Park, Jong Won;Kim, Young Kyu;Han, Seung Hwan;Lee, Seung Woo
International Journal of Highway Engineering
/
v.16
no.1
/
pp.1-10
/
2014
PURPOSES : This study aimed to evaluate the long-term performance of bonded concrete overlay in Korean Highway, and factors influencing the performances. METHODS : The evaluation for long-term performance of bonded concrete overlay is investigated based on the following study : i) The pavement distress of number of bonded concrete overlay sections in Korean highway are collected through field measurement, and PCI for each section is calculated. ii) Performance of LTPP data of bonded concrete overlay sections in U.S.A is analysed. And it is compared with bonded concrete overlay of Korean highway. iii) An analysis of the factors influencing to long-term performance of bonded concrete overlay is investigated. RESULTS : Performance analysis was confirmed that the overlay thickness was affecting significantly on the Bonded Concrete Overlay life. The comparison of LTPP data(U.S.A) and field measurement data(Korean) was showed. CONCLUSIONS : It was showed that the performance of Korean bonded concrete overlay is relatively lower than that of the bonded concrete overlay in U.S.A. The cause of lower performance can be explained by the lack of overlay thickness.
Park, Jong Won;Kim, Young Kyu;Han, Seung Hwan;Lee, Seung Woo
International Journal of Highway Engineering
/
v.15
no.2
/
pp.47-55
/
2013
PURPOSES : This study aimed to evaluate the feasibility of AASHTO86 design method for Bonded Concrete Overlay. METHODS : The Feasibility of AASHTO86 design method for Bonded Concrete Overlay is investigated based on the following study : i) Sensitivity analysis of designed service life of Bonded Concrete Overlay by major design input for AASHTO86 guide. ii) Comparison of actual Bonded Concrete Overlay life and predicted Bonded Concrete Overlay life by AASHTO86. iii) Finding the stress component influence the potential distress of Bonded Concrete Overlay based on 3-d FEM analysis. iv) Exploring the limitation of AASHTO86 in the aspect of design input. RESULTS : Sensitivity analysis showed that the condition of existing pavement significantly on the Bonded Concrete Overlay life. Also the overlay thickness affect the Bonded Concrete Overlay life. The comparison of actual Bonded Concrete Overlay life and predicted Bonded Concrete Overlay life showed relatively good agreement when the early distress sections are excluded in comparison. Bonding stress occurred at the interface may be larger than the bond strength used in the specification of Bonded Concrete Overlay construction. CONCLUSIONS : Bonded Concrete Overlay life predicted by the AASHTO86 may not be reliable. Number of points to improve the reliability in the design of Bonded Concrete Overlay are suggested in this study.
Park, Jong Won;Kim, Young Kyu;Lee, Seung Woo;Han, Seung Hwan
International Journal of Highway Engineering
/
v.15
no.4
/
pp.1-9
/
2013
PURPOSES : Bonded concrete overlay is a favorable maintenance method since the material properties are similar to existing concrete pavements. In addition, bonded concrete overlay has advantage of structural performance since the overlay layer and the existing pavement perform as a monolithic layer. It is important to have suitable bond strength criteria to secure the performance of bonded concrete overlay. This study aimed to investigate the factors influencing bond strength characteristics between existing concrete pavement and overlay material. METHODS: Bond strength between overlay and existing pavement are measured and analyzed for various conditions such as the type of overlay materials, compressive and flexure strength of overlay and existing pavement, and deterioration status of existing pavement. RESULTS: The strength of overlay material does not significantly influence the bond strength. The overlay of ultra-rapid hardening cement generally gives low bond strength. However, ultra rapid hardening polymer modified concrete gives robust bond strength. The deterioration of existing concrete significantly decrease the bond strength. CONCLUSIONS: Bond strength of bonded concrete overlay highly depends on condition of existing concrete pavement rather than overlay material.
