다이아몬드 강화 Cr 기반 소재의 정량적 마모 특성 평가 (Quantitative Assessment of Wear Characteristics of Cr-based Coating Reinforced with Diamond)

  • 후인 옥-팟;부 아 린;정구현
    • Tribology and Lubricants
    • /
    • 제38권1호
    • /
    • pp.15-21
    • /
    • 2022
  • Diamond reinforced Cr-based coating has been proposed as wear-resistant materials. In this study, the friction and wear characteristics of diamond reinforced Cr-based coating are experimentally assessed. The experiments are performed using a pin-on-reciprocating plate tribo-tester under various normal forces with boundary lubrication. The stainless-steel ball is used as a counter material. Prior to the experiments, mechanical properties such as elastic modulus and hardness are determined using nanoscale instrumented indentation. The hardness of the specimen is further determined using a Vickers hardness tester. The specimens before and after the experiments are carefully observed using a confocal microscope to understand the wear characteristics. In addition, the wear volume and wear rate of the specimens are determined based on the confocal microscope data. The results show that the friction coefficients are 0.096-0.100 under 20-40 N normal forces. Furthermore, the wear rates of the diamond reinforced Cr-based coating and the stainless steel ball under 20-40 N normal forces are found to be 12.8 × 10-8 mm3/(Nm)-15.5 × 10-8 mm3/(Nm) and 1.9 × 10-8 mm3/(Nm)-3.9 × 10-8 mm3/(Nm), respectively. However, the effect of the normal force on wear rates is not clearly observed, which may be associated with the flattening of the ball. The results of the study may be useful for the tribological applicability of diamond reinforced Cr-based coating as wear-resistant materials.

초초임계압 발전용 소재의 표면처리층의 고온 안정성 평가 (High-Temperature Stability Evaluation of Various Surface Treated Layers of Materials for Ultra-Super Critical Power Plants)

  • 류경환;송태권;이재현;김길수;이선호;엄기원
    • 한국재료학회지
    • /
    • 제16권5호
    • /
    • pp.329-335
    • /
    • 2006
  • In order to improve thermal efficiency of the fossil fuel power plants, we need to develop advanced materials with superior durability in the ultra-super critical state, which requires surface modifications for superior surface properties. In this study, we coated the Incoloy 901 and 12-17Cr steels for turbine buckets and valves with nitriding, boriding, and $Cr_3C_2-NiCr$ HVOF(high velocity oxygen flow) method. Then the samples were heat treated at $650^{\circ}C$ for 100 hours in vacuum. We analyzed the evolution behaviors of nitrides such as $Fe_3N,\;Fe_4N$, and CrN and borides such as FeB and $Fe_2B$ with XRD and SEM/EDS by comparing hardnesses and compositions of the coated layers before and after the heat treatments.

금속의 내식성 향상을 위한 환경 친화형 무크롬 유기화합물의 표면처리 (Surface treatments of environmentally friendly Cr-free organic compounds for corrosion protection of metals)

  • 이원기;박찬영
    • 한국환경과학회지
    • /
    • 제12권7호
    • /
    • pp.801-807
    • /
    • 2003
  • This work aims the search of environmentally friendly pre-treatment technologies to develop chromate replacements for metal finishing industries due to its toxicological properties. Since the corrosion resistance of steel was strongly related to water permeation, galvanized steel sheets were treated with various hydrophobic silane compounds and water-suspended polymer solution. Also, plasma gas discharge was applied to modify the surface of a polymer coated-steel sheet to be hydrophobic. The surface hydrophobicity of materials was introduced by CF$_3$H plasma exposure. The corrosion property before and after the plasma treatment was investigated in a slat spray tester with 3.5 wt.% NaCl at 35$^{\circ}C$. The results showed that both silane/polymer double coatings and plasma treatment of the galvanized steel exhibited significant retardation of corrosion.

SP-Creep 시험에 의한 고온 크리프 특성 평가 기술 개발(I) - 보일러 과열기 튜브 - (Development of Evaluation Technique of High Temperature Creep Characteristics by Small Punch-Creep Test Method (I) - Boiler Superheater Tube -)

  • 백승세;나성훈;나의균;유효선
    • 대한기계학회논문집A
    • /
    • 제25권12호
    • /
    • pp.1995-2001
    • /
    • 2001
  • In this study, a small punch creep(SP-Creep) test using miniaturized specimen(10${\times}$10${\times}$0.5mm) is described to develop the new creep test method for high temperature structural materials. The SP-Creep test is applied to 2.25Cr-lMo(STBA24) steel which is widely used as boiler tube material. The test temperatures applied for the creep deformation of miniaturized specimens are between 550∼600$^{\circ}C$. The SP-Creep curves depend definitely on applied load and creep temperature, and show the three stages of creep behavior like in conventional uniaxial tensile creep curves. The load exponent of miniaturized specimen decreases with increasing test temperature, and its behavior is similar to stress exponent behavior of uniaxial creep test. The creep activation energy obtained from the relationship between SP-Creep rate and test temperature decreases as the applied load increases. A predicting equation or SP-Creep rate for 2.25Cr-lMo steel is suggested. and a good agreement between experimental and calculated data has been found.

