For this research, prepared water soluble milk casein resin and waterborne polyurethane-acrylic resin. Use these resin, this article has been analyzed about change of mechanical properties by increasing amount of casein resin in polyurethane-acrylic resin on coated leather. According to measure data for solvent resistance, WPA(waterborne polyurethane-acrylic resin) resin and WPA-C1, C2, C3(samples of polyurethane-acrylic resin with milk casein resin) had good property. As known in the results, increase of casein constant did not influence to big change of hybrid resin properties. As test of tensile strength, WPA had lowest tensile characteristic(1.598 $kg_f/mm^2$) and WPA-C3 had highest tensile characteristic(1.718 $kg_f/mm^2$). Also best properties of abrasion was WPA-C3(06.021 mg.loss). In elongation case, WPA had best properties(754 %) in this experiment.
자가중합형 아크릴릭 레진에 polyp를 혼합하지 않은 대조군, 그리고 레진 분말에 대한 polyP(사슬길이 13과 18의 혼합물인 Calgon)의 무게비를 1%로 혼합한 polyP 1%군, 2% 혼합한 polyP 2%군 및 3% 혼합한 polyP 3%군으로 분류하여 경화시킨 후, 경화된 각각의 레진과 실험균주 S. mutans GS5, S. sobrinus 6715, S. gordonii G9B및 Challis, 그리고 P. gingivalis 2561과 Candida albicans ATCC90027을 대상으로 레진표면에 대한 미생물들의 부착의 정도, 성장 억제효과 및 접촉각의 변화를 관찰하여 그 결과로 미루어 아크릴릭 레진에 포함된 polyP는 구강 미생물에 대해 직접적으로 강한 항균 효과를 나타내지는 않는 것으로 판단되나 미생물의 부착 특히 우식원인균인 mutans streptococci의 부착을 방해하는 것으로 가늠되며, 이는 polyP의 첨가에 의한 아크릴릭 레진 표면에서 일어난 소수성의 변화가 일부 관여하는 것으로 여겨진다. PolyP가 혼합된 아크릴릭 레진의 장착은 일반적인 아크릴릭 레진으로 제작된 가철성 장치를 장착한 후 나타날 수 있는 우식 이환의 가능성을 감소시킬 수 있는 임상적 적용 가능성을 제시하였다고 여겨진다.
In this study we experimented that how polyurethane effect to acrylic-polyurethane resin in Full-Grain leather coatings. First of all, we consummated waterborne acrylic emulsion and waterborne polyurethane resin, Than we prepared F.G leathers which were coated by acrylic resin and acrylic-polyurethane resins. According to measured data for solvent resistance, acrylic resin and acrylic-polyurethane resins had good property. Sample a(WAC) had most low strength($2.10kg_f/mm^2$) and sample d(WAC 93 : WPU 7) had most high strength($3.41kg_f/mm^2$). Also we knew that most good property of abrasion is d(47.4 mg). In elongation case, a(WAC) had most good result(645 %) in this experiment.
Antistatic acrylic resin is made from n-butyl methacrylate, methyl methacrylate, dimethyl amino ethyl methacrylate(DMAEMA), 2-ethyl hexyl methacrylate, hydroxy ethyl methacrylate, 2,2'-azobis iso-butyronitrile by synthesis. To achieve a lowest surface resistance of antistatic acrylic resin was applied to a variety of synthesis processes. The acrylic resin has been determined from the value of surface resistance and -then the antistatic acrylic resin including dimethyl amino ethyl methacrylate of the 10%, 20% and 30% is synthesized. Finally, dimethyl sulfate(DMS) on a variety of weight ratios is added to antistatic acrylic resin. When DMAEMA / DMS weight ratio is 1/1, antistatic acrylic resin isn't haze the lower the surface resistance. Compared to the traditional antistatic agent, all aspects of the physical properties is outstanding.
PURPOSE. The aim of this study was to compare the color stability, water sorption and cytotoxicity of thermoplastic acrylic resin for the non-metal clasp dentures to those of thermoplastic polyamide and conventional heat-polymerized denture base resins. MATERIALS AND METHODS. Three types of denture base resin, which are conventional heat-polymerized acrylic resin (Paladent 20), thermoplastic polyamide resin (Bio Tone), thermoplastic acrylic resin (Acrytone) were used as materials for this study. One hundred five specimens were fabricated. For the color stability test, specimens were immersed in the coffee and green tee for 1 and 8 weeks. Color change was measured by spectrometer. Water sorption was tested after 1 and 8 weeks immersion in the water. For the test of cytotoxicity, cell viability assay was measured and cell attachment was analyzed by FE-SEM. RESULTS. All types of denture base resin showed color changes after 1 and 8 weeks immersion. However, there was no significant difference between denture base resins. All specimens showed significant color changes in the coffee than green tee. In water sorption test, thermoplastic acrylic resin showed lower values than conventional heat-polymerized acrylic resin and thermoplastic polyamide resin. Three types of denture base showed low cytotoxicity in cell viability assay. Thermoplastic acrylic resin showed the similar cell attachment but more stable attachment than conventional heat-polymerized acrylic resin. CONCLUSION. Thermoplastic acrylic resin for the non-metal clasp denture showed acceptable color stability, water sorption and cytotoxicity. To verify the long stability in the mouth, additional in vitro studies are needed.
