• Title/Summary/Keyword: AC transport losses

Search Result 35, Processing Time 0.031 seconds

Effect of the Neighboring Tape′s AC Currents on Transport Current Loss of a Bi-2223 Tape (인접 교류전류가 Bi-2223테이프의 통전손실에 미치는 영향)

  • 류경우;최병주
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.3
    • /
    • pp.251-256
    • /
    • 2001
  • Bi-2223 tapes have been developed for low-field power applications at liquid nitrogen temperature. When the Bi-2223 tapes are used in an application such as a power transmission cable or a power transformer, they are supplied with an AC transport current simultaneously. AC loss taking into account such real applications is a crucial issue for power applications fo the Bi-2223 tapes to be feasible. In this paper, the transport losses for different AC current levels and arrangements of the neighboring tapes have been measured in a 1./5 m long Bi-2223 tape. The significant increase of the transport losses due to neighboring tape's AC currents is observed. An increase of the transport losses caused by a decrease of the Bi-2223 tape's critical current is a minor effect. The measured trasprot losses could not be explained by a dynamic resistance loss based on DC voltage-current characteristics in combination with the neighboring tape's AC currents.The trasport losses do not depend on the frequency of the neighboring tape's AC currents but is arrangements in the range of small current especially.

  • PDF

AC loss analysis and experimental evaluation of a high temperature superconductor (고온초전도선재의 교류손실 해석 및 실험)

  • Ryu, Kyung-Woo
    • Proceedings of the KIEE Conference
    • /
    • 2001.11b
    • /
    • pp.96-100
    • /
    • 2001
  • Bi-2223 tapes have been developed for low-field power applications at liquid nitrogen temperature. When the Bi-2223 tapes are used in an application such as a power transmission cable or a power transformer, they are supplied with an AC transport current and exposed to an external magnetic field generated by neighboring tape's AC currents simultaneously. AC loss taking into account such real applications is a crucial issue for power applications of the Bi-2223 tapes to be feasible. In this paper, the transport losses for different AC current levels and arrangements of the neighboring tapes have been measured in a 1.5 m long Bi-2223 tape. The significant increase of the transport losses due to neighboring tape's AC currents is observed. An increase of the transport losses caused by a decrease of the Bi-2223 tape's critical current is a minor effect. The measured transport losses could not be explained by a dynamic resistance loss based on DC voltage-current characteristics in combination with the neighboring tape's AC currents. The transport losses do not depend on the frequency of the neighboring tape's AC currents but its arrangements in the range of small current especially.

  • PDF

Ac Losses of Ag sheathed Bi-2223 High-$T_{c}$ Superconducting Wire (은 피복 Bi-2223 고온 초전도 선재의 교류손실)

  • 김영석;장현만;정종만;백승명;곽민환;김상현
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 1999.02a
    • /
    • pp.54-57
    • /
    • 1999
  • AC losses per cycle properties at 77K have been investigated on the Ag sheathed Bi2223 wire through two kinds of measuring methods(transport method and magnetic method). In case of transport method, the absolute value of losses agree with the results of Norris theory(strip and ellipse). In case of 19-filamentary tape, AC transport losses almost agree with those of magnetic method. In case of 1-filamentary tape, However, AC losses of magnetic method is smaller than AC transport losses

  • PDF

Current Distribution and Numerical Analysis of AC Losses on Multi-Layer HTS Cable (다층 고온 초전도 케이블의 전류 분포 및 교류손실 해석)

  • 김영석;이병성;장현만;곽민환;김상현
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.452-455
    • /
    • 2000
  • Superconducting power cable is one of the most promising energy application of high-T$_{c}$ superconductors (HTS). A prototype HTS cable have been constructed multi-layer cable using Bi-2223 tape and tested. The AC transport losses under self field were investigated at 77K on the 19 filamentary tape and multi-layer HTS cables. And we carried out numerical analysis using bean model. The result shows that the total transport current of HTS cable in L$N_2$ was 475[A], and transport current passed through almost the outer layer (2-layer). Also, AC transport losses in outer layer of HTS cable was proportion to I$^2$ and higher than losses of inner layer. In case of Ip=Ic, calculated numerical loss density was concentrated on the edge of tape and most of loss density in cable was distributed outer layer more than inner layer. As magnetic distribution was concentrated on outer layer.r.

  • PDF

Total AC Loss by simultaneously applied AC transport current and AC external magnetic field in BSCCO Tape

  • Park Myungjin;Lim Hyoungwoo;Cha Gueesoo;Lee Jikwang
    • Progress in Superconductivity and Cryogenics
    • /
    • v.7 no.4
    • /
    • pp.10-13
    • /
    • 2005
  • Transport current and magnetic field which is generated by transport current make AC current - AC mag-netic field condition(AC-AC condition) in AC power application system using HTS tape. Therefore, characteristics of AC loss under the AC-AC condition are necessary to estimate AC loss of power device with accuracy such as HTS transformer. In this paper, we researched transport current loss, magnetization loss by perpendicular magnetic field and total loss which is represented as summation of both losses under the AC-AC condition in single HTS tape. As a result, magnetization loss showed increasing behavior under 65mT and decreasing behavior upper 65mT by influence of transport current. Transport current loss was increased continuously through out whole measurement ranges in the AC-AC condition. Total loss in HTS tape was dominated entirely by magnetization loss.

