BZCT 세라믹의 마이크로파 특성에 관한 연구 (Microwave Dielectric Properties of BZCT Ceramics)

  • 이문기;최의선;류기원;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제15권10호
    • /
    • pp.870-875
    • /
    • 2002
  • Ba(Zn$_1$-xCox)TaO$_3$[BZCT] ceramics were Prepared by the conventional mixed oxide method. The ceramics were sintered at the temperature of 1450∼1550$\^{C}$ for 5 hr in air. The crystal structure of BZCT ceramics was investigated by the XRD. The microstructure of the specimens were observed by SEM. The structural properties of BZCT specimens were investigated as a function of composition and sintering temperature. All BZCT ceramics sintered over 1550$\^{C}$ were showed a polycrystalline complek perovskite structure without second phases and any unreacted materials. The density of BZCT (70/30) specimen sintered at 1550$\^{C}$ was 6.31g/㎤. In the case of the BZCT(70/30) ceramics sintered at 1550$\^{C}$ for 5 hours, dielectric constant, qualify factor and temperature coefficient of resonant frequency for microwave dielectrics application were a good value of 29, 16,468 at 10㎓ and -4.4 ppm/$\^{C}$, respectively.

소결온도에 따른 BZCT 세라믹스의 구조적 특성 (Structural Properties of BZCT Ceramics with Sintering Temperature)

  • 김지헌;이문기;정장호;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.115-117
    • /
    • 2001
  • $Ba(Zn_{1-x}Co_x)TaO_3$[BZCT] ceramics were prepared by the conventional mixed oxide method. The ceramics were sintered at the temperature of $1450{\sim}1550^{\circ}C$ for 5hr. in air. The structural properties of the BZCT ceramics as a function of composition and sintering temperature were investigated by the XRD and SEM. The crystal structure of BZCT ceramics was investigated by the XRD. The microstructure of the specimens were observed by SEM. All the BZCT ceramics sintered above the $1550^{\circ}C$ were showed as a polycrystalline complex perovskite structure without second phases and any unreacted materials. The density of BZCT (70/30) specimen sintered at $1550^{\circ}C$ was $6.31g/cm^3$.

  • PDF

$Ba(Zn_{0.8}Co_{0.2})_{1/3}Ta_{2/3}O_3$ 세라믹스의 구조적 특성 (Structural Properties of $Ba(Zn_{0.8}Co_{0.2})_{1/3}Ta_{2/3}O_3$ Ceramics)

  • 김지헌;임성수;이성갑;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 일렉트렛트 및 응용기술
    • /
    • pp.88-92
    • /
    • 2002
  • $Ba(Zn_{0.8}Co_{0.2})_{1/3}Ta_{2/3}O_3$ [BZCT(80/20)] ceramics were prepared by the conventional mixed oxide method. The ceramics were sintered at the temperature of $1450{\sim}1550^{\circ}C$ for 5hr. in air. The structural properties of BZCT(80/20) ceramics were investigated as a function of sintering temperature. The BZCT(80/20) ceramics sintered at $1550^{\circ}C$ showed a polycrystalline complex perovskite structure without second phases and any unreacted materials. Increasing the sintering temperature, the bulk density and ordering were increased. The bulk density of the BZCT(80/20) ceramics sintered at $1550^{\circ}C$ was 7.50[$g/cm^2$]. Increasing the sintering temperature, the average grain size were increased and pore were decreased.