• 제목/요약/키워드: 316 Stainless Steel

검색결과 458건 처리시간 0.032초

열간정수압압축 시 확산기구 및 Power-law크립기구를 고려한 분말 치밀화거동의 모델링 (Modelling the Densification Behaviour of Powders Considering Diffusion and Power-Law Creep Mechanisms during Hot Isostatic Pressing)

  • 김형섭
    • 한국분말재료학회지
    • /
    • 제7권3호
    • /
    • pp.137-142
    • /
    • 2000
  • In order to analyze the densification behaviour of stainless steel powder compacts during hot isostatic pressing (HIP) at elevated temperatures, a power-law creep constitutive model based on the plastic deformation theory for porous materials was applied to the densification. Various densification mechanisms including interparticle boundary diffusion, grain boundary diffusion and lattice diffusion mechanisms were incorporated in the constitutive model, as well. The power-law creep model in conjunction with various diffusion models was applied to the HIP process of 316L stainless steel powder compacts under 50 and 100 MPa at $1125^{\circ}C$. The results of the calculations were verified using literature data. It could be found that the contribution of the diffusional mechanisms is not significant under the current process conditions.

  • PDF

분말야금 스테인리스 스틸의 산화특성에 미치는 조성 및 조직변화의 영향 (The Effects of Composition and Microstructure Variation on the Oxidation Characteristics of Stainless Steels Manufactured by Powder Metallurgy Method)

  • 이종필;홍지현;박동규;안인섭
    • 한국분말재료학회지
    • /
    • 제22권1호
    • /
    • pp.52-59
    • /
    • 2015
  • As well-known wrought stainless steel, sintered stainless steel (STS) has excellent high-temperature anti-corrosion even at high temperature of $800^{\circ}C$, and exhibits good corrosion resistance in air. However, when temperature increases above $900^{\circ}C$, the corrosion resistance of STS begins to deteriorate and dramatically decreases. In this study, the effects of phase and composition of STS on high-temperature corrosion resistances are investigated for STS 316L, STS 304 and STS 434L above $800^{\circ}C$. The morphology of the oxide layers are observed. The oxides phase and composition are identified using X-ray diffractometer and energy dispersive spectroscopy. The results demonstrate that the best corrosion resistance of STS could be improved to that of 434L. The poor corrosion resistance of the austenitic stainless steels is due to the fact that $NiFe_2O_4$ oxides forming poor adhesion between the matrix and oxide film increase the oxidation susceptibility of the material at high temperature.

청정도 가스 이송용 재료의 특성과 전해연마에 관한 연구 (A Study on the Characteristics of Electro Polishing and Utility Materials for Transit High Purity Gas)

  • 이종형;박신규;양성현
    • 한국산업융합학회 논문집
    • /
    • 제7권3호
    • /
    • pp.259-263
    • /
    • 2004
  • In the manufacture progress of LCD or semiconductor, there are used many kinds of gas like erosion gas, dilution gas, toxic gas as a progress which used these gas there are required high puritize to increase accumulation rate of semiconductor or LCD materials work progress of semiconductor or LCD it demand many things like the material which could minimize metallic dust that could be occured by reaction between gas and transfer pipe laying material, illumination of the surface, emition of the gas, metal liquation, welding etc also demand quality geting stricted. Material-Low-sulfur-contend (0.007-0010), vacuum-arc-remelt(VAR), seamless, high-purity tubing material is recommend for enhance welding lower surface defect density All wetted stainless steel surface must be 316LSS elecrto polishinged with ${\leq}0.254{\mu}m$($10.0{\mu}in$) Ra average surface finish, $Cr/Fe{\geq}1.1$ and $Cr_2O_3$ thickness ${\geq}25{\AA}$ From the AES analytical the oxide layer thickness (23.5~36 angstroms silicon dioxide equivalent) and chromum to iron ratios is similar to those generally found on electropolished stainless steel., molybdenum and silicon contaminants ; elements characteristic of stainless steel (iron, nickel and chromium); and oxygen were found on the surface Phosphorus and nitrogen are common contaminants from the electropolish and passivation steps.

