• 제목/요약/키워드: 316 Stainless Steel

검색결과 458건 처리시간 0.026초

고온 크리프 구조물의 장시간 한계응력강도 예측 (Prediction of Long-Term Stress Intensity Limit of High-Temperature Creep Structures)

  • 김우곤;류우석;김현희
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.648-653
    • /
    • 2003
  • In order to predict stress intensity limit of high-temperature creep structures, creep work-time equation, defined as $W_ct^P=B$, was used, and the results of the equation were compared with isochronous stress-strain curve (ISSC) ones of ASME BPV NH Code. For this purpose, the creep strain tests with. time variations for commercial type 316 stainless steel were conducted with different stresses; 160 MPa, 150 MPa, 145 MPa, 140 MPa and 135 MPa at $593^{\circ}C$. The results of log $W_c$ and log t plots showed a good linear relation up to $10^5$ hr. The constants p, B and stress intensity limit values showed comparatively good agreement to those of ASME NH ISSC. It is believed that the relation can be simply obtained with only several short-term 1% strain data without ISSC which can be obtained by long-term creep data.

  • PDF

스테인레스강 316LN의 전자빔용접과 협개선TIG 용접특성 비교 (The Comparison of Characteristic between Electron Beam Welding and Narrow-gap TIG welding with 316LN Stainless Steel)

  • 정인철;김용재;이경운;심덕남
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.82-84
    • /
    • 2005
  • Among the advanced welding processes which are superior to conventional process, Electron beam welding and Narrow-gap TIG welding are most prospective in being applicable for the heavy industry field. With STS316LN, which is high strengthened austenitic stainless steel, the characteristic evaluation for these welding processes was carried out through the mechnical tests and property analyses. For the tensile strength EBW is better while in reverse for the yield strength. In Narrow-gap TIG the distribution of hardness values has some deviation according to the thickness direction while EBW has a tendency of a litter high hardness values in weld metal. After EB welding brings the reduction of nitrogen content, in TIG welding weld metal depends on the contents of welding material. Both processes have almost austenitic structure, but weld metal of EBW is also shown terrific structure

  • PDF

실온 펄스도금법을 이용한 STS 316L 표면의 Ni 도금 저가형욕 연구 (Study of Ni-coating on 316L Stainless Steel by Pulse Electroplating in Various Bath Conditions at Room Temperature)

  • 정세진;조계현
    • 한국표면공학회지
    • /
    • 제35권1호
    • /
    • pp.53-63
    • /
    • 2002
  • Ni coating was carried out by pulse plating at room temperature. So, experimental conditions for Ni-coating were based on Watt's bath, and new additives(propionic acid) were introduced in the Watt's bath electrolyte as $H_3$$BO_3$ alternatives. By adding propionic acid, coating layer demonstrated a good adhesion and uniformity without special pre-treatment of the 316L stainless steel at room temperature. With a decrease of amount of propionic acid and applied average current density, cathode current efficiency increased. Also, edge effect was decreased with decreasing a peak current and increasing a pulse frequency in the same bath condition. It was found that the optimum condition for Ni coating was a current density of 10~20mA/$\textrm{cm}^2$ at below 500 mA peak current in the $5m\ell/\ell$ propionic acid solution.

Hybrid Microstructure and Mechanical Properties of HRS Processed SUS316L and Titanium Materials

  • Fujiwara, Hiroshi;Ohta, Koichi;Noro, Atsushi;Ameyama, Kei
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.540-541
    • /
    • 2006
  • SUS316L stainless steel, commercial pure Titanium and Ti-6Al-4V alloy powders applied by Mechanical Milling (MM) process are sintered by Hot Roll Sintering (HRS) process. Microstructure and mechanical properties of those HRS materials is investigated. The microstructures of materials produced by HRS process consist of fine grains and work-hardened structure, that is, the hybrid microstructure. Tensile test of the HRS material demonstrated the good mechanical properties. These results show that the HRS process is very effective to the improvement of mechanical properties in the SUS316L stainless steel, commercial pure Titanium and Ti-6Al-4V alloy.

  • PDF

AISI316L stainless steel에 저온 프라즈마 침탄처리 후 질화처리 시 $N_2$ 가스조성이 표면특성에 미치는 영향 (Effects of $N_2$ gas composition on the surface properties of AISI316L stainless steel during low temperature plasma nitriding after low temperature plasma carburizing)

  • 정광호;이인섭
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2007년도 추계학술대회 논문집
    • /
    • pp.157-158
    • /
    • 2007
  • AISI316L강의 내식성과 표면경도를 동시에 향상시키기 위한방법으로 저온 플라즈마 침탄과 저온 플라즈마 질화를 동일한 로 내에서 연속적으로 실시하였다. 여러 가지 공정인자 중 저온 플라즈마 질화 시 $N_2$가스가 표면에 미치는 영향을 조사 하였다. 모든 시편의 표면에 N에 의해 확장된 오스테나이트 (${\gamma}_N$)가 형성되었으며, 형성된 ${\gamma}_N$로 인하여 표면경도가 약 $3{\sim}4$배 증가하였다. $N_2$가스가 증가할수록 ${\gamma}_N$층의 두께가 증가 하였다.

