• Title/Summary/Keyword: Aluminum bat

Search Result 3, Processing Time 0.016 seconds

Effects of Bat Type on the Swing Motion of High School Baseball Athletes

  • Choi, Min Ra;Song, Sung Woo;Cha, Myung Joo;Shin, Min Young;Lee, Ki Kwang
    • Korean Journal of Applied Biomechanics
    • /
    • v.28 no.2
    • /
    • pp.87-92
    • /
    • 2018
  • Objective: The purpose of this study was to investigate the factors affecting two kinds of bat swing behavior through kinematic analysis. Method: A total of 32 high school baseball players participated in this study. The ball was placed on the tee-ball in a position where the subject could easily swing and the standard bat swing was performed as quickly and as accurately as possible using aluminum bats and wooden bats. Results: The aluminum bat showed a rapid swing speed of about 1.79 m/sec compared to the wooden bat. The speed of the batted ball was found to be significantly greater for the aluminum bat than for the wooden bat. In addition, although the difference between the shoulder-pelvis rotation angle according to the type of bat was not indicated, there was a statistically significant difference between the aluminum bat and the wooden bat in terms of the rotational angular velocity. Conclusion: Even though the results can explain the difference between the bat swing speed and the speed of the batted ball depending on the bat's material, it is difficult to explain the difference depending on the type of bat at the shoulder-pelvis rotation angle. However, shoulder-pelvic rotation angular velocity appears to be higher for the aluminum bat, and the differences in the type of bat is considered to be related to the batting swing factor.

A Study on Lifespan and Longevity for Pipistrellus abramus (Chiroptera, Vespertilionidae) in Korea (한국에서 집박쥐(Pipistrellus abramus)의 장기 생존과 수명에 관한 연구)

  • Kim, Sung-Chul;Jeon, Young-Shin;Han, Sang-Hoon;Chung, Chul-Un
    • Korean Journal of Environmental Biology
    • /
    • v.36 no.4
    • /
    • pp.550-553
    • /
    • 2018
  • The lifespan of bats is longer compared to that of other similarly sized mammals, and it is recorded that some bats' lifespan is more than 30 years. However, it is known that the lifespan of Pipistrellus abramus using human residential areas as their habitats is less than five years. We have put aluminum rings on the forearms of 284 P. abramus starting from 2008. Interestingly, in June 2018, a female adult bat was recaptured ten years after the aluminum ring was attached. The results of this study on the lifespan of P. abramus is new and it's likely to form the baseline for lifespan studies and habitat management of P. abramus in the future.

Laser Cladding with Al-36%Si Powder Paste on A319 Al Alloy Surface to Improve Wear Resistance (A319 알루미늄 합금 표면에 Al-36%Si 합금분말의 레이저 클래딩에 의한 내마모성 향상)

  • Lee, Hyoung-Keun
    • Journal of Welding and Joining
    • /
    • v.35 no.2
    • /
    • pp.58-62
    • /
    • 2017
  • A319 aluminum alloy containing 6.5% Si and 3.5% Cu as major alloying elements has been widely used in machinery parts because of its excellent castability and crack resistance. However it needs more wear resistance to extend its usage to the severe wear environments. It has been known that hyper-eutectic Al-Si alloy having more than 12.6% Si contains pro-eutectic Si particles, which give better wear resistance and lubrication characteristics than hypo-eutectic Al-Si alloy like A319 alloy. In this study, it was tried to clad hyper-eutectic Al-Si alloy on the surface of A319 alloy. In the experiments, Al-36%Si alloy powder was mixed with organic binder to make a fluidic paste. The paste was screen-printed on the A319 alloy surface, melted by pulsed Nd:YAG laser and alloyed with the A319 base alloy. As experimental parameters, the average laser power was changed to 111 W, 202 W and 280 W. With increasing the average laser power, the melting depth was changed to $142{\mu}m$, $205{\mu}m$ and $245{\mu}m$, and the dilution rate to 67.2 %, 72.4 % and 75.7 %, and the Si content in the cladding layer to 16.2 %, 14.6 % and 13.7 %, respectively. The cross-section of the cladding layer showed very fine eutectic microstructure even though it was hyper-eutectic Al-Si alloy. This seems to be due to the rapid solidification of the melted spot by single laser pulse. The average hardness for the three cladding layers was HV175, which was much higher than HV96 of A319 base alloy. From the block-on-roll wear tests, A319 alloy had a wear loss of 5.8 mg, but the three cladding layers had an average wear loss of 3.5 mg, which meant that an increase of 40 % in wear resistance was obtained by laser cladding.