  • In this study we aims to evaluate the effects of 1/3 mol% $Co_3O_4$ addition on the reaction, microstructure development, resultant electrical properties, and especially the bulk trap and grain boundary properties of $ZnO-Bi_2O_3-Sb_2O_3$ (Sb/Bi=2.0, 1.0, and 0.5) system (ZBS). The samples were prepared by conventional ceramic process, and characterized by XRD, density, SEM, I-V, impedance and modulus spectroscopy (IS & MS) measurement. In addition of $Co_3O_4$ in $ZnO-Bi_2O_3-Sb_2O_3$ (ZBSCo), the phase development, density, and microstructure were controlled by Sb/Bi ratio. Pyrochlore on cooling was reproduced in all systems. The more homogeneous microstructure was obtained in ZBSCo (Sb/Bi=1.0) system. In ZBSCo, the varistor characteristics were improved drastically (non-linear coefficient ${\alpha}$=23~50) compared to ZBS. Doping of $Co_3O_4$ to ZBS seemed to form $V^{\cdot}_o$(0.33 eV) as dominant defect. From IS & MS, especially the grain boundary of Sb/Bi=0.5 system is composed of electrically single barrier (0.93 eV) and somewhat sensitive to ambient oxygen with temperature.

Lake Water Treatment using Ceramic Ultrafiltration Membrane System with Periodic Water-backflushing

  • Park, Jin-Yong;Kyung, Gee-Yong;Han, Song-Hee;Kim, Hyun-Woo;Lee, Hyuk-Chan
    • Korean Membrane Journal
    • /
    • v.8 no.1
    • /
    • pp.50-57
    • /
    • 2006
  • We treated lake water by ceramic ultrafiltration membranes and found the optimal backflushing period and trans-membrane pressure (TMP) of periodic water-backflushing system. The optimal filtration time interval at fixed BT = 3 sec was 30 for A002 membrane in all viewpoints of $J/J_0,\;R_f$, and $V_T$, and we could acquire the highest $V_T$ value in the membranes used here. However, the highest $V_T$ was acquired at FT = 60 sec for M9, and at FT = 90 sec for C005 membrane. Then the lower TMP reduced the membrane fouling during filtration of lake water, and could maintain the higher permeate flux compared with the initial flux. However, the largest value $V_T$ could be obtained at the highest TMP condition for M9 membrane at fixed FT = 60 sec and BT = 3 sec. The quality of treated water in our UF ceramic system was Turbidity = $0.20{\sim}4.88NTU$, $COD_{Mn} = 0.00{\sim}2.58 mg/L$, $TDS = l8{\sim}71 mg/L$, and $NH_3-N = 0.004{\sim}1.689 mg/L$.

Implants and all-ceramic restorations in a patient treated for aggressive periodontitis: a case report

  • Hong, Jin-Sun;Yeo, In-Sung;Kim, Sung-Hun;Lee, Jai-Bong;Han, Jung-Suk;Yang, Jae-Ho
    • The Journal of Advanced Prosthodontics
    • /
    • v.2 no.3
    • /
    • pp.97-101
    • /
    • 2010
  • A 23-year-old female with aggressive periodontitis was treated using dental implants and LAVA system. The severely compromised teeth were extracted irrespective of initial conservative periodontal treatment. An implant-supported overdenture with 4 implants was fabricated for the maxilla and all-ceramic restorations for the mandible. Esthetic and functional goals were achieved with team approach involving periodontists and prosthodontists. This case report describes a treatment procedure for a generalized aggressive periodontitis patient with severe bone resorption.

hydration of the Fly Ash-CaO System in the Presence of Various Chemical Activators (화학 활성화제에 의한 플라이애쉬-생석회계의 수화반응)

  • 송종택;김재영;류동우;고상렬;한경섭
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.2
    • /
    • pp.185-195
    • /
    • 1998
  • This experiment carried out in order to investigate the effect of the chemical activators for acceleration of hydration the system of Fly ash-Cao The paste was consisted of 80wt% Fly ash and 20wt% CaO with 1. 3. 5wt% of 4 activators(N{{{{ alpha _2 }}S{{{{ OMICRON _4 }}, CaC{{{{ {l }_{2 } }}, NaOH, Ca(N{{{{ OMICRON _3 {)}_{2 } }} and W/S ratio of 0.42 After curing for 1, 3, 7, 14, 28 days the paste hydration was characterized by the measurement of compressive strength XRD analysis SEM observation the combined water and the reaction amount of Ca(OH)2 determination. As a result of this ex-periment all of the system which involved Na2SO4 or NaOH had a god compressive strength. In the case of 7 days curing a system which added CaCl2 showed the highest compressive strength among all especially NaOH system showed a high increase in strength as a dosage of it increased. Hydration products were different according to activatores added. Only C-S-H was observed in NaOH system. As the reaction amount of Ca(OH)2 and combined water were increased the compressive strength increased. There were few differences in the comparision of strength between ignited loss 3.1% and loss 9.3% of fly ash.