More than sixty percentage of highway in South Korea were constructed by concrete pavements and more than half of the concrete pavements were twenty years or older. Maintenance and rehabilitation of aged cement concrete pavements required early transportation opening due to difficulty of preparing bypass roads, given South Korea's transportation condition and so far, mostly asphalt concrete overlay has been used. However, asphalt concrete pavement maintenance and rehabilitation is costly because of early damage and at the same time, it causes inconvenience to the road users. Recently, as an effective method of rehabilitation for aged cement concrete pavement, bonded concrete overlay is being attempted. Therefore, utilizing various data on year-by-year basis is needed to rationally analyze of the damage on asphalt concrete overlay and bonded concrete overlay is necessary. However, in South Korea database of Serviceability damage on asphalt concrete overlay and bonded concrete overlay does not exist. In this research, performance is evaluated by the LTPP (Long Term Pavement Performance) Data of U.S.A, which accumulated various damage data of asphalt concrete overlay and bonded concrete overlay. However, the pattern distress of asphalt concrete overlay and bonded concrete overlay are different. Therefore, the pavement distress data of each section is collected into database and distress are calculated PCI(Pavement Condition Index) in order to compare life of asphalt concrete overlay and bonded concrete overlay.
PURPOSES : Recently, bonded concrete overlay has been used as an alternative solution in concrete pavement rehabilitation since its material properties are similar to those of the existing concrete pavements. Deteriorated concrete pavements need rapid rehabilitation in order to prevent traffic jams on Korean expressways. Moreover, speedy and effective repair methods are required. Therefore, the use of bonded concrete overlay with ultra-rapid hardening cement has increased in an effort to reopen promptly the expressways in Korea. However, mobile mixer is required for ultra-rapid hardening cement concrete mixing in the construction site. The use of mobile mixer causes various disadvantages aforementioned such as limitation of the construction supply, open-air storage of mixing materials, increase in construction cost, and etc. In this study, therefore, hydration accelerator in-situ mixing on polymer modified concrete produced in concrete plant is attempted in order to avoid the disadvantages of existing bonded concrete overlay method using ultra-rapid hardening cement. METHODS : Bonded concrete overlay materials using ultra-rapid hardening cement should be meet all the requirements including structural characteristics, compatibility, durability for field application. Therefore, This study aimed to evaluate the application of hydration accelerator in-situ mixing on polymer modified concrete by evaluating structural characteristics, compatibility, durability and economic efficiency for bonded concrete overlay. RESULTS : Test results of structural characteristics showed that the compressive, flexural strength and bond strength were exceed 21MPa, 3.15MPa and 1.4MPa, respectively, which are the target strengths of four hours age for the purpose of prompt traffic reopening. In addition, tests of compatibility, such as drying shrinkage, coefficient of thermal expansion and modulus of elasticity, and durability (chloride ions penetration resistance, freezing-thawing resistance, scaling resistance, abrasion resistance and crack resistance), showed that the hydration accelerator in-situ mixing on polymer modified concrete were satisfied the required criteria. CONCLUSIONS : It was known that the hydration accelerator in-situ mixing on polymer modified concrete overlay method was applicable for bonded concrete overlay and was a good alternative method to substitute the existing bonded concrete overlay method since structural characteristics, compatibility, durability were satisfied the criteria and its economic efficiency was excellent compare to the existing bonded concrete overlay methods.
Proceedings of the Korea Concrete Institute Conference
/
1997.04a
/
pp.635-642
/
1997
This research focused on the development of concrete overlay and test, which was conducted at 88 Highway 105k, 2 lanes of 290 m. The field application test consists of 6 cm and 10 cm bonded concrete overlay and 25 cm unbonded concrete overlay, using the slag cement for opening lanes for traffic early. The overlay were placed in a day. The whole period of traffic closing wes 8 day and it was reopened to traffic after concrete overlay has cured for 3 day. 5 cracks were founded when the field test section was investigated after 1 month, but all these may not make significant problems to overlay because these initiated and growed at the same line of repair section. The rideability and skid resistance become much better like in the new pavement after overlay. The structural capacity against deflection was much. which were verified by FWD(Falling Weight Deflectometer). The field test section is being used in a good condition and the results of field application and pavement performance analysis are encouraging. This rehabilitation methods may be adopted in Korea after a more field performance verifications.
