Chloride ion diffusion at the corner of rectangular-shaped concrete structures is presented. At the corner of rectangular-shaped concrete, chloride ion diffusion is in two-dimensional process. Chloride ions accumulate from two orthogonal directions, so that corrosion-free life of concrete structures is significantly reduced. A numerical procedure based on finite element method is used to solve the two-dimensional diffusion process. Orthotropic property of diffusion coefficient of concrete is considered and chloride ion profile obtained from numerical analysis is used to produce transformed diffusion coefficient. Comparisons of experimental data are also carried out to show the reliability of proposed numerical analysis. As a result of two-dimensional chloride diffusion, corrosion-free life of concrete structure for railway is estimated using probability of corrosion initiation. In addition, monographs that produces transformed diffusion coefficient and corrosion-free life of concrete structure are made for maintenance purpose.
Crack on concrete surface allows more rapid penetration of chlorides. Crack width and depth are dominant parameters for chloride behavior, however their effects on chloride penetration are difficult to quantify. In the present work, the previous anisotropic (1-D) model on chloride diffusion in concrete with single crack is improved considering crack shape and roughness. In the previous model, parallel-piped shape was adopted for crack shape in steady-state condition. The previous model with single crack is improved considering wedge shape of crack profile and roughness. For verifying the proposed model, concrete samples for nuclear power plant are prepared and various crack widths are induced 0.0 to 1.2 mm. The chloride diffusion coefficients in steady-state condition are evaluated and compared with simulation results. The proposed model which can handle crack shape and roughness factor is evaluated to decrease chloride diffusion and can provide more reasonable results due to reduced area of crack profile. The roughness effect on diffusion is evaluated to be 10-20% of reduction in chloride diffusion.
Lee, Bang Yeon;Ismail, Mohamed A.;Kim, Hyeok-Jung;Yoo, Sung-Won;Kwon, Seung-Jun
Computers and Concrete
/
제20권2호
/
pp.185-196
/
2017
Durability problems initiated from steel corrosion are unseen but critical issues, so that many researches are focused on chloride penetration evaluation. Even if RC (Reinforced Concrete) structures are exposed to normal environment, chloride ingress varies with concrete surface conditions and exposed period. This paper presents an analysis technique for chloride behavior evaluation considering time effect on diffusion and surface conditions assumed as double-layered system. For evaluation of deteriorated surface condition, field investigation was performed for concrete pavement exposed to deicing agent for 18 years. In order to consider enhanced surface concrete, chloride profiles in surface-impregnated concretes exposed to chloride attack for 2 years from previous research were investigated. Through reverse analysis, effectively deteriorated/enhanced depth of surface and the related reduced/enlarged diffusion coefficient in the depth are simulated. The proposed analysis technique was evaluated to handle the chloride behavior more accurately considering changes of chloride ingress within surface layer and decreased diffusion coefficient with time. For the concrete surface exposed to deicing agent, the deteriorated depth and enlarged diffusion coefficient are evaluated to be 12.5~15.0 mm and 200% increasing diffusion coefficient, respectively. The results in concrete containing enhanced cover show 10.0~12.5 mm of impregnated depth and 85% reduction of chloride diffusion in tidal and submerged conditions.
International Journal of Concrete Structures and Materials
/
제10권1호
/
pp.61-73
/
2016
In predicating the probability distribution of chloride diffusion coefficient of recycled aggregate concrete ($D_{RAC}$), the morphological characteristics of three phases, i.e., the old attached mortar, the natural aggregate and the new mortar, should all be taken into account. The present paper attempts to develop a probability density evolution method (PDEM) to achieve this. After verifying the derived PDEM results with experimental results, the effects of old attached mortar to the $D_{RAC}$ are examined in a quantitative manner. It is found that (1) the variation of the attached mortar content is much sensitive to $D_{RAC}$; (2) given the probability distribution of the content and chloride diffusion coefficient of old mortar, the probability distribution of DRAC can be analysed based on the PDEM; and (3) the critical chloride diffusion coefficient at a certain assurance rate can be obtained by the PDEM. The analysis results of this investigation will be valuable to the durability design for RAC.
