• Title/Summary/Keyword: Bending fatigue

Search Result 659, Processing Time 0.028 seconds

Structural Performance and Usability of Void Slab Established in T-deck Plate (T형 데크 플레이트 중공형 슬래브의 구조성능 및 사용성능)

  • Hong, Eun-Ae;Chung, Lan;Paik, In-Kwan;Yun, Sung-Ho;Cho, Seung-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.24 no.6
    • /
    • pp.677-684
    • /
    • 2012
  • In recent years, extension of life span of buildings is becoming an important issue in our society. To improve the life span of buildings, rhamen structure construction and long-spanned structures are advantageous. And in order to achieve this goal, structural elements of buildings must be light and slender. As an alternative method, general porous slabs are used frequently domestically and internationally. But the study on the porous slabs using T-deck plate and assembly of light weight precast construction is insufficient at present. In this study, flexural and fatigue tests were performed on six specimens to verify structural performance and serviceability. The main parameters of the specimens were light weight and T-deck plate construction possibility as well as slab thickness. The test results indicated that the strength of porous slabs using T-deck plate and assembly of light weight were much better than general RC slabs and porous slabs without T-deck plate. And stiffness was much better than that of other tested slabs.

Performance Evaluation of Stress Absorbing Membrane Interlayer Using Epoxy Asphalt Binder (에폭시 아스팔트 바인더를 이용한 응력흡수층의 성능평가)

  • Jo, Shin Haeng;Lee, Bong Lim;Kim, Nakseok
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.37 no.6
    • /
    • pp.1043-1051
    • /
    • 2017
  • Asphalt overlay on deteriorated concrete pavement has a problem of early damage due to reflective cracking. There is a need for a new method capable of reducing reflection cracking and ensuring the durability of pavement. The purpose of this study was to obtain durability of asphalt overlay with stress absorbing membrane interlayer (SAMI) using epoxy asphalt binder. The tensile performance, durability, water resistance and bonding performance of Epoxy-SAMI were evaluated by various tests. As a result of tests, Epoxy-SAMI meets the quality standard of the bridge waterproofing material. The repeated direct tensile test was carried out to investigate the effect of reflective cracking reduction. When the Epoxy-SAMI was applied, it had 1.2~1.56 times higher reflective cracking resistance than PSMA asphalt concrete with the thickness of 10cm even if the section thickness decreased. 4-point bending beam test results showed the number of fatigue failures increased 7.5 times when Epoxy-SAMI was applied. The Epoxy-SAMI was found to be effective in improving the durability of the asphalt pavement overlay because it serves to prevent reflective cracking, increase lifespan, and function as a waterproof layer.

Application of Prefabricated Retaining Walls with Steel Lagging (강재 요소를 적용한 조립식 흙막이 벽체에 관한 연구)

  • Hong, Jong woo;Choi, Jae Soon
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.35 no.6
    • /
    • pp.1277-1285
    • /
    • 2015
  • It has been known that the conventional retaining wall system with timber lagging and H pile has several problems such as the irregular gap between H-piles, cutting or adding to standard timber, back fill over first step excavation, and especially break-down accident at the disjoint of wall system. In the practical excavation, these problems may lead to worker's accident and the inefficiency of construction economy. To solve the above problems, a new method using prefabricated retaining wall was proposed and verified. The characteristics of the new method is to replace timber wall as free-sliding steel-lagging and connector. To check its verification and application, laboratory tests such as bending strength, tensile strength, and fatigue strength were carried out. Also, a pilot test in the field and numerical simulations under various ground conditions were performed. From the researches, it is found that the prefabricated retaining wall plate can be superior to the conventional timber lagging plate in the strength. It is also found that the proposed methods can be effective in the reuse of retaining wall plate and safe in the disjoint of wall system. Finally, it is desired that the proposed method will be effective in the reduction of the imported timbers and helpful in the safety of retaining wall construction.

Study on the Nonlinear Electromagnetic Acoustic Resonance Method for the Evaluation of Hidden Damage in a Metallic Material (금속 재료의 잠닉손상 평가를 위한 비선형 전자기음향공진 기법에 관한 연구)

  • Cho, Seung-Wan;Cho, Seung-Hyun;Park, Choon-Su;Seo, Dae-Cheol;Jhang, Kyung-Young
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.34 no.4
    • /
    • pp.277-282
    • /
    • 2014
  • Recently, much attention has been paid to nonlinear ultrasonic technology as a potential tool to assess hidden damages that cannot be detected by conventional ultrasonic testing. One nonlinear ultrasonic technique is measurement of the resonance frequency shift, which is based on the hysteresis of the material elasticity. Sophisticated measurement of resonance frequency is required, because the change in resonance frequency is usually quite small. In this investigation, the nonlinear electromagnetic acoustic resonance (NEMAR) method was employed. The NEMAR method uses noncontact electromagnetic acoustic transducers (EMATs) in order to minimize the effect of the transducer on the frequency response of the object. Aluminum plate specimens that underwent three point bending fatigue were tested with a shear wave EMAT. The hysteretic nonlinear parameter ${\alpha}$, a key indicator of damage, was calculated from the resonance frequency shift at several levels of input voltage. The hysteretic nonlinear parameter of a damaged sample was compared to that of an intact one, showing a difference in the values.

