Study on the Superplasticity in Al-Li Alloy Systems (AI-Li계 합금의 초소성에 관한 연구)

  • Jin, Y.C.;Kook, J.S.;Kim, Y.S.;Hong, E.S.;Lee, M.S.;Lee, M.H.;Yoo, C.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.5 no.1
    • /
    • pp.41-49
    • /
    • 1992
  • The effects of alloying elements on the superplastic properties of Al-Li based alloys had been investigated. The intermediate thermo-mechanical treated (ITMT) Al-2.0wt%Li, Al-2.0wt%Li-1.0wt%Mg, Al-2.0wt%Li-0.12wt%Zr and Al-2.0wt%Li-1.2wt%Cu-1.0wt%Mg-0.12wt%Zr alloys were tested in tension at various temperature (400, 450, 500 and $550^{\circ}C$) and strain rate($6.7{\times}10^{-3}$, $1.0{\times}10^{-2}$, $1.6{\times}10^{-2}$ and $5.0{\times}10^{-2}/sec$). The results were as follows : The superplasticity in binary, ternary and pentanary alloys appeared at 500 to $550^{\circ}C$, and good strain rate for superplasticity. $1.6{\times}10^{-2}/sec{\sim}1.0{\times}10^{-2}/sec$ for a binary alloy and $1.0{\times}10^{-2}/sec{\sim}6.7{\times}10^{-3}/sec$ for ternary and pentanary alloys. A Zr-added ternary alloy had best value of elongation (730%) in four alloys at $550^{\circ}C$ of tension temperature and $1.0{\times}10^{-2}/sec$ of strain rate. The strain rate was greatly dependent on tension temperature and true strain rate was more than 1.0 at all test temperature and strain rate. In binary and Mg-added teranry alloys. the necks were slightly formed and their fracture surface had lips shape, but Zr-added ternary and pentanary alloy fractured along the grain boundary without necking. Their dislocations moved to grain boundary during superplasticity deformation and arranged perpendicular to grain boundary. Super plastic deformation was made by grain boundary slip of dislocation slip creep and model of core and mantle.

  • PDF

Aging Behaviors of a Rapidly Solidified AI-Li-Cu Alloy (급냉응고된 Al-Li-Cu 합금의 시효거동)

  • Hong, Y.J.;Kim, S.H.;Kang, M.C.;Kim, I.B.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.6 no.3
    • /
    • pp.138-143
    • /
    • 1993
  • Effects of aging treatment on the microstructural evolution of a rapidly solidified Al-Li-Cu alloy were investigated by differential scanning calorimetry (DSC) and transmission electron microscopy(TEM). It was found that the precipitation sequence was: supersaturated solid solution ${\alpha}^{\prime}$ ${\rightarrow}$ metastable ${\delta}^{\prime}$ + stable precipitate $T_1$ ${\rightarrow}$ stable precipitates ${\delta}+T_1$. Two exothermic and two endothermic peaks are detected by DSC analysis. The two exothermic and endothermic peaks corresponded to ${\delta}^{\prime}$ and ${\delta}+T_1$ precipitation and dissolution reactions respectively. The enthalpy of ${\delta}^{\prime}$ precipitation decreased with increasing of aging temperature and time until the finishing point of precipitation. The activation energy for precipitation of ${\delta}^{\prime}$ was measured as 80KJ/mol and the energy for dissolution was 93KJ/mol. These values arc higher than those of AI-Li binary alloy. Peak hardness value (Hv 170) was obtamed at $210^{\circ}C$ for 1hr aging treatment which coincided with finishing point of ${\delta}^{\prime}$ precipitation.