This paper mainly discusses the influence of the aggregate properties including grading, shape, content and distribution on the chloride diffusion coefficient, as well as the initiation time of steel corrosion from a probabilistic point of view. Towards this goal, a simulation method of random aggregate structure (RAS) based on elliptical particles and a procedure of finite element analysis (FEA) at meso-scale are firstly developed to perform the analysis. Next, the chloride diffusion coefficient ratio between concrete and cement paste $D_{app}/D_{cp}$ is chosen as the index to represent the effect of aggregates on the chloride diffusion process. Identification of the random distribution of this index demonstrates that it can be viewed as actually having a normal distribution. After that, the effect of aggregates on $D_{app}/D_{cp}$ is comprehensively studied, showing that the appropriate properties of aggregates should be decided by both of the average and the deviation of $D_{app}/D_{cp}$. Finally, a case study is conducted to demonstrate the application of this mesoscopic method in predicting the initiation time of steel corrosion in reinforced concrete (RC) structures. The mesoscopic probabilistic method developed in this paper can not only provide more reliable evidences on the proper grading and shape of aggregates, but also play an important role in the probability-based design method.
균열을 가진 콘크리트에서는 균열폭으로 유입되는 염화물 이온에 의해 열화가 가속화된다. 본 연구는 균열을 가진 콘크리트의 염화물 확산에 대한 모델링으로, 정상상태를 가정하여 1차원 (이방성) 및 2차원 (등방성) 균열 모델링을 수행하였다. 기존의 균열 모델링에서는 직사각형 균열패턴으로 모델링을 수행하였으나, 본 연구에서는 조도를 가진 쐐기형 형태로 균열을 모델링하였다. 검증을 위하여 1차원 유입에 대해서는 콘크리트 시편에 균열을 유입하여 염화물 영동실험을 수행하였으며, 2차원 유입에 대해서는 기존의 실험결과를 이용하여 검증을 수행하였다. 모든 경우에서 균열형태를 쐐기형으로 고려하여 염화물 확산성이 감소되었으며, 조도를 고려함으로서 합리적인 결과가 도출되었다. 특히 0.10~0.15의 조도계수를 고려할 때, 실험값에 가장 근접한 결과를 나타내었다.
콘크리트 표면의 상태에 따라 염화물은 증가 또는 감소하게 되며 이는 철근부식 및 내구수명에 매우 중요한 인자가 된다. 콘크리트의 내구성 저하를 방지하기 위해 표면함침과 같이 많은 표면강화 기술이 개발되었으나 이중 콘크리트 구조와 확산계수의 시간의존성을 고려한 염화물 해석방법은 매우 제한적이다. 본 논문에서는 표면 강화된 이중구조 콘크리트에 대해 시간의존성 확산계수를 도입하여 염화물 해석기법을 제안하였으며, 역해석을 통하여 기존의 실험결과와 비교하였다. 2년간 비말대, 해수중, 조석대 상태에 노출된 표면 함침된 콘크리트 시편에 대해 표면염화물량과 확산계수를 도출하고 Life-365에서 제안한 확산계수 식과 비교 분석하였다. 시간의존성을 고려한 결과 비말대 시편의 오차는 0.28에서 0.20 수준으로, 조석대 시편은 0.29에서 0.11 수준으로, 해수중에서는 0.54에서 0.40 수준으로 오차가 감소함을 알 수 있었다. 또한 Life365에서 사용되는 확산계수식을 사용할 경우, 과다한 확산계수로 인해 상대오차가 커지고 높은 침투깊이(e)와 낮은 확산계수비($D_1/D_2$)를 필요로 함을 알 수 있다.
