The Oxidation Behavior of Sintered STS 316L at High-Temperature in the Air (STS 316L 소결체의 대기중 고온산화 거동)

  • Kim, Hye Seong;Lee, Jong Pil;Park, Dong Kyu;Ahn, In Shup
    • Journal of Powder Materials
    • /
    • v.20 no.6
    • /
    • pp.432-438
    • /
    • 2013
  • In this study, analysis on the oxidation behavior was conducted by a series of high-temperature oxidation tests at both $800^{\circ}C$, $900^{\circ}C$ and 1000 in the air with sintered STS 316L. The weight gain of each oxidized specimen was measured, the oxidized surface morphologies and composition of oxidation layer were analyzed with Scanning Electron Microscope-Energy Dispersive x-ray Spectroscopy (SEM-EDS), finally, the phase change and composition of the oxidized specimen were shown by X-Ray Diffraction (XRD). As a result, the weight gain increased sharply at $1000^{\circ}C$ when oxidation test was conducted for 210 hours. Also, a plentiful of pores were observed in the surface oxidation layers at $900^{\circ}C$ for 210 hours. In addition, the following conclusions on oxidation behavior of sintered STS 316L can be obtained: $Cr_2O_3$ can be formed on pores by influxing oxygen through open-pores, $(Fe_{0.6}Cr_{0.4})_2O_3$ can be generated on the inner oxidation layer, and $Fe_2O_3$ was on the outer oxidation layer. Also, $NiFe_2O_4$ could be precipitated if the oxidation time was kept longer.

Characterization and Mechanical Properties of Stainless Steel 316L Fabricated Using Additive Manufacturing Processes (적층식 제조 공정을 활용한 스테인레스 316L 제작기술의 특징과 기계적 속성)

  • Choi, Cheol;Jung, Mihee
    • KEPCO Journal on Electric Power and Energy
    • /
    • v.7 no.1
    • /
    • pp.129-135
    • /
    • 2021
  • Recently, additive manufacturing (AM) technology such as powder bed fusion (PBF) and directed energy deposition (DED) are actively attempted as consumers' needs for parts with complex shapes and expensive materials. In the present work, the effect of processing parameters on the mechanical properties of 316L stainless steel coupons fabricated by PBF and DED AM technology was investigated. Three major mechanical tests, including tension, impact, and fatigue, were performed on coupons extracted from the standard components at angles of 0, 45, 90 degrees for the build layers, and compared with those of investment casting and commercial wrought products. Austenitic 316L stainless steel additively manufactured have been well known to be generally stronger but highly vulnerable to impact and lack in elongation compared to casting and wrought materials. The process-induced pore density has been proved the most critical factor in determining the mechanical properties of AM-built metal parts. Therefore, it was strongly recommended to reduce those lack of fusion defects as much as possible by carefully control the energy density of the laser. For example, under the high energy density conditions, PBF-built parts showed 46% higher tensile strength but more than 75% lower impact strength than the wrought products. However, by optimizing the energy density of the laser of the metal AM system, it has been confirmed that it is possible to manufacture metal parts that can satisfy both strength and ductility, and thus it is expected to be actively applied in the field of electric power section soon.

Electrochemical Characteristics and Damage Behavior in Cathode Operating Conditions of 316L Stainless Steel with Test Time and Applied Potential in Metallic Bipolar Plates for PEMFC (고분자 전해질 연료전지 양극 작동 환경에서 실험 시간 및 작동 전압 변수에 따른 316L 스테인리스강의 전기화학적 특성과 손상 거동)

  • Shin, Dong-Ho;Kim, Seong-Jong
    • Corrosion Science and Technology
    • /
    • v.20 no.6
    • /
    • pp.451-465
    • /
    • 2021
  • In this investigation, electrochemical characteristics and damage behavior of 316L stainless steel polymer electrolyte membrane fuel cell(PEMFC) were analyzed by potentiodynamic and potentiostatic tests in cathode operating condition of PEMFC. As the result of potentiodynamic polarization test, range of passive region was larger than range of active region. In the result of potentiostatic test, damage depth and width, pit volume, and surface roughness were increased 1.57, 1.27, 2.48, and 1.34 times, respectively, at 1.2 V compared to 0.6 V at 24 hours. Also, as a result of linear regression analysis of damage depth and width graph, trend lines of damage depth and width according to applied potentials were 16.6 and 14.3 times larger, respectively. This demonstrated that applied potential had a greater effect on pitting damage depth of 316L stainless steel. The damage tendency values were 0.329 at 6 hours and 0.633 at 24 hours with applied potentials, representing rapid growth in depth direction according to the test times and applied potentials. Scanning electron microscopy images revealed that surface of specimen exhibited clear pitting damage with test times and applied potentials, which was thought to be because a stable oxide film was formed by Cr and Mo.

