Corrosion Behavior of Solution-Treated Mg-8%Al-X%Zn Casting Alloys (용체화처리된 주조용 Mg-8%Al-X%Zn 합금의 부식 거동)

  • Jun, Joong-Hwan;Hwang, In-Je
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.28 no.3
    • /
    • pp.126-133
    • /
    • 2015
  • The aim of this study is to investigate the effect of solution treatment on the corrosion behavior of Mg-8%Al-(0-1)%Zn casting alloys in 1M NaCl aqueous solution. After the solution treatment, all alloys showed single ${\alpha}$-(Mg) phase microstructure by dissolution of ${\beta}(Mg_{17}Al_{12})$ phase into the ${\alpha}$-(Mg) matrix. The $H_2$ evolution volume decreased with an increase in Zn content, which indicates that the addition of Zn plays a beneficial role in decreasing corrosion rate of the Mg-Al-Zn alloy in solution-treated state. The microstructural evaluations on the corrosion products and corroded surfaces after the immersion test in 1 M NaCl solution revealed that the incorporation of more $Al_2O_3$ and ZnO into the corrosion product, by which the penetration of $Cl^-$ ions is impeded, are thought to be responsible for the better corrosion resistance in relation with the Zn addition.

The Effect of P and Mo for Thermal and Chemical Properties of Fe-PC-B-Al-Mo Amorphous Alloys (Fe-P-C-B-Al-Mo계 비정질합금의 열적.화학적 성질에 미치는 P 및 Mo의 영향)

  • Gook, Jin-Seon;Chon, Woo-Young
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.15 no.2
    • /
    • pp.76-81
    • /
    • 2002
  • The melt-spun amorphous $Fe_{77-X}P_{13}C_4B_4Al_2Mo_X$(x=4~10) and $Fe_{82-X}P_XC_4B_4Al_2Mo_8$(x=9~15) alloys were found to exhibit a large supercooled liquid region(${\Delta}T_x$) exceeding 40 K before crystallization. The largest ${\Delta}T_x$ for the glassy alloys containing Mo reaches as large as 65 K for the $Fe_{69}P_{13}C_4B_4Al_2Mo_8$ alloy. The corrosion behavior of the amorphous $Fe_{77-X}P_{13}C_4B_4Al_2Mo_X$(x=4~15) and $Fe_(82-X)P_XC_4B_4Al_2Mo_8$ (x=9~17) alloys were examined by electrochemical measurements in 9M $H_2SO_4$ solution at 303 K. The addition of Mo(or P) for replacing some portion of Fe is effective in improving the corrosion resistance of the investigated Fe-based glassy alloys. They are spontaneously passivated and have a wide passive region with low passive current density.

Efficient Organic Light-emitting Diodes with Aluminum-doped Zinc Oxide Anodes (알루미늄 도핑된 산화아연 양극을 적용한 고효율 유기발광다이오드)

  • Lee, Ho-Nyeon;Lee, Young-Gu;Jung, Jong-Guk;Lee, Seung-Eui;Oh, Tae-Sik
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.20 no.8
    • /
    • pp.711-715
    • /
    • 2007
  • Properties of organic light-emitting diodes (OLEDs) with aluminum-doped zinc oxide (ZnO:Al) anodes showed different behaviors from OLEDs with indium tin oxide (ITO) anodes according to driving conditions. OLEDs with ITO anodes gave higher current density and luminance in lower voltage region and better EL and power efficiency under lower current density conditions, However, OLEDs with ZnO:Al anodes gave higher current density and luminance in higher voltage region over about 8V and better EL and power efficiency under higher current density over $200mA/cm^2$. These seemed to be due to the differences in conduction properties of semiconducting ZnO:Al and metallic ITO. OLEDs with ZnO:Al anodes showed nearly saturated efficiency under high current driving conditions compared with those of OLEDs with ITO anodes. This meant better charge balance in OLEDs with ZnO:Al anodes. These properties of OLEDs with ZnO:Al anodes are useful in making bright display devices with efficiency.