In this study, we experimented that how to synthesis waterborne urethane-acrylic hybrid resin for leather coatings. First of all, We had analyzed data by FT-IR, SEM and TGA for the machanical properties. By TGA analysis polymers showed heat distortion temperature. and by FT-IR measurement we confirmed that synthesis of urethane and acrylic. In the experiment, solvent resistance, polyurethane and acrylic grades 4-5 showed both a high. Tensile strength measured in the waterborne polyurethane > Acrylic emulsion showed strength in the order. Films were obtained by coating the water born resin on leveled surfaces and allowing them to dry at room temperature for 72hrs. After demolding, the films were kept in a desiccator to avoid moisture contant at $25^{\circ}C$ for 45hrs before the measurements. In this result, the mechanical propersies of waterborne polyurethane-acrylic hybrid resin showed that how effect to resin in leather coating between polyurethane content and acrylic content. Therefore, acrylic emulsion had most high solvent resistance glade and waterborne polyurethane had good result in abrasion test and tensile strength.
One of the primary advantages of acrylic resin teeth is their ability to bond chemically to the denture base resins. Fracture od acrylic resin teeth from a maxillary denture, however, is not uncommon. Bonding failures have been attributed to faulty boil-out procedures that fail to eliminate all traces of wax from the ridge lap surfaces of the teeth and to contamination of the ridge lap surface by careless application of tinfoil substitute. Attempts to increase the strength of the bond between acrylic resin teeth and heat-cured denture base resin include grinding the glossy ridge lap surface (in fluid system), painting the ridgelap surface of the teeth with monomer-polymer solution, and cutting retention grooves in the ridge lap surface of the teeth. This latter method has been tested by applying a tensile force in a labial direction to the incisal part of the lingual surface of the acrylic resin teeth. A progressive shear compressive load was applied at an angle to the lingual surface of acrylic resin teeth bonded to denture base acrylic resin. No statistically singificant advantage was derived by preparing retention grooves of different shapes in the ridgelap surface of the denture teeth.
In this study we experimented that how chain extension influences to waterborne urethane-acrylic hybrid resin for leather garment coatings. We knew that polyurethane-acrylic hybrid resins had 5 grades of solvent resistance. Tensile strength measured in the polyurethane-acrylic resin(EDA 5.37 g, 1.928 kgf/$mm^2$) had the most strong strength. Also polyurethane-acylic hybrid resin(EDA 5.37 g. 30.2 mg. loss) had better result than other hybrid resins. EDA contents higher, we obtained low elongation and low flexibility. In this result, chain extension of waterborne polyurethane-acrylic hybrid resin showed the effect in leather coating with ratio of EDA.
To prepare the waterborne silicone acrylic resin coatings, acrylic resin was prepared by a radical polymerization. Glass transition temperature(Tg) of the acrylic copolymer was fixed at 30℃ and the contents of tertiary amine monomer(DMAEMA), were varied to be 5, 10, 15 and 20 wt%, hydroxyl monomer, and carboxyl monomer were fixed 10 wt%, and 4 wt% respectively. γ-Glycidoxypropyltrimethoxysilane(GPTMS) containing epoxy group was used for curing agents. The eqivalent ratio of amine to epoxy was 1:1. The prepared coatings exhibited excellent adhesion to various substrates, and various physical properties of the coatings were satisfactory. The gloss retension and color difference were improved at low tertiary amine concentration. The coatings containing 10wt% tertiary amine concentration have especially good weather resistant properties.
Statement of the problem. The fracture of acrylic resin dentures remains an unsolved problem. Therefore, many investigations have been performed and various approaches to strengthening acrylic resin, for example, the reinforcement of heat-cured acrylic resin using glass fibers, have been suggested over the years. But problems such as poor workability, rough surface, poor adhesion of glass fiber resin complex are not solved yet. Purpose. The aim of the present study was to investigate the effect of short glass fibers on the transverse strength of heat-polymerized denture base acrylic resin and roughness of resin complex after abrasion test. Material and methods. To avoid fiber bunching and achieve even fiber distribution, glass fiber bundles were mixed with acrylic resin powder in conventional mixer with a non-cutting blade, to produce the glass fiber($10{\mu}m$ diameter, 3mm length, silane treated) resin composite. Glass fibers were incorporated at 0%, 3%, 6% and 9% by weight. Transverse strength were measured. After abrasion test, surface roughness was evaluated and scanning electron microscope view was taken for clinical application. Results. 1. 6% and 9% incorporation of 3mm glass fibers in the acrylic resin enhanced the transverse strength of the test specimens(p<0.05). 2. Before abrasion test, incorporation of 0%, 3%, 9% glass fiber in the resin showed no dirrerence in roughness statisticaly(p>0.05). 3. After abrasion test, incorporation of 0%, 3%, 6% glass fiber in the resin showed same surface roughness value statistically(p>0.05). 4. In SEM, surface roughness increased as the percentage of the fibers increased. 5. In the areas where glass fiber bunchings are formated, a remarkably high roughness was noticed. Conclusion. 6% and 9% addition of silane-treated short glass fibers into denture base acrylic resin increased transverse strength significantly. Before and after abrasion test, incorporation of 0%, 3%, 6% glass fiber in the resin showed same surface roughness value statistically.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.