고로슬래그 골재를 사용한 콘크리트 특성에 대한 실험적 연구 (The Experimental study on the property of concrete which used Blast furnace slag aggregate)

  • 박정우;김상미;김광기;임남기;정상진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.489-494
    • /
    • 2001
  • Several studies have reported that Granulated Blast-Furnace Slag improved the properties of concrete. The Granulated Blast-Furnace Slag could be a good alternative in the shortage of aggregate situation. Slag shows the possibility of influential aggregate and effect of environment preservation. This study presents that the basic properties of fresh concrete using Air-cooled Blast-furnace slag aggregate and Water-cooled Blast-furnace slag aggregate. Testing Factors of this study are concrete slump, slump loss, bleeding, and air contents. The result of this study is below. 1) In case of proportion slag and grave is 50 to 50, the biggest slump value is measured. 2) In the concrete using of air-cooled Blast-furnace slag aggregate, the bleeding capacity is a little. In the concrete using of Water-cooled Blast-furnace slag aggregate, the bleeding capacity goes up to 50% increase. 3) As substitution rate of the granulated blast-furnace slag goes up, air content is increased.

  • PDF

고로슬래그미분말을 사용한 고유동콘크리트의 특성 (Properties of Self Compacting Concrete Using Ground Granulated Blast Furnace Slag)

  • 김은겸;박천세;전찬기;이호석;최재진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.579-584
    • /
    • 2002
  • In this research, the physical properties of self compacting concrete using ground granulated blast furnace slag as a part of cement were investigated. Concrete using ground granulated blast furnace slag was prepared with various ground granulated blast furnace slag replacement(20~80 volume %) for cement and the quantities of coarse aggregate in concrete were 50%, 55% and 60% of ratio of absolute volume of coarse aggregate. The workability, flowing characteristics, air content and compressive strength of concrete using ground granulated blast furnace slag were tested and the results were compared with those of ordinary portland cement concrete. In the experiment, we acquired satisfactory results at the point of flowing characteristics and strengths of concrete using ground granulated blast furnace slag within tile replacement ratio of 50% and the optimum quantity of coarse aggregate in concrete was found to be 50%~55% of ratio of absolute volume of coarse aggregate.

  • PDF

수재사 모르터의 강도특성에 관한 연구 (An Experimental Study on the Quality of Mortar Strength using the Quenched Blast-Furnace Slag)

  • 임남기;이영도;양범석;김영회;최문식;정상진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.207-214
    • /
    • 1997
  • Strength experimental on mortar which use Quenched Blast-Furnace Slag as aggregate was carried our for a fundamental study of application possibility of Quenched Blast-Furnace Slag as aggregate. It gives the following results. The strength of mortar use Quenched Blast-Furnace Slag is decrease as substitution rate is higher. As W/C rate increase, the strength decrease, but the strength decrease of fine aggregate rate 1:3 is lower than 1:2. The relation with fine aggregate is that the amount of fine aggregate is inversely proportional to strength. Th relation with age is proportional to strength and strength rate of going is lower than general mortar in 28 age the change of strength proportionately with W/C rate is that as W/C rate increases, th strength is drop ; it shows that it has same tendency as general mortar sand or crushed sand, but while W/C rate increase the strength is as high as general mortar. The reason can be assumed that water content per unit needed to Quenched Blast-Furance Slag is more than in case of sand. In addition, the relation with substitution rate is that the strength is the strongest at substitution rate 25% and 50% ; that is , sometimes it is higher than mortar which use sand 100%. In addition, long age strength of mortar which use Quenched Blast-Furnace Slag as aggregate is about to be studied in the last.

  • PDF

고로슬래그 골재를 사용한 다공성 콘크리트의 물리·역학적 특성에 미치는 고로슬래그 미분말, 황토 및 보강섬유의 효과 (Effect of Blast Furnace Slag, Hwang-toh and Reinforcing Fibers on The Physical and Mechanical Properties of Porous Concrete Using Blast Furnace Slag Coarse Aggregate)