  • PDF

Dental application of glass-ceramic materials for aesthetic restoration (심미수복을 위한 글라스-세라믹 재료의 치과 응용)

  • Bae, Tae Sung
    • The Journal of the Korean dental association
    • /
    • v.58 no.7
    • /
    • pp.435-442
    • /
    • 2020
  • Porcelain is the first ceramic material to be introduced into dentistry. Porcelain jacket crown was introduced by Dr. Charles H Land in 1886, which was an excellent aesthetic dental restoration but has not been widely used due to high firing shrinkage and low tensile strength. Then metal-ceramic system, which combines the esthetic properties of ceramics and the mechanical properties of metals, was introduced and nowadays it is still used in dental clinical field. However, the metal-ceramic system has shown some problems, such as increased lightness by reflection of light at opaque layer, shadow beneath the gingival line due to the block-out of light by metal coping, exposure of metal in margin part, bond failure between metal and porcelain, oxidation of metal coping during firing the porcelain, etc. Recently, along with the advance of fabrication methods of dental ceramics, the all-ceramic restorations with high esthetic and mechanical properties has increased and gradually replaced metal-ceramic restorations. Especially, CAD/CAM technology has opened a new era in fabricating the dental ceramic restorations. This overview will take a look at the past, present and future possibility of the dental ceramic materials.

  • PDF

The Effect of Repeated Firing on the Color Difference of a Metal-Ceramic System with Different Porcelain Powder (다른 특성을 가지는 도재가 반복소성에 따라 색조변화에 미치는 영향)

  • Hwang, Jae-Sun
    • Journal of Technologic Dentistry
    • /
    • v.31 no.1
    • /
    • pp.23-36
    • /
    • 2009
  • The goal of esthetic restoration is to achieve morphologic, optical, and biologic acceptance. Creation of a natural looking ceramic restoration, which blends harmoniously with surrounding dentition, is not always achieved. A successful color match is an important aspect of any esthetic dental restoration. Since natural enamel has inherent translucency, it is important that ceramic restorations reproduce the translucency and color of the natural teeth. However, the final color match of porcelain crowns to adjacent natural dentition remains some problem. Difficulties related to color matching arise from the structural differences that exist between metal ceramic crowns and natural teeth, the limited range of available ceramic shades, inadequate shade guides, different types of metal alloys, repeated firing, the condensation technique, and varying compositions of ceramic materials. Many factors contribute to the esthetic success of dental restoration: optical properties such as color and its elements of hue, value, and chroma; translucency and opacity; light transmission and scattering; and metamerism and fluorescence. The purpose of this study was to determine the color changes of metal-ceramic system with different veneering porcelain powder after repeated firing. The objectives of this in vitro study were to measure the lightness($L^*$), chromaticity($a^*$), chromaticity($b^*$), chroma($C^*$), hue(h), reflectance(%), color difference(${\Delta}E$). The following conclusions were obtained: 1. An increase in the number of firings resulted in decrease in lightness($L^*$) but increase in chromacticity($a^*$) with all porcelain. After the second sintering resulted in decrease in chromacticity($b^*$) with opaque-dentin porcelain and dentin porcelain but in increase with enamel porcelain and translucency porcelain. And after the second sintering resulted in decrease in chroma($C^*$) with opaque-dentin porcelain and dentin porcelain, but on the whole side in decrease with enamel porcelain and translucency porcelain. 2. After the second firing, a increase in the number of firings resulted in decrease reflectance(%) in all wavelength. 3. There were noticeable color differences(${\Delta}E$) between first sintering and multiple firings(dentin porcelain: 5.29~8.15, opaque-dentin porcelain: 4.83~8.2, enamel porcelain: 8.93~13.15, translucency porcelain: 9.37~12.91), but the color difference(${\Delta}E$) after second sintering were down to 4.87 in all porcelain. 4. Given the NBS Criteria, a 'trace' was not found this study but a 'slight' was found 2-3, 3-5 in dentin porcelain, 2-3 in opaque-dentin porcelain, 3-5, 5-10 in enamel porcelain and translucency porcelain, a 'noticeable' was 2-5, 3-10, 5-10 in dentin porcelain and opaque-dentin porcelain, 2-3, 2-5, 3-10 in enamel porcelain 2-3, 3-10 in translucency porcelain, an 'appreciable' was 1-2, 1-3, 2-10 in dentin porcelain 1-2, 1-3, 2-10, 3-10 in opaque-dentin porcelain, 2-10 in enamel porcelain, 2-5, 2-10 in translucency porcelain, a 'much' was 1-5, 1-10 in dentin porcelain and opaque-dentin porcelain, 1-2, 1-3, 1-5 in enamel porcelain 1-2, 1-3, 1-5, 1-10 in translucency porcelain, a 'very much' was 1-10 in enamel porcelain.

