• 제목/요약/키워드: Al doping

검색결과 339건 처리시간 0.029초

인광재료를 이용한 고효율 적색 유기발광 다이오드에 관한 연구 (A Study on the High-Efficiency Red OLEDs using Phosphorescent Materials)

  • 심주용;전현성;조재영;정진하;윤석범;강명구;오환술
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.428-429
    • /
    • 2006
  • In this thesis, verifies electrical-optical characteristics of phosphorescent materials. basic structure of fabricating devices is glass/ITO/$\alpha$-NPD($300{\AA}$)/CBP:Guest($300{\AA}$)/BCP($80{\AA}$)/$Alq_3(100{\AA})$/Al($1000{\AA}$). In efficiency, fabrication of organic light emitting diodes using $Ir(btp)_2acac$ phosphorescent material is external quantum efficiency 0.268% as doping concentration 3%. At CIE coordinates, phosphorescent material $Ir(btp)_2acac$ following materials moves high purity red color(x=0.6686, y=0.3243). The brightness shows $285cd/cm^2$.

  • PDF

Li:ZnO를 이용하여 제조한 FBAR의 열처리 온도에 따른 주파수 특성 (Frequency characteristics of Li doped ZnO thin film resonator annealed by various temperatures)

  • 김봉석;김응권;황현석;강현일;이규일;이태용;송준태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.309-310
    • /
    • 2006
  • In this paper, frequency characteristic of FBAR was studied as a function of annealing temperature. we have used Li dopant to enhance electrical properties of ZnO thin film. Li:ZnO thin film was deposited on Al(300 nm)/$SiO_2$(500 nm)/Si($500\;{\mu}m$) and each layer was patterned. Thermal treatment was executed in range of between 300 and $600^{\circ}C$ in $O_2$ ambient. We observed that the resistivity of ZnO is enhanced under the influence of Li doping and return loss in FBAR frequency properties is improved through annealing.

  • PDF

A study of Physically Implanted Surface Islands by direct Nd:YAG Laser Beam Irradiation

  • Oh, Chang-Heon;Cheon, Suyoung;Lim, Changjin;Lee, Jeongjun;Jeon, Jihyun;Kim, Kyoung-Kook;Chung, Chan-Moon;Cho, Soohaeng
    • Applied Science and Convergence Technology
    • /
    • 제26권4호
    • /
    • pp.66-69
    • /
    • 2017
  • Physically implanted surface islands of Nano Carbon Tube (NCT) and ${\alpha}-F_2O_3$ particles have been produced on Al-doped ZnO (AZO)/glass surfaces by simple and direct ND:YAG laser beam irradiation. Sheet resistance of the reconstructed surface increased by about 3.6% of over AZO. Minimal surface damage can be repaired by ND:YAG laser beam irradiation in conjunction with proper impurities. Implanted islands of NCT, which are considered to be a good conductive impurity, on AZO increased the sheet resistance by about 1.8%, while implanted islands of ${\alpha}-F_2O_3$, an insulating impurity, on AZO increased sheet resistance by about 129% compared with a laser beam treated AZO. This study provides insight regarding surface implantations of nanowires and micro-circuits, doping effects for semiconductors and optical devices, surface area and impurity effects for catalysis.

Investigation of Polypyrrole Coatings Containing Nanosized Metal Oxides for Corrosion Protection of AA2024 Al Alloy

  • Fekri, F.;Shahidi, M.;Foroughi, M.M.;Kazemipour, M.
    • Journal of Electrochemical Science and Technology
    • /
    • 제10권2호
    • /
    • pp.148-158
    • /
    • 2019
  • The corrosion protection of AA2024 PPy coated samples doping with nanosized metal oxides, including $TiO_2$ and $CeO_2$ nanoparticles and $Nd_2O_3$ nanorods, during exposure to the solutions of 0.1 M $H_2SO_4$ and 3.5% NaCl was evaluated by electrochemical impedance spectroscopy (EIS) and linear polarization resistance (LPR) techniques. The nanorods of $Nd_2O_3$ were synthesized by cathodic pulse electrochemical deposition technique. The barrier properties of the different PPy coatings containing nanosized metal oxides immersed in $H_2SO_4$ solution were ranked as follows: $Nd_2O_3$ > $TiO_2$ > $CeO_2$. Therefore, the $Nd_2O_3$ coating sample provided the highest corrosion protection at any time of immersion up to 72 hours after immersing in $H_2SO_4$ solution. On the other hand, the $CeO_2$ coating sample displayed the best anticorrosive properties among the other coating samples after immersion in NaCl solution up to 28 days. This is due to the inhibition effect of cerium ions on aluminum alloys at near-neutral solutions.

