The low-field tunnel-type magnetoresistance (MR) properties of sol-gel derived $La_{0.7}Pb_{0.3}MnO_3(LPMO)$ thin film deposited on different substrate have been investigated. Polycrystalline thin films were fabricated by spin-coating on $SiO_2/Si(100)$ substrate and that with yttria-stabilized zirconia (YSZ) buffer layer, while c-axis-oriented thim film was grown on $LaAlO_3(001)$ (LAO) single crystal substrate. The full width half maximum (FWHM) of the rocking curve scan of LPMO/LAO film is $0.32^{\circ}$. Tunnel-type MR ratio is 0.52 % in $LPMO/SiO_2/Si$(100) film and that of $LPMO/YSZ/SiO_2/Si$(100) film is as high as 0.68 %, whereas that of LPMO/LAO(001) film is less than 0.4 % under the applied field of 500 Oe at 300 K. Well-pronounced MR hysteresis was registered with an MR peak in the vicinity of the coercive field. The low-field tunnel-type MR characteristics of thin films deposited on different substrates originates from the behavior of grain boundary properties.
Kim, Geun-Woo;Seo, Yong-Jun;Sung, Chang-Hoon;Park, Keun-Young;Cho, Ho-Je;Heo, Si-Nae;Koo, Bon-Heun
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.25
no.10
/
pp.805-810
/
2012
Transparent conducting oxides (TCOs) have wide range of application areas in transparent electrode for display devices, Transparent coating for solar energy heat mirrors, and electromagnetic wave shield. $SnO_2$ is intrinsically an n-type semiconductor due to oxygen deficiencies and has a high energy-band gap more than 3.5 eV. It is known as a transparent conducting oxide because of its low resistivity of $10^{-3}{\Omega}{\cdot}cm$ and high transmittance over 90% in visible region. In this study, co-doping effects of Al and Y on the properties of $SnO_2$ were investigated. The addition of Y in $SnO_2$ was tried to create oxygen vacancies that increase the diffusivity of oxygen ions for the densification of $SnO_2$. The addition of Al was expected to increase the electron concentration. Once, we observed solubility limit of $SnO_2$ single-doped with Al and Y. $\{(x/2)Al_2O_3+(x/2)Y_2O_3\}-SnO_2$ was used for the source of Al and Y to prevent the evaporation of $Al_2O_3$ and for the charge compensation. And we observed the valence changes of aluminium oxide because generally reported of valence changes of aluminium oxide in Tin - Aluminium binary system. The electrical properties, solubility limit, densification and microstructure of $SnO_2$ co-doped with Al and Y will be discussed.
This study aimed to investigate the changes in chemical components that occur when weak clay is mixed with steel slag modified with calcium oxide, and to understand the expression characteristics of compressive strength according to hydrophilicity and curing time. XRF testing, SEM imaging, vane shear strength and uniaxial compressive strength testing were conducted. Calcium (Ca) released from the steel slag increases the Ca content in clay by increasing the number of crystal particles and forming a coating layer known as calcium silicate hydrate (CaO-SiO2-H2O) through chemical reactions with SiO2 and Al2O3 components. The weak clay stabilized with steel slag is classified into an initial inactive zone where strength relatively does not increase and an activation zone where strength increases over curing time. The vane shear strength of the initial inactive area was found to be 4.4 to 18.4 kN/m2 in the state of the weight mixing ratio Rss 30% (steel slag 30% + clay 70%). In the case of the active area, the maximum uniaxial compressive strength increased to 431.8 kN/m2 after 480 hours of curing time, which increased due to the apparent adhesion strength of clay through pozzolanic reaction. Therefore, considering the strength expression characteristics of stabilized mixed clay based on the mixing ratio (Rss) during the recycling of steel slag can enhance its practicality in civil engineering sites.
Park, H. J.;Lee, S. Y.;Yang, S. C.;Lee, S. Y.;Kim, S. S.;Han, J. G.