Microstructural Analysis of STS316L Samples Manufactured by Powder Bed Fusion and Post-heat Treatments (Powder Bed Fusion 공정으로 제조한 STS 316L의 미세조직과 후속 열처리 특성)

  • Song, S.Y.;Lee, D.W.;Cong, D.V.;Kim, J.W.;Lee, S.M.;Joo, S.H.;Kim, Jin-Chun
    • Journal of Powder Materials
    • /
    • v.29 no.1
    • /
    • pp.14-21
    • /
    • 2022
  • In the powder bed fusion (PBF) process, a 3D shape is formed by the continuous stacking of very fine powder layers using computer-aided design (CAD) modeling data, following which laser irradiation can be used to fuse the layers forming the desired product. In this method, the main process parameters for manufacturing the desired 3D products are laser power, laser speed, powder form, powder size, laminated thickness, and laser diameter. Stainless steel (STS) 316L exhibits excellent strength at high temperatures, and is also corrosion resistant. Due to this, it is widely used in various additive manufacturing processes, and in the production of corrosion-resistant components with complicated shapes. In this study, rectangular specimens have been manufactured using STS 316L powder via the PBF process. Further, the effect of heat treatment at 800 ℃ on the microstructure and hardness has been investigated.

CREEP-FATIGUE CRACK GROWTH AND CREEP RUPTURE BEHAVIOR IN TYPE 316 STAINLESS STEELS- EFFECT OF HOLD TIME AND AGING TREATMENT

  • Mi, J.W.;Won, S.J.;Kim, M.J.;Lim, B.S.
    • International Journal of Automotive Technology
    • /
    • v.1 no.2
    • /
    • pp.71-77
    • /
    • 2000
  • High temperature materials in service are subjected to mechanical damage due to operating load and metallurgical damage due to operating temperature. Therefore, when designing or assessing life of high temperature components, both factors must be considered. In this paper, the effect of tensile hold time on high temperature fatigue crack growth and long term prior thermal aging heat treatment on creep rupture behavior were investigated using STS 316L and STS 316 austenitic stainless steels, which are widely used for high temperature components like in automotive exhaust and piping systems. In high temperature fatigue crack growth tests using STS 316L, as tensile hold time increased, crack growth rate decreased in relatively short tensile hold time region. In long term aged specimens, cavity type microcracks have been observed at the interface of grain boundary and coarsened carbide.

  • PDF

A study on electrochemical protection diagrams of steel in nitric and sulfuric acid solutions (질산과 황산 용액중의 철강의 전기방식도에 관한 연구)

  • 전대희;김진경
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.13 no.2
    • /
    • pp.43-63
    • /
    • 1989
  • Various kinds of corrosion prevention methods have been developed. It is known that the method of electrochemical protection is more effective and economical than any other method on the large scale metal structures in corrosive solutions. Strong acid solutions such as nitric and sulfuric acid solutions are often used in industries, and the expensive stainless steel is almost exclusively used for the equipment that comes in contact with such acid solutions. However, it is more reasonable that carbon steel is used rather than stainless steel depending upon concentration of those acid solutions from the economical viewpoint. In this study, the typical strong acid solution such as nitric and sulfuric acid solutions are chosen for the experiment and the selected materials of specimen are the stainless steels of SUS 304L and SUS 316L, the carbon steels of SS 41, SM 50 and RA 32, and highly pure lead. Electrochemical protection diagrams can be drawn with data from the external cathodic and anodic polarization curves of SUS 304L, SUS 316L and SM 50 steels in 5-60% nitric acid solutions and from those polarization curves of SS 41, RA 32, SM 50 and SUS 316L steels, and highly pure lead in 2.5-98% sulfuric acid solutions at the slow scanning rate. The data obtained with using the determination method of the optimum cathodic protection potential, the Tafel extrapolation method and the characteristics of anodic polarization curves. The main results obtained from the diagrams are as follows: 1) In nitric acid solution : (1) Corrosion potentials exist in each of those corrosion zones on the stainless steels in the lower concentration than about 12% solutions and on the high tensile strength steels in the lower concentration than about 30% solutions, but the corrosion current (density) in each zone is small on the above mentioned former steels and large on the latter ones. (2) The stainless steels can be self-passivated in the higher concentration than 15% solutions, and the high tensile strength steels gives rise to the same phenomenon in the higher concentration than 35% solutions. (3) The stainless steels in the lower concentration than 60% solutions and the high tensile strength steels in the higher concentration than 35% solutions can be used without protection, but the latter steels must ve protected anodically in the lower conccentration than about 30% solutions. 2) In sufuric acid solution : (1) The carbon steels can be self-passivated in the higher concentration than 45% solutions, and the SUS 316L steel in higher concentration than 75% solutions and the lead in all concentration solutions also gives rise to the same phenomenon. (2) The lead in the lower concentration than 80% solutions and the SUS 316L steel in the higher concentration than 80% solutions can be used without protection. (3) The carbon steels in the higher concentration than 50% solutions also can be used without protecting economically, but the SUS 316L steel in the 20-70% solutions are considerably corrosive without protecting anodically.

