• Title/Summary/Keyword: Au sputtered

Search Result 21, Processing Time 0.021 seconds

Deposition Optimization and Bonding Strength of AuSn Solder Film (AuSn 솔더 박막의 스퍼터 증착 최적화와 접합강도에 관한 연구)

  • Kim, D.J.;Lee, T.Y.;Lee, H.K.;Kim, G.N.;Lee, J.W.
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.14 no.2 s.43
    • /
    • pp.49-57
    • /
    • 2007
  • Au-Sn solder alloy were deposited in multilayer and co-sputtered film by rf-magnetron sputter and the composition control and analysis were studied. For the alloy deposition condition, each components of Au or Sn were deposited separately. On the basis of pure Sn and Au deposition, the deposition condition for Au-Sn solder alloy were set up. As variables, the substrate temperature, the rf-power, and the thickness ratio were used for the optimum composition. For multilayer solder alloy, the roughness and the composition of solder alloy were controlled more accurately at the higher substrate temperature. In contrast, for co-sputtered solder, the substrate temperature influenced little to the composition, but the composition could be controlled easily by rf-power. In addition, the co-sputtered solder film mostly consisted of intermetallic compound, which formed during deposition. The compound were confirmed by XRD. Without flux during bonding of solder alloy film on leadframe, the adhesion strength were measured. The maximum shear stress was $330(N/mm^2)$ for multilayer solder with Au 10wt% and $460(N/mm^2)$ for co-sputtered solder with Au 5wt%.

  • PDF

Development of the Large-area Au/Pd Transfer-printing Process Applying Both the Anti-Adhesion and Adhesion Layers (접착방지막과 접착막을 동시에 적용한 대면적 Au/Pd 트랜스퍼 프린팅 공정 개발)

  • Cha, Nam-Goo
    • Korean Journal of Materials Research
    • /
    • v.19 no.8
    • /
    • pp.437-442
    • /
    • 2009
  • This paper describes an improved strategy for controlling the adhesion force using both the antiadhesion and adhesion layers for a successful large-area transfer process. An MPTMS (3-mercaptopropyltrimethoxysilane) monolayer as an adhesion layer for Au/Pd thin films was deposited on Si substrates by vapor self assembly monolayer (VSAM) method. Contact angle, surface energy, film thickness, friction force, and roughness were considered for finding the optimized conditions. The sputtered Au/Pd ($\sim$17 nm) layer on the PDMS stamp without the anti-adhesion layer showed poor transfer results due to the high adhesion between sputtered Au/Pd and PDMS. In order to reduce the adhesion between Au/Pd and PDMS, an anti-adhesion monolayer was coated on the PDMS stamp using FOTS (perfluorooctyltrichlorosilane) after $O_2$ plasma treatment. The transfer process with the anti-adhesion layer gave good transfer results over a large area (20 mm $\times$ 20 mm) without pattern loss or distortion. To investigate the applied pressure effect, the PDMS stamp was sandwiched after 90$^{\circ}$ rotation on the MPTMS-coated patterned Si substrate with 1-${\mu}m$ depth. The sputtered Au/Pd was transferred onto the contact area, making square metal patterns on the top of the patterned Si structures. Applying low pressure helped to remove voids and to make conformal contact; however, high pressure yielded irregular transfer results due to PDMS stamp deformation. One of key parameters to success of this transfer process is the controllability of the adhesion force between the stamp and the target substrate. This technique offers high reliability during the transfer process, which suggests a potential building method for future functional structures.

Effect of the Electrode Type on the Dielectric and Piezoelectric Properties of Piezoelectric PMN-PZT Single Crystals (압전 PMN-PZT 단결정의 유전 및 압전 특성에 미치는 전극 종류의 영향)

  • Lee, Jong-Yeb;Oh, Hyun-Taek;Choi, Kyoon;Lee, Ho-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.1
    • /
    • pp.77-82
    • /
    • 2015
  • The effect of the electrode type on the dielectric and piezoelectric properties of $Pb(Mg_{1/3}Nb_{2/3})O_3-PbZrO_3-PbTiO_3$ (PMN-PZT) single crystals was investigated in an effort to improve their properties for various piezoelectric applications. First, three different types of PMN-PZT single crystals [PMN-PZT-A (piezoelectrically soft type; dielectric constant ~ 10,000), PMN-PZT-B (piezoelectrically soft type; phase-transition temperature between the rhombohedral and tetragonal phases ($T_{RT}$) ~ $145^{\circ}C$), PMN-PZT-C (piezoelectrically hard type; high mechanical quality factor ($Q_m$) ~ 1,000)] were fabricated using the solid-state single crystal growth (SSCG) method. Then, four different types of electrodes [sputtered Au, sputtered Cr/Au, sputtered Ti/Au, and fired Ag] were formed on the single crystals, and their dielectric and piezoelectric properties were measured. The single crystals with a sputtered Ti/Au electrode showed the highest dielectric and piezoelectric constants but the lowest coercive electric field ($E_C$). The single crystals with a fired Ag electrode showed the lowest dielectric and piezoelectric constants but the highest coercive electric field ($E_C$). This dependence on the type of electrode was most significant in the piezoelectrically hard PMN-PZT-C single crystals. However, the effects of the electrode type on the phase transition temperatures ($T_C$, $T_{RT}$) and dielectric loss were negligible. These results clearly demonstrate that it is important to select an appropriate electrode so as to maximize the dielectric and piezoelectric properties of single crystals in each type of piezoelectric application.