A Study on the Micro Vibration Forming of Al-based Superplastic Alloy and Zr-based Bulk Metallic Glass (Al계 초소성합금과 Zr계 비정질합금의 마이크로 진동성형에 관한 연구)

  • Son, Seon-Cheon;Park, Kyu-Yeol;Na, Young-Sang
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.16 no.6
    • /
    • pp.193-200
    • /
    • 2007
  • Micro forming is a suited technology to manufacture very small metallic parts(several $mm{\sim}{\mu}m$). Al5083 superplastic alloy with very small grains has a great advantage in achieving micro deformation under low stress due to its relatively low strength at a specific high temperature range. Micro forming of $Zr_{62}Cu_{17}Ni_{13}Al_8$ bulk Metallic glass(BMG) as a candidate material for this developing process are feasible at a relatively low stress in the supercooled liquid state without any crystallization during hot deformation. In this study, the micro formability of Al5083 superplastic alloy and bulk metallic glass, $Zr_{62}Cu_{17}Ni_{13}Al_8$, was investigated with the specially designed micro vibration forming system using pyramid-shape, V-shape and U-shape micro die pattern. With these dies, micro vibration forming was conducted by varying the applied load, time. Micro formability was estimated by comparing the hight of formed shape using non-contact surface profiler system. The vibration load effect to metal flow in the micro die and improve the micro formability of Al5083 superplastic alloy and $Zr_{62}Cu_{17}Ni_{13}Al_8$ bulk Metallic glass(BMG).

Fabrication of Aluminum Alloy Composites Reinforced with SiC whisker an $Al_2O_3-SiO_2$ Short Fiber by Squeeze Casting (용탕단조에 의한 $Al_2O_3-SiO_2$ 단섬유 및 SiC whisker강화 알루미늄 합금기 복합재료의 제조)

  • Hong, Sung-Kil;Yun, Jung-Yul;Choi, Jung-Chul
    • Journal of Korea Foundry Society
    • /
    • v.17 no.1
    • /
    • pp.28-35
    • /
    • 1997
  • SiC whisker and $Al_2O_3-SiO_2$ short fiber reinforced AC8A, AC8B and AC8B(J) marix composites were fabricated by squeeze casting method. Preform deformation, change of reinforcement volumefraction and formation of macro-segregation in two composites were investigated by using micro Vickers hardness test, analysis of macro and micro structures with OM, SEM and EDAX. $Al_2O_3-SiO_2$ short fiber preform manufactured with 5% $SiO_2$ binder in this study was considerably deformed and cracked, nevertheless, the short fibers were distributed homogeneously in the composites. In SiC whisker reinforced composites, on the other hand, preform deforming and cracking were not occurred, however, macro segregation zone formed along the infiltration routes by interface reaction during infiltration of molten metal into the preform was observed at center-low area in the composites. The decrease of hardness in the macro segregation zone resulted from the depletion of Si and Mg atoms.

  • PDF

Microstructure and High Temperature Strength of Rapidly Solidified Al-8wt%Fe Alloy (급속응고된 Al-8wt%Fe 합금의 미세조직 및 고온강도)

  • 최병준
    • Journal of Powder Materials
    • /
    • v.5 no.3
    • /
    • pp.192-198
    • /
    • 1998
  • Microstructure and mechanical properties were examined on rapidly solidified Al-8wt%Fe alloy. High temperature strength test was also undertaken, and it is shown that the refinement in microstructure resulting from extremely rapid cooling rates gives rise to improved high temperature strength, but the elongation to fracture of this material decreases with increasing temperature, particularly in the temperature range up to 30$0^{\circ}C$. Specimens heat-treated for 100 hrs were analyzed with TEM micrographs to understand the thermal stability of this material.

  • PDF

Corrosion Behaviour of Fe-XAl-0.3Y Alloys at High Temperature Sulfidation Environment(Ps2=10-3Pa) (Fe-XAl-0.3Y 합금의 고온 황화환경(Ps2=10-3Pa)에서의 부식거동)

  • Lee Byung Woo;Park Hwa Soon
    • Korean Journal of Materials Research
    • /
    • v.14 no.8
    • /
    • pp.547-551
    • /
    • 2004
  • The sulfidation behaviour of Fe-XAl-0.3Y(X=5, 10, 14, 25 $wt.\%$) alloys was investigated at 1123 K in $H_2/H_{2}S$ gas atmosphere for $1\sim24$ hrs using SEM/EDX, XRD and EPMA. The weight changes of Fe-XAl-0.3Y alloys followed the parabolic rate law, Sulfidation rates of iron aluminide alloys with high Al content were one-twentieth lower than that of 5Al alloys. This is due to the formation of protective $Al_{2}O_3$ oxides on the surface of 10Al, 14Al and 25Al alloys. By calculating partial pressure of impurity oxygen contained $H_2/H_{2}S$ gas, the $Al_{2}O_3$ oxides formation could be explained using Fe-Al-S-O thermodynamic stability diagram. The sulfidation product scales of the 5Al alloy showed that thick iron sulfide scale(FeS) containing porosities formed during early stages of sulfidation. With continued sulfidation, aluminum sulfide was formed at the alloy/scale interface.

