• Title/Summary/Keyword: Alloy Solidification

Search Result 369, Processing Time 0.021 seconds

Dissimilar Metal Welding of Inconel 600 and STS304 by a continuous wave Nd:YAG Laser (연속파형 Nd:YAG레이저를 이용한 Inconel 600와 STS 304의 이종금속용접)

  • Shin, Ho-Jun;Yoo, Young-Tae;Song, Seong-Wook
    • Proceedings of the KSME Conference
    • /
    • 2004.04a
    • /
    • pp.1120-1125
    • /
    • 2004
  • Welding characteristics of STS304 stainless steel and Inconel 600 using a continuous wave Nd:YAG laser are experimentally investigated. Alloy 600 being used in steam generator tubing of pressurized water reactor(PWR) exposed to some corrosion environment, stress corrosion cracking can occur on this material. Presented here are the results from a series of experiments in which dissimilar metal welds were made using the gas tungsten arc welding process with pure argon shielding gas. But It is well known that solidification cracking susceptibility of austenitic alloys depends on the solidification temperature range and amount/distribution of solute rich liquid that exists at the terminal stages of solidification. An experimental study was conducted to determine effects of welding parameters and to optimize those parameters that have the most influence on eliminating or reducing the extent welding zone formation at dissimilar metal welds.

  • PDF

Design and Evaluation of Aluminum Casting Alloys for Thermal Managing Application (방열소재용 알루미늄 주조합금 설계 및 특성평가)

  • Shin, Je-Sik;Kim, Ki-Tae;Ko, Se-Hyun;An, Dong-Jin;Kim, Myung-Ho
    • Journal of Korea Foundry Society
    • /
    • v.33 no.1
    • /
    • pp.22-31
    • /
    • 2013
  • In order to develop an aluminum alloy, that can combine high thermal conductivity and good castability and anodizability, aluminum alloys with low Si content, such as Al-(0.5~1.5)Mg-1Fe-0.5Si and Al-(1.0~1.5)Si-1Fe-1Zn, were designed. The developed aluminum alloys exhibited 170~190% thermal conductivity (160~180 W/mK), 60~85% fluidity, and equal or higher ultimate tensile strength compared with those of the ADC12 alloy. In each developed alloy system, the thermal conductivity decreased and the strength increased with the increment of Mg and Si, which are the significant alloying elements. The fluidity was in reverse proportion to the Mg content and in proportion to the Si content. The Al-(0.5~1.5)Mg-1Fe-0.5Si alloys exhibited better fluidity in thick-wall castings, while the Al-(1.0~1.5)Si-1Fe-1Zn alloys were better in thin-wall castability due to their lower surface energies. The fluidity behavior was complexly affected by the heat release for the solidification, viscosity, solidification range, and the type, quantity, and formation juncture of the main secondary phase.

Microstructural Characteristics of Al-Cr Coated Zr Alloy Fabricated by Laser Surface Melting Process (레이저 표면 용융공정으로 Al-Cr 코팅한 Zr합금의 미세조직 특성)

  • Kim, Jeong-Min;Lee, Jae-Cheol;Kim, Il-Hyun;Kim, Hyun-Gil
    • Korean Journal of Materials Research
    • /
    • v.27 no.10
    • /
    • pp.563-568
    • /
    • 2017
  • In this study, the coating of an Al-Cr layer on the surface of a Zircaloy-4 alloy was carried out through plasma pretreatment coating and a laser surface melting process. Two different conditions for laser treatment, severe or minimal surface melting of the Zr alloy substrate, were applied to form the final coating. When there was significant surface melting of the Zr alloy, the solidification microstructure of the newly formed coating layer was mainly composed of needle-shaped $Al_3Zr$, Al(Cr) and $Al_7Cr$ phases. On the other hand, the solidification microstructure of the coating layer was mainly composed of Al(Cr) and $Al_7Cr$ phases when there was minimal surface melting of Zr base in the laser process. However, when the coating was maintained at $1100^{\circ}C$ for 2 hours, significant inter-diffusion occurred between the phases in the coating. As a result, the upper part of the coating layer was observed to mainly consist of $Al_3Zr$ and $Al_8Cr_5$ phases, regardless of the laser treatment conditions.

Quasicrystals And Related Approximant Phases in Mg-Zn-Y (Mg-Zn-Y 합금에서 준결정 및 준결정 유사상)

  • Park, Eun-Soo;Ok, Jae-Bum;Kim, Won-Tae;Kim, Do-Hyang
    • Applied Microscopy
    • /
    • v.32 no.1
    • /
    • pp.31-37
    • /
    • 2002
  • As-cast microstructure of Mg-rich $Mg_{68}Zn_{28}Y_4$ has been investigated by a detailed transmission electron microscopy. The as-cast $Mg_{68}Zn_{28}Y_4$ alloy consisted of three different types of phases: $10{\sim}20{\mu}m$ size primary solidification phase, dendritic phase grown from the primary phase and a eutectic structure formed at the later stage of solidification. The primary solidification phase has an icosahedral structure with a large degree of phason strain. 1/1 rhombohedral approximant phase with lattice parameters: $a=27.2{\AA}\;and\;{\alpha}=63.43^{\circ}$ is first observed in Mg-Zn-Y system. The rhombohedral structure can be obtained by introducing phason strain in the six dimensional face centered hyper-cubic lattice. The decagonal phase nucleates with orientation relationship with the icosahedral phase, and $Mg_4Zn_7$ nucleates with orientation relationship with the decagonal phase, indicating a close structural similarity between the three phases. Gradual depletion of Y during solidification plays an important role in heterogeneous nucleation of decagonal and $Mg_4Zn_7$ phases from icosahedral and decagonal phases respectively.