TFA-MOD 방법에 의한 YBCO 박막제조에서 nano size $Y_2O_3$ 첨가효과 (Effect of nano size $Y_2O_3$ addition on the superconducting properties and microstructure of YBCO thin film prepared by TFA-MOD method.)

  • 박진아;김병주;홍계원;이희균;유재무;김영국
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제8권3호
    • /
    • pp.13-17
    • /
    • 2006
  • The effect of the addition of the nano size $Y_2O_3$ powder on the microstructurte and superconducting properties of YBCO thin film deposited on LAO single crystalline substrate by TFA-MOD method was studied. Nano size $Y_2O_3$ powder was added to the stoichiometric precursor solution with a cation ratio of Y : Ba . Cu = 1 : 2 : 3 prepared using TFA as chelating agent. Precursor solutions with and without $Y_2O_3$ addition were coated on $LaAlO_3(100)$ single crystalline substrates by dip coating method. Calcination and conversion heat treatments were performed in controlled atmosphere containing moisture Current carrying capacity(Jc) of YBCO film was enhanced about 50% by $Y_2O_3$ doping and it is thought to be due to the better connectivity of YBCO grains and/or the flux pinning by the $Y_2O_3$ particles embedded in YBCO grains.

Excimer-Based White Phosphorescent OLEDs with High Efficiency

  • Yang, Xiaohui;Wang, Zixing;Madakuni, Sijesh;Li, Jian;Jabbour, Ghassan E.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.1520-1521
    • /
    • 2008
  • There are several ways to demonstrate white organic light emitting diodes (OLEDs) for displays and solid state lighting applications. Among these approaches are the stacked three primary or two complementary colors light-emitting layers, multiple-doped emissive layer, and excimer and exciplex emission [1-10]. We report on white phosphorescent excimer devices by using two light emitting materials based on platinum complexes. These devices showed a peak EQE of 15.7%, with an EQE of 14.5% (17 lm/W) at $500\;cd/m^2$, and a noticeable improvement in both the CIE coordinates (0.381, 0.401) and CRI (81). Devices with the structure ITO/PEDOT:PSS/TCTA (30 nm)/26 mCPy: 12% FPt (10 nm) /26 mCPy: 2% Pt-4 (15 nm)/BCP (40 nm)/CsF/Al [device 1], ITO/PEDOT:PSS/TCTA (30 nm)/26 mCPy: 2% Pt-4 (15 nm)/26 mCPy: 12% FPt (10 nm)/BCP (40 nm)/CsF/Al [device 2], and ITO/PEDOT:PSS/TCTA (30 nm)/26 mCPy: 2% Pt-4: 12% FPt (25 nm)/BCP (40 nm)/CsF/Al [device 3] were fabricated. In these cases, the emissive layer was either the double-layer of 26 mCPy:12% FPt and 15 nm 26 mCPy: 2% Pt-4, or the single layer of 26mCPy with simultaneous doping of Pt-4 and FPt. Device characterization indicates that the CIE coordinates/CRI of device 2 were (0.341, 0.394)/75, (0.295, 0.365)/70 at 5 V and 7 V, respectively. Significant change in EL spectra with the drive voltage was observed for device 2 indicating a shift in the carrier recombination zone, while relatively stable EL spectra was observed for device 1. This indicates a better charge trapping in Pt-4 doped layers [10]. On the other hand, device 3 having a single light-emitting layer (doped simultaneously) emitted a board spectrum combining emission from the Pt-4 monomer and FPt excimer. Moreover, excellent color stability independent of the drive voltage was observed in this case. The CIE coordinates/CRI at 4 V ($40\;cd/m^2$) and 7 V ($7100\;cd/m^2$) were (0.441, 0.421)/83 and (0.440, 0.427)/81, respectively. A balance in the EL spectra can be further obtained by lowering the doping ratio of FPt. In this regard, devices with FPt concentration of 8% (denoted as device 4) were fabricated and characterized. A shift in the CIE coordinates of device 4 from (0.441, 0.421) to (0.382, 0.401) was observed due to an increase in the emission intensity ratio of Pt-4 monomer to FPt excimer. It is worth noting that the CRI values remained above 80 for such device structure. Moreover, a noticeable stability in the EL spectra with respect to changing bias voltage was measured indicating a uniform region for exciton formation. A summary of device characteristics for all cases discussed above is shown in table 1. The forward light output in each case is approximately $500\;cd/m^2$. Other parameters listed are driving voltage (Bias), current density (J), external quantum efficiency (EQE), power efficiency (P.E.), luminous efficiency (cd/A), and CIE coordinates. To conclude, a highly efficient white phosphorescent excimer-based OLEDs made with two light-emitting platinum complexes and having a simple structure showed improved EL characteristics and color properties. The EQE of these devices at $500\;cd/m^2$ is 14.5% with a corresponding power efficiency of 17 lm/W, CIE coordinates of (0.382, 0.401), and CRI of 81.