  • PDF

316L 스테인리스강의 상온 반복 거동에 대한 수정 다층 모델의 적용성 검토 (Applicability Evaluation of Modified Overlay Model on the Cyclic Behavior of 316L Stainless Steel at Room Temperature)

  • 임재용;이순복
    • 대한기계학회논문집A
    • /
    • 제28권10호
    • /
    • pp.1603-1611
    • /
    • 2004
  • The validity of 'modified overlay model' to describe the cyclic behavior of annealed 316L stainless steel at room temperature was investigated. Material parameters(~f$_{i}$, m$_{i}$b, η, E) fur the model were obtained through constant strain amplitude test. The strain amplitude dependency of elastic limit and cyclic hardening, which were the characteristics of this model, were considered. Eight subelements were used to describe the nonlinearity of the hysteresis loops. The calculated hysteresis curve in each condition (0.5%, 0.7%, 0.9% train amplitude test) was very close to the experimental one. Two tests, incremental step test and 5-step test, ere performed to check the validity of 'modified overlay model'. The elastic limit was saturated to the one of the highest strain amplitudes of the block in the incremental step test, so it seemed to be Masing material at the stabilized block. Cyclic hardening was successfully described in the increasing sequence of the strain amplitude in 5-step test. But, the slight cyclic softening followed by higher strain amplitude would not be able to simulate by'modified overlay model'. However, the discrepancy induced was very small between the calculated hystereses and the experimental ones. In conclusion,'Modified overlay model'was proved to be appropriate in strain range of 0.35%~ 1.0%..0%.

STS304L 및 STS316L 용접부의 응력 부식 균열 개선을 위한 저온 분사 코팅의 잔류 응력 감소 효과에 대한 연구 (A Study on Residual Stress Reduction Effect of Cold Spray Coating to Improve Stress Corrosion Cracking of Stainless Steel 304L and 316L Welds)

  • 박광용;심덕남;하종문;이상동;조성우
    • 한국압력기기공학회 논문집
    • /
    • 제19권2호
    • /
    • pp.102-108
    • /
    • 2023
  • A Chloride-induced stress corrosion cracking (CISCC) of austenite stainless steel in dry cask storage system (DCSS) can occur with extending service time than originally designed. Cold spray coating (CSC) not only form a very dense microstructure that can protect from corrosive environments, but also can generate compressive stress on the surface. This characteristic of CSC process is very helpful to increase the resistance for CISCC. CSC with several powders, such as 304L, 316L and Ni can be optimized to form very dense coating layer. In addition, the impact energy generated as the CSC powder collides with the surface of base metal at a speed of Mach 2 or more can remove the residual tensile stress of welding area and serve the compress stress. CSC layers include no oxidation and no contamination with under 0.2% porosity, which is enough to protect from the penetration of corrosive chloride. Therefore, the CSC coating layer can be accompanied by a function that can be disconnected from the corrosive environment and an effect of improving the residual stress that causes CISCC, so the canister's CISCC resistance can be increased.

STS 316L 소결재료의 내식특성에 미치는 합금원소 첨가방법의 영향 (The Effect of the Additive Elements Alloying Method on the Corrosion Resistance of Sintered STS 316L)

  • 김혜성;김유영;박동규;안인섭
    • 한국분말재료학회지
    • /
    • 제20권3호
    • /
    • pp.203-209
    • /
    • 2013
  • In this study, STS 316L powders with 3 wt.% Cu and 1 wt.% Sn known as corrosion-resistance reinforcement elements, are prepared to make different kinds of specimens, in which, 3 wt.% Cu and 1 wt.% Sn are added in different forms by mixing, alloying and fully alloying. After sintering in the same condition, the corrosion resistance, wear resistance and their mechanical properties of specimens are tested respectively. According to the comparison, STS 316L specimen sintered at $1270^{\circ}C$ showed the most excellent mechanical property: HRB 78 (hardness), 1130.7 MPa (RCS), 26.6% (Fraction Wear), It was similar with the specimen made of STS316L and fully alloyed Cu and Sn powders, meanwhile, the latter one appears the best corrosion resistance, 75hrs-salt immersion test results. In addition, the specimens with Cu and Sn powders additive showed relatively worse wear resistance in compared with STS316L specimen.

THE DEVELOPMENT OF SUS 316L BONE PLATE FORGING PROCESS BY COMPUTER SIMULATION TECHNOLOGY

  • Hwang Robert S.;Jou Jin-Long;Wang Kai-Hung;Chen Yi-An
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 The 8th Asian Symposium on Precision Forging ASPF
    • /
    • pp.36-39
    • /
    • 2003
  • Due to the strength and biocompatibility requirement, the stainless steel SUS 316L is widely used for trauma internal fixation device. SUS 316L can be hardened and strengthened only by cold work. In this work, the material compression test is performed both in laboratory and computer simulation by a FEM analysis software DEFORM to correlate the hardness to strain. This data is then used for preform design and predict the hardness of the finish bone plate forging. Finally, we compared the hardness between the actual forging and computer analysis results. Although the predicted hardness from computer simulation. is 55HV higher than the final forging sample, we can get good compatibility on the hardening tendency of cold forging.

  • PDF

비수용성용액을 이용한 SUS316 전해연마시 첨가제 영향 고찰 (Effect of additives of non aqueous solution on the elelctrolytic polishing behaviors of austenitc stainless steel 316)

  • 김성완;김경태;이종석;김학성
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2012년도 춘계학술발표회 논문집
    • /
    • pp.303-304
    • /
    • 2012
  • 공업적으로 널리 사용되는 내식강의 전해연마는 주로 고농도의 인산염 전해액 기반에 황산과 질산 첨가된 용액에서 $70^{\circ}C$ 이상의 고온에서 행해지다 보니 폐액 처리와 작업 환경이 좋지 않아 기피 기술로 인식 되어 있다. 본 연구에서는 환경 친화적인 상온 공정을 개발 하고자 에틸렌 글리콜 용액에 여러 가지 첨가제를 첨가하여 그 효과를 살펴보고 최적 조성과 공정 조건을 확립 하고자 하였다. 틸렌 글리콜에 물과 질산 암모니움을 첨가하여 점도와 pH, 전류 전압 특성을 구하고 여기에 첨가제인 설파메이트와 암모니움 클로라이드 첨가량을 정하고 각각의 효과를 확인 하였다. 이러한 결과를 바탕으로 SUS 316 재질에 대한 최적 연마조건을 설정하기 위해 조도 변화, 광택도 및 표면 조직 변화와 전해연마기구를 비교 검토하였다.

  • PDF

반복 응력-변형률 시험을 통한 반복하중 조건에서 원전 주요 구조재료의 변형거동 평가 (Evaluation of Deformation Behavior of Nuclear Structural Materials under Cyclic Loading Conditions via Cyclic Stress-Strain Test)

  • 김진원;김종성;권형도
    • 한국압력기기공학회 논문집
    • /
    • 제13권1호
    • /
    • pp.75-83
    • /
    • 2017
  • This study investigated deformation behavior of major nuclear structural materials under cyclic loading conditions via cyclic stress-strain test. The cyclic stress-strain tests were conducted on SA312 TP316 stainless steel and SA508 Gr.3 Cl.1 low-alloy steel, which are used as materials for primary piping and reactor pressure vessel nozzle respectively, under cyclic load with constant strain amplitude and constant load amplitude at room temperature (RT) and $316^{\circ}C$. From the results of tests, the cyclic hardening and softening behavior, stabilized cyclic stress-strain behavior, and ratcheting behavior of both materials were investigated at both RT and $316^{\circ}C$. In addition, appropriate considerations for cyclic deformation behavior in the structural integrity evaluation of major nuclear components under excessive seismic condition were discussed.

Performance evaluation of plasma nitrided 316L stainless steel during long term high temperature sodium exposure

  • Akash Singh;R. Thirumurugesan;S. Krishnakumar;Revati Rani;S. Chandramouli;P. Parameswaran;R. Mythili
    • Nuclear Engineering and Technology
    • /
    • 제55권4호
    • /
    • pp.1468-1475
    • /
    • 2023
  • Enhancement of wear resistance of components used in fast reactors is necessary for long service life of the components. Plasma nitriding is a promising surface modification technology to impart high hardness and improved wear resistance of various steel components. This study discusses the characterization of chrome nitrided SS316L casing ring used in secondary sodium pump of fast breeder reactor and its stability under long term sodium exposure. Microstructural and hardness analysis showed that stress relieved component could be chrome nitrided successfully to a thickness of about 100 ㎛. Assessment of in-sodium performance of the chrome nitrided casing ring subjected to long term exposure up to 5000h at 550℃, showed retention of chrome nitrided layer with a case depth almost similar to that before sodium exposure. A slight decrease in the hardness was observed due to prolonged high temperature sodium exposure. Tribological studies indicate very low coefficient of friction indicating the retention of good wear resistance of the coating even after long term sodium exposure.