는 B첨가의 영향 (Effects of Boron Addition on the Graphitization Behavior in High Carbon Steel)

  • 우기도;박영구;김석원;진영철;류재화;나종필
    • 열처리공학회지
    • /
    • 제11권2호
    • /
    • pp.140-149
    • /
    • 1998
  • The graphitization is affected by the addition of small amount of the elements, such as Si, Al, Ni, B, Cr and Mn etc. Boron is well known as the most effective element for the graphitization of cementite in high carbon steels. But a study on quantitative analysis of B effect on the graphitization is few reported. Therefore the effect of boron addition in Fe-0.65%C-1.0%Si-0.5%Mn steels on the graphitization is investigated quantitatively using hardness tester, optical microscope and scanning electron microscope, neutron induced microscopic radiography. The graphitization in high carbon steels is promoted with 0.003~0.005%B addition. But the graphitization in steels which has no boron takes long holding time at $680{\sim}720^{\circ}C$. The hardness of quenched steel containing 0.003%B is higher than that of 0.005%B added steel due to complete dissolution of fine graphites into the austenite. The 0.003%B added high carbon steel graphitized at $680^{\circ}C$ for 25hr is useful steel for the agricultural implements and automobile parts which needed a good formability and high hardness.

  • PDF

미생물 성장을 억제하기 위하여 수용성 절삭유에 과다하게 첨가한 붕소와 아민 사례 연구 (Ethanolamine and boron abuse to limit microbial growth in water-synthetic metalworking fluids)

  • 박동욱;백도현
    • 한국산업보건학회지
    • /
    • 제15권3호
    • /
    • pp.270-276
    • /
    • 2005
  • This study was conducted to examine whether a specific synthetic metalworking fluid (MWF), "A", in use for 10 months without replacement, displayed microbial resistance and to identify the additives associated with the control of microbial growth. Three synthetic MWF products ("A", "B", and "C") were studied every week for two months. Microbial deterioration of the fluids was assessed through evaluation by endotoxin, bacteria and fungi levels in the MWFs. In addition, formaldehyde, boron, ethanolamine, and copper levels were also studied to determine whether they influence microbial growth in water-based MWFs. Throughout the entire study in the sump where MWF "A" was used, bacteria counts were lower than 103 CFU/mL, and endotoxins never exceeded 103 EU/mL. These levels were significantly lower than levels observed in sumps badly deteriorated with microbes. Boron levels in MWF "A" ranged from 91.7 to 129.6 ppm, which was significantly higher than boron levels found in other MWF products. The total level of ethanolamine (EA) in MWF "A" ranged from 35,595 to 57,857 ppm (average 40,903 ppm), which was over ten times higher than that found in other MWFs. Monoethanolamine (MEA), diethanolamine (DEA) and triethanolamine (TEA) concentrations in MWF "A" were also significantly higher than seen in other MWFs. However, although EA and boron might improve anti-microbial performance, their abuse can pose a serious risk to workers who handle MWFs. From an industrial hygiene perspective, our study results stress that the positive synergistic effect of boron and EA in reducing microbial activity in MWF must be balanced with the potentially negative health effects of such additives. Our study also addresses the disadvantage of failing to comprehensively report MWF additives on Material Safety Data Sheets (MSDS). Future research in MWF formulation is needed to find the best level of EA and boron for achieving optimal synergistic anti-microbial effects while minimizing employee health hazards.

BOTANI: High-fidelity multiphysics model for boron chemistry in CRUD deposits

  • Seo, Seungjin;Park, Byunggi;Kim, Sung Joong;Shin, Ho Cheol;Lee, Seo Jeong;Lee, Minho;Choi, Sungyeol
    • Nuclear Engineering and Technology
    • /
    • 제53권5호
    • /
    • pp.1676-1685
    • /
    • 2021
  • We develop a new high-fidelity multiphysics model to simulate boron chemistry in the porous Chalk River Unidentified Deposit (CRUD) deposits. Heat transfer, capillary flow, solute transport, and chemical reactions are fully coupled. The evaporation of coolant in the deposits is included in governing equations modified by the volume-averaged assumption of wick boiling. The axial offset anomaly (AOA) of the Seabrook nuclear power plant is simulated. The new model reasonably predicts the distributions of temperature, pressure, velocity, volumetric boiling heat density, and chemical concentrations. In the thicker CRUD regions, 60% of the total heat is removed by evaporative heat transfer, causing boron species accumulation. The new model successfully shows the quantitative effect of coolant evaporation on the local distributions of boron. The total amount of boron in the CRUD layer increases by a factor of 1.21 when an evaporation-driven increase of soluble and precipitated boron concentrations is reflected. In addition, the concentrations of B(OH)3 and LiBO2 are estimated according to various conditions such as different CRUD thickness and porosity. At the end of the cycle in the AOA case, the total mass of boron incorporated in CRUD deposits of a reference single fuel rod is estimated to be about 0.5 mg.