Journal of the Korean institute of surface engineering
/
v.31
no.6
/
pp.334-344
/
1998
Yew coating pmccss t.o form a surface layer ol CrN phasc on mild steel (A81 1020!, AlSI Hi3, 1Cr-0.5Mo steel (ASTM A213 and Nickrl-base superalloy (Inconel 718) was developed. Surlaces of various alloys t,n.ateii by chromizing for the formation ol Cr diffusion layer was subsequently trcaled by plasma nitriding in order t.o form the hard CrS coating layer on the surfaces. This duplex plasma surface tri-atments of chromizing and plasma nitriding have induced a lormation of a duplex-lrcated surfacr hyer of approximat~ls 70-80 $\mu\textrm{m}$thickncss with a iargcly improved microiiardnrss up to approxiniateW 1500Hv(50gf). The main cause for the lage improvment in the surface hardncss is altribilted to [.he fact that CrN and $Fe_xN$ phases are created successfully by ccliromizins and plasma nilriding treatment. High tenipera1,urc wear resislance of the duplex-treated mild steel and HI3 steels at $600^{\circ}C$ was examined. Comparing the duplex-treated specimens with the specimens treated only by chromizing, the rcsults shovmi that, thc wear volume of the duplex-treated mild skcl and 1113 stcel aSt.er a wear test, at $600^{\circ}C$ were reduced hy a Iactor of 8 and 3, respectively. Characteristics of the CrS phase by duplrx treatment were compared with $CrN_x$,/TEX> film by ion plating and the wear behaviors of CrN film lormed by two different nroccsses arc nea.riy identical.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2016.11a
/
pp.33-55
/
2016
PVD(Physical Vapour Deposition)코팅은 70년대 미국의 Multi-arc이란 기업에 의해 질화물계나 탄화물계 피막 증착이 가능한 아크이온플레팅(Arc Ion Plating) 기술이 산업에 소개되어, 주로 내마모나 내구성을 요구하는 금형, 절삭공구, 산업용 부품 분야 등에 적용되면서 꾸준한 성장세를 거듭해 왔다. 최근 들어 PVD기술은 그 수요의 급증과 더불어 보다 진화된 형태의 코팅장치 및 코팅피막들이 산업에 소개 되고 있다. 먼저 절삭가공분야에는 new composition, nano composite, multi-element composition, multi-layer, SML(Self Modification Layer)등의 코팅피막들이 단독 또는 조합된 형태로 개발되어 철계 소재를 대상으로 고경도 소재의 고속가공, 저경도~중경도 소재의 중속~고속 광범위영역에서 동시 절삭을 가능케 하였고, 비철.비금속 소재 절삭용으로 종전의 가스방식의 DLC(a-C:H)코팅을 훨씬 능가하는 ta-C Plus(Ultra super DLC) 코팅이 개발되어 고 Si함량의 Al-Si계 합금, Cu-W계, 고 섬유 CFRP, CFRM 및 반소결 상태의 세라믹 소재들을 황삭에서 정삭까지 단일 공정으로 절삭이 가능한 고성능 공구들이 개발보급되고 있다. 금속 성형분야에는 고장력 강판을 냉간에서 성형 가능한 Lubricative multi-layer coating, 열간 또는 고온에서 성형이 가능한 functional multi layer과 이형성이 더한층 개선된 dimpled(or embossed) functional multi layer 코팅들이 개발되어 산업현장에 빠르게 확산되고 있다. PVD 코팅의 또 다른 주요 적용분야로 의료분야를 들 수 있는데, 이는 코팅의 대다수가 고경도의 생체친화적인 특성을 가진데 착안되었으며, 흔히 현대성 질환이라 일컫는 과민성 체질, 과체중 및 허약체질 환자의 증가와 각종 재해 및 사고의 증가 및 인간 수명 증가에 따른 인공적인 시술의 요구증가에 편승하여 이 분야의 시장 또한 가파르게 성장하고 있다. 또한 대량으로 양산 적용단계에 접어든 자동차 핵심부품들을 비롯해서 각종 산업용, 방산용 기계 부품에도 성능 향상, 내구성 향상, 환경친화성 등 다양한 목적으로 확대 적용되고 있는 사례들을 본 발표를 통해 간략하게나마 소개하고자 한다.
