Al 7075/CFRP Hybrid 복합재료의 파손특성에 대한 AE 특성 연구 (AE Characteristics for Fracture Mechanism of Al 7075/CFRP Hybrid Composite)

  • 이진경;이준현;송상헌;윤한기
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2001년도 춘계학술발표대회 논문집
    • /
    • pp.268-271
    • /
    • 2001
  • When compared to other composite materials such as FRP and MMC, hybrid composite material is more attractive one due to the high specific strength and the resistance to fatigue. However, the fracture mechanism of hybrid composite material is extremely complicated because of the bonding structure of metals and FRP. Recently, nondestructive technique has been used to evaluate the fracture mechanism of these composite materials. In this study, AE technique has been used to clarify the fracture mechanism and the degree of damage for Al 7075/CFRP hybrid composite material. It was found that AE event, energy and amplitude among AE parameters were effective to evaluate fracture process of Al 7075/CFRP composite material. In addition, the relationship between the AE signal and the characteristics of failure surface using optical microscope was discussed.

  • PDF

Al 7075/CFRP 샌드위치 복합재료의 강도 및 손상특성에 대한 비파괴 평가 (Nondestructive Evaluation on Strength Characteristic and Damage Behavior of Al 7075/CFRP Sandwich Composite)

  • 이진경;윤한기;이준현
    • 대한기계학회논문집A
    • /
    • 제26권11호
    • /
    • pp.2328-2335
    • /
    • 2002
  • A hybrid composite material has many potential usage due to the high specific strength and the resistance to fatigue, when compared to other composite materials such as fiber reinforced plastic(FRP) and metal matrix composite(MMC). However, the fracture mechanism of hybrid composite material is extremely complicated because of the bonding structure of metals and FRP. In this study, Al 7075 sheets and carbon epoxy preprags were used to fabricate the hybrid composite. Recently, nondestructive technique has been used to evaluate the fracture mechanism of these composite materials. AE technique was used to clarify the microscopic damage behavior and failure mechanism of A17075/CFRP hybrid composite. It was found that AE paralneters such as AE event, energy and amplitude were effective to evaluate the failure process of Al 7075/CFRP composite. In addition, the relationship between the AE signal and the characteristics of fracture surface using optical microscope was discussed.

Al/CFRP 하이브리드 복합재료의 인장파괴거동 (The Behavior of Tensile Fracture for Al/CFRP Hybrid Composite Material)

  • 강지웅;권오헌;유진규
    • 한국안전학회지
    • /
    • 제24권2호
    • /
    • pp.23-29
    • /
    • 2009
  • The hybrid composite materials are recently used in many field as an advanced material due to their high resistance to fracture. However, hybrid composite materials have several problems, especially delamination, compared with homogeneous materials such as an aluminum alloy, etc. In this study, we carried out the tensile test to study the tension failure appearances and tensile ultimate strength of CFRP/Al/CFRP hybrid composite materials. The CFRP material used in the experiment is a commercial material known as CU175NS in unidirectional carbon prepreg. Also Al/CFRP/Al hybrid composites with three kind length of a single edge crack were investigated for the relationship between an aluminium volume fraction and a crack length. The crack length was measured by a traveling microscope under a universal dynamic tester. Futhermore the stress intensity factor behavior was examined according to a volume fraction and an initial crack length ratio to a width.

Al 7075/CFRP 하이브리드 복합재료의 미시적 파괴특성에 대한 AE특성평가 (Evaluation of AR Characteristics on Microscopic Fracture Mechanism of A17075/CERP Hybrid Composite)

  • 이진경;이준현;윤한기
    • Composites Research
    • /
    • 제15권5호
    • /
    • pp.1-6
    • /
    • 2002
  • 하이브리드 복합재료는 FRP나 MMC와 같은 복합재료에 비하여 높은 비강도, 내피로 특성을 가지고 있기 때문에 많은 관심을 받고 있다. 그러나 하이브리드 복합재료는 금속과 FRP의 결합구조로 되어있기 때문에 매우 복잡한 파손기구를 가지고 있다. 최근에는 비파괴 기법을 이용하여 이러한 복합재료의 파손기구를 평가하고자 하는 연구가 수행되어지고 있다. 본 연구에서는 음향방출 기법을 이용하여 Al7075/CFRP 하이브리드 복합재료에 대한 손상정도 및 파손기구를 명확히 하고자 하였다. 특히 AE 사상수, 에너지, 진폭과 같은 AE 파라미터들은 Al7075/CFRP 하이브리드 복합재료의 파손과정을 평가하는데 효과적이었다. 더불어, 광학현미경을 이용하여 AE 신호와 시험편의 표면소상 특성과의 관계를 비교, 검토하였다.