Effects of a Au-Cu Back Layer on the Properties of Spin Valves

  • In, Jang-Sik;Kim, Sang-Hoon;Kang, Jae-Yong;Tiwari, Ajay;Hong, Jong-Ill
    • Journal of Magnetics
    • /
    • v.12 no.3
    • /
    • pp.118-123
    • /
    • 2007
  • We have studied the effect of Au-Cu back layer system ${\sim}10{\AA}$ thick on the properties of a spin valve. The back layers were Cu, Au, co-sputtered $Cu_xAu_{1-x}$, laminated $[Au/Cu]_n$. and bi-layer [Au/Cu]. When Au was added to the Cu, the resistance of the spin valve abruptly increased most likely due to impurity scattering. The GMR values were not increased significantly for all the structures. In the case of co-sputtered $Cu_xAu_{1-x}$, the changes in the resistance, ${\Delta}R$, was increased at a composition of ${\sim}Au_{0.5}Cu_{0.5}$. This increase in ${\Delta}R$ is due to increase in the resistance and not from the enhanced spin-dependent scattering. The structural analyses showed that the orthorhombic $Au_{0.5}Cu_{0.5}$ was formed in the back layer instead of the face-centered tetragonal $Au_{0.5}Cu_{0.5}$ as we expected. Thermal annealing over $400^{\circ}C$ may be required to have face-centered tetragonal in the $10{\AA}$ thick ultra-thin film. In the case of a laminated or bi-layered back layer, the properties of the spin valve were improved, which may be attributed to the increase in the mean free path of conduction electrons.

Stretchable Deformation-Resistance Characteristics of Metal Thin Films for Stretchable Interconnect Applications II. Characteristics Comparison for Au, Pt, and Cu Thin Films (신축 전자패키지 배선용 금속박막의 신축변형-저항 특성 II. Au, Pt 및 Cu 박막의 특성 비교)

  • Park, Donghyun;Oh, Tae Sung
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.24 no.3
    • /
    • pp.19-26
    • /
    • 2017
  • Stretchable deformation-resistance characteristics of Au, Pt, and Cu films were measured for the stretchable packaging structure where a parylene F was used as an intermediate layer between a PDMS substrate and a metal thin film. The 150 nm-thick Au and Pt films, sputtered on the parylene F-coated PDMS substrate, exhibited the initial resistances of $1.56{\Omega}$ and $5.53{\Omega}$, respectively. The resistance increase ratios at 30% tensile strain were measured as 7 and 18 for Au film and Pt film, respectively. The 150 nm-thick Cu film, sputtered on the parylene F-coated PDMS substrate, exhibited a very poor stretchability compared to Au and Pt films. Its resistance was initially $18.71{\Omega}$, rapidly increased with applying tensile deformation, and finally became open at 5% tensile strain.

Molecular dynamics study of redeposition effect by Ar ion bombardments on Au, Pd(001) (Ar이온 충돌에 의한 Au, Pd(001) 표면에서 재증착 효과의 분자동역학 연구)

  • Kim, S.P.;Kim, S.J.;Kim, D.Y.;Chung, Y.C.;Lee, K.R.
    • Journal of the Korean Vacuum Society
    • /
    • v.17 no.2
    • /
    • pp.81-89
    • /
    • 2008
  • Atomic behavior during ion beam sputtering was investigated by using classical molecular dynamics simulation. When Ar ion bombards on Au and Pd(001) surface with various incidence energies and angles, some atoms which gained substantial energy by impacting Ar ion were sputtered out and, simultaneously, others were landed on the surface as if surface atoms were redeposited. It was observed that the redeposited atoms are five times for Au and three times for Pd as many as sputtered atoms irrespective of both incidence energy and angle. From sequential ion bombarding calculations, contrary to the conventional concepts which have described the mechanism of surface pattern formation based only on the erosion theory, the redeposition atoms were turned out to play a significant role in forming the surface patterns.