Kim, Jong-Guk;Gang, Yong-Jin;Kim, Do-Hyeon;Jang, Yeong-Jun
Proceedings of the Korean Institute of Surface Engineering Conference
/
2017.05a
/
pp.91-91
/
2017
트라이볼로지란? 상대운동을 하면서 서로 영향을 미치는 두면 및 이와 관련된 문제로 마찰, 마모, 윤활에 대한 것을 말한다. 트라이볼로지는 1960대에 조사 연구되기 시작하면서 학문적으로 많은 정리가 이루어졌고, 현재 현대사회에서 문제가 되고 있는 에너지 및 환경 문제를 해결할 수 있는 핵심 요소로 떠오르고 있다. 특히 4차 산업혁명시대를 맞이하여 많은 부분에서는 인공지능, 클라우딩, 빅 데이터 및 로봇 등을 이야기하고 이에 대한 투자 및 개발을 이야기하고 있지만, 이 4차 산업을 뒷받침할, 강인한 제조업이 없으면 불가능한 혁명이라고 말 할 수 있다. 특히 트라이볼로지는 제조업의 무인 자동화 및 무인 로봇 등 이를 필요로 하는 산업 기기와 같은 전반적인 부품 및 소재의 마모를 감소시켜, 기계 장치의 신뢰성을 증가시킬 수 있다. 마찰은 두 물체 상호간의 열 발생을 억제 시키고, 마모는 물체의 표면 경도가 높으면 높을수록 마모량이 적어진다고 알려져있다. 따라서 트라이볼로지와 관련한 표면 처리의 경우, 고온 환경에서의 사용성 증대 및 고경도화 그리고 저마찰을 위한 방향으로 개발 발전되어져 왔다. 트라이볼로지 코팅 중 내마모 코팅의 경우, 티타늄 원소를 기본으로 알루미늄(Al) 및 실리콘(Si)를 합금화하면서, 고경도화 및 내열성을 증대시키는 방향으로 발전되어 왔다. 그에 따라 표면경도의 경우, 4000 Hv, 내열성 $1200^{\circ}C$에 도달였다. 하지만 여전히 철계와의 마찰계수는 0.3 이상으로 이를 낮추는 방법이 요구되고 있다. 최근 트라이볼로지 코팅 중 카본을 함유한 비정질 다이아몬드상 카본 막 (Diamond like Carbon Film : DLC) 이나, Diamond 막의 수요 증가는 마찰을 낮추어 융착마모를 줄이려는 노력으로 볼 수 있다. 특히 수소를 포함하지 않는 고경도 탄소막인 ta-C(tetrahedral amorphous-Carbon)의 수요는 증대되고 있으며, 이에 대한 후막화 및 양산화 기술의 개발의 현재 isssu로 대두되고 있다.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2018.06a
/
pp.75-75
/
2018
Commercially pure titanium (CP-Ti) and Ti-6Al-4V alloys have been widely used in implant materials such as dental and orthopedic implants due to their corrosion resistance, biocompatibility, and good mechanical properties. However, surface modification of titanium and titanium alloys is necessary to improve osseointegration between implant surface and bone. Especially, when titanium oxide nanotubes are formed on the surface of titanium alloy, cell adhesion is greatly improved. In addition, plasma electrolytic oxide (PEO) coatings have a good safety for osseointegration and can easily and quickly form coatings of uniform thickness with various pore sizes. Recently, the effects of bone element such as magnesium, zinc, strontium, silicon, and manganese for bone regeneration are researching in dental implant field. The purpose of this study was researched on the surface morphology of PEO-treated Ti-6Al-4V alloy after anodic titanium oxide treatmentusing various instruments. Ti-6Al-4V ELI disks were used as specimens for nanotube formation and PEO-treatment. The solution for the nanotube formation experiment was 1 M $H_3PO_4$ + 0.8 wt. % NaF electrolyte was used. The applied potential was 30V for 1 hours. The PEO treatment was performed after removing the nanotubes by ultrasonics for 10 minutes. The PEO treatment after removal of the nanotubes was carried out in the $Ca(CH_3)_2{\cdot}H_2O+(CH_3COO)_2Mg{\cdot}4H_2O+Mn(CH_3COO)_2{\cdot}4H_2O+Zn(CH_3CO_2)_2Zn{\cdot}2H_2O+Sr(CH_2COO)_2{\cdot}0.5H_2O+C_3H_7CaO_6P$ and $Na_2SiO_3{\cdot}9H_2O$ electrolytes. And the PEO-treatment time and potential were 3 minutes at 280V. The morphology changes of the coatings on Ti-6Al-4V alloy surface were observed using FE-SEM, EDS, XRD, AFM, and scratch tester. The morphology of PEO-treated surface in 5 ion coating solution after nanotube removal showed formation or nano-sized mesh and micro-sized pores.