An Electrical Properties of Prototype HTS Cable using Bi-2223 tape (Bi-2223 선재를 이용한 Prototype 고온 초전도 케이블의 전기적 특성)

  • Kim, Young-Seok;Lee, Byung-Sung;Jang, Hyun-Man;Kwak, Min-Hwan;Kim, Sang-Hyun
    • Proceedings of the KIEE Conference
    • /
    • 2000.07c
    • /
    • pp.1551-1553
    • /
    • 2000
  • Superconducting power cable is one of the most promising energy application of high-$T_c$ superconductors (HTS). A prototype HTS cable have been constructed multi-layer cable using Bi-2223 tape and tested. The result shows that the total transport current of HTS cable in $LN_2$ was 475[A], and transport current passed through almost the outer layer (2-layer). Also, AC transport losses in outer layer of HTS cable was proportion to $I^2$ and higher than losses of inner layer. As magnetic distribution were concentrated on outer layer.

  • PDF

A Study of Characteristic of Electrical-magnetic and Neutron Diffraction of Long-wire High-superconductor for Reducing Energy Losses

  • Jang, Mi-Hye
    • Transactions on Electrical and Electronic Materials
    • /
    • v.9 no.6
    • /
    • pp.265-272
    • /
    • 2008
  • In this paper, AC losses of long wire Bi-2223 tapes with different twist pitch of superconducting core were fabricated, measured and analyzed. These samples produced by a powder-in-tube method are multi-filamentary tape with Ag matrix. Also, it's produced by non-twist. The critical current measurement was carried out under the environment in Liquid nitrogen and in zero field by 4-prob method. And the Magnetic measurement was carried out under the environment of applied time-varying transport current by transport method. From experiment, the susceptibility measurements were conducted while cooling in a magnetic field. Flux loss measurements were conducted as a function of ramping rate, frequency and field direction. The AC flux loss increases as the twist-pitch of the tapes decreased, in agreement with the Norris Equation. Neutron-diffraction measurements have been carried out investigate the crystal structure, magnetic structures, and magnetic phase transitions in Bi-2223([Bi, Pb]:Sr:Ca:Cu:O).

Characteristics of Bi-based High $T_c$ Superconducting Current Lead (Bi계 고온초전도 전류 리드의 특성)

  • 백승명;이병성;김영석;곽민환;김상현
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.73-76
    • /
    • 1999
  • We have fabricated and tested a Bi-based high temperature superconducting current lead system. Ag sheathed Bi-2223 mono-filament tapes of $I_c=8.4$ A at 77 K under self-field condition were fabricated using powder-in-tube(P1T) method. Multi-layer current leads can be made by stacking of Ag sheathed Bi-2223 mono-filament wires. The critical current of this 10-layer current lead is about 68 A. The contact resistance across the copper-current lead interface has been studied using current-voltage characteristics. At temperature below critical temperature the resistive contribution of the interface to the total contact resistance dominates. We have measured AC transport losses in a current lead at 77 K, 60 Hz by a transport method.

  • PDF

Analysis of AC losses in HTS coils by temperature variations

  • Kim, Yungil;Lee, Ji-Kwang;Lee, Seyeon;Kim, Woo-Seok;Lee, Siyoung;Choi, Kyeongdal
    • Progress in Superconductivity and Cryogenics
    • /
    • v.20 no.4
    • /
    • pp.50-54
    • /
    • 2018
  • We analyzed the temperature dependency of the AC losses in high temperature superconducting (HTS) coils. In the case of a short sample of an HTS tape, the magnetization loss at 4.2 K could be higher than the one at 77 K for a same transport current. It happens when the perpendicular magnetic field is above a certain magnitude. The AC loss characteristics of solenoidal coils have been analyzed at the temperatures of 65 K and 77 K. They were categorized by the aspect ratios. The operating current of a solenoid was normally set about 70 % of the critical current. An HTS solenoid with the same operating current of 77 K causes larger AC losses at 65 K in the most cases of the HTS solenoids. We also analyzed the AC loss characteristics due to the temperature variations for three types of superconducting magnetic energy storages. Two of them were solenoidal types and the other was toroidal type. The results showed the tendency for the coils to have higher AC losses at lower temperature with the same operating currents and scenarios.

Fabrication, AC Loss Measurement and Analysis of Bi-2223 Conductors with Respect to Various Twist Pitch (트위스트 피치를 고려한 Bi-2223 선재 제작과 AC 손실 측정 및 분석)

  • Jang, Mi-Hye;Chu, Yong;Lim, Jun-Hyung;Joo, Jin-Ho;Ko, Tae-Kuk
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.49 no.11
    • /
    • pp.589-595
    • /
    • 2000
  • In this papre, AC losses of Bi-2223 tapes with different twist pitch of superconducting core were fabricated, measured and analyzed. These samples produced by a powder-in-tube method are multi-filamentary tape with Ag matrix. Also, it's produced by non-twist and different twist pitch(8, 10, 13, 30, 50, 70 mn). The critical current measurement was carried out under the environment in Liquid nitrogen and in zero field by 4-probe method. And the AC loss measurement was carried out under the environment of applied time-varying transport current by transport method. From experiment, the critical current is larger non-twist than twisted filament. And, the AC loss by Norris equation is higher non-twisted tape than 13mm twisted tape. Also, it is confirmed that of AC loss of tape having non-twist pitch larger than those having differnet twist pitch.

  • PDF