• Title/Summary/Keyword: AISI 304

Search Result 86, Processing Time 0.033 seconds

A Study on Tensile Characteristics of AISI 304 Stainless Steel under Room and Elevated Temperatures (AISI 304강의 상온/고온 인장특성에 관한 연구)

  • Park, Sung-Ho;Park, No-Seok;Kim, Jae-Hoon
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.12 no.5
    • /
    • pp.35-42
    • /
    • 2008
  • This study describes the tensile test results of AISI type 304 under room and elevated temperatures. The tensile tests for AISI type 304, which is widely used for airframe structural applications, are performed according to ASTM standard. Normal probability plot was used to evaluate A and B Basis value for tensile strengths. Ramberg-Osgood parameter assuming an exponential relationship between stress and small plastic strain was obtained by least square estimate for test data. After room and elevated temperature tensile tests the surface of fractured specimens was observed by SEM images and EDX.

Finite Element Analysis of Nd:YAG Pulse Laser Welding for AISI 304 Stainless Steel Plate (AISI 304 스테인리스 강판의 Nd:YAG 펄스 레이저 용접에 관한 유한요소해석)

  • Nam Gi-Jeong;Kim Kwan-Woo;Hong Jin-Uk;Lee Jae-Hoon;Suh Jeong;Cho Hae-Yong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.30 no.4 s.247
    • /
    • pp.428-434
    • /
    • 2006
  • Pulse laser welding of AISI 304 stainless steel plate was simulated to find optimal welding conditions by using commercial finite element code MARC. Due to geometric symmetry, a half model of AISI 304 stainless steel plate was considered and user subroutines were applied to boundary condition for the heat transfer. Material properties such as conductivity, specific heat, mass density and latent heat were given as a function of temperature. A moving heat source was designed on the basis of experimental data. As a result, Nd:YAG laser welding for AISI 304 stainless steel was successfully simulated and it should be useful to determine optimal welding condition.

The low temperature plasma nitrocarburizng of AISI304L and AISI316L stainless steel (AISI304L과 AISI316L강의 저온프라즈마 질탄화 처리 )

  • Jeong, Gwang-Ho;Lee, In-Seop
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2007.11a
    • /
    • pp.153-154
    • /
    • 2007
  • AISI316L강은 AISI304L강과 기본 조성은 같지만 316L강이 약 2.5%의 Mo가 첨가되어 있다. 저온 플라즈마 질탄화 시 모재에 첨가된 Mo의 영향을 조사하기 위하여 처리온도를 변화시켜 실험하였다. 같은 처리온도의 경우 경화층의 두께는 316L강이 비교적 두껍게 형성되었다. 316L강의 경우 $450^{\circ}C$이하에서 약 25 ${\mu}m$까지 형성되었고, 306L강의 경우 $400^{\circ}C$에서 약 10 ${\mu}m$까지 형성되었다. $400^{\circ}C$ 이하에서 경화층은 두 가지시편 모두 확장된 오스테나이트 (${\gamma}_N,\;{\gamma}_c$)로 이루어져 있으나, 304L의 경우 $430^{\circ}C$부터 석출물(CrN)이 형성되기 시작하였다. 316L의 경우 $450^{\circ}C$까지 석출물이 형성되지 않았고, $480^{\circ}C$에서 석출물 (CrN)이 관찰되었다. 석출물이 형성된 시편을 제외한 모든 시편의 내식성은 모제보다 증가 하였다.

  • PDF

Cryogenic Charpy Impact Test based on GTAW Method of AISI 304 Stainless Steel for LNG Pipeline (AISI 304 스테인리스 강으로 제작된 LNG배관 용접부의 극저온 샤르피 충격시험)

  • Kim, Jeong-Hyeon;Choi, Sung-Woong;Park, Doo-Hwan;Lee, Jae-Myung
    • Journal of Welding and Joining
    • /
    • v.32 no.3
    • /
    • pp.89-94
    • /
    • 2014
  • AISI 304 austenitic stainless steel is widely used for LNG pipes for LNG transmission thanks to its good metallurgical and mechanical properties. In the present research, impact toughness of a gas tungsten arc welded AISI 304 stainless steel pipe was evaluated between room and liquid nitrogen ($-196^{\circ}C$) test temperatures. In addition, a comparative study was made of the fracture behavior of FCC crystal structured stainless steel weldments and BCC crystal structured mild steels(A-grade and SS400). The results showed a slight decrease in the impact energy of the AISI 304 base metal, heat affected zone(HAZ), and welded zone with decreasing test temperature. In addition, the welded metal has the highest absorbed impact energy, followed by HAZ and the base metal.

Finite element analysis for prediction of weld bead shape of Nd:YAG pulse laser welding for AISI 304 stainless steel plate (AISI 304 스테인리스 강판의 Nd:YAG 펄스 레이저 용접비드 형상예측을 위한 유한요소해석)

  • Cho Haeyong;Kim Kwanwoo;Hong Jinuk;Lee Jaehoon;Suh Jeong
    • Laser Solutions
    • /
    • v.8 no.1
    • /
    • pp.19-25
    • /
    • 2005
  • Pulse laser welding of AISI 304 stainless steel plate was simulated to optimize welding conditions by using commercial finite element code MARC. Due to geometric symmetry, a half model of AISI 304 stainless steel plate was considered. for the heat transfer analysis, user subroutines were applied to boundary condition. The material properties such as conductivity, specific heat, and mass density were given as a function of temperature and the latent heat associated with a given temperature range was considered. A moving heat source was designed on the basis of experimental data. As a result, Nd:YAG laser welding for AISI 304 stainless steel was successfully simulated and it should be useful to determine optimal welding condition.