Lateral-Torsional Buckling Strength of I-girder with Corrugated Steel Webs under Linear Moment Gradient (선형 모멘트 구배가 작용하는 파형강판 I-거더의횡-비틂 좌굴 강도)

  • Moon, Jiho;Lim, Nam-Hyoung;Lee, Hak-Eun
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.32 no.3A
    • /
    • pp.149-160
    • /
    • 2012
  • Corrugated steel plates have several advantages such as high resistance for shear without stiffeners, minimization of welding process, and high fatigue resistance. To take advantage of these benefits, several researchers have attempted to use corrugated steel plate as a web of I-girders. The lateral-torsional buckling is the major design aspect of such I-girders. However, lateral-torsional buckling of the I-girder with corrugated steel webs still needs to be investigated especially for a real loading condition such as non-uniform bending. This paper investigated the lateral-torsional buckling strength of the I-girder with corrugated steel webs under linear moment gradient by using finite element analysis. From the results, it was found that the buckling behavior of the I-girder with corrugated steel webs differed depending on the number of periods of the corrugation. Also, a simple equation for the moment gradient correction factor of the I-girder with corrugated steel webs was suggested. The inelastic lateral-torsional buckling strength of the I-girder with corrugated steel webs was then discussed based on current design equations for ordinary I-girders and the results of finite element analysis.

Pin Pull Characteristics of Pin Lead with Variation of Mechanical Properties of Pin Lead in PGA (Pin Grid Array) Package (PGA (Pin Grid Array) 패키지의 Lead Pin의 기계적 특성에 따른 Pin Pull 거동 특성 해석)

  • Cho, Seung-Hyun;Choi, Jin-Won;Park, Gyun-Myoung
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.17 no.1
    • /
    • pp.9-17
    • /
    • 2010
  • In this study, von Mises stress and total strain energy density characteristics of lead pin in PGA (Pin Grid Array) packages have been calculated by using the FEM (Finite Element Method). FEM computation is carried out with various heat treatment conditions of lead pin material under $20^{\circ}$ bending and 50 mm tension condition. Results show that von Mises stress locally concentrated on lead pin corners and interface between lead pin head and solder. von Mises stress and total strain energy density decrease as heat treatment temperature of lead pin increases. Also, round shaped corner of lead pin decreases both von Mises stress and total strain energy density on interface between lead pin head and solder. This means that PGA package reliability can be improved by changing the mechanical property of lead pin through heat treatment. This has been known that solder fatigue life decreases as total strain energy density of solder increases. Therefore, it is recommended that both optimized lead pin shape and optimized material property with high lead pin heat treatment temperature determine better PGA package reliability.

Experimental Analysis of Large Size Concrete-Filled Glass Fiber Reinforced Composite Piles Subjected to the Flexural Compression (대구경 콘크리트 충전 복합소재 파일의 휨-압축 거동에 대한 실험적 분석)

  • Lee, Sung Woo;Choi, Sokhwan
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.29 no.5A
    • /
    • pp.519-529
    • /
    • 2009
  • Fiber reinforced composite materials have various advantages in mechanical and chemical aspects. Not only high fatigue and chemical resistance, but also high specific strength and stiffness are attained, and therefore, damping characteristics are beneficial to marine piles. Since piles used for marine structures are subjected to compression and bending as well, detailed research is necessary. Current study examine the mechanical behavior under flexural and/or compressive loads using concrete filled fiber reinforced plastic composite piles, which include large size diameter. 25 pile specimens which have various size of diameters and lengths were fabricated using hand lay-up or filament winding method to see the effect of fabrication method. The inner diameters of test specimens ranged from 165 mm to 600 mm, and the lengths of test specimens ranged from 1,350 mm to 8,000 mm. The strengths of the fill-in concrete were 27 and 40 MPa. Fiber volumes used in circumferential and axial directions are varied in order to see the difference. For some tubes, spiral inner grooves were fabricated to reduce shear deformation between concrete and tube. It was observed that the piles made using filament winding method showed higher flexural stiffness than those made using hand lay-up. The flexural stiffness of piles decreases from the early loading stage, and this phenomenon does not disappear even when the inner spiral grooves were introduced. It means that the relative shear deformation between the concrete and tube wasn't able to be removed.