PVDF 수침용 고주파수 초음파 탐촉자의 검출장과 Cr-Ni 강에서의 결함 검출능 측정 (Characteristics of High Frequency Ultrasonic Transducer Employing Polyvinylidene Fluoride and Detectability of Flaw in Cr-Ni Steel)

  • 김병극;이승석
    • 비파괴검사학회지
    • /
    • 제17권1호
    • /
    • pp.23-30
    • /
    • 1997
  • 최근 시료 내부의 미세 결함의 측정을 위하여 초음파의 발생 소자로 polyvinylidene fluoride(PVDF)나 polyvinylidene fluoride trifluoroethylene P(VDF-TrFE) 압전 재료를 사용한 광대역 고주파수 초음파 탐촉자가 이용되고 있다. 중심 주파수 80MHz의 PVDF 수침용 집속형 초음파 탐촉자의 특성과 물과 시료에서의 초음파의 검출장을 측정하였으며 강재 시편에서의 결함 검출능을 측정하였다. 물과 강재 시험편에서 고주파수 초음파의 감쇠가 결함 검출능을 좌우하는 주요 변수이었다. 작은 결정립을 지닌 크롬-니켈강 재료를 사용하여 12mm 깊이에 직경 $50{\mu}m$에서 $560{\mu}m$ 범위의 flat-bottom hole들을 가공한 시편을 준비하였고 C-scan과 B-scan을 수행하였다. 직경 $280{\mu}m$ 이상의 flat-bottom hole들은 검출되었고 파장에 대한 결함 크기의 비가 약 0.48 이하의 결함은 검출되지 않았다. 시편에 초음파의 고주파수 성분이 입사되었으나 약 25MHz 이상의 고주파수 성분이 시편내의 초음파의 전파 경로에서 모두 감쇠되어 더 작은 결함에 대한 검출장이 형성되지 못했다.

  • PDF

유지시간 효과를 고려한 12Cr 내열강의 열피로 및 저주기 피로 특성 (Thermal-Mechanical and Low Cycle Fatigue Characteristics of 12Cr Heat Resisting Steel with Hold Time Effects)

  • 하정수;고승기;옹장우
    • 한국자동차공학회논문집
    • /
    • 제3권1호
    • /
    • pp.1-12
    • /
    • 1995
  • Isothermal and thermal-mechanical fatigue characteristics of 12Cr heat resisting steel used for high temperature applications were investigated including hold time effects. Isothermal low cycle fatigue test at $600^{\circ}C$ and in-phase, out-of-phase thermal-mechanical fatigue test at 350 to $600^{\circ}C$ were conducted using smooth cylindrical hollow specimen under strain-control with total strain ranges from 0.006 to 0.015. Regardless of thermal-mechanical and isothermal fatigue tests, cyclic softening behavior was observed and much more pronounced in the thermal-mechanical fatigue tests with hold times due to the stress relaxation during the hold time. The phase difference between temperature and strain in thermal-mechanical fatigue tests resulted in significantly shorter fatigue life for out-of-phase compared to in-phase. The differences in fatigue lives were dependent upon the magnitudes of plastic strain ranges and mean stresses. During the hold time in the strain-controlled fatigue tests, the increase in the plastic strain range and the stress relaxation were observed. It appeared that the increase in plastic strain range per cycle and the introduction of creep damage made important contributions to the reduction of thermal-mechanical fatigue life with hold time, and the life reduction tendency was more remarkable in the in-phase than in the out-of-phase thermal-mechanical fatigue. Isothermal fatigue tests performed under the combination of fast and slow strain rates at $600^{\circ}C$ showed that the fatigue life decreased as the strain rate and frequency decreased,especially for the low strain ranges.

  • PDF

후방복사된 초음파를 이용한 12Cr강 부식 피로특성 평가 (Evaluation of Corrosion Fatigue Characteristics of 12Cr Steel Using Backward Radiated Ultrasound)

  • 권성덕;윤석수;송성진;배동호
    • 비파괴검사학회지
    • /
    • 제20권5호
    • /
    • pp.397-401
    • /
    • 2000
  • 화력발전 플랜트의 터빈 블레이드(blade) 재료인 12Cr 합금강의 고속 열화 시편에 대한 레일리(Rayleigh) 표면탄성파의 산란과 속도의 주파수 의존특성을 액체/고체 경계 면에서 표면파의 발생기구에 의해 나타나는 후방복사 초음파 세기의 입사각 의존성으로 간접 평가하고 부식피로 특성과 비교 분석하였다. 후방복사 현상이 발생하는 입사각 폭은 부식온도와 반비례하였으며 이는 효과적 부식층의 두께 증가로 설명되었다. 이 프로파일의 폭은 피로시험에서 균열성장 관계식인 파리스(Paris) 법칙의 지수 m과 선형적으로 반비례하여 열화시편의 부식 피로 특성의 비파괴적 평가에 있어 후방복사된 초음파를 이용한 기술이 매우 유용함을 보여 보여주었다.

  • PDF

CrMoV강 용접부의 주기적 열시효처리에 따른 미세조직, 미세경도 및 인장강도 특성 (A Characteristic of microstructural evolution, microhardness and tensile properties