• 제목/요약/키워드: BSCCO 2212

검색결과 86건 처리시간 0.027초

에피택시 성장으로 제작한 BSCCO 박막의 단결정 형성 (Single Crystal Formation of BSCCO Thin Films by Epitaxy Growth)

  • 천민우;양승호;박용필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 추계학술대회 논문집 Vol.17
    • /
    • pp.671-674
    • /
    • 2004
  • BSCCO thin films have been fabricated by epitaxy growth at an ultra-low growth rate. The growth rates of the films was set in the region from 0.17 to 0.27 nm/min. MgO(100) was used as a substrate. In order to appreciate stable existing region of Bi 2212 phase with temperature and ozone pressure, the substrate temperature was varied between 655 and 820 $^{\circ}C$ and the highly condensed ozone gas pressure(PO3) in vacuum chamber was varied between $2.0{\times}10^{-6}$ and $2.3{\times}10^{-5}$ Torr. Bi 2212 phase appeared in the temperature range of 750 and 795 $^{\circ}C$ and single phase of Bi 2201 existed in the lower region than $785\;^{\circ}C$. Whereas, $PO_3$ dependance on structural formation was scarcely observed regardless of the pressure variation. And high quality of c-axis oriented Bi 2212 thin film with $T_c$(onset) of about 90 K and $T_c$(zero) of about 45 K is obtained. Only a small amount of CuO in some films was observed as impurity, and no impurity phase such as $CaCuO_2$ was observed in all of the obtained films.

  • PDF

12 kVA급 BSCCO 한류소자 제작 및 특성 실험 (Fabrication and fault test of 12 kVA class BSCCO SFCL element)

  • 오성용;임성우;김혜림;현옥배;장건익
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제10권1호
    • /
    • pp.24-27
    • /
    • 2008
  • For the development of superconducting fault current limiters(SFCLs) having large current capacity, we fabricated an SFCL element that consists of Bi-2212 superconductor and Cu-Ni alloy tubes. First, Ag was plated on the surface of the Bi-2212 for the enhancement of soldering process. On the Ag-plated Bi-2212 tube, a Cu-Ni alloy tube was soldered using optimized solders and soldering conditions. The BSCCO/Cu-Ni composite was processed mechanically to have a helical shape for the improvement of the SFCL characteristics. The total current path of the SFCL element was 1330 mm long with 12 turns, and had critical current of 340 A at 77 K. Finally, we carried out the fault test using the fabricated SFCL element. It showed successful current limiting performance under the fault condition of 50 $V_{rms}$ and 5.5 kA. From the results, the rated voltage of the SFCL element was decided to be 0.4 V/cm, and the power capacity was 12 kVA at 77 K. The fabrication process of the SFCL and the fault test results will be presented.

IBS법으로 제작한 BSCCO 박막의 상안정 영역 (BSCCO Thin Films Fabricated by ion Beam Sputtering Method)

  • 양승호;양동복;박용필
    • 한국정보통신학회:학술대회논문집
    • /
    • 한국해양정보통신학회 2003년도 춘계종합학술대회
    • /
    • pp.538-541
    • /
    • 2003
  • BSCCO superconducting thin films have been fabricated by co-deposition using IBS(Ion Beam Sputtering) method. Despite setting the composition of thin film Bi2212 or Bi2223, in both cases, Bi2201, Bi2212 and Bi2223 phase were appeared. It was confirmed the obtained field of stabilizing phase was represented in the diagonal direction of the right below end in the Arrhenius plot of temperature of the substrate and PO$_3$, and it was distributed in the rezone. The XRD peak of the generated film continuously changed according to the substrate temperature.

  • PDF

변형된 two powder 제조 공정법에 의한 BSCCO 2223 제조 및 미세구조발달 (Fabrication and microstructural development of BSCCO-2223 by modified two powder process)

  • 고재웅;유재무;박명제;박성창;김해두;정형식
    • 한국초전도학회:학술대회논문집
    • /
    • 한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
    • /
    • pp.397-400
    • /
    • 1999
  • We have fabricated BSCCO 2223 by modified two powder process and investigated 2223 phase formation and grain growth. Phase evolution and reactivity of 2223 were remarkably sensitive to size of 2212 grains and liquid phase. Larger size of 2212 phase increased liquid formation temperature. The Avrami relation was well suited for describing the kinetics of grain growth in BSCCO 2223.

  • PDF

공증착법으로 제작한 BSCCO 초전도 박막의 부착계수 해석 (Analysis of Sticking Coefficient in BSCCO Superconductor Thin Film Fabricated by Co-deposition)

  • 안인순;천민우;박용필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.300-303
    • /
    • 2001
  • BSCCO thin films are fabricated via a co-deposition process by an ion beam sputtering with an ultra-low growth rate, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element exhibits a characteristic temperature dependence : almost a constant value of 0.49 below $730^{\circ}C$ and decreases linearly with temperature over $730^{\circ}C$. This temperature dependence can be elucidated from the evaporation and sublimation rates of bismuth oxide, $Bi_{2}O_{3}$, from the film surface. It is considered that the liquid phase of the bismuth oxide plays an important role in the Bi 2212 phase formation in the co-deposition process.