PHYSICAL PROPERTIES AND SURFACE TOPOGRAPHY OF ORTHODONTIC STAINLESS STEEL WIRES : COMPARING A NEW KOREAN PRODUCT WITH OTHERS FROM FOREIGN COMPANIES (여러 스테인레스 스틸 호선의 물성 및 표면의 비교)

  • Lee, Sung-Ho;Kim, Tae-Woo;Chang, Young-Il
    • The korean journal of orthodontics
    • /
    • v.31 no.1 s.84
    • /
    • pp.149-157
    • /
    • 2001
  • The purpose of this study was to investigate the property of a new Korean stainless steel wire(Jinsung Ind.) comparing with other foreign Products. Five types of stainless steel wires (Standard, Resilient, HI-T of Unitek, Stainless steel of Ormco and Jinsung Ind.) in 0.016x0.022 and 0.019x0.02 were tested to observe for Composition analysis, size difference, tensile properties, flexure bending property, tortion property, surface hardness and surface topography by means of SEM. The findings suggest that: 1. In maximum tensile strength of tensile properties, Unitek Hi-T showed the greatest value, followed by Unitek Resilient, Jinsung Stainless Steel, Ormco Stainless Steel, Unitek Standard in 0.016x0.022, and Unitek Hi-T showed highest value, followed by Jinsung Stainless Steel, Ormco Stainless Steel, Unitek Resilient, Unitek Standard in 0.019x 0.025. 2. In elongation rate, Unitek Standard showed the greatest value, fellowed by Ormco Stainless Steel, Unitek Hi-T, Unitek Resilient, Jinsung Stainless Steel in 0.016x0.022, and Unitek Hi-T showed the highest value, followed by Unitek Standard, Ormco Stainless Steel, Jinsung Stainless Steel, Unitek Resilient in 0.019x0.025. 3. In modulus of elasticity, Jinsung Stainless Steel showed the greatest value, followed by Unitek Hi-T, Unitek Resilient, Ormco Stainless Steel, Unitek Standard in 0.016x0.022, and Unitek Resilient showed the highest value followed by Jinsung Stainless Steel, Ormco Stainless Steel, Unitek Hi-T, Unitek Standard in 0.019x0.025. 4. In bending fatigue test, Jinsung Stainless Steel showed the greatest fracture resistance, followed by Unitek Hi-T, Unitek Standard, Unitek Resilient, Ormco Stainless Steel in 0.016x0.022, and Unitek Hi-T showed the greatest fracture resistance followed by Jinsung Stainless Steel, Unitek Resilient, Unitek Standard, Ormco Stainless Steel in 0.019x0.025. 5. In twist test, Unitek Resilient showed the greatest fracture resistance, followed by Jinsung Stainless Steel, Unitek Hi-7, Ormco Stainless Steel, Unitek Standard in 0.016x0.022, and Jinsung showed the greatest fracture resistance, followed by Unitek Resilient, Unitek Standard, Ormco Stainless Steel, Unitek Hi-T. 6. In surface topography, every products showed indentation and pitting. Jinsung stainless steel wire showed long thin indentation and relatively smooth surface. Unitek wires showed indentation and pitting and Ormco wire showed a lot of irregular pittings.

  • PDF

Numerical Examinations of Damage Process on the Chuteway Slabs of Spillway under Various Flow Conditions (여수로 방류에 따른 여수로 바닥슬래브의 손상 발생원인 수치모의 검토)

  • Yoo, Hyung Ju;Shin, Dong-Hoon;Kim, Dong Hyun;Lee, Seung Oh
    • Journal of Korean Society of Disaster and Security
    • /
    • v.14 no.4
    • /
    • pp.47-60
    • /
    • 2021
  • Recently, as the occurrence frequency of sudden floods due to climate variability increased, the damage of aging chuteway slabs of spillway are on the rise. Accordingly, a wide array of field survey, hydraulic experiment and numerical simulation have been conducted to find the cause of damage on chuteway slabs. However, these studies generally reviewed the flow characteristics and distribution of pressure on chuteway slabs. Therefore the derivation of damage on chuteway slabs was relatively insufficient in the literature. In this study, the cavitation erosion and hydraulic jacking were assumed to be the causes of damage on chuteway slabs, and the phenomena were reproduced using 3D numerical models, FLOW-3D and COMSOL Multiphysics. In addition, the cavitation index was calculated and the von Mises stress by uplift pressure distribution was compared with tensile and bending strength of concrete to evaluate the possibility of cavitation erosion and hydraulic jacking. As a result of numerical simulation on cavitation erosion and hydraulic jacking under various flow conditions with complete opening gate, the cavitation index in the downstream of spillway was less than 0.3, and the von Mises stress on concrete was 4.6 to 5.0 MPa. When von Mises stress was compared with tensile and bending strength of concrete, the fatigue failure caused by continuous pressure fluctuation occurred on chuteway slabs. Therefore, the cavitation erosion and hydraulic jacking caused by high speed flow were one of the main causes of damage to the chuteway slabs in spillway. However, this study has limitations in that the various shape conditions of damage(cavity and crack) and flow conditions were not considered and Fluid-Structure Interaction (FSI) was not simulated. If these limitations are supplemented and reviewed, it is expected to derive more efficient utilization of the maintenance plan on spillway in the future.