Bulk Processing of an Amorphous $AI_{85}Ni_{10}Y_{5}$ Alloy Ribbon and Mechanical Properties by Annealing Treatment (비정질 $AI_{85}Ni_{10}Y_{5}$ 합금 리본의 벌크화와 어닐링에 따른 기계적 특성)

  • 고병철;김종현;유연철
    • Transactions of Materials Processing
    • /
    • v.8 no.6
    • /
    • pp.626-633
    • /
    • 1999
  • $Al_{85}Ni_{10}Y_5$ (at. %) amorphous alloy ribbons have been produced by rapidly solidification process and consolidated by the conventional powder metallurgy method. The grains with ∼90 nm were obtained in the Al85Ni10Y5 alloy extrudates by hot-pressing followed by hot-extusion. To investigate the effect of heat treatment on microstructural change of the extrudates, heat treatment was carried out from 200℃ to 400℃ at the step of 50℃. In addition, mechanical properties of the extrudates were analysed from torsion test at the temperature range or 400∼500℃ under a strain rates of 0.2, 0.5, and 1.0/sec. The extrudates showed a flow stress of ∼190 MPa and low elongation of ∼150% at 400℃, contributing to the enhancement of ductility and hardness for extrudates. Also, grain boundary sliding was occurred in the $Al_{85}Ni_{10}Y_5$ alloy during hot deformation.

  • PDF

Cu-based Bulk Amorphous Alloys in the Cu-Zr-Ti-Ni-Pd System (Cu-Zr-Ti-Ni-Pd계 비정질 벌크합금의 형성과 성질)

  • Kim, Sung-Gyoo;Bae, Cha-Hurn
    • Journal of Korea Foundry Society
    • /
    • v.22 no.6
    • /
    • pp.304-308
    • /
    • 2002
  • The new Cu-Zr-Ti-Ni-Pd amorphous alloy system has been introduced and manufactured using melt-spinning and Cu-mold die casting methods. Amorphous formability, the supercooled liquid region before crystallization and mechanical properties of the alloys were examined. The reduced glass transition temperature(Trg = Tg/Tm) and the supercooled liquid region(${\Delta}$Tx = Tx-Tg) of $Cu_{49}Zr_{30}Ti_{10}Ni_5Pb_6$ alloy were 0.620 and 57 K respectively. $Cu_{49}Zr_{30}Ti_{10}Ni_5Pb_6$ amorphous alloy was produced in the rod shape with 2mm diameter using the Cu-mold die casting. The hardness value of the amorphous bulk alloy was 432 DPN.

Load Relaxation and Creep Transition Behavior of a Spray Cast Hypereutectic Al-Si Based Alloy (분무 주조 과공정 Al-Si계 합금의 응력이완 및 Creep 천이 거동)

  • Kim M. S.;Bang W.;Park W. J.;Chang Y. W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.05a
    • /
    • pp.176-179
    • /
    • 2005
  • Spray casting of hypereutectic Al-Si based alloy has been reported to provide distinct advantages over ingot metallurgy (IM) or rapid solidification/powder metallurgy (RS/PM) process in terms of microstructure refinement. Hypereutectic Al-Si based alloys have been regarded attractive for automotive and aerospace application, due to high specific strength, good wear resistance, low coefficient of thermal expansion, high thermal stability, and good creep resistance. In this study, hypereutectic Al-25Si-2.0Cu-1.0Mg alloy was prepared by OSPREY spray casting process. High temperature deformation behavior of the hypereutectic Al-Si based alloy has been investigated by applying the internal variable theory proposed by Chang et al. The change of strain rate sensitivity and Creep transition were analyzed by using the load relaxation test and constant creep test.

  • PDF

Effect of Fe, Mn Content on the Castability of Al-4%Mg-0.9%Si Alloys for High Pressure Die Casting (고압 금형 주조용 Al-4%Mg-0.9%Si 합금의 주조특성에 미치는 Fe, Mn 함량의 영향)

  • Kim, Heon-Joo
    • Journal of Korea Foundry Society
    • /
    • v.33 no.2
    • /
    • pp.55-62
    • /
    • 2013
  • Effect of Fe and Mn contents on the castability of Al-4wt%Mg-0.9wt%Si system alloy has been studied. According to the analysis of cooling curve for Al-4wt%Mg-0.9wt%Si-0.3wt%Fe-0.3/0.5wt%Mn alloy, ${\alpha}-Al_{15}(Fe,Mn)_3Si_2$ and ${\beta}-Al_5FeSi$ phases crystallized above eutectic temperature of $Mg_2Si$. Therefore, these phases affected both the fluidity and shrinkage behaviors of the alloy during solidification. As Fe and Mn contents of Al-4wt%Mg-0.9wt%Si system alloy increased from 0.1 wt% to 0.4 wt% and from 0.3 wt% to 0.5 wt% respectively, the fluidity of the alloy decreased by 26% and 33%. When Fe content of the alloy increased from 0.1 wt% to 0.4 wt%, 23% decrease of macro shrinkage and 19% increase of micro shrinkage appeared. Similarly, Mn content of the alloy increased from 0.3 wt% to 0.5 wt%, 11% decrease of macro shrinkage and 14% increase of micro shrinkage appeared. Judging from the castability of the alloy, Al-4wt%Mg-0.9wt%Si alloy with low content of Fe and Mn, 0.1 wt% Fe and 0.3 wt% Mn, is recommendable.