Development of Palladium, Gold and Gold-Palladium Containing Metal-Carbon Nanoreactors: Hydrogen Adsorption

  • Mayani, Vishal J.;Mayani, Suranjana V.;Kim, Sang Wook
    • Bulletin of the Korean Chemical Society
    • /
    • 제35권5호
    • /
    • pp.1312-1316
    • /
    • 2014
  • Metal-carbon nanoreactors (MCNRs) were prepared from a pristine carbon cage (CC) using a simple and efficient template method with nano silica ball (NSB), pyrolysis fuel oil (PFO) and transition metals, such as palladium and gold. Metal nanoparticles were embedded in approximately 25 and 170 nm sized, highly ordered carbon cages. The newly developed Pd, Au and Au-Pd doped carbon nanoreactors were characterized by microanalysis, $N_2$ adsorption-desorption isotherm, powder X-ray diffraction (XRD), thermo-gravimetric analysis (TGA), scanning electron microscopy coupled with energy dispersive spectroscopy (SEM-EDS), transmission electron microscopy and inductively coupled plasma (ICP) analysis. The ordered MCNRs have exhibited dynamic hydrogen adsorption capability compared to the carbon cage.

The Synthesis of Diamond Thin Films by MPECVD Using Organic Compounds (유기 화합물을 이용한 MPECVD에 의한 다이아몬드 박막 합성)

  • Ku, Ja-Chun;Oh, Jeong-Seob;Whang, Ki-Woong
    • Proceedings of the KIEE Conference
    • /
    • 대한전기학회 1990년도 추계학술대회 논문집 학회본부
    • /
    • pp.97-100
    • /
    • 1990
  • Diamond thin films were synthesized by the MPECVD (Microwave Enhanced Chemical Deposition) using the mixture of the hydrogen and organic compounds($CH_3COCH_3$, $CH_3OH$). In X-ray Diffraction, the d values of all the deposits on the Si substrates with the experimental conditions coincide with those of natural diamond in POD (Powder Diffraction Data). The changes of the morphology of all the deposits were examined by SEM. The amount of amorphous carbon or graphite in the diamond films were increased as the acetone concentration was increased. The morphology of the diamond particles can be changed from ball-like to euhedral by adding the small amount of the methanol in the reaction gases of the high acetone concentration.

  • PDF

Properties of ITO Sol as a function of Concentration (ITO Sol의 농도에 따른 특성평가)

  • Kang, Ho-Min;Sin, Sang-Hyun;Kim, Kyung-Wu;Park, Ki-Woon;Kang, Dong-Heon;Kim, Young-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.988-991
    • /
    • 2002
  • ITO (Indium Tin Oxide) powder was synthesized by precipitation method. ITO colloidal solutions for coating on glass were fabricated by ball milling method. ITO colloidal solution with variation of concentration from 2% to 15% were fabricated ITO thin film measured sheet resistance and transmittance. In the result, 15% sol showed the lowest value of sheet resistance, 2% sol showed the highest value of transmittance. In addition, effect of annealing temperature and $SiO_2$ film were investigated.

  • PDF

High Temperature Friction Characteristic of $Al-SiC_{p}$ Composite Coating Prepared by Plasma Thermal Spray (플라즈마 용사에 의해 제조한 $Al-SiC_{p}$ 복합재료 코팅층의 고온마찰특성)

  • 민준원;유승을;서동수
    • Tribology and Lubricants
    • /
    • 제19권5호
    • /
    • pp.274-279
    • /
    • 2003
  • $Al-SiC_{p}$ composite layer was prepared by plasma thermal spray on aluminum substrate. The homogeneously dispersed composite powder for thermal spray was fabricated by mechanical alloying with ball mill. The friction tests of the composite layers and commercial aluminum alloys for comparison were performed in the temperature range of 20∼$260^{\circ}C$ with the interval of $40^{\circ}C$ with steel counter-face. Friction coefficient was recorded during test sequence, and the microstructure of surface and debris was investigated by optical and scanning electron microscope. Friction coefficients of composite and aluminum alloys at room temperature were similar except pure aluminum. As the temperature increase, friction coefficient was increased rapidly in AC4C, AC2A. But friction coefficient of $Al-SiC_{p}$ composite was not increased so much up to $220^{\circ}C$. Consequently, the reinforcement of $SiC_{p}$ into aluminum matrix increased the stability of friction coefficient as well as wear resistance.

Studies of the Mullite-Cordierite Composites as a Substrate Material (기판재료로서의 물라이트-코디어라이트 복합재료에 관한 특성)

  • 김경용;김윤호;정형진;김석수;김병호
    • Journal of the Korean Ceramic Society
    • /
    • 제27권3호
    • /
    • pp.394-400
    • /
    • 1990
  • Mullite and cordierite were prepared by the sol-gel route. Boehmite, fumed silica and Mg(NO3)2$.$6H2O were their starting materials. Mullite and cordierite powder were mixed by various weight percent. These mixed sols were ball-milled for 48hrs, dried at 100$^{\circ}C$, pressed, cold isostatic pressed and sintered at 1490$^{\circ}C$ for 2hrs. Mullite-cordierite composites sintered at 1490$^{\circ}C$ for 2hrs had>98% of theoretical density. Bending strength of the sintered bodies were 329-249MPa, dielectric constant 7.1-6.7 at 1MHz and thermal expansion coefficient at 800$^{\circ}C$ was matched with Si in the range of 30-35wt% cordierite.