  • PDF

Evaluations of Microstructure and Electrochemical Anodic Polarization of AISI 304L and AISI 316L Stainless Steel Weld Metals with Creq/Nieq Ratio (Creq/Nieq비에 따른 AISI 304L 및 AISI 316L 스테인리스강 용접부의 미세조직 및 전기화학적 양극분극 평가)

  • Kim, Yeon Hee;Jang, Ah Young;Kang, Dong Hoon;Ko, Dae Eun;Shin, Yong Taek;Lee, Hae Woo
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.12
    • /
    • pp.1090-1096
    • /
    • 2010
  • This pitting corrosion study of welded joints of austenitic stainless steels (AISI 304L and 316L) has addressed the differentiating solidification mode using three newly introduced filler wires with a flux-cored arc welding process (FCAW). The delta ferrite (${\delta}$-ferrite) content in the welded metals increased with an increasing equivalent weight ratio of chromium/nickel ($Cr_{eq}/Ni_{eq}$). Ductility dip cracking (DDC) was observed in the welded metal containing ferrite with none of AISI 304L and 0.1% of AISI 316L. The potentiodynamic anodic polarization results revealed that the $Cr_{eq}/Ni_{eq}$ ratio in a 3.5% NaCl solution didn't much affect the pitting potential ($E_{pit}$). The AISI 316L welded metals with ${\ddot{a}}$-ferrite content of over 10% had a superior $E_{pit}$ value. Though the AISI 316L welded metal with 0.1% ferrite had larger molybdenum contents than AISI 304L specimens, it showed a similar $E_{pit}$ value because the concentration of chloride ions and the corrosion product induced severe damage near the DDC.

Press Formability of Austenitic AISI304 Stainless Steel (오스테나이트계 AISI304 스테인레스강판의 프레스 성형특성)

  • Nam, J.B.;Ryoo, D.Y.;Kim, Y.S.
    • Transactions of Materials Processing
    • /
    • v.3 no.1
    • /
    • pp.38-50
    • /
    • 1994
  • Fundamental deformation mechanism and plastic behavior of AISI304 austenitic stainless steel were investigated to evaluate press formability. Local and uniform deformation capacity of AISI304 steel were compared to those of ferritic AISI430 steel and Al killed low carbon steel. Nine kinds of austenitic stainless steels having different austenite stabilities were made in laboratory scale to examine the transformation behavior in various deformation mode and variation of mechanical properties. Deformation path and strain distributions along edge corner of commercial sink die were illustrated and effect of austenite stability on press forming of sink die was clarified with experiments using square cup drawing tools.

  • PDF

A Study on the Cleaning of AISI 304 Stainless Steel Surface for Gold Plating (금도금을 위한 AISI 304 스테인레스강 표면의 세정)

  • 한범석;장현구
    • Journal of the Korean institute of surface engineering
    • /
    • v.28 no.1
    • /
    • pp.23-33
    • /
    • 1995
  • AISI 304 stainless steel has high resistance to corrosion due to the presence of a self-healing chromium oxide film on the surface, which also accounts for the difficulty in plating. Surface cleaning of this alloy is of fundamental importance in gold plating since its effectiveness puts an upper limit on the quality of the final coating. The cleaning of AISI 304 stainless steel was investigated with elimination of artificial passive oxide film and degreasing of remaining buffing wax as stearic acid. The familiar cleaning methods i.e. ultrasonic cleaning, electro-cleaning and activation treatment were fabricated in this study. Activation treatment showed best cleaning efficiency for elimination of passive oxide film among these methods, which was also confirmed by AES (Auger electron spectrometer) analysis. However, the best condition of cleaning was obtained by combining these methods. Electrocleaning time, for degreasing the stearic acid layer, was decreased with increasing amount of added KCN.

  • PDF

A Corrosion Resistance Evaluation of Welded AISI 304 Stainless Steel by Electrochemical Methods. (전기화학적 방법에 의한 AISI 304 스테인리스강 용접부의 내식성 평가)

  • 백신영;김관휴
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.14 no.1
    • /
    • pp.83-89
    • /
    • 1990
  • Electrochemical methods have been proposed as non-destructive, rapid and quantitative means for determining the degree of sensitization associated with Chromium depleted zones surrounding precipitates of Cr carbide and formation of secondary phase in stainless steel. In this study, the specimen of AISI 304 stainless steel and its welded sections, which welded by TIG, MIG, $CO_2$ and ARC, were tested corrosion resistance by electrochemical methods in 0.5N HCl and 1N $H_2SO_4$ with or without 0.01N KSCN. The results were confirmed that electrochemical methods could be used as a test method of corrosion resistance evaluation for the welded AISI 304 stainless steel.

  • PDF