Electrical Conduction Mechanisms of $RuO_2$ Based Thick Film Resistor ($RuO_2$계 후막저항체의 전기전도기구)

  • 구본급;김호기
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.12
    • /
    • pp.1529-1535
    • /
    • 1994
  • Electrical conduction mechanisms of RuO2-based thick film resistors were investigated with frequency depandence on AC conductivity. Electrical conduction mechanisms of lower resistivity system (100{{{{ OMEGA }}/sq) sintered at 600~90$0^{\circ}C$ were all metallic conduction mechanism. In case of higher resistivity (10K{{{{ OMEGA }}/sq) system, the electrical conduction mechanisms were very depenent on sintering temperature. When sintering temperature was $600^{\circ}C$, the electrical conduction mechamism was ionic, and as increasing the sintering temperature, the electrical conduction mechanism was changed from ionic to hopping conduction mechanism.

  • PDF

EFFECT OF ETCHING TIME ON SHEAR BOND STRENGTH OF RESIN CEMENTS TO REINFORCED ALL-CERAMIC CROWNS (불산 처리 시간이 강화형 전부도재관과 레진 시멘트의 전단 결합강도에 미치는 영향)

  • Kim Kyoung-Il;Choi Keun-Bae;Ahn Seung-Geun;Park Charn-Woon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.42 no.5
    • /
    • pp.501-513
    • /
    • 2004
  • Purpose : The purpose of this study was to evaluate the effects of etching time on shear bond strength of four resin cements to IPS Empress 2 ceramic. Material and Methods: Forty rectangular shape ceramic specimens ($10{\times}15{\times}3.5mm$ size) were used for this study. The ceramic specimens divided into four groups and were etched with 10% hydrofluoric acid for 0, 10, 30, 60, 180, 300, 420, 600, and 900 seconds respectively. Etched surfaces of ceramic specimens were coated with ceramic adhesive system and bonded with four resin cement (Variolink II, Panavia F, Panavia 21, Super-Bond C&B) using acrylic glass tube. All cemented specimens were tested under shear loading untill fracture on universal testing machine at a crosshead speed 1mm/min: the maximum load at fracture (kg) was recored. Shear bond strengh data were analyzed with oneway analysis of variance and Tukey HSD tests (p<.05). Etched ceramic surfaces (0-, 60-, 300-, and 600-seconds etching period) and fracture surfaces after shear testing were examined mophologically using scanning electron microscopy. Results : Ceramic surface treatment with 10% hydrofluoric acid improved the bond strength of three resin cement except for Super-Bond C&B cement. Variolink II (41.0$\pm$2.4 MPa) resin cement at 300-seconds etching time showed statistically higher shear bond strength than the other resin cements (Panavia F: 28.3$\pm$2.3 MPa, Panavia 21: 21.5$\pm$2.2 MPa, Super-Bond C&B: 16.7$\pm$1.6 MPa). Ceramic surface etched with 10% hydrofluoric acid for 300 seconds showed more retentive surface texture. Conclusion: Within the limitation of this study, Variolink II resin cement are suitable for cementation of Empress 2 all-ceramic restorations and etching with 10% hydrofluoric acid for 180 to 300 seconds is required to enhance the bond strength.

Dispersion Behavior of Transparent Dielectric Glass Frits in the Multi-Solvent and Ammonium-Type Dispersant System (다성분 용매와 암모늄계 분산제가 적용된 투명 유전체 프릿트 슬립의 분산거동)

  • Kim, Joo-Won;Chun, Young-Hwan;Hwang, Jong-Hee;Lee, Sang-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.10 s.293
    • /
    • pp.635-639
    • /
    • 2006
  • Dispersion behavior of the slurries consisted of Pb or Bi-based glass frits, which are used for the fabrication of green sheet as PDP front panel transparent dielectric, was examined in non-aqueous solvent system. Measurements of sedimentation height and viscosity were conducted to determine proper dispersion condition in the various solvent and dispersant system. Azotropic compound and ethyl acetate were used as the solvent and ammonium-type dispersant was applied to the slurries. All slurries were dispersed well in azotropic solvent system involving 20$\sim$50 vol% ethyl acetate at 2$\sim$3 wt% dispersant content. Especially, dispersion behavior was notably improved in the addition of ethyl acetate in the Bi-based frit slurry.