  • PDF

Roles of Fundamental and Additional Hardening Precipitates on the Changes of Mechanical Properties and Electrical Resistivity in Al-Li Alloys Containing Cu and Mg (Cu, Mg을 함유한 Al-Li 합금의 기계적 성질과 전기저항 변화에 미치는 기본 및 추가 강화상들의 역할)

  • Chung, D.S.;Song, K.H.;Woo, K.D.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.7 no.2
    • /
    • pp.77-87
    • /
    • 1994
  • Roles of fundamental and additional hardening precipitates on the changes of mechanical properties and electrical resistivity during precipitation decomposition in binary Al-Li, ternaty Al-Li-Cu and multi-Li-Cu-Mg-Zr alloys have been investigated by the detailed measurement of electrical resistivity, hardness and tensile strength and the observation of transmission electron micrographs. Peek hardness and tensile strength in multi-component Al-Li-Cu-Mg-Zr Alloy had higher than that of the other alloys and the results of measurement of hardness, strength and electrical resistivity in each alloys aged at 90 and $190^{\circ}C$, precipitation behaviors and mechanical properties in binary, ternary and multi-component Al-Li alloys were contributed to the ${\delta}^{\prime}$ precursory phase of ${\delta}^{\prime}$, $T_1$, G.P.B. zone and S' phases, repectively.

  • PDF

A Study on RF High Power Durability of Al-Cu Alloy Electrodes Used in Ladder-type SAW(surface acoustic wave) Filters (Al-Cu 합금 전극막 구조를 갖는 사다리형 SAW filter의 RF-고전력 내구성 특성 고찰)

  • 김남철;이기선;서수정;김지수;김윤동
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.5
    • /
    • pp.435-443
    • /
    • 2001
  • As power durable RF SAW filters, AL-(0∼2wt%)Cu alloy multi-layered thin electrodes were deposited on 42° LiTaO$_3$ piezoelectric substrates by magnetron sputtering process, and then ladder-type RF SAW filters, satisfying the electrical specification of CDMA transmission band, were fabricated through optimizing SAW resonator structures. The temperature of film electrodes in SAW filter was increased with RF power, and reached the maxima to cause a failure of SAW filters at the cut-off frequencies of the RF filter band. As RF power increases, the electrodes of Al-Cu alloy showed higher power durability than that of pure Al. The multi-layer laminated film of Al-1wt.% Cu/Cu/Al-1wt%Cu resulted in the best power durability up to 4W of RF power. Every film electrode, however, was destroyed within seconds whenever applying a critical RF power to SAW filters, regardless of the composition and structure of film electrodes. The breakdown of film electrodes under FR power seems to believe due to the fatigue of electrodes caused by repetitive cyclic stress of surface acoustic wave, which is amplified as RF power increases.

  • PDF

A Study on the Effect of Modifiers Affecting the Modification of the Al-Si Alloys (Al-Si 합금의 개량화에 미치는 각종 개량화제의 영향에 관한 연구)

  • Park, Joon-Peuo;Kim, Kyoung-Min;Cho, Soon-Hyung;Yoon, Eui-Park
    • Journal of Korea Foundry Society
    • /
    • v.11 no.4
    • /
    • pp.314-322
    • /
    • 1991
  • In this study, Na, Li, Sb, Sr were added as the modifiers to improve the mechanical proper ties of Al-Si alloys and their effects were compared one another Thermal analysis was carried out to measure the degree of undercooling, that is, the basic mechanism of modifying effect. The measurements of holding time and analyses of components of Al-Si alloys were carried out to compare the fading of the modifiers. Greater degree of undercooling was measured from the modified alloy than the normal alloys. In the modified alloy, the shape of Si was changed into a fine fiber phase or a lamellar phase from the coarse plate phase. There are not modifying effect of Sb below the $1.5^{\circ}C$ /sec of cooling rate. As the cooling rate increases, similar effects appears in the non-modified alloys like the modified alloys. Na and Li were faded in short time and were difficult to control on the melt, but Sb and Sr were scarcely faded for 6 hours of holding and were easy to control on the melt. Na and Sr are the good modifiers in terms of microstructure. Sb is the best modifier, but Na, Li are the inadequate modifiers in terms of fading.