  • PDF

Enhanced Electron Emission from Carbon Nanotube Paste after Firing

  • Kang, Sung-Kee;Choi, Jong-Hyung;Han, Jae-Hee;Yoo, Ji-Beom;Park, Chong-Yun;Nam, Joong-Woo;Jung, J.E.;Kim, J.M.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2003년도 International Meeting on Information Display
    • /
    • pp.849-851
    • /
    • 2003
  • After multi-walled carbon nanotubes (MWNT) powder was crushed with ball milling process, it was mixed with organic vehicles. And then CNT paste was printed on ITO coated glass substrate. The field emission characteristics of CNT pastes fired in air atmosphere was better than that of CNT paste fired in Ar ambient due to less organic residues after firing.

  • PDF

Fabrication and characterization of graphite nanofiber reinforced aluminum matrix composites (탄소나노섬유 강화 알루미늄 복합재료의 제조 및 특성)

  • Jang J.H.;Oh K.H.;Han K.S.
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 한국복합재료학회 2004년도 추계학술발표대회 논문집
    • /
    • pp.35-38
    • /
    • 2004
  • Graphite nanofiber (GNF) and carbon nanotube (CNT) are novel fiber reinforcing materials which have outstanding physical and mechanical properties. Aluminum matrix composites reinforced graphite nanofiber were fabricated by conventional powder metallurgy (PM) method. The composites were prepared through ultrasonication, ball milling, and hot isostatic pressing. A uniform distribution of GNF in aluminum matrix could be obtained. To measure the mechanical properties of GNF-Al composites testings were done in indentation and compression. The compressive strength was enhanced according to reinforcing graphite nanofiber while the hardness was decreased. This study makes the high performance composites for future applications.

  • PDF

Preparation and Piezoelectrical Properties of PMN-PZT Ceramics Prepared by High-Energy Ball Milling (고에너지볼밀법을 이용한 PMN-PZT 세라믹스의 제조와 압전특성)

  • Myoung, Seong-Jae;Koo, Bon-Keup
    • Journal of the Korean Ceramic Society
    • /
    • 제42권10호
    • /
    • pp.685-690
    • /
    • 2005
  • Pb(Zr,Ti)$O_{3}$Pb($Mn_{1/3}$$Nb_{2/3}$)$O_{3}$ powder was successfully synthesised by high-energy milling method, and the behavior of low­temperature sintering and piezoelectrical properties of Pb(Zr,Ti)$O_{3}$-Pb($Mn_{1/3}$$Nb_{2/3}$)$O_{3}$ ceramics were investigated as a function of mechanical alloying time. In order to confirm whether the Perovskite phase in this composition was formed by mechanical activation technique or not, we performed X-Ray Diffraction pattern analysis (XRD). The microstructure for the sintered samples were characterized using a Scanning Electronic Microscope (SEM). And the piezoelectrical properties ($k_{p}$ and $Q_{m}$) of the sintered samples was measured using HP 4194A impedance analyzer.

Properties of Wollastonite-Reinforced Glass-Ceramics Made from Waste Automobile Glass and Waste Shell

  • Yun, Yeon-Hum;Yoon, Chung-Han;Kim, Chi-Kyun;Hwang, Kyu-Seog
    • Resources Recycling
    • /
    • 제13권1호
    • /
    • pp.54-58
    • /
    • 2004
  • Wollastonite-type glass ceramics were prepared by milling and firing at various temperatures using an automobile waste glass and waste shell as starting materials. Powder mixture ground by disk-type ball mill for 3 hours was pressed into a disk. The pressed specimen was fired at $850^{\circ}C$,$950^{\circ}C$ and $1050^{\circ}C$ for 1 hour in air. From FE-SEM observation, with an increase of the firing temperature from $850^{\circ}C$ to $1050^{\circ}C$, whisker-type phase was grown to about 10 $\mu\textrm{m}$ in length. Specimen fired at $1050^{\circ}C$ showed the formation of well-crystallized whisker-type wollastonite grains and the highest compressive strength.

Fabrication and Characterization of BSCCO System High-Temperature Superconductor Tube Using Centrifigal Forming Process (원심성형법을 이용한 BSCCO계 고온초전도튜브 제조 및 특성 분석)

  • 박용민;장건익
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • 제13권9호
    • /
    • pp.801-804
    • /
    • 2000
  • High-temperature superconductor of Bi-2212 system was fabricated by CFP(Centrifugal Forming Process). To make a uniform specimen slurry was prepared in the ratio of 7:3(powder : binder) and ball milled for 24 hours. Milled slurry was charged into a rotating mold with 450 rpm and dried at room temperature. Then the specimen was performed binder burn-out at 35$0^{\circ}C$ and heated for partial melting to 86$0^{\circ}C$. XRD analysis of most specimens were shown 2212 phase and observed a local plate shped microstructure with a well aligned c-axis direction from SEM images. Measured T$_{c}$(Critical temperature) was about 64 K.K.