Die-upset magnets from a mechanically-milled Pr(Co,In)$_5$-type alloy are known to have a peculiar texture; the easy magnetization axis (c-axis) is perpendicular to the pressing direction. This peculiar texture is thought to be linked closely to the anisotropic mechanical properties of Pr(Co,In)$_5$-type hexagonal compounds. The hardness of the Pr(Co,In)$_5$-type crystal was measured using selectively grown grains in an annealed $Pr_{17}Co_{82}In_1$ alloy button, and the crystallographic orientation was determined by observing the magnetic domain image. The hardness (549 VHN) on the plane with a 'cogwheel'-type domain image was significantly higher than that (510 VHN) on the plane with a 'cigar'-type domain image, indicating that the inter-layer bonding force between the (000l) basal planes is stronger than that between the (hki0) planes. This suggests that the most probable slip plane is the (hki0) plane parallel to the c-axis. During die-upsetting of the Pr(Co,In)$_5$-type alloys the deformation proceeds by (hki0) plane slip, and the c-axis rotates to ultimately become oriented perpendicular to the pressing direction. It is proposed that the peculiar texture in the die-upset Pr(Co,In)$_5$-type magnets is probably developed by slip deformation of the (hki0) plane of the Pr(Co,In)$_5$-type grains.
Journal of the korean academy of Pediatric Dentistry
/
제25권1호
/
pp.76-92
/
1998
The purpose of this study was to evaluate the possible efficacy of Nd-YAG laser as a dentin conditioner by observing the laser irradiation dentin surface under scanning electron micrograph and measuring shear bond strength of restored light-cured glass ionomer mold. Fifty intact premolars were prepared for shear bond strength tests. The teeth were randomly divided into five groups as follows; Group I. no treatment Group II. 10% poly acrylic acid, 20 sec Group III. laser treatment 2 w, 20 Hz, 2 sec Group IV. laser treatment 2 w, 20 Hz, 5 sec Group V. laser treatment 2 w, 20 Hz, 10 sec Samples of each group were restored with light-cured glass ionomer cement after dentin conditioning and then measuring the shear bond strength of each specimen were measured using universal testing machine. Additional ten premolars were prepared for SEM analysis The result from the this study can be summarized as follows. 1. Shear bond strength of polyacrylic acid-treated group (II) was significantly higher than other groups (p<0.05). 2. No statistically significant difference could be found between three laser-treated groups (III, IV, V) in shear bond strength(p>0.05) 3. According to the result of observation under SEM, Polyacrylic acid was shown to have removed the smear layer effectively and opened the dentinal tubules, whereas the laser has produced the irregular surface mainly composed of melted and fused structure. The microcracks found in laser-treated groups increased in number with irradiation time and formed the regular mesh-type in 10 sec-irradiation group. 4. The ultrastructural change of dentin surface created by laser irradiation was found to the improper for bonding of the glass ionomer restorative materials. And the lower shear bond strength of laser irradiated group might have been due to the failure to form the suit able dentin surface for the glass ionomer to penetrated into and form the proper micromechanical retention.
Fe-based amorphous coatings were fabricated on a soda-lime glass substrate by the vacuum kinetic spray method. The effect of the gas flow rate, which determines particle velocity, on the deposition behavior of the particle and microstructure of the resultant films was investigated. The as-fabricated microstructure of the film was studied by field emission scanning electron microscopy (FE-SEM) and high resolution transmission electron microscopy (HR-TEM). Although the activation energy for transformation from the amorphous phase to crystalline phase was lowered by severe plastic deformation and particle fracturing under a high strain rate, the crystalline phases could not be found in the coating layer. Incompletely fractured and small fragments 100~300 nm in size, which are smaller than initial feedstock material, were found on the coating surface and inside of the coating. Also, some pores and voids occurred between particle-particle interfaces. In the case of brittle Fe-based amorphous alloy, particles fail in fragmentation fracture mode through initiation and propagation of the numerous small cracks rather than shear fracture mode under compressive stress. It could be deduced that amorphous alloy underwent particle fracturing in a vacuum kinetic spray process. Also, it is considered that surface energy caused by the formation of new surfaces and friction energy contributed to the bonding of fragments.
Park, Sung-Cheol;Kim, Jae-Won;Kim, Ki-Hyun;Park, Se-Ho;Lee, Young-Min;Park, Young-Bae
Journal of the Microelectronics and Packaging Society
/
제17권1호
/
pp.41-46
/
2010
The interfacial adhesion strengths between screen-printed Ag film and epoxy resin-coated polyimide were evaluated by $180^{\circ}$ peel test method. Measured peel strength value was initially around $164.0{\pm}24.4J/m^2$, while the heat treatment during 24h at $120^{\circ}C$ increase peel strength up to $220.8{\pm}19.2J/m^2$. $85^{\circ}C/85%$ RH temperature/humidity treatment decrease peel strength to $84.1{\pm}50.8J/m^2$, which seems to be attributed to hydrolysis bonding reaction mechanism between metal and adhesive epoxy resin coating layer.