An experimental study on effect of vapor-cooled heat stations in a 5.5 liter cryogenic vessel has been performed. The cryogenic vessel is made of stainless steel of thickness of 1mm and insulated by the combined insulation of vacuum, MLI(multi-layer insulation) and vapor-cooled radiation shield. Vapor-cooled heat stations are also constructed based on the 1-dimensional thermal analysis to reduce the heat inleak through a filling tube. Thermal analysis indicates that the vapor-cooled heat stations can substantially enhance the performance of vessel for cryogenic fluids with high $C_p/h_{fg}$ where $C_p$ the specific heat and $h_{fg}$ the heat of vaporization, such as $LH_2$ and LHe. The experimental results for $LN_2$ shows that the total heat inleak into inner vessel consists of 14% radiation and 86% conduction through the filling tube. Therefore, it is expected that the conduction heat in leak of the vessel for high $C_p/h_{fg}$ cryogenic fluids can be significantly reduced. powders. The amount of copper coating was 20wt%. In order to examine corrosion behavior of the electrodes, the corrosion current and the current density, in 6M KOH aqueous solution after removal of oxygen in the solution, were measured by potentiodynamic and cyclic voltamo methods. The results showed that Co in the alloy increased corrosion resistance of the electrode whereas Ni decreased the stability of the electrode during the charge-discharge cycles. The electrode used Si sealant as a binder showed a lower corrosion current density than the electrode used PTFE and the electrode used Cu-coated alloy powders showed the best corrosion resistance.
Kim, S.M.;Lee, T.H.;Kang, S.J.;Cho, Y.H.;Koo, J.M.
Journal of the Korean Society for Heat Treatment
/
v.24
no.4
/
pp.209-216
/
2011
Surface coatings were prepared on SKD11 core mold steel by plasma electrolytic oxidation (PEO). The coatings were investigated about the formation condition of core mold steel. SKD11 were coated by PEO in a mix solution of Sodium Aluminate $NaAlO_2$ (10 g/l), Sodium Silicate powder $Na_2SiO_3$ (0.5 g/l), Sodium tungstate dihydrate $Na_2WO_42H_2O$ (0.5 g/l) at less than $30^{\circ}C$. The electrical condition were voltage : 500~600 V; Pulse : 600~1800 Hz; current density 15~20 $A/dm^2$ various time : 3 min~40 min. The coatings surface morphology, cross-section, friction coefficient, hardness were investigated. The PEO coatings on SKD11 core mold steel showed the extended service life.
To improve ferroelectric properties of PZT, many studies have attempted to fabricate dense PZT films. The AD process has an advantage for forming dense ceramic films at room temperature without any additional heat treatment in low vacuum. Thick films coated by AD have a higher dielectric breakdown strength due to their higher density than those coated using conventional methods. To improve the breakdown strength, glass (SiO2-Al2O3-Y2O3, SAY) is mixed with PZT powder at various volume ratios (PZT-xSAY, x = 0, 5, 10 vol%) and coating films are produced on silicon wafers by AD method. Depending on the ratio of PZT to glass, dielectric breakdown strength and energy storage efficiency characteristics change. Mechanical impact in the AD process makes the SAY glass more viscous and fills the film densely. Compared to pure PZT film, PZT-SAY film shows an 87.5 % increase in breakdown strength and a 35.3 % increase in energy storage efficiency.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.