Bi-2223 선재를 이용한 Prototype 고온 초전도 케이블의 전기적 특성 (An Electrical Properties of Prototype HTS Cable using Bi-2223 tape)

  • 김영석;이병성;장현만;곽민환;김상현
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2000년도 하계학술대회 논문집 C
    • /
    • pp.1551-1553
    • /
    • 2000
  • Superconducting power cable is one of the most promising energy application of high-$T_c$ superconductors (HTS). A prototype HTS cable have been constructed multi-layer cable using Bi-2223 tape and tested. The result shows that the total transport current of HTS cable in $LN_2$ was 475[A], and transport current passed through almost the outer layer (2-layer). Also, AC transport losses in outer layer of HTS cable was proportion to $I^2$ and higher than losses of inner layer. As magnetic distribution were concentrated on outer layer.

  • PDF

Bi-2223계 Prototype 고온 초존도 케이블의 전류 통전 특성 (The Characteristics on Transport Current of Bi-2223 Based Prototype HTS Cable)

  • 김영석;이병성;곽민환;장현만;김상현
    • 한국전기전자재료학회논문지
    • /
    • 제13권7호
    • /
    • pp.630-635
    • /
    • 2000
  • Superconducting power cable is one of the most promising energy application of high-T$\sub$2/ superconductor(HTS). Thus we investigated previously the electrical and mechanical characteristics on Bi-2223 Ag sheathed tape. And a prototype HTS cable have been designed constructed and tested. In case of 19-filament type transport losses agree with the results of norris theory(strip). The critical current of HTS cable(1, 19-filament) in LN$_2$was 116[A], 240[A] and degradation coefficient(k) was 0.71, 0.73 respectively. In case of 19-filament cable critical current was decreased because of mechanical strain at pitch. And AC loss of HTS cable(19-filament) was 0.7 [W/m] in 240[A] loading

  • PDF

열처리에 따른 BSCCO 용사피막의 초전도특성 (Superconductor characteristics of BSCCO spray films by Heat treatment)

  • 도형준;박경채
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2007년 추계학술발표대회 개요집
    • /
    • pp.282-284
    • /
    • 2007
  • The superconductor characteristics of BSCCO spray films by Heat treatment was studied. $Bi_2Sr_2CaCu_2O_x$(Bi-2212) is high-Tc superconductor(HTS) coatings have been prepared by Heat treatment. Where high current carrying capabilities are required and therefore thick film and bulk material are called for, the Bi2Sr2Ca1Cu2O8-d(Bi-2212)compound has evoleved as one of the most promising. and the Bi-2212 HTS coating layer is synthesized through the peritectic reaction between Sr-Ca-Cu oxide coating layer and Bi-Cu oxide coating layer by partial melting process. The superconducting characteristics depends on the spray distance which was related to the spray particle melt. The Bi-2212 HTS layer consists of the whisker growth and secondary phase in 2212 layer were observed.

  • PDF

액체질소로 냉각된 Bi-2223 선재의 퀜치 전파 특성에 관한 연구 (A Study on the Quench Propagation Properties of Bi-2223 Wire cooled in Liquid Nitrogen)

  • 윤경용;배덕권;안민철;강형구;이찬주;윤용수;이상진;고태국
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제7권1호
    • /
    • pp.32-36
    • /
    • 2005
  • With the successful commercialization of Bi-2223 powder-in-tube wire , various attempts in the R & D of the high-Tc superconducting (HTS) magnets for high magnetic field applications are being implemented actively. Operating temperature of HTS magnet has to be maintained at the designed level but the magnetic energy and mechanical disturbance can cause unstable operational temperature of HTS magnet. Especially the generated heat energy of inner HTS winding Is apt to be accumulated . so the normal region appears in HTS winding. This paper deals with the quenching characteristics of three kinds of selected Bi-2223 wires : the High Current Density Wire (HC-A) and the High Strength Wire (HS-A) made by AMSC and HTS wire(HW-I) made by Innost The Innost wire has the highest minimum quench energy (MQE). The High Current Density Wire has the highest normal zone Propagation velocity (NZPV).

Bi-2223/Ag 고온초전도선재의 가공균일성에 미치는 인발공정연구 I (Bi-2223/Ag HTS Drawing Process Study for Uniform Deformation I)

  • 김상철;하홍수;오상수;이동훈;양주생;하동우;권영길;한일용;이종건
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 초전도 자성체
    • /
    • pp.55-58
    • /
    • 2002
  • PIT method which is used at fabricating Bi-2223/Ag HTS wire includes a drawing process, conventional deformation method. Drawing of meta1(Ag) and ceramic (BiSrCaCuO) composite is also difficult and significant for uniform deformation. In this paper, parameters of uniform deformation was studied at Bi-2223/ Ag multifilamentary HTS wire. Powder and rod as a starting precursor was compared at 55 filament and 54 filament Bi-2223/Ag HTS wire, respectively. Micro-hardness and area COV of the filaments was also evaluated when the diameters were decreased through drawing operations.