  • 이진형;박찬기
    • 한국농공학회논문집
    • /
    • 제52권5호
    • /
    • pp.53-60
    • /
    • 2010
  • The effects of blast furnace slag, hwang-toh, and reinforcing fiber on the physical and mechanical properties of porous concrete using blast furnace slag coarse aggregates have been evaluated in this study. The effect of the depending on replacement ratio of blast furnace slag to cement was investigated such that the replacement ratio was varied to 0 %, 25 % and 50 %. Also, the replacement ratios of hwang-toh were 0, 20 and 30 %. The polyvinyl alcohol fiber was used for the reinforcing fiber. A series of pH, unit mass, and void ratio tests have been performed to study the physical properties of the porous concrete using blast furnace slag coarse aggregates with the polyvinyl alcohol fiber and the replacement ratios of blast furnace slag, hwang-toh, while a series of compressive tests have been performed to evaluate the strength property depending on polyvinyl alcohol fiber and the replacement ratios of blast furnace slag, hwang-toh. The test results indicated that the physical and mechanical properties of porous concrete using blast furnace slag coarse aggregates is affected by the replacement ratio of blast furnace slag, and the fiber contents. According to the tests with polyvinyl alcohol fiber contents, the void ratio was decreased and the compressive strength was upgraded.

고로슬래그를 사용한 건식 및 습식 재생 잔골재 모르타르의 물리적 특성에 관한 연구 (A Study on the Physical Properties of Recycled Fine Aggregate (by Dry and Wet Type Production formula) Mortar Using Blast Furnace Slag)

  • 심종우;이세현;서치호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.501-504
    • /
    • 2006
  • Recycled aggregate mortar contains plenty of calcium hydroxide to improve the strength of blast furnace slag, although the surface mortar made of recycled aggregate deteriorates adhesion to cement paste and blast furnace slag has a low initial strength. Therefore, this study assumes that the combination with both recycled aggregate and blast furnace slag will produce a better performance. The results of the experiment show that dry mortar made of recycled aggregate provides with higher strength than wet mortar does at the 3-day and 7-day age, while lower at the 28-day age. It indicates that a large amount of cement mortar made of dry recycled aggregate has deteriorated adhesion strength. The mixes with 30% and 50% of blast furnace slag and 50% and 75% of recycled aggregate provide with much better strength at the 7-day age, although they usually have latent hydraulic property at the 28-day age. It indicates that calcium hydroxide($Ca(OH){_2}$) in recycled aggregate has affected ground granulated blast furnace slag.

  • PDF

고로슬래그를 사용한 습식 순환 잔골재 모르타르의 강도 특성에 관한 연구 (A Study on the Strength Property of Recycled Fine Aggregate (Wet Type) Mortar with Blast Furnace Slag)

  • 심종우
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제14권5호
    • /
    • pp.153-160
    • /
    • 2010
  • 고로슬래그 미분말을 순환골재 모르타르 및 콘크리트의 제조에 활용할 경우, 순환골재에서 용출된 $Ca(OH)_2$가 고로슬래그에 대한 자극제 역할을 수행하여 수화반응을 개선할 수 있을 것으로 판단되고 고로슬래그를 통해 알칼리 저감 효과를 얻을 것으로 예상되어 본 연구를 진행하게 되었다. 그 결과 고로슬래그 미분말을 혼입 사용한 순환 잔골재 모르타르는 재령 3일에서는 고로슬래그 혼입율에 따라 강도가 감소하는 결과를 나타냈다. 이는 고로슬래그의 수화반응이 일어나지 않았기 때문으로 판단되며 또한, 순환 잔골재 혼입률에 관계없이 고로슬래그 미분말의 혼입률이 증가함에 따라 재령 3일 측정한 수화활성도도 저하되는 것으로 나타났다. 재령 7일에서는 순환 잔골재에서 용출된 수산화칼슘($Ca(OH)_2$)이 자극제 역할을 수행하여 고로슬래그 미분말을 혼입한 배합의 압축강도 발현이 천연 잔골재를 사용한 모르타르보다 서서히 증가하는 결과를 보이기 시작하였으며 이로 인해 재령 7일 측정한 고로슬래그 미분말을 단계별로 혼입한 배합의 수화활성도가 고로슬래그를 혼입하지 않은 배합보다 높아지는 것으로 나타났다. 재령 28일에서는 고로슬래그 미분말 혼입률 30% 배합에서는 고로슬래그의 수화반응으로 인해 천연 잔골재를 사용한 배합보다 높은 압축강도를 보이기 시작하였으며 이때 측정한 수화활성도는 천연 잔골재를 사용한 배합과 특별한 차이를 보이지 않았으며, 이는 지속적으로 수산화칼슘($Ca(OH)_2$)이 공급되지 못하였기 때문으로 판단된다.

