• 제목/요약/키워드: Bifacial silicon solar cell

검색결과 5건 처리시간 0.021초

Biracial Silicon Solar Cells with Spin-on Doping and Electroless Plating

  • U. Gangopadhyay;Kim, Kyung-Hae;S.K. Dhungel;D. Mangalaraj;Park, J.H.;J. Yi
    • Transactions on Electrical and Electronic Materials
    • /
    • 제5권1호
    • /
    • pp.7-10
    • /
    • 2004
  • A new method for fabrication of transistor like structure of the bifacial solar cell using spin-on doping and electroless plating has been proposed and the basic characteristics of the bifacial cell have been investigated. It is found that 9% increase in short circuit current is achieved with bifacial connection than the unifacial connection. Some unwanted effect of the series resistance on collection efficiency under different mode of illumination has been pointed out. Loss mechanisms inherent in the transistor like bifacial structure have also been discussed.

N형 양면 수광 태양전지를 위한 레이저 공정의 후면 패시베이션 적층 구조 영향성 (Effect of Laser Ablation on Rear Passivation Stack for N-type Bifacial Solar Cell Application)

  • 김기륜;장효식
    • 한국재료학회지
    • /
    • 제30권5호
    • /
    • pp.262-266
    • /
    • 2020
  • In this paper, we investigated the effect of the passivation stack with Al2O3, hydrogenated silicon nitride (SiNx:H) stack and Al2O3, silicon oxynitride (SiONx) stack in the n type bifacial solar cell on monocrystalline silicon. SiNx:H and SiONx films were deposited by plasma enhanced chemical vapor deposition on the Al2O3 thin film deposited by thermal atomic layer deposition. We focus on passivation properties of the two stack structure after laser ablation process in order to improve bifaciality of the cell. Our results showed SiNx:H with Al2O3 stack is 10 mV higher in implied open circuit voltage and 60 ㎲ higher in minority carrier lifetime than SiONx with Al2O3 stack at Ni silicide formation temperature for 1.8% open area ratio. This can be explained by hydrogen passivation at the Al2O3/Si interface and Al2O3 layer of laser damaged area during annealing.

Optimization of the Phosphorus Doped BSF Doping Profile and Formation Method for N-type Bifacial Solar Cells

  • Cui, Jian;Ahn, Shihyun;Balaji, Nagarajan;Park, Cheolmin;Yi, Junsin
    • Current Photovoltaic Research
    • /
    • 제4권2호
    • /
    • pp.31-41
    • /
    • 2016
  • n-type PERT (passivated emitter, rear totally diffused) bifacial solar cells with boron and phosphorus diffusion as p+ emitter and n+ BSF (back surface field) have attracted significant research interest recently. In this work, the influences of wafer thickness, bulk lifetime, emitter, BSF on the photovoltaic characteristics of solar cells are discussed. The performance of the solar cell is determined by using one-dimensional solar cell simulation software PC1D. The simulation results show that the key role of the BSF is to decrease the surface doping concentration reducing the recombination and thus, increasing the cell efficiency. A lightly phosphorus doped BSF (LD BSF) was experimentally optimized to get low surface dopant concentration for n type bifacial solar cells. Pre-oxidation combined with a multi-plateau drive-in, using limited source diffusion was carried out before pre-deposition. It could reduce the surface dopant concentration with minimal impact on the sheet resistance.

실리콘 이종접합 태양전지 개발동향 (Recent Development of High-efficiency Silicon Heterojunction Technology Solar Cells)

  • 이아름;유진수;박성은;박주형;안승규;조준식
    • Current Photovoltaic Research
    • /
    • 제9권4호
    • /
    • pp.111-122
    • /
    • 2021
  • Silicon heterojunction technology (HJT) solar cells have received considerable attention due to advantages that include high efficiency over 26%, good performance in the real world environment, and easy application to bifacial power generation using symmetric device structure. Furthermore, ultra-highly efficient perovskite/c-Si tandem devices using the HJT bottom cells have been reported. In this paper, we discuss the unique feature of the HJT solar cells, the fabrication processes and the current status of technology development. We also investigate practical challenges and key technologies of the HJT solar cell manufacturers for reducing fabrication cost and increasing productivity.

광흡수층 두께에 따른 투광형 비정질 실리콘 박막 태양전지의 양면발전 성능특성 (Impact of Absorber Thickness on Bifacial Performance Characteristics of Semitransparent Amorphous Silicon Thin-Film Solar Cells)

  • 서영훈;이아름;신민정;조아라;안승규;박주형;유진수;최보훈;조준식
    • Current Photovoltaic Research
    • /
    • 제7권4호
    • /
    • pp.97-102
    • /
    • 2019
  • Bifacial and semitransparent hydrogenated amorphous silicon (a-Si:H) thin-film solar cells in p-i-n configuration were prepared with front and rear transparent conducting oxide (TCO) electrodes using plasma-enhanced chemical vapor deposition method. Fluorine-doped tin oxide and tin-doped indium oxide films were used as front and rear TCO contacts, respectively. Film thickness of intrinsic a-Si:H absorber layers were controlled from 150 nm to 450 nm by changing deposition time. The dependence of performance characteristics of solar cells on the front and rear illumination direction were investigated. For front illumination, gradual increase in the short-circuit current density (JSC) from 10.59 mA/㎠ to 14.19 mA/㎠ was obtained, whereas slight decreases from 0.83 V to 0.81 V for the open-circuit voltage (VOC) and from 68.43% to 65.75% for fill factor (FF) were observed. The average optical transmittance in the wavelength region of 380 ~ 780 nm of the solar cells decreased gradually from 22.76% to 15.67% as the absorber thickness was changed from 150 nm to 450 nm. In case of the solar cells under rear illumination condition, the JSC increased from 10.81 to 12.64 mA/㎠ and the FF deceased from 66.63% to 61.85%, while the VOC values were maintained at 0.80 V with increasing the absorber thickness from 150 nm to 450 nm. By optimizing the deposition parameters, a high-quality bifacial and semitransparent a-Si:H solar cell with 350 nm-thick i-a-Si:H absorber layer exhibited the conversion efficiencies of 7.69% for front illumination and 6.40% for rear illumination, and average visible optical transmittance of 17.20%.