  • PDF

플라즈마 용사 및 열처리 공정을 통한 Bi-2212/2223 초전도체 thick film 제조의 기술 개발 (Technique development of Bi-2212/2223 superconductor thick film manufacturing by plasma spraying and heat treatment)

  • Lee, Seon-Hong;Cho, Sang-Hum;Ko, Young-Bong;Park, Kyeung-Chae
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.262-264
    • /
    • 2005
  • $Bi_{2}Sr_{2}CaCu_{2}O_{x}$(Bi-2212) and $Bi_{2}Sr_{2}Ca_{2}Cu_{3}O_{y}$(Bi-2223) high-$T_{c}$ superconductor(HTS) coating have been prepared by plasma spraying and heaat treatment. The Bi-2212 HTS coating later is synthesized through the peritectic reaction between Sr-Ca-Cu oxide coating layer and Bi-Cu oxide coating later, and $Bi_{2}Sr_{2}CaCu_{2}O_{y}$(Bi-2212) superconducting phase grow by partial melting process. The superconducting characteristic depends strongly on the conditions of the partial melting process. the Bi-2212 HTS layer consists of the whiskers grown in the diffusion direction. Above the 2212 layer, Bi-2223 phase and secondary phase was observed. The secondary phase is distributed uniformly over the whole surface. This is caused to the microcrack on the coatings surface. Despite everything, the film shows superconducting with an onset $T_{c}$ of about 115K. There are two changes steps. One changes (1step) at 115K is due to the diamagnetism of the Bi-2223 phase and the other changes (2step) at 78K is due to the diamagnetism of the Bi-2212 phase.

  • PDF

열처리 조건에 따른 Bi-2212 초전도 튜브의 특성 (Characteristics of Bi-2212 Superconductor Tube Depending on Heat-treatment Conditions)

  • 박용민;장건익
    • 한국전기전자재료학회논문지
    • /
    • 제14권7호
    • /
    • pp.606-610
    • /
    • 2001
  • Bi-2212 HTS tube was fabricated by centrifugal forming and partial melting processes. Bi-2212 bulk tube has been optimized to achieve smooth surface and uniform thickness. The slurry was prepared in the mixing ratio of 10:1 between Bi-2212 powder and binder and initially charged into the rotating mold under the speed of 300~450 rpm. Heat-treatment was performed at the temperature ranges of 860~89$0^{\circ}C$ in air for partial melting. the HTS tube fabricated by centrifugal forming process at 89$0^{\circ}C$ under the rotating speed of 450 rpm was highly densified and the plate-like grains with more than 20${\mu}{\textrm}{m}$ were well oriented along the rotating axis. The measured Tc and J$_{c}$ at 10K on specimen heat treated at 89$0^{\circ}C$ was around 85 K and 1,200 A/$\textrm{cm}^2$ respectively.y.

  • PDF

Bi-2223/Ag 고온초전도 선재의 기계적 특성 평가 (Evaluation of mechanical properties of Bi-2223/Ag HTS tapes)

  • 하홍수;이동훈;양주생;최정규;윤진국;하동우;오상수;권영길;김상철
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제4권1호
    • /
    • pp.45-59
    • /
    • 2002
  • Evaluation of the mechanical properties of Bi-2223/Ag HTS tapes was carried out by the tension and bending tests. Most of the Bi-2223/Ag tapes retained critical current up to 10 kgf/mm$_2$ axial tension stress, and 0.2% tension strain at room temperature. Applied tension strain exceeding 0.3% in superconducting tapes at 77 K leaded to rapid degradation of the critical current. It was observed that the more filaments, the better axial tension property at 77 K, self-field The influence of bending strain on critical current degradation was revealed to be less sensitive for Bi-2223/Ag HTS tapes with a more number of filaments and higher silver ratio.

조성이 다른 전구체 분말에 따른 Bi-2223/Ag 초전도 테이프의 특성 변화 (Properties of Bi-2223/Ag HTS tapes using different content of precursors)

  • 하동우;양주생;하홍수;오상수;황선역;이동훈;최정규;이언용;권영길
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 춘계학술대회 논문집 초전도 자성체 연구회
    • /
    • pp.69-72
    • /
    • 2003
  • Bi-2223 superconducting wires were fabricated by stacking, drawing process with different precursor powders and different heat-treatment histories. The precursor powders were 2 kinds of Pb content. And a part of the tapes were experienced pre-annealing process which caused tetragonal structure of Bi-2212 phase to orthorhombic structure of it was during drawing process. We confirmed the transformation of Bi-2212 phase from tetragonal structure to orthorhombic structure and reduction of second phases. XRD and DC magnetization analysis were performed in order to investigate the fraction of Bi-2223 phase in Bi-2223/Ag HTS tape. We could achieve best Ic of 70 A class at the Bi-2223/Ag tape using low Pb content of precursor powder and experienced pre-annealing process. DC magnetization analysis was useful to investigate the fraction of Bi-2223 phase in the Bi-2223/Ag tape.

  • PDF

Bi-2223 팬케익부하 충전용 히터-트리거 스위칭 장치의 설계 및 제작 (Design and Fabrication of Heater-triggered Switching System for the Charging of Bi-2223 Pancake Load)

  • 김영식;윤용수;배덕권;안민철;임대준;김호민;고태국
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제6권1호
    • /
    • pp.43-48
    • /
    • 2004
  • This paper deals with design and fabrication of heater-triggered switching system for the high-Tc superconducting (HTS) power supply with series-connected double-pancake load. Amongst all components, heater triggering is the most important element for the performance of HTS power supply. To fabricate the optimal heater-triggered system, its characteristics have been analysed through the simulation and expriment. The thermal analysis of switching parts of the Bi-2223 solenoid according to the heater input was carried out. Based upon the analysis, 8A electromagnet current and 1.5A DC Heater current were optimally derived, and 8s and 20s for the pumping period were selected in this experiment. In the experiment. the maximum pumping current reached about 24A with Bi-2223 pancake load of 6mH.