  • PDF

CAD/CAM Zirconia All Ceramic Restoration and Red-White Esthetics

  • Jo, Jong-Man
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.13 no.1
    • /
    • pp.31-39
    • /
    • 2004
  • For the prosthodontic results which are compatible with esthetics to be fulfilled, the first prerequisite would be periodontal intervention and stability, the second one may be functional competency and the ultimate goal should be ascribed to esthetic considerations. Other words, esthetic dentistry is a whole entity which encompasses the biological stability of the periodontium, physical accuracy of the prosthodontic structure and finally, the beauty which can be found in natural dentition. It also implies the harmonized lip line which reveals the well-balanced tooth morphology and health gum profiles (Red-White Esthetics). Largely, there lie some differences in the input system of the 3-dimentional data from the prepared abutments between respective computer-assisted systems available now. But the manufacturing systems (CAM) are very similar between them, to say, comprise numeric control systems with whole 3-dimensional milling units according to the restorations to be made. Now the author is going to present CAD/CAM Zirconia All Ceramic Restoration on the topics for the Red-White Esthetics, periodontal control and maintenance, treatment for the discolored teeth, post & core build-up works for the devitalized teeth, characteristics of the Zirconium oxide All Ceramics, fabrication procedures, clinical considerations and its application to diverse clinical situations.

  • PDF

MARGINAL FIT OF GLASS INFILTRATED ALUMINA CORE FABRICATED FROM ALUMINA TAPES (알루미나 테이프를 사용한 유리 침투형 알루미나 코아의 변연적합도)

  • Oh, Nam-Sik;Lee, Myung-Hyun;Kim, Dae-Joon;Lee, Keun-Woo;Lee, Sun-Hyeong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.36 no.6
    • /
    • pp.832-845
    • /
    • 1998
  • The purpose of this study was to compare the marginal fit of all ceramic crowns prepared from alumina slip casting, which is consistent with the conventional In-ceram system, and those fabricated from alumina tapes which is currently under development in an effort to alleviate complexities involved in the forming procedure of the In-ceram crown core. All ceramic crowns, made of In-ceram(slip casting) and alumina tapes(Doctor blade casting), were prepared with $90^{\circ}\;and\;135^{\circ}$ shoulder margins. The crowns were cemented with a glass ionomer cement and embeded in epoxy resin. The embedded crowns were sectioned faciolingually and mesiodistally and marginal discrepancies and marginal gaps were measured under the Measurescope MM II. The measurements were analyzed using Wilcoxon rank sum test and Kruskal-Wallis test and the results were as follows: 1. In the case of $90^{\circ}$ shoulder margin, the combined marginal discrepancies and marginal gaps were $78.3{\mu}m\;and\;44.4{\mu}m$ respectively, for the all ceramic crowns fabricated using the alumina tapes. In comparison, the values were $65{\mu}m\;and\;25.5{\mu}m$ for the In-ceram crowns. For the marginal gaps a statistical difference existed (p<0.05) but no significant difference was observed for the marginal discrepancy (p>0.05). 2. In the case of $135^{\circ}$ shoulder margin, the combined marginal discrepancy and marginal gaps were $82.1{\mu}m\;and\;40.2{\mu}m$ respectively, for the all ceramic crowns formed with the tapes. As compared with the marginal discrepancy and gaps of the $90^{\circ}$ shoulder margin in the fabricated from the alumina tapes, no significant statistical differencies were discerned in both cases (p>0.05). 3. There was no statistically significant difference in the fits among four locations around the margins of the all ceramic crowns fabricated using the alumina tapes. The results obtained in this study showed that the marginal fits of the glass infiltrated alumina cores fabricated from the alumina tapes are slightly higher value than those prepared using the In-ceram but the difference is within a clinically acceptable range.

  • PDF

Effect of Additives on the Strength Characteristics of MDF Cement Composites (MDF 시멘트 복합재료의 강도 특성에 미치는 첨가재의 영향)

  • 김태현;최상흘
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.11
    • /
    • pp.893-899
    • /
    • 1992
  • Composite specimens, which are composed MDF cement of HAC-PVA system were prepared by adding carbon fiber, hydrated silica and SiC powder, and we studied effect of additives on the flexural strength of the composites. All of additives is effective in the improvement of flexural strength of the composite specimens. The size of average pore diameter in the specimens which have high flexural strength property was small. Specimen mixed with hydrated silica was effective in the particle compact property. Flexural strength of carbon fiber reinforced MDF cement composites were improved because of crack deflection of carbon fiber in cementitious matrix.

  • PDF