Al 7075/CFRP 다적층 하이브리드 복합재료의 피로수명에 대한 연구 (A study on fatigue life of Al 7075/CFRP multilayered hybrid composite materials)

  • 윤한기;김연겸;박준수;이경봉
    • 한국해양공학회지
    • /
    • 제10권4호
    • /
    • pp.92-102
    • /
    • 1996
  • In this research, to develope the A1 7075/CFRP multilayered hybrid composites, CRALL(Carbon Reinforced aluminum lamiate) specimens were processed by autoclavecuring system that curing temperature, time, surface pretreatment condition of aluminum were constant. Andthe fatigye life and failure mechanism on CFRP volume fraction and fiber orientation of CRALLspecimens were investigated. A fatigue life was greatly influenced by effect of CFRP fiber volume fraction but it was less effected than those of fiber orientation. The fatigue failure arised from interface delamination of CFRP and aluminum sheet after shear fracture of aluminum layer. The failure mechanism is assumed that the aluminum laminates which divide the CFRP into many thim layers tend to arrest the failure propagation.

  • PDF

준정적 축 압축하중을 받는 Al/CFRP/GFRP 혼성부재의 에너지흡수 특성 (Energy Absorption Characteristics of the Al/CFRP/GFRP Hybrid Member under Quasi-static Axial Compressive Load)

  • 김선규;허욱;임광희;정종안
    • 한국생산제조학회지
    • /
    • 제21권4호
    • /
    • pp.588-592
    • /
    • 2012
  • This study concentrates the effect of hybridisation on the collapse mode and energy absorption for composite cylinders. The static collapse behavior of laminated(Al/CFRP/GFRP) circular-cylindrical composite shell under quasi-static axial compressive load has been investigated experimentally. Eight different hybrids of laminated(Al/CFRP/GFRP) circular-cylindrical composite shell were fabricated by autoclave. Eight types of composites were tested, namely, Al/carbon fiber/epoxy, Al/glass fiber/epoxy, Al/carbon-carbon-glass/epoxy, Al/carbon-glass-carbon/epoxy, Al/carbon-glass-glass/epoxy, Al/glass-glass-carbon/epoxy, Al/glass-carbon-glass/epoxy and Al/glass-carbon-carbon/epoxy. Collpase modes were highly dominated by the effect of hybridisation. The results also showed that the hybrid member with material sequence of Al-glass-carbon-carbon/epoxy exhibited good energy absorption capability.

Al5052/CFRP 복합소재의 표면특성이 접착성과 기계적특성에 미치는 영향 (Effect of Surface Roughness of Al5052/CFRP Composites on the Adhesion and Mechanical Properties)

  • 이민식;김현호;강충길
    • Composites Research
    • /
    • 제26권5호
    • /
    • pp.295-302
    • /
    • 2013
  • 본 연구에서는 차량용 Al5052/CFRP 복합재를 U-채널 몰드에서 컴프레션 몰딩 공정을 통해 제작하였다. Al5052는 샌드블라스팅을 통해 표면처리를 하였다. 표면처리를 하지 않은 판재와 표면거칠기(Ra)가 $1.85{\mu}m$ 및, $4.25{\mu}m$인 Al5052판재를 이용하여 실험을 수행하였다. 표면거칠기가 Al5052/CFRP 복합재의 접착성과 기계적 특성에 대한 영향을 전단시험과 굽힘실험을 통하여 평가하였다. 전단 시험에서는 표면거칠기가 $1.85{\mu}m$$4.25{\mu}m$ 시험편이 표면처리를 하지 않은 시험편보다 각각 3, 5배의 전단강도의 증가를 보였다. 굽힘시험에서는 표면처리를 하지 않았을 때 굽힘강도가 200 MPa에서 표면처리 후 400 MPa로 증가함을 알 수 있었다.