  • PDF

Synthesis of Nano-Sized Y3Al5O12:Ce3+ Phosphors Prepared by High Energy Beads Milling Process and Their Luminescence Properties

  • Song, Hee-Jo;Kim, Dong-Hoe;Park, Jong-Hoon;Han, Byung-Suh;Hong, Kug-Sun
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.386-386
    • /
    • 2012
  • For white light emitting diode (LED) applications, it has been reported that Y3Al5O12:Ce3+ (YAG:Ce) in nano-sized phosphor performs better than it does in micro-sized particles. This is because nano-sized YAG:Ce can reduce internal light scattering when coated onto a blue LED surface. Recently, there have been many reports on the synthesis of nano-sized YAG particles using bottom-up method, such as co-precipitation method, sol-gel process, hydrothermal method, solvothermal method, and glycothermal method. However, there has been no report using top-down method. Top-down method has advantages than bottom-up method, such as large scale production and easy control of doping concentration and particle size. Therefore, in this study, nano-sized YAG:Ce phosphors were synthesized by a high energy beads milling process with varying beads size, milling time and milling steps. The beads milling process was performed by Laboratory Mill MINICER with ZrO2 beads. The phase identity and morphology of nano-sized YAG:Ce were characterized by X-ray powder diffraction (XRD) and field-emission scanning electron microscopy (FESEM), respectively. By controlling beads size, milling time and milling steps, we synthesized a size-tunable and uniform nano-sized YAG:Ce phosphors which average diameters were 100, 85 and 40 nm, respectively. After milling, there was no impurity and all of the peaks were in good agreement with YAG (JCPDS No. 33-0040). Luminescence and quantum efficiency (QE) of nano-sized YAG:Ce phosphors were measured by fluorescence spectrometer and QE measuring instrument, respectively. The synthesized YAG:Ce absorbed light efficiently in the visible region of 400-500 nm, and showed single broadband emission peaked at 550 nm with 50% of QE. As a result, by considering above results, high energy beads milling process could be a facile and reproducible synthesis method for nano-sized YAG:Ce phosphors.

  • PDF

Short Channel SB-FETs의 Schottky 장벽 Overlapping (Schottky barrier overlapping in short channel SB-MOSFETs)

  • 최창용;조원주;정홍배;구상모
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.133-133
    • /
    • 2008
  • Recently, as the down-scailing of field-effect transistor devices continues, Schottky-barrier field-effect transistors (SB-FETs) have attracted much attention as an alternative to conventional MOSFETs. SB-FETs have advantages over conventional devices, such as low parasitic source/drain resistance due to their metallic characteristics, low temperature processing for source/drain formation and physical scalability to the sub-10nm regime. The good scalability of SB-FETs is due to their metallic characteristics of source/drain, which leads to the low resistance and the atomically abrupt junctions at metal (silicide)-silicon interface. Nevertheless, some reports show that SB-FETs suffer from short channel effect (SCE) that would cause severe problems in the sub 20nm regime.[Ouyang et al. IEEE Trans. Electron Devices 53, 8, 1732 (2007)] Because source/drain barriers induce a depletion region, it is possible that the barriers are overlapped in short channel SB-FETs. In order to analyze the SCE of SB-FETs, we carried out systematic studies on the Schottky barrier overlapping in short channel SB-FETs using a SILVACO ATLAS numerical simulator. We have investigated the variation of surface channel band profiles depending on the doping, barrier height and the effective channel length using 2D simulation. Because the source/drain depletion regions start to be overlapped each other in the condition of the $L_{ch}$~80nm with $N_D{\sim}1\times10^{18}cm^{-3}$ and $\phi_{Bn}$ $\approx$ 0.6eV, the band profile varies as the decrease of effective channel length $L_{ch}$. With the $L_{ch}$~80nm as a starting point, the built-in potential of source/drain schottky contacts gradually decreases as the decrease of $L_{ch}$, then the conduction and valence band edges are consequently flattened at $L_{ch}$~5nm. These results may allow us to understand the performance related interdependent parameters in nanoscale SB-FETs such as channel length, the barrier height and channel doping.