  • PDF

Creep Life Prediction of Friction Welded Joints (Cu-Alloy/STS316L) for Nuclear Power Plant (원자력 발전소용 마찰용접재 (Cu합금/STS316L)의 크리프 수명예측)

  • 유인종;공유식;오세규;김선진
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2001.10a
    • /
    • pp.258-263
    • /
    • 2001
  • In this paper, the real-time prediction of high temperature creep life was carried out for the friction welded joints of dissimilar heat resistintg steels (CulCr0.5Zr-STS316L). Various life prediction methods such as LMP (Larson-Miller Parameter) and ISM (initial strain method) were applied. The creep behaviors of those steels and the welds under static load were examined by ISM combined with LMP at 300, 400 and 50$0^{\circ}C$, and the relationship between these two methods was investigated. A real-time creep life (tsub/r/, hr) prediction equation by initial strain ($\varepsilon_0$, %) under any creep stress ($\sigma$, MP$\alpha$) at any high temperature (T, K) was developed

  • PDF

스퍼터링 방법을 이용한 사극 자석 진공용기 시제품 제작

  • Na, Dong-Hyeon;Park, Jong-Do;Ha, Tae-Gyun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.259-259
    • /
    • 2013
  • 4세대방사광 가속기의 언듈레이터 사이에 설치되는 사극자석 진공용기는 내경 12 mm, 길이 300 mm인 매우 얇고 긴 형태로 제작되어야 하며, 비자성체이면서 전기 전도도와 내부 표면 거칠기 또한 우수하여야 한다. 스테인리스강 316 L EP 튜브는 비자성체로써 기계가공성 및 내부 표면 거칠기가 우수하다. 또한 내부에 DC Magnetron Sputtering을 통하여 알루미늄 층을 형성함으로써 높은 전기 전도도를 확보할 수 있다. 여기서는 스테인리스강 316 L EP 튜브를 이용하여 손쉽게 사극 자석 진공용기를 제작한 후, Cylindrical Magnetron Sputtering System을 구성하여 내부에 균일한 알루미늄 층을 증착하는 공정에 대해 설명하려고 한다. 또한 치밀한 알루미늄 산화막을 형성하는 공정에 대하여 현재까지 수행한 결과를 정리하여 보고하며 앞으로의 개발 과정도 다루고자 한다.

  • PDF

THE DEVELOPMENT OF SUS 316L BONE PLATE FORGING PROCESS BY COMPUTER SIMULATION TECHNOLOGY

  • Hwang Robert S.;Jou Jin-Long;Wang Kai-Hung;Chen Yi-An
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2003.10b
    • /
    • pp.36-39
    • /
    • 2003
  • Due to the strength and biocompatibility requirement, the stainless steel SUS 316L is widely used for trauma internal fixation device. SUS 316L can be hardened and strengthened only by cold work. In this work, the material compression test is performed both in laboratory and computer simulation by a FEM analysis software DEFORM to correlate the hardness to strain. This data is then used for preform design and predict the hardness of the finish bone plate forging. Finally, we compared the hardness between the actual forging and computer analysis results. Although the predicted hardness from computer simulation. is 55HV higher than the final forging sample, we can get good compatibility on the hardening tendency of cold forging.

  • PDF