원통단면 탄소복합재와 혼성 구조부재의 굽힘 특성 평가 (Bending Characteristic Evaluations Circular Cross-section Carbon Composite and Hybrid Structural Material)

  • 김정호;정종안;김지훈
    • 한국생산제조학회지
    • /
    • 제21권3호
    • /
    • pp.421-424
    • /
    • 2012
  • Carbon Fiber reinforced composite material can be designed for the optimized performances of structural member that have achieve appropriate mechanical properties with cross-sectional shape, fiber direction, stacking sequence and thickness. So there are needed extensive databases each optimal design of CFRP structural member by impact through the preparation of different shape, interface number, thickness and stacking angle. When pressure is applied to structural member, compression, bending and torsion is shown on the corresponding member. For the effective utilization of fiber reinforced composite material as main structural member, optimized design technology should be established to maximize mechanical properties for compression, bending and torsion. In this paper, CFRP prepreg sheet with different stacking angle is manufactured in CFRP and hybrid(Al+CFRP) with circular cross-section. Strength and stiffness is gotten respectively by flexure test. CFRP structure and hybrid structure can be compared with each other. The best design guideline can be analyzed by use of this study result.

CFRP로 보강한 하이브리드 복합재료의 비파괴검사법을 이용한 피로균열 지연의 연구 (A Study on Fatigue Crack Retardation Using NDT Test in a Hybrid Composite Material Reinforced with a CFRP)

  • 윤한기;박원조;허정원
    • Composites Research
    • /
    • 제12권3호
    • /
    • pp.1-7
    • /
    • 1999
  • Al2024-T3 판재에 카본/에폭시(carbon/epoxy) 라미네이트를 섬유배열 방향 $0^{\circ}$/$90^{\circ}$$\pm$$45^{\circ}$로 2 Plies 보강하여 CPAL(Carbon Patched ALuminum alloy)재를 제작하고, 응력비 R=0.2, 0.5에서 피로균열전파 실험을 실시하였다. X-Ray와 초음파 C-Scan 장비를 이용하여 A/2024-T3 판재의 균열과 CFRP 라미네이트 박리 거동을 조사하여 피로균열 지연 거동과 지연기구(mechanism)를 연구하였다. A/2024-T3 시험편에 비해서 CPAL 시험편은 피로균열전파속도가 현저하게 지연되었으며, 지연 정도는 $0^{\circ}$/$90^{\circ}$ CPAL이 $\pm$$45^{\circ}$ CPAL 시험편보다 크고, 응력비 R=0.2에서 응력비 R=0.5보다 크게 나타났다. CPAL 시험편의 피로균열 지연 효과는 균열후방의 박리 및 비박리 CFRP 라미네이트가 A/2024-T3 판재의 균열열림(COD)을 감소시키는 균열브리징미케니즘(crack bridging medhanism) 때문에 발생함을 확인하였다.

  • PDF

자동차용 경량화 A17075 / CFRP 샌드위치 판넬의 강도와 충격손상 특성 (Strength and Impact Damage Characteristics of A17075/CFRP Sandwitch Pannel by Using Automobiles)

  • 윤한기;이종호;박이현;이제헌
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 추계학술대회 논문집
    • /
    • pp.295-300
    • /
    • 2002
  • To establish an optimum condition in the surface treatment and curing process will be an important parameters for the fabrication of multilayered hybrid composite materials, A17075/CFRP (CARALL : carbon fiber reinforce aluminum laminates). Effects of carbon fiber direction and thickness variation in tensile strength were investigated. And impact damage behavior of carbon fiber reinforce plastic (CFRP) and CARALL were investigated also, it was found that a partial stress increase in order of epoxy adhesive, A17075, CFRP. And the partial stress of CFRP carried out a great portion of applied stress. The impact damage resistance of CARALL was higher than that of CFRP. This is because both side Al sheet of CARALL absorb a great of impact damage.