  • PDF

증착 환경 변화에 따른 인이 첨가된 ZnO 박막의 물성연구

  • 정영의;이승환;황선민;조창우;배종성;박성균
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.299-299
    • /
    • 2012
  • 투명전도산화물 박막은 디스플레이, 태양전지, 압전소자 등 다양한 응용분야에 많이 이용되고 있는 소재이다. 그 중에서 현재 산업에서 활용 빈도가 높은 투명전도막의 재료는 ITO를 기반으로 하는 물질이다. 하지만 인듐의 높은 생산단가와 플라즈마 노출시 열화로 인한 문제점 때문에 기존의 ITO를 대체하기 위한 새로운 재료에 관심이 증대되고 있다. 본 연구에서는 대표적인 ITO 대체 물질 중의 하나인 ZnO 박막에 대해서 증착환경변화에 따른 물성변화를 조사하였다. 먼저 대기중에서 안정화된 ZnO 박막을 얻기 위해서 인(P) 2% 첨가된 ZnO 세라믹을 고상반응법으로 제작하고, 펄스레이저 증착법을 이용하여 Al2O3(0001)기판에 산소분압을 30~150 mTorr로 변화를 주어 P-ZnO 박막을 제작하였다. 이 때 증착온도는 $400^{\circ}C$로 고정하였다. X선 회절 결과로부터 산소분압에 상관없이 ZnO (002)방향으로 증착되었다. 하지만 결정립의 크기는 산소분압이 증가하면서 줄어들고, ZnO (002)피크로부터 얻어진 격자상수(c-축)는 벌크 값에 가까워짐을 알 수 있었다. 하지만 P첨가로 인해서 박막의 격자상수는 순수한 ZnO 벌크 값 보다 큰 것으로 알 수 있다. 산소분압 변화에 따른 P-ZnO 박막의 산화 상태는 X-선 광전자 분광기를 이용하여 측정하였다. 그 결과 산소 core-level의 스펙트럼은 자연산화, 산소 vacancy, Zn-O 결합으로 구성되어짐을 알 수 있었다. 산소분압이 증가하면 Zn-O 결합은 증가하지만 산소 vacancy는 감소함을 알 수 있었다. 전기적 특성 결과 P-ZnO 박막은 30 mTorr에서는 n형 반도체 특성, 100 mtorr에서 p형 반도체의 특성이 나타내었고, 산소분압이 증가하면 다시 n형 반도체 특성을 나타냄을 알 수 있었다. 광학적 특성 결과 P-ZnO 박막은 산소분압에 상관없이 가시광선 영역에서 80%이상의 투과율을 나타내었으며, 산소분압이 증가할수록 에너지 갭이 증가하였다.

  • PDF

TCNQ를 사용한 유기 발광 소자의 특성 변화 (Property change of organic light-emitting diodes using a TCNQ)

  • 나수환;이원재;홍진웅;정동회;한원근;김태완
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.275-276
    • /
    • 2009
  • We have studied physical properties of organic light-emitting diodes (OLEDs) in a device with 7,7,8,8-tetracyanoquinodimethane (TCNQ). Since the TCNQ has a high electron affinity, it is widely used for a charge-transport and injection layer. And the TCNQ-derivatives have also been used to control the conductivity of the materials. It is known that a charge injection and transport in OLEDs with a TCNQ-derivative enhances a performance of the devices such as operating voltage and efficiency. To see how the TCNQ affects on the device performance, we have made a reference device in a structure of ITO(170nm)/TPD(40nm)/$Alq_3$(60nm)/LiF(0.5nm)/Al(100nm). And several type of devices were manufactured by doping TCNQ either in TPD or $Alq_3$ layer. The TCNQ layer was also formed in between the organic layers. N,N'-diphenyl-N,N'-di(m-tolyl)-benzidine (TPD), tri(8-hydroxy quinoline) aluminium ($Alq_3$), and TCNQ layers were formed by thermal evaporation at a pressure of $10^{-6}$ torr. The deposition rate was $1.0{\sim}1.5\;{\AA}/s$ for TPD, and $1.0{\sim}1.5\;{\AA}$ for $Alq_3$. The LiF was thermally evaporated at a deposition rate of $0.2\;{\AA}/s$ successively. The device with TCNQ-derivative improved the turn-on voltage compared to the one without TCNQ-derivative.

  • PDF