  • PDF

Effects of Porous Microstructure on the Electrochemical Properties of Si-Ge-Al Base Anode Materials for Li-ion Rechargeable Batteries (리튬이차전지용 다공성 Si-Ge-Al계 음극활물질의 전기화학적 특성)

  • Cho, Chung Rae;Kim, Myeong Geun;Sohn, Keun Yong;Park, Won-Wook
    • Journal of Powder Materials
    • /
    • v.24 no.1
    • /
    • pp.24-28
    • /
    • 2017
  • Silicon alloys are considered promising anode active materials to replace Li-ion batteries by graphite powder, because they have a relatively high capacity of up to 4200 mAh/g, and are environmentally friendly and inexpensive ECO-materials. However, its poor charge/discharge properties, induced by cracking during cycles, constitute their most serious problem as anode electrode. In order to solve these problems, Si-Ge-Al alloys with porous structure are designed as anode alloy powders, to improve cycling stability. The alloys are melt-spun to obtain the rapidly solidified ribbons, and then ball-milled to make fine powders. The powders are etched using 1 M HCl solution, which gives the powders a porous structure by removing the element Al. Subsequently, in this study, the microstructures and the characteristics of the etched powders are evaluated for application as anode materials. As a result, the etched porous powder shows better electrochemical properties than as-milled Si-Ge-Al powder.

Li:Al cathode layer and its influence on interfacial energy level and efficiency in polymer-based photovoltaics

  • Park, Sun-Mi;Jeon, Ji-Hye;Park, O-Ok;Kim, Jeong-Won
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.08a
    • /
    • pp.72-72
    • /
    • 2010
  • Recent development of organic solar cell approaches the level of 8% power conversion efficiency by the introduction of new materials, improved material engineering, and more sophisticated device structures. As for interface engineering, various interlayer materials such as LiF, CaO, NaF, and KF have been utilized between Al electrode and active layer. Those materials lower the work function of cathode and interface barrier, protect the active layer, enhance charge collection efficiency, and induce active layer doping. However, the addition of another step of thin layer deposition could be a little complicated. Thus, on a typical solar cell structure of Al/P3HT:PCBM/PEDOT:PSS/ITO glass, we used Li:Al alloy electrode instead of Al to render a simple process. J-V measurement under dark and light illumination on the polymer solar cell using Li:Al cathode shows the improvement in electric properties such as decrease in leakage current and series resistance, and increase in circuit current density. This effective charge collection and electron transport correspond to lowered energy barrier for electron transport at the interface, which is measured by ultraviolet photoelectron spectroscopy. Indeed, through the measurement of secondary ion mass spectroscopy, the Li atoms turn out to be located mainly at the interface between polymer and Al metal. In addition, the chemical reaction between polymer and metal electrodes are measured by X-ray photoelectron spectroscopy.

  • PDF

Hot Corrosion Behavior of Al-Y Coated Haynes 263 in Lithium Molten Salt under Oxidation Atmosphere (리튬용융염계 산화성분위기에서 Al-Y 코팅한 Haynes 263의 고온 부식거동)

  • Cho Soo-Hang;Lim Jong-Ho;Chung Jun-Ho;Seo Chung-Seok;Park Seoung-Won
    • Korean Journal of Materials Research
    • /
    • v.15 no.3
    • /
    • pp.155-160
    • /
    • 2005
  • The electrolytic reduction of spent oxide fuel involves the liberation of oxygen in a molten LiCl electrolyte, which results in a chemically aggressive environment that is very corrosive fir typical structural materials. So, it is essential to choose the optimum material f3r the process equipment handling molten salt. In this study, the corrosion behavior of Al-Y coated Haynes 263 in a molten salt of $LiCl-Li_2O$ under oxidation atmosphere was investigated at $650^{\circ}C$ for $72\~168$ hours. The corrosion rate of Al-Y coated Haynes 263 was low while that of bare Haynes 263 was high in a molten salt of $LiCl-Li_2O$. Al-Y coated Haynes 263 improved the corrosion resistance better than bare Haynes 263 alloy. An Al oxide layer acts as a protective film which Prohibits Penetration of oxygen. Corrosion Products were formed $Li(Ni,Co)O_2$ and $LiTiO_2$ on bare Haynes 263, but $LiAlO_2,\;Li_5Fe_5O_8\;and\;LiTiO_2$ on Al-Y coated Haynes 263.