Cr-Mo계 금형강의 기계적 성질에 미치는 합금원소 및 템퍼링의 영향 (Effects of Alloying Element and Tempering on the Mechanical Properties of Cr-Mo Plastic Mold Steels)

  • 김남규;김병옥;이오연
    • 열처리공학회지
    • /
    • 제25권4호
    • /
    • pp.196-205
    • /
    • 2012
  • The purpose of this study is to enhance the hardenability and the mechanical properties by the addition of alloying elements such as Ni, Cr, Mo and B for the development of Cr-Mo plastic mold steel with uniform hardness and microstructure. The ingots were prepared by vacuum induction melting and forged to ${\Phi}35mm$ round bar. Forged bars were quenched and tempered at $200{\sim}600^{\circ}C$ for 1.5 hour. Jominy test, boron distribution observation, microstructual observation, tensile test and charpy impact test were conducted. It was confirmed that the hardenablity of these steels was improved by increasing of alloying elements and further promoted by the addition of boron. The critical rate of cooling required to obtain the bainitic structure for 0.27C-1.23Cr-0.28Mo-B steel was $0.5^{\circ}C/sec$. Hardness and strength of Cr-Mo steels decreased with increasing tempering temperature, but elongation and reduction of area increased with increasing tempering temperature. However, impact energy tempered at $400^{\circ}C$ showed the lowest value in the range $200{\sim}600^{\circ}C$ due to the temper embrittlement.

Microstructure and Mechanical Properties of Ni3Al Matrix Composites with Fine Aluminum Oxide by PM Method

  • Han, Chang-Suk;Choi, Dong-Nyeok
    • 한국재료학회지
    • /
    • 제28권9호
    • /
    • pp.495-498
    • /
    • 2018
  • Intermetallic compound matrix composites have been expected to be established as high temperature structural components. $Ni_3Al$ is a representative intermetallic alloy, which has excellent ductility even at room temperature by adding certain alloying elements. $Ni_3Al$ matrix composites with aluminum oxide particles, which are formed by the in-situ reaction between the alloy and aluminum borate whiskers, are fabricated by a powder metallurgical method. The addition of aluminum borate whiskers disperses the synthetic aluminum oxide particles during sintering and dramatically increases the strength of the composite. The uniform dispersion of reaction synthesized aluminum oxide particles and the uniform solution of boron in the matrix seem to play an important role in the improvement in strength. There is a dramatic increase in strength with the addition of the whisker, and the maximum value is obtained at a 10 vol% addition of whisker. The $Ni_3Al$ composite with 10 vol% aluminum oxide particles $0.3{\mu}m$ in size and with 0.1 wt% boron powder fabricated by the conventional powder metallurgical process does not have such high strength because of inhomogeneous distribution of aluminum oxide particles and of boron. The tensile strength of the $Ni_3Al$ with a 10 vol% aluminum borate whisker reaches more than twice the value, 930 MPa, of the parent alloy. No third phase is observed between the aluminum oxide and the matrix.

Si0.8Ge0.2계 합금에서 열전특성에 미치는 B의 영향 (Influence of Boron Content on the Thermoelectric Properties of p-type Si0.8Ge0.2 Alloy)

  • 황성두;최우석;박익민;박용호
    • 한국분말재료학회지
    • /
    • 제14권4호
    • /
    • pp.272-276
    • /
    • 2007
  • P-type thermoelectric material $Si_{0.8}Ge_{0.2}$ was sintered by Hot Press process (HP) and the effect of boron ($0.25{\sim}2$ at%) addition on the thermoelectric properties were reported. To enhance the thermoelectric performances, the $Si_{0.8}Ge_{0.2}$, alloys were fabricated by mechanical alloying (MA) and HP. The carrier of p-type SiGe alloy was controlled by B-doping. The effect of sintering condition and thermoelectric properties were investigated. B-doped SiGe alloys exhibited positive seebeck coefficient. The electrical conductivity and thermal conductivity were increased at the small amount of boron content ($0.25{\sim}0.5$ at%). However, they were decreased over 0.5 at% boron content. As a result, the small addition of boron improved the Z value. The Z value of 0.5 at% B doped $Si_{0.8}Ge_{0.2}$ B alloy was $0.9{\times}10{-4}/K$, the highest value among the prepared alloys.

Tribological Properties of Sputtered Boron Carbide Coating and the Effect of ${CH}_4$ Reactive Component of Processing Gas

  • Cuong, Pham-Duc;Ahn, Hyo-Sok;Kim, Jong-Hee;Shin, Kyung-Ho
    • KSTLE International Journal
    • /
    • 제4권2호
    • /
    • pp.56-59
    • /
    • 2003
  • Boron carbide thin coatings were deposited on silicon wafers by DC magnetron sputtering using a ${B}_4$C target with Ar as processing gas. Various amounts of methane gas (${CH}_4$) were added in the deposition process to better understand their influence on tribological properties of the coatings. Reciprocating wear tests employing an oscillating friction wear tester were performed to investigate the tribological behaviors of the coatings in ambient environment. The chemical characteristics of the coatings and worn surfaces were studied using X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES). It revealed that ${CH}_4$addition to Ar processing gas strongly affected the tribologcal properties of sputtered boron carbide coating. The coefficient of friction was reduced approximately from 0.4 to 0.1, and wear resistance was improved considerably by increasing the ratio of ${CH}_4$gas component from 0 to 1.2 vol %. By adding a sufficient amount of ${CH}_4$(1.2 %) in the deposition process, the boron carbide coating exhibited lowest friction and highest wear resistance.