A Study on the Preparation of MgO-Al2O3-SiO2 System Ceramic Powders by Spray Pyrolysis Method (분무열분해법에 의한 MgO-Al2O3-SiO2계 화합물의 분체합성 및 그 특성)

  • 박정현;박찬욱;조경식
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.4
    • /
    • pp.397-407
    • /
    • 1988
  • Spinel, mullite and cordierite powders have synthesized from Mg(NO3)2.6H2O, Al(NO3).9H2O and SiCl4 solution by spray pyrolysis method. The two-fluid nozzle was used as an atomizer. The powders of sinel and mullite were synthesized above 80$0^{\circ}C$, but the cordierite composition was noncrystalline for all synthersizing temperature. Those noncrystalline powders were crystallized to $\alpha$-cordierite during calcining at 130$0^{\circ}C$ for 2hrs. The synthesized spinel, mullite and cordierite powders seem to be consisted of agglomerated hollow spherical particles. For all powders, the particle size ranged from submicron to about 3${\mu}{\textrm}{m}$ and mean particle size was about 1.4${\mu}{\textrm}{m}$ in diameter. The specific surface area values of spinel, mullite and cordierite powders were maximum for powders prepared at 100$0^{\circ}C$, and those were 45.9, 25.8 and 13.6$m^2$/gr, respectively.

  • PDF

A Study on Hybrid material of Making Dental restorations by CAD/CAM System (치과 CAD/CAM용 복합소재를 이용한 치과보철물의 제작에 대한 연구)

  • Choi, Beom-Jin
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.23 no.2
    • /
    • pp.86-94
    • /
    • 2014
  • In recent years, perhaps the biggest driver in new material development is the desire to improve crown and bridge esthetics compared to the traditional PFM or all-metal restorations. As such, zirconia, leucite-containing glass ceramic and lithium disilicate glass ceramic have become prominent in the dental practice. Each material type performs differently regarding strength, toughness, ease of machining and the final preparation of the material prior to placement. For example, glass ceramic are typically weaker materials which limits its use to single-unit restorations. On the other hand, zirconia has a high fracture toughness which enables multi-unit restorations. This material requires a long sintering procedure which excludes its use for fast chair side production. Developed hybrid material of CAD/CAM is contained nano ceramic elements. This new material, called a Resin Nano Ceramic is unique in durability and function. The material is not a resin or composite. It is also not a pure ceramic. The material is a mixture of both and consists of ceramic. Like a composite, the material is not brittle and is fracture resistant. Like a glass ceramic, the material has excellent polish retention for lasting esthetics. The material is easily machined chair side or in a dental lab, polishes quickly to an esthetic finish and if necessary, can be useful restoratives.

Retrospective clinical and radiographic evaluation of restored endodontically treated teeth

  • Paula Pontes Garcia ;Aline Cappoani ;Ricardo Susin Schelbauer ;Gisele Maria Correr ;Carla Castiglia Gonzaga
    • Restorative Dentistry and Endodontics
    • /
    • v.45 no.4
    • /
    • pp.49.1-49.11
    • /
    • 2020
  • Objectives: The aim of this study was to perform a clinical and radiographic analysis of endodontically treated teeth (ETT) restored with cast metal posts (CMPs) or prefabricated glass fiber posts (GFPs) and crowns. Materials and Methods: Fifty ETT were restored with 25 CMPs and 25 GFPs at a private dental clinic between 2001 and 2016. The restorations consisted of 12 all-ceramic crowns, 31 metal-ceramic crowns, and 7 composite resin crowns. Demographic data, type of teeth, type of post-and-core system, time of placement, crown restorations, the number of proximal contacts, the type of antagonist, and reports of any complications after post-and-core placement were recorded for each patient. Assessments were performed at baseline (radiographic) and follow-up (radiographic and clinical). Data were analyzed by the McNemar test, the Pearson χ2 test, and Kaplan-Meier survival curves (α = 0.05). The mean follow-up was 67.6 months. Results: No significant difference was observed for any of the radiographic parameters when the baseline and final radiographs were compared. In the clinical evaluation, anatomical form (p = 0.009) and occlusion (p = 0.001) showed significant differences according to the type of crown restoration; specifically, metal-ceramic and all-ceramic crowns outperformed composite resin crowns. Conclusions: CMPs and GFPs showed favorable results for restoring ETT after 6 years of follow-up. All-ceramic and metal-ceramic crowns showed higher survival rates and better clinical outcomes.