To investigate the role of RH and temperature on the transport of chloride in the concrete, two groups of specimens were configured. For both groups, mix design was based on w/c=0.45, $400kg/m^3$ cement, $794kg/m^3$ fine aggregate and $858kg/m^3$ coarse aggregate. After specimen fabrication these were exposed to four different RH (35, 55, 75 and $95\%$ RH) and temperature (0, 20, 30 and $40^{\circ}C$) conditions. After 3 and 6 months $15\%$ NaCl exposure 5mm cores were taken. These cores were sliced and individual cores were ground to powder. In addition, to evaluate the effect of temperature on the chloride binding some powder samples were leached in the each of four temperature chambers. Chloride titration fur these was performed using FDOT acid titration method. Based upon the resultant data conclusions were reached regarding that 1) effective diffusion coefficient, $D_e$, increased with increasing exposure RH, suggesting that the size and number of water paths increased with elevated moisture content in the specimens, 2) $D_e$ increased with increasing temperature in the range of 0 to $40^{\circ}C$ possibly by elevated thermal activation of chloride ions and reduced chloride binding at higher temperature, 3) water soluble chloride concentration, $[Cl^-]_s$, increased with increasing temperature, and 4) chloride concentration profile for initially dry concrete specimens was higher than for the initially wet ones indicating pronounced capillary suction (sorption) occurred for the dry concrete specimens.
본 연구에서는 해안 환경에 노출된 콘크리트 구조물의 내구성 평가에 대한 모델을 표면 염소이온농도 $(C_s)$의 시간에 대한 증가와 염소이온 확산계수 (D) 및 임계염소이온농토 $(C_{lim})$를 고려하여 제안하였다. 또한 콘크리트 구조물의 정밀한 내구수명 예측을 위하여 $C_s$와 D의 시간의존성이 고려되었으며, 시간에 따라 변화하는 $C_s$를 고려한 Fick의 제2법칙의 정밀해를 구하였다. $C_s$의 시간의존성에 대해서는, 기존 실험 결과를 바탕으로 시간에 대한 대수 함수 형태의 $C_s$ 모델을 제안하였으며, D의 시간의존성을 고려하기 위하여 구조물의 전체 노출 기간에 대한 시간의 평균값을 적용하였다. 또한 염해 환경 하에 있는 철도 구조물이 100년의 내구 수명을 보장할 수 있도록 하기 위해, 본 논문에서 제안된 모델과 시방서 기준에 근거하여 내구성 설계를 수행하였다. 제안된 모델은 유럽에서 널리 사용되고 있는 성능 중심의 설계 기법에 의해 검증되었으며, 이로부터 기존의 시방서 설계기준은 해안 환경에 노출된 콘크리트 구조물의 내구 성능을 과소 평가하여 매우 보수적인 설계결과를 유발하고 있음을 알 수 있다. $C_s$와 D의 시간의존성을 고려한 본 모델은 기존 시방기준의 이러한 문제점을 개선하여 염해를 받는 콘크리트 구조물의 내구수명을 정확하고 합리적으로 평가할 수 있을 것이다.
Cement of three alkalinities (equivalent alkalinities of 0.36,0.52 and 0.97) was employed in fabricating a set of classical G109 type specimens. To-date, these have been subjected to a one week wet-one week dry cyclic pending using 15 w/o NaCl solution. At the end of the dry period, potential and macro-cell current were measured to indicate whether the top reinforcing steel was in the passive or active state. Once this bar became active, the specimen was autopsied and the extent of corrosion was documented. Subsequent to visual inspection, concrete powder samples were collected from the upper region of the top rebar trace; and at a certain times concrete cores were taken from non-reinforced specimens. Using these, determinations were made of (1) critical chloride concentration for corrosion initiation ($Cl_{th}^-$), (2) effective chloride diffusion coefficient ($D_e$), and (3) pore water alkalinity ($[OH^-]$). The pore water alkalinity was strongly related to the alkali content of cement that was used in the mix. The chloride concentration, ($Cl^-$), was greater at active than at passive sites, presumably as a consequence of electro migration and accumulation of these species at active site subsequent to corrosion initiation. Accordingly, ($Cl^-$) at passive sites was considered indicative of the threshold concentration fur corrosion initiation. The $Cl_{th}^-$ was increased with increasing Time-to-corrosion ($T_i$). Consequently, the HA(High Alkalinity) specimens exhibited the highest $Cl_{th}^-$ and the NA(Normal Alkalinity) was the least. This range exceeds what has previously been reported in North America. In addition, the effective diffusion coefficient, $D_e$, was about 40 percent lower for concrete prepared with the HA cement compared to the NA and LA(Low Alkalinity) ones.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.