Tribological properties of sputtered boron carbide coating and the effect of $CH_4$ reactive component of processing gas

  • Cuong Pham Duc;Ahn Hyo-Sok;Kim Jong-Hee;Shin Kyung-Ho
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2003년도 학술대회지
    • /
    • pp.78-84
    • /
    • 2003
  • Boron carbide thin coatings were deposited on silicon wafers by DC magnetron sputtering using a $B_4C$ target with As as processing gas. Various amounts of methane gas $(CH_4)$ were added in the deposition process to better understand their influence on tribological properties of the coatings. Reciprocating wear tests employing an oscillating friction wear tester were performed to investigate the tribological behaviors of the coatings in ambient environment. The chemical characteristics of the coatings and worn surfaces were studied using X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES). It revealed that $CH_4$ addition to As processing gas strongly affected the tribologcal properties of sputtered boron carbide coating. The coefficient of friction was reduced approximately from 0.4 to 0.1, and wear resistance was improved considerably by increasing the ratio of $CH_4$, gas component from 0 to $1.2\;vol\;\%$. By adding a sufficient amount of $CH_4\;(1.2\%)$ in the deposition process, the boron carbide coating exhibited lowest friction and highest wear resistance.

  • PDF

금속급(金屬級) 실리콘에서 슬래그 처리(處理)에 의한 붕소(硼素)의 제거(除去) (Removal of Boron from Metallurgical Grade Silicon by Slag Treatment)

  • 사공성대;손호상;최병진
    • 자원리싸이클링
    • /
    • 제20권3호
    • /
    • pp.55-61
    • /
    • 2011
  • 금속급 실리콘(MG-Si)을 태양전지용 실리콘(SOG-Si)으로 정제하기 위한 경제적인 프로세스를 구축하기 위하여 1823 K에서 CaO-$SiO_2$ 계 슬래그에 의한 붕소의 제거에 대하여 조사하였다. 본 연구에서 CaO-$SiO_2$$CaCO_3-SiO_2$ 슬래그의 염기도(%CaO/$%SiO_2$) 증가에 따라 B의 제거율은 각각 63%와 73%까지 증가하였다. 그러나 Ar 가스에 의한 슬래그와 실리콘의 교반 시간의 영향은 나타나지 않았다. 그리고 CaO-$SiO_2$ 계 슬래그에 $Na_2CO_3$를 첨가하였으나 그 영향은 크지 않았다. $CaCO_3-SiO_2$ 슬래그(염기도=1.2)에 의해 3회 처리한 결과 B의 농도는 1.03 ppm까지 감소하였다.

붕산농도 거동분석을 위한 종합적 붕산주입 및 희석모델 개발 (Development of Integrated Boration and Dilution Model for Boron Concentration Behavior Analysis)

  • Chi, Sung-Goo;Park, Han-Kwon;Kuh, Jung-Eui
    • Nuclear Engineering and Technology
    • /
    • 제24권1호
    • /
    • pp.30-39
    • /
    • 1992
  • 본 연구에서는 붕산주입 및 회석운전동안에 노심의 붕산농도를 변화시키기 위한 보충수 유량을 예측하고 화학 및 체적제어계통을 포함한 원자로 냉각재계통내에 있는 각종 계통에서 붕산농도 거동분석을 위한 종합적 붕산주입 및 희석모델(INBAD)이 제안되었다. 이 모델은 기존의 노심코드와 새로 개발된 붕산주입 및 희석모델로 구성되어 있으며 붕산주입 및 희석모델은 단일 cell 모델 및 다중 cell모델을 이용하여 본 연구목적에 맞게 개발되었다. 또한, 본 모델에서는 보다 실제적인 붕산농도 거동분석을 위하여 가변적 가압기 가열기 출력 및 선택적인 보충수 운전형태 (직접주입 또는 간접주입)가 모사되었다. 이 모델의 유용성을 증명하기 위하여 영광 3,4호기 설계자료를 이용하여 각종 계통에서 직접주입 및 간접주입운전에 대한 붕산농도 거동분석을 수행하였고, 노심의 붕산농도에 대한 가압기 가열기의 영향을 검토하였다. 그 결과 본 모델은 붕산주입 및 희석운전시에 각종 계통에서 붕산농도 변화를 정확히 예측할 수 있음을 보여 주었다.

  • PDF