고로수쇄 슬래그 잔골재의 품질에 대한 고찰 (A Study on the Quality of the Water Coold Blast Furnace Slag Fine Aggregate)

  • 문한영;최연왕;김기형
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1990년도 봄 학술발표회 논문집
    • /
    • pp.24-28
    • /
    • 1990
  • The purpose of this study is to examine through the experimental study whether the water cooled unprocessed blast furnace slag produced in the country is useful for the fine aggregate of concrete or not. The results of this study show that the quality of the water cooled blast furnace slag is inferior to that of natural river sand and that the concrete made by substituting the water cooled blast furnace slag for fine aggregate have a tendency to decrease to some extent in strength. But if the water cooled blast furnace slag is transformed into more hardened state material, to use it as the fine aggregate of concrete will be possible.

  • PDF

Optimal Mixture Proportion for High Performance Concrete Incorporating Ground Granulated Blast furnace Slag

  • Choi Jae-Jin;Kim Eun-Kyum;Yoo Jung-Hoon
    • 콘크리트학회논문집
    • /
    • 제17권3호
    • /
    • pp.473-480
    • /
    • 2005
  • In this study, a mix design for self compacting concrete was based on Okamura's method and concrete incorporated just a ground granulated blast furnace slag. Replacement ratio of slag is in the range of $20-80\%$ of cement matrix by volume. For the optimal self compactability in mixture incorporating ground granulated blast furnace slag, the paste and mortar tests were first completed. Then the slump flow, elapsed time of 500mm slump flow, V funnel time and filling height by U type box were conducted in concrete. The volume of coarse aggregate in self compacting concrete was in the range of $50-60\%$ to the solid volume percentage of coarse aggregate. Finally, the compressive and splitting tensile strengths were determined in the hardened self compacting concrete incorporating ground granulated blast furnace slag. From the test results, it is desirable for self compacting concrete that the replacement of ground granulated blast furnace slag is in the range of $40-60\%$ of cement matrix by volume and the volume of coarse aggregate to the solid volume percentage of coarse aggregate with a limit of $55\%$.

고로슬래그를 사용한 고강도 부순모래 경화콘크리트의 물성에 관한 실험적 연구 (An Experimental Study on the Properties of the High Strength Crushed Sand Concrete Using Blast-Furnace Slag)

  • 최영화;김종인
    • 한국산업융합학회 논문집
    • /
    • 제8권3호
    • /
    • pp.169-176
    • /
    • 2005
  • The purpose of this study is to develop the high strength crushed sand concrete in conditions of water binder ratios of 25, 30, 35% and blast-furnace slag substitutions of 0, 15, 30, 45%. Additionally, in case of water binder ratio of 30%, the maximum size of coarse aggregate is two kinds of 13, 19 mm. The conclusions of this study are as follows ; 1. The compressive strength appeared lower in early age as compared with that of plain concrete according to increasing of the blast-furnace slag substitution. But, the compressive strength was respectively 5, 6, 10% larger than that of plain concrete in case of 25, 30, 35% water binder ratios, 28 days, 30% blast-furnace slag substitution and 19mm coarse aggregate. 2. According to increasing of the blast-furnace slag substitution, the modulus of elasticity and the tensile strength of concrete increased. 3. The length change by the shrinkage increased when the larger coarse aggregate was used, and decreased according to higher blast-furnace slag substitution.

  • PDF

폐내화물 골재 치환율이 고로슬래그 미분말과 순환골재 사용 모르타르의 품질에 미치는 영향 (Influence of Replacement Ratio of Wasted Refractory Aggregate on the Properties of Mortar using Blast Furnace Slag and Recycled Aggregate)

  • 송원루;문병룡;김민상;이제현;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 춘계 학술논문 발표대회
    • /
    • pp.139-140
    • /
    • 2016
  • In this research, the possibility of wasted refractory aggregate pulverized from refractory block as an expansive admixture and additional alkaline stimulant for class two and three blast furnace slag cements (BSC) was assessed with its high content of free CaO or free MgO. As the replacement ratios of wasted refractory powder and blast furnace slag were increased, flow and air content were decreased, while unit volume weight was increased under same conditions. Compressive strength of mortar was increased with increased replacement ratio of wasted refractory powder, especially, in the case of class three BSC, the highest compressive strength was obtained when wasted refractory aggregate was replaced 2%.

  • PDF