A study on the growth of AlN single crystals (AlN 단결정 성장에 관한 연구)

  • Kang, Seung-Min
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.6
    • /
    • pp.279-282
    • /
    • 2013
  • Recently, it has been interested much that AlN (Aluminum Nitride) crystals can be applied to UV LEDs and high power devices as like GaN and SiC crystals. The reports about commercial grade of AlN wafers in the world have been absent, however several results for growth of large size of AlN single crystals have been reported from abroad. In this report, the result of AlN single crystals of a diameter of about 8 mm grown are reported. Optical microscopic characterization was applied to observe the form of the crystals and the crystal quality was evaluated by FWHM measurement by DCXRD rocking curve analysis.

The Thermal Stability of Mechanically Alloyed Quaternary Al-8wt.%(Ti+V+Zr) Alloys (기계적 합금화한 Al-8wt.%(Ti+V+Zr) 4원계 합금의 열적 안정성에 관한 연구)

  • 김주영
    • Journal of Powder Materials
    • /
    • v.2 no.3
    • /
    • pp.247-254
    • /
    • 1995
  • The theoretical optimum quaternary composition for improving the thermal stability of Al-Ti alloy was recently proposed. On the basis of the suggestion, quaternary Al-Ti-V-Zr alloy powders corresponding to the optimum compositions, one of which belongs to the region of the smallest lattice misfit between the matrix and the precipitates and the other belongs to the region of the smallest rate constant of coarsening, were prepared by mechanical alloying and the powders were vacuum-hot-pressed at $430^{\circ}C$ under the pressure of 800 MPa. The thermal stability of the specimens was evaluated by hardness testing after isothermal aging up to 400 hrs at various temperatures. The decrease of hardness of Al-Ti-V-Zr alloys was smaller than that of Al-Ti alloys. It was considered to be due to the formation of $Al_3Zr$ type and$Al_3Ti$ type quaternary precipitates having smaller lattice misfit than $Al_3Ti$ and the increase of volume fraction of All0v during the isothermal aging. The quaternary Al-Ti-V-Zr alloys corresponding to the smallest lattice misfit showed the most improved thermal stablilty and it was mainly considered to be due to the formation of All0v.

  • PDF

Relationship Between Corporate Social Responsibility Expenditures and Performance in Jordanian Commercial Banks

  • BANI-KHALED, Sakhr M.;EL-DALABEEH, Abdel Rahman K.;AL-OLIMAT, Nofan H.;AL SHBAIL, Mohannad O.
    • The Journal of Asian Finance, Economics and Business
    • /
    • v.8 no.3
    • /
    • pp.539-549
    • /
    • 2021
  • This study aims to examine the relationship between corporate social responsibility (CSR) expenditures and both financial and non-financial performance of Jordanian commercial banks during the period 2008-2018. To measure the variables of interest, secondary data published on Amman Stock Exchange (ASE) website were processed to become preliminary data suitable for the nature of the study. The study sample amounted to 13 commercial banks, which represent all Jordanian commercial banks listed on ASE.. The study found that there is a positive, statistically significant relationship between CSR expenditures and financial performance, as the study showed that the return on equity (ROE) has a positive and significant relationship with CSR expenditure, while the return on assets (ROA) and Tobin's Q model have a statistically significant negative relationship with CSR expenditure, while the market stock price (MSP) had a positive, but not statistically significant. The study also found that there is a positive, statistically significant relationship between CSR expenditures and non-financial performance, which was represented by total deposits and total training expenditures in Jordanian commercial banks. Accordingly, the study recommends encouraging banks to prepare sustainability reports and CSR reports, which are considered comprehensive, and not only with disclosures within the annual reports.