Etching Characteristics of Au Film using Capacitively Coupled CF4/Ar Plasma

  • Kim, Gwang-Beom;Hong, Sang-Jeen
    • Journal of the Speleological Society of Korea
    • /
    • no.82
    • /
    • pp.1-4
    • /
    • 2007
  • In this paper, the etching of Au films using photoresist masks on Si substrates was investigated using a capacitively coupled plasma etch reactor. The advantages of plasma etch techniques over current methods for Au metalization include the ability to simplify the metalization process flow with respect to resist lift-off schemes, and the ability to cleanly remove etched material without sidewall redeposition, as is seen in ion milling. The etch properties were measured for different gas mixing ratios of CF4/Ar, and chamber pressures while the other conditions were fixed. According to statistical design of experiment (DOE), etching process of Au films was characterized and also 20 samples were fabricated followed by measuring etch rate, selectivity and etch profile. There is a chemical reaction between CF4 and Au. Au- F is hard to remove from the surface because of its high melting point. The etching products can be sputtered by Ar ion bombardment.

Effect of Colloidal Silica and Pre-Coating of Cathode on Copper Electrodeposited Film (구리 전착층에 미치는 콜로이달실리카 및 음극 Pre-Coating의 영향)

  • Lee, Sang-Baek;Yun, Jeong-Mo;Park, Hyeong-Ho;Bae, In-Seong;Kim, Byeong-Il
    • Korean Journal of Materials Research
    • /
    • v.11 no.7
    • /
    • pp.569-574
    • /
    • 2001
  • The crystal structure, surface morphology and preferred orientation of the copper electrodeposit were investigated by the using sulfate bath with $SiO_2$suspensions and the cathode substrate Au sputtered. As by the addition of colloidal silica in copper electrolytic bath and Au pre-coating on substrate, the crystal particles of deposits was fined-down, made uniform and the account of particles were increased. Hardness of copper electrodeposits with colloidal silica increased about 15% in comparison with that of pure copper deposit film and (111), (200) and (311) plane of X-ray diffraction patterns were almost swept away, so preferred orientation of the copper deposits changed from (111) to (110) plane by codeposit $SiO_2$ and precoating the substrate.

  • PDF

Etching Characteristics of Au Thin Films using Inductively Coupled CF4 / Cl2 / Ar Plasma

  • Kim Dong-Pyo;Kim Chang-Il
    • Transactions on Electrical and Electronic Materials
    • /
    • v.4 no.3
    • /
    • pp.1-4
    • /
    • 2003
  • The etching of Au thin films has been performed in an inductively coupled $CF_4 / Cl_2 / Ar$ plasma. The etch properties including etch rate and selectivity were examined as $CF_4$ content adds from o to $30\%$ to $Cl_2/Ar$ plasma. The $Cl_2/(Cl_2 + Ar)$ gas mixing ratio was fixed at $20\%$. Other parameters were fixed at an rf power of 700 W, a dc bias voltage of -150 V, a chamber pressure of 15 mTorr, and a substrate temperature of $30^{\circ}C$. The highest etch rate of the Au thin film was 370 nm/min at a $10\%$ additive $CF_4$ into $Cl_2/Ar$ gas mixture. The surface reaction of the etched Au thin films was investigated using x-ray photoelectron spectroscopy (XPS) analysis. The XPS analysis shows that the intensities of Ail peaks are changed, indicating that there is a chemical reaction between Cl and Au. Au-Cl is hard to remove on the surface because of its high melting point. However, etching products can be sputtered by Ar ion bombardment.

Ion beam induced surface modifications of sapphire and gold film deposition: studies on the adhesion enhancement and mechanisms (Ion Beam을 이용한 사파이어($Al_2O_3$) 표면개질 및 금(Au) 박막증착: 접합성 향상 및 접학기구에 대한 연구)

  • 박재원;이광원;이재형;최병호
    • Journal of the Korean Vacuum Society
    • /
    • v.8 no.4B
    • /
    • pp.514-518
    • /
    • 1999
  • Gold (Au) is not supposed to react with sapphire(single crystalline ) under thermodynamic equillibrium, therefore, a strong adhesion between these two dissimilar materials is not expected. However, pull test showed that the gold film sputter-deposited onto annealed and pre-sputtered sapphire exhibited very strong adhesion even without post-deposition annealing. Strongly and weakly adhered samples as a result of the pull testing were selected to investigate the adhesion mechanisms with Auger electron spectroscopy. The Au/ interfaces were analyzed using a new technique that probes the interface on the film using Auger electron escape depth. It revealed that one or two monolayers of Au-Al-O compound formed at the Au/Sapphire interface when AES in the UHV chamber. It showed that metallic aluminum was detected on the surface of sapphire substrates after irradiating for 3 min. with 7keV Ar+ -ions. These results agree with TRIM calculations that yield preferential ion-beam etching. It is concluded that the formation of Au-Al-O compound, which is responsible for the strong metal-ceramic bonding, is due to ion-induced cleaning and reduction of the sapphire surface, and the kinetic energy of depositing gold atoms, molecules, and micro-particles as a driving force for the inter-facial reaction.

  • PDF