Park, Ho-Jun;Im, Geun-Bae;Son, Sang-Yeong;Song, In-Seop;Park, Jeong-Ho
The Transactions of the Korean Institute of Electrical Engineers C
/
제51권9호
/
pp.449-454
/
2002
A rectangular straight microchannel, integrated with the resistance temperature detectors(RTDs) for temperature sensing and a micro-heater for generating the Temperature gradient along the channel, was fabricated. Its dimension is 57${\mu}{\textrm}{m}$(H)$\times$200${\mu}{\textrm}{m}$(W)$\times$48,050${\mu}{\textrm}{m}$(L), and RTDs were placed at the inner-channel wall. Si wafer was used as a substrate. For the fabrication of RTDs, 5300$\AA$ thick Pt/Ti layer was sputtered on a Pyrex glass wafer. Finally, the glass wafer was bonded with Si wafer by anodic bonding, so that the RTDs are located inside the microchannel. Temperature coefficient of resistance(TCR) values of the fabricated Pt-RTDs were 2800~2950ppm$^{\circ}C$ and the variation of TCR value In the range of O~10$0^{\circ}C$ was less than 0.3%. Therefore, it was proved that the fabricated Pt-RTDs without annealing were excellent as temperature sensors. The temperature distribution in the microchannel was investigated as a function of mass flow rate and heating power. The temperature increase rate diminished with decreasing the applied power and increasing the mass flow rate. It was confirmed from the comparison with the simulation results that the temperature measured inside the microchannel is more accurate than measuring the temperature measured at the outer wall. The proposed temperature sensing method and microchannel are expected to be useful in microfluidics researches.
Seo, Hee-Don;Lee, Youn-Hee;Park, Jong-Dae;Choi, Se-Gon
Journal of Sensor Science and Technology
/
제2권1호
/
pp.19-27
/
1993
Capacitive pressure sensor for low pressure measurements has been fabricated by using $n^{+}$ epitaxial layer electrochemical etching stop and glass-to-silicon electrostatic bonding technique. The sensor had hybrid configuration of a sensor chip, which consists of sensor capacitor and reference capacitor, and two output signal detection IC chips. A fabricated sensor, with a $1.0{\times}1.0 mm^{2}$ square size and a $10{\mu}m$ thick flat diaphragm, showed a 7.1 pF zero pressure capacitance, and 5.2 % F.S, sensitivity in 10 KPa pressure range. By using a capacitance to voltage converter, the thermal zero shift of 0.051 %F.S./$^{\circ}C$ and the thermal sensitivity shift of 0.12 %F.S./$^{\circ}C$ for temperature range of $5{\sim}45^{\circ}C$ were obtained.
A vacuum pressure-difference technique for making a nano-precision replica is investigated for various applications. Master patterns for replication were fabricated using a nano-replication printing (nRP) process. In the nRP process, any picture and pattern can be replicated from a bitmap figure file in the range of several micrometers with resolution of 200nm. A liquid-state monomer is solidified by two-photon absorption (TPA) induced by a femto-second laser according to a voxel matrix scanning. After polymerization, the remaining monomers were removed simply by using ethanol droplets. And then, a gold metal layer of about 30nm thickness was deposited on the fabricated master patterns prior to polydimethylsiloxane molding for preventing bonding between the master and the polydimethylsiloxane mold. A few gold particles attached on the polydimethylsiloxane stamp during detaching process were removed by a gold selecting etchant. After fabricating the polydimethylsiloxane mold, a nano-precision polydimethylsiloxane replica was reproduced. More precise replica was produced by the vacuum pressure-difference technique that is proposed in this paper. Through this study, direct patterning on a glass plate, replicating a polydimethylsiloxane mold, and reproducing polydimethylsiloxane replica are demonstrated with a vacuum pressure-difference technique for various micro/nano-applications.
The W thin films were deposited on Si3N4 by a PECVD technique. The effects of substrate temperature and gas flow ratio on the properties of the W films were investigated. The deposition of W films were limited by surface reaction at the temperature range of 150>~$250^{\circ}C$, W films had the deposition rate of 150~530 $\AA$/min and stress of 0.85~$14.35\times10 ^9 \textrm {dynes/cm}^2}$ at various substrate temperatures and $SiH_4/WF_6$ flow ratios. $SiH_4/WF_6$ flow ratio affected the deposition rate and stress of the W films, expecially, excessive flow of SiH4 abruptly changed the structure, chemical bonding, and stress of the W films. Among the deposited W films on TiN, Ti, Mo, NiCr and Al adhesion layer, the one on the Al had the best adhesion property.
Due to excellent corrosion resistance, in particular against sea water, Al-2wt.$\%$Zn alloys have been used as the sacrifice anode material for tube of the ORV. Al-2wt.$\%$Zn alloys thermal-sprayed coating, however, were spalled on the lower part of ORV due to the lack of bonding strength between base material and coating layer and the dropping energy of sea water, To overcome the problems of the thermal spray coating, we developed the cladded tube manufacturing process by coextrusion of the clad and base metal. The corrosion resistance of cladded tube was improved by two times at least, compared with that of the present thermal spray coated vaporizer tubes.
Stainless-clad (SC) bimetallic steels that are manufactured by metallurgically bonding stainless steels as cladding metal and conventional mild steels as substrate metal, are kind of advanced steel plate products. Such advanced composite steels are gaining increasingly widespread usage in a range of engineering structures and have great potential to be used extensively for large civil and building infrastructures. Unfortunately, research work on the SC bimetallic steels from material level to structural design level for the applications in structural engineering field is very limited. Therefore, the aim of this paper is to investigate the material behaviour of the SC bimetallic steels under the cyclic loading which structural steels usually could encounter in seismic scenario. A number of SC bimetallic steel coupon specimens are tested under monotonic and cyclic loadings. The experimental monotonic and cyclic stress-strain curves of the SC bimetallic steels are obtained and analysed. The effects of the clad ratio that is defined as the ratio of the thickness of cladding layer to the total thickness of SC bimetallic steel plate on the monotonic and cyclic behaviour of the SC bimetallic steels are studied. Based on the experimental observations, a cyclic constitutive model with combined hardening criterion is recommended for numerical simulation of the cyclic behaviour of the SC bimetallic steels. The parameters of the constitutive model for the SC bimetallic steels with various clad ratios are calibrated. The research outcome presented in this paper may provide essential reference for further seismic analysis of structures fabricated from the SC bimetallic steels.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.