  • PDF

BSCCO 박막에서 단일상 형성을 위한 열역학 조건 (Thermodynamic Conditions for Formation of Single Phase in BSCCO Thin Films)

  • 이동규;박용필
    • 한국전기전자재료학회논문지
    • /
    • 제15권2호
    • /
    • pp.173-177
    • /
    • 2002
  • High quality BSCCO thin films have been fabricated by means of an ion beam sputtering at various substrate temperatures, T$\sub$sub/, and ozone gas pressures, pO$_3$. The correlation diagrams of the BSCCOphases with T$\sub$sub/ and pO$_3$ are established in the 2212 and 2223 phases come out as stable phases depending on T$\sub$sub/ and pO$_3$. From these results, the thermodynamic evaluation of ΔH and ΔS, which are related with Gibbs\` free energy change for single Bi2212 or Bi2223 phase, were performed.

공증착법으로 제작한 BSCCO 초전도 박막의 부착계수 해석 (Analysis of Sticking Coefficient in BSCCO Superconductor Thin Film Fabricated by Co-deposition)

  • 안인순;천민우;박용필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.300-303
    • /
    • 2001
  • BSCCO thin films are fabricated via a co-deposition process by an ion beam sputtering with an ultra-low growth rate, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element exhibits a characteristic temperature dependence : almost a constant value of 0.49 below 730$^{\circ}C$ and decreases linearly with temperature over 730$^{\circ}C$. This temperature dependence can be elucidated from the evaporation and sublimation rates of bismuth oxide, Bi$_2$O$_3$, from the film surface. It is considered that the liquid phase of the bismuth oxide plays an important role in the Bi 2212 phase formation in the co-deposition process.

  • PDF

단상막 형성을 위해 기판온도와 산화 가스압에 따른 Bi-2223 초전도 박막의 생성 영역에 관한 연구 (A Study on Produced Region of Bi-2223 Superconducting Thin Films versus substrate temperature and oxide gas pressures for formation of single-phase Film)

  • 양승호;박용필
    • 한국정보통신학회:학술대회논문집
    • /
    • 한국해양정보통신학회 2007년도 춘계종합학술대회
    • /
    • pp.536-539
    • /
    • 2007
  • BSCCO 박막은 다양한 기판온도와 산화 가스압에 변화에서 증발법에 의해 제작되었다. 박막조성을 Bi2212 또는 Bi2223으로 설정했음에도 불구하고, 어느 경우나 Bi2201, Bi2212 및 Bi2223상이 생성되었다. 이들 안정상의 생성 영역은 기판 온도-산화 가스압의 Arrhenius 플롯에서 우측 하단 방향으로 경사진 직선으로 표시되며 매우 좁은 영역에 분포되어 있다. 생성막의 XRD 피크는 기판 온도에 따라 연속적으로 변화했다. 이는 Bi2201, Bi2212, Bi2223의 각상이 결정 구조 내에 혼합되어 있는 혼합 결정계의 존재를 나타내고 있으며, 각 상의 단상막은 매우 좁은 온도, 가스압 범위에서만 생성되었다.

  • PDF

BSCCO-2212/$SrSO_4$ 벌크 초전도체의 제작 및 특성평가 (Fabrication and characterizations of the BSCCO-2212/$SrSO_4$ bulk superconductors)

  • 김규태;장석헌;박의철;황수민;주진호;홍계원;김찬중;김혜림;현옥배
    • Progress in Superconductivity
    • /
    • 제8권1호
    • /
    • pp.108-112
    • /
    • 2006
  • We fabricated Bi-2212/$SrSO_4$ bulk superconductors by the casting process and evaluated the effects of the powder mixing method and annealing temperature on the texture, microstructure, and critical current. In the process, the Bi-2212 powders were mixed with $SrSO_4$ by hand-mixing(HM) and planetary ball milling(PBM) method and then the powder mixtures were melted at $1100^{\circ}C{\sim}1200^{\circ}C$, solidified, and annealed. We observed that the rod made by the PBM had a more homogeneous microstructure and smaller $SrSO_4$ and second phases than that of the rod made by the HM, resulting in increased $I_c$. The $I_c$ of the rod also depended on the annealing temperature and the highest $I_c$ was obtained to be 200 A when prepared by HM at $1200^{\circ}C$ and annealed at $810^{\circ}C$ which is probably due to the moderate density and 2212 texture and the smaller and less second phase compared to that at higher temperature. The possible causes of the variations of $I_c$ with the powder mixing method and annealing temperature were related to the microstructural evolution based on the SEM, EPMA, and DTA analyses.

  • PDF