A Study on the Fracture Strength of All-Ceramic Crown according to the Zirconia Coping Design using CAD/CAM System (CAD/CAM을 이용하여 제작한 전부도재관의 지르코니아 코핑 디자인에 따른 파절강도에 관한 연구)

  • Bulgan, L.;Cho, In-Ho;Shin, Soo-Yeon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.22 no.2
    • /
    • pp.111-123
    • /
    • 2006
  • A Study on the Fracture Strength of All-Ceramic Crown according to the Zirconia Coping Design using CAD/CAM System L. Bulgan, In-Ho Cho, Soo-Yeon Shin Department of Prosthodontics, Graduate School, Dankook University The fracture strength of prosthesis is important, because it affects the function, and long term success of prosthesis and teeth. The purpose of this study was to compare the fracture strength of zirconia coping designs. Experimental test group were classified into three designs according to coping design, Modified design: Zirconia coping margin was located at 1mm above the axiogingival line angle. Collarless design: The coping margin terminated at the axiogingival line angle Butt design: The coping margin was extended to the finishing line of prepared margin. A $Cercon^{(R)}$(Degussa, Germany) CAD/CAM system was used to make the zirconia coping. Fracture strength was measured using loading machine at a cross head speed of 1mm/min. The results were statistically analyzed using the one-way ANOVA and multiple comparison test. Statistical significance was set in advance at the probability level of less than 0.05. The result : I. Collarless($738N{\pm}155N$) and Modified($755N{\pm}185N$) groups showed significantly a lower fracture strength than Butt($1057N{\pm}262N$) group(p<0.05). II. There were no statistical differences of the fracture strength between Modified($755N{\pm}185N$) and Collarless($738N{\pm}155N$) groups. III. When comparing the fractured surface, all the group showed porcelain fracture, which were fractured at the labial surface of baked porcelain The butt design of the zirconia coping has higher fracture strength than modified and collarless design.

Wear of primary teeth caused by opposed all-ceramic or stainless steel crowns

  • Choi, Jae-Won;Bae, Ik-Hyun;Noh, Tae-Hwan;Ju, Sung-Won;Lee, Tae-Kyoung;Ahn, Jin-Soo;Jeong, Tae-Sung;Huh, Jung-Bo
    • The Journal of Advanced Prosthodontics
    • /
    • v.8 no.1
    • /
    • pp.43-52
    • /
    • 2016
  • PURPOSE. This study was conducted to evaluate the effects of full-coverage all-ceramic zirconia, lithium disilicate glass-ceramic, leucite glass-ceramic, or stainless steel crowns on antagonistic primary tooth wear. MATERIALS AND METHODS. There were four study groups: the stainless steel (Steel) group, the leucite glass-ceramic (Leucite) group, the lithium disilicate glass-ceramic (Lithium) group, and the monolithic zirconia (Zirconia) group. Ten flat crown specimens were prepared per group; opposing teeth were prepared using primary canines. A wear test was conducted over 100,000 chewing cycles using a dual-axis chewing simulator and a 50 N masticating force, and wear losses of antagonistic teeth and restorative materials were calculated using a three-dimensional profiling system and an electronic scale, respectively. Statistical significance was determined using One-way ANOVA and Tukey's test (P<.05). RESULTS. The Leucite group ($2.670{\pm}1.471mm^3$) showed the greatest amount of antagonist tooth wear, followed by in decreasing order by the Lithium ($2.042{\pm}0.696mm^3$), Zirconia ($1.426{\pm}0.477mm^3$), and Steel groups ($0.397{\pm}0.192mm^3$). Mean volume losses in the Leucite and Lithium groups were significantly greater than in the Steel group (P<.05). No significant difference was observed between mean volume losses in the Zirconia and Steel groups (P>.05). CONCLUSION. Leucite glass-ceramic and lithium disilicate glass-ceramic cause more primary tooth wear than stainless steel or zirconia.

Mechanical safety evaluation of ceramic ball head for total hip replacement using finite element method (인공고관절 전치환술에서 세라믹 볼 헤드의 기계적 안정성 평가를 위한 유한요소 해석)

  • Han, Sung-Min;Chu, Jun-Uk;Chun, Heoung-Jae;Kim, Jung-Sung;Choi, Kui-Won;Youn, In-Chan
    • Journal of Biomedical Engineering Research
    • /
    • v.31 no.6
    • /
    • pp.449-455
    • /
    • 2010
  • A ceramic articulating system in total hip replacement thought to be superior to metal-on-polyethylene due to its extremely low coefficient of friction and potential for high resistance to wear. But ceramic is brittle, which makes it mechanically and theoretically susceptible to fracture under certain mechanical conditions. In the current study, nine different models of ceramic ball heads were mechanically evaluated using 3D finite element(FE) analyses. It was found that the maximum stress in all ceramic models was lower than ceramic flexural strength, and it satisfied the requirements of the FDA Gaudience for artificial hip implant. Thus, ceramic ball head models introduced in the current study could be mechanically safe for clinical applications.