KSCE Journal of Civil and Environmental Engineering Research
/
v.31
no.4D
/
pp.555-564
/
2011
More than sixty percentages of the highway constructed by concrete pavements in South Korea and over half of the concrete pavements were twenty years or older. The most of South Korea road is hard to provide a bypass in conditions of network of roads. Asphalt concrete overlay has been used for the overlay of aged concrete pavement. However, the cost of maintenance and rehabilitation in an asphalt overlay is expensive by early damage. Therefore, bonded concrete overlay was recently attempted in South Korea as an alterative method of rehabilitation for aged concrete pavement. Hence, it needed to investigate the factors to find performance of the bonded concrete overlay life. However, there is no performance data of the concrete overlay in South Korea. This study was to make a database of an affecting of the pavement life and draws statistical analysis of the performance data on the LTPP (Long Term Pavement Performance) database of U.S.A.
Asphalt concrete overlay method is used by general maintenance and rehabilitation of construction for aged concrete pavement in Korea. However, in case of the AC overlay method to extend service life of the existing concrete pavements, various distresses of reflection crack, pothole and rutting are the typical problems of the asphalt overlay on existing concrete pavement since it has different physical characteristics between asphalt overlay and existing concrete pavement. To achieve this, application of concrete overlay method is required instead of AC overlay method. Concrete overlay method has advantages that can reduce maintenance cycle and costs since it has excellent bearing value for heavy vehicles and no rutting. However, technical problems of detour road construction, traffic control and other disadvantages happened by long curing time. Thus, in this study and experimental research were launched to evaluate the workability, durability and resistance against environmental loading of Very Rapid Hardening Acrylic Polymer Modified Concrete(VRH-APMC) for application of bonded concrete overlay method. Test results showed that the compressive and bond strength were exceed 21MPa and 1.4MPa of target strength after four hours for rapid traffic opening properties. And tests of resistance against environmental loading results showed that VRH-APMC secured excellent durability. Thus, it was known that VRH-APMC was suitable material for large scale bonded concrete overlay method, and it was possible to use maintenance and rehabilitation method which needs enough workability and rapid traffic opening.
KSCE Journal of Civil and Environmental Engineering Research
/
v.33
no.3
/
pp.1153-1163
/
2013
Bonded concrete overlay is a favorable maintenance method since the material properties are similar to existing concrete pavements. In addition, bonded concrete overlay has advantage of structural performance based on being bonded together, both for the overlay layer and the existing pavement which perform as one monolithic layer. Therefore, it is important to have a suitable bond strength criteria for long term performance of bonded concrete overlay. This study aimed to investigate the affecting of bond strength on various bond characteristics, and to compare the bond strength between direct tensile test and indirect tensile test due to various conditions such as overlay materials, compressive and flexure strength of existing pavement, and deterioration status of existing pavement. As a result of this study, bond strength occurred by both of direct and indirect tensile test due to monotonic load is highly correlated such as coefficient of determination of 0.75 and P-value of 0.002. However, bond strength by indirect tensile test was relatively higher than bond strength by direct tensile test. It was known that correlation between direct and indirect tensile test was possible to use the characteristics analysis of bond fatigue behavior based on bond strength due to cyclic load which can simulate real field behavior of bonded concrete overlay.
Park, Je-Seon;Lee, Joo-Hyung;Kim, Tea-Kyung;Yun, Kyung-Ku
Journal of Industrial Technology
/
v.18
/
pp.363-370
/
1998
This study focused on the development of an alternative stress estimation procedure to instantly calculate the critical stresses bonded concrete pavement. Closed form analysis is commonly used to analyze pavement structures. This type of analysis assumes linearelastic material properties and static loading conditions. The well-known ILLI-SLAB finite element program was used for the analysis. Bonded concrete overlay analyzed the stress distribution, behavior and load carrying capacity under track load is made evaluation standard of bonded concrete overlay. In the study, the following results were derived ; The properties of strength is that compress and 3-point bending strength of existing pavement is deteriorated with $184kg/cm^2$, $59kg/cm^2$ but compress and splitting tensile strength of overlay is satisfied with $465kg/cm^2$, $45kg/cm^2$. Load transfers is happen at adjacent slab by interlocking under track load. The stress distribution under interior, corner and edge load is described high loading position surrounding then loading position.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.