  • PDF

AISI 316 스테인레스강의 $CO_2$ 레이저 용접 (High Power $CO_2$ Laser Beam Welding of AISI 316 Stainless Steel)

  • 김재도
    • Journal of Welding and Joining
    • /
    • 제9권2호
    • /
    • pp.29-36
    • /
    • 1991
  • 6mm 두께의 AISI 316 스테인레스강의 레이저 용접 특성에 대해서 고찰하였다. 3kW C $O_{2}$레이저를 사용하였으며, 레이저 빔은 TE $M_{00}$모우드였고 연속파이었다. 용입 깊이, 비드 폭, 고온 크랙, 가공등의 특성을 고찰하는데 있어서, 레이저 출력은 1kW에서 2.5kW까지, 용접 속도는 5.1m/min까지 적용하였다. 3차원 열전달 방정식에 의한 용입 깊이와 비드 폭에 대한 예측치와 실험 결과를 비교하였는데, 서로 잘 일치하였다.다.

  • PDF

Stress-assisted oxidation behaviour of inconel 52M/316 austenitic stainless-steel dissimilar weld joints in a simulated pressurised water reactor

  • Xu, Youwei;Yang, Binhui;Shi, Yu
    • Nuclear Engineering and Technology
    • /
    • 제54권10호
    • /
    • pp.3778-3787
    • /
    • 2022
  • The stress-assisted oxidation behaviour of Inconel 52 M/316 austenitic stainless-steel (SS) dissimilar weld joints (DMWJ) in a simulated pressurised water reactor environment was investigated. A corrosion galvanic couple formed between the Inconel 52 M and 316 SS due to differences in their nonferrous metal content. The electric field from the corrosion couple attracted metal cations (e.g. Fe2+, Cr3+) to the Inconel 52 M that were deposited as FeCr2O4. An additional corrosion galvanic couple was generated due to variations in the plastic deformation of the DMWJ. The superposition of electric fields from the different couples resulted in ridge-like oxide depositions in the fusion zone.

Microstructure and properties of 316L stainless steel foils for pressure sensor of pressurized water reactor

  • He, Qubo;Pan, Fusheng;Wang, Dongzhe;Liu, Haiding;Guo, Fei;Wang, Zhongwei;Ma, Yanlong
    • Nuclear Engineering and Technology
    • /
    • 제53권1호
    • /
    • pp.172-177
    • /
    • 2021
  • The microstructure and texture of three 316L foils of 25 ㎛ thickness, which were subjected to different manufacturing process, were systematically characterized using advance analytical techniques. Then, the electrochemical property of the 316L foils in simulated pressurized water reactor (PWR) solution was analyzed using potentiodynamic polarization. The results showed that final rolling strain and annealing temperature had evident effect on grain size, fraction of recrystallization, grain boundary type and texture distribution. It was suggested that large final rolling strain could transfer Brass texture to Copper texture; low annealing temperature could limit the formation of preferable orientations in the rolling process to reduce anisotropy. Potentiodynamic polarization test showed that all samples exhibited good corrosion performance in the simulated primary PWR solution.

조사취화를 모사한 스테인레스강의 파괴저항선도를 예측하기위한 유한요소 손상해석기법 (Finite Element Damage Analysis Method for J-Resistance Curve Prediction of Cold-Worked Stainless Steels)

  • 서준민;김지수;김윤재
    • 한국압력기기공학회 논문집
    • /
    • 제14권1호
    • /
    • pp.1-7
    • /
    • 2018
  • Materials in nuclear power plants can be embrittled by neutron irradiation. According to existing studies, the effect of the material property by irradiation embrittlement can be approximately simulated by cold working (pre-strain). In this study, finite element damage analysis method using the stress-modified fracture strain model is proposed to predict J-Resistance curves of irradiated SUS316 stainless steel. Experimental data of pre-strained SUS316 stainless steel material are obtained from literature and the damage model is determined by simulating the tensile and fracture toughness tests. In order to consider damage caused by the pre-strain, a pre-strain constant is newly introduced. Experimental J-Resistance curves for various degrees of pre-strain are well predicted.

316L 스테인리스강 원통 구조물의 열라체팅 변형 시험 및 해석 (Test and Analysis of Thermal Ratcheting Deformation for 316L Stainless Steel Cylindrical Structure)

  • 이형연;김종범;이재한
    • 대한기계학회논문집A
    • /
    • 제26권3호
    • /
    • pp.479-486
    • /
    • 2002
  • In this study, the progressive inelastic deformation, so called, thermal ratchet phenomenon which can occur in high temperature structures of liquid metal reactor was simulated with thermal ratchet structural test facility and 316L stainless steel test cylinder. The thermal ratchet deformation at the reactor baffle cylinder of the liquid metal reactor can occur due to the moving temperature distribution along the axial direction as the sodium free surface moves up and down under the cyclic heat-up and cool-down transients. The ratchet deformation was measured with the laser displacement sensor and LVDTs after cooling the structural specimen which is heated up to 55$0^{\circ}C$ with steep temperature gradients along the axial direction. The temperature distribution of the test cylinder along the axial direction was measured with 28 channels of thermocouples and was used for the ratchet analysis. The thermal ratchet deformation was analyzed with the constitutive equation of nonlinear combined hardening model which was implemented as ABAQUS user subroutine and the analysis results were compared with those of the test. Thermal ratchet load was applied 9 times and the residual displacement after 9 cycles of thermal load was measured to be 1.79mm. The ratcheting deformation shapes obtained by the analysis with the combined hardening model were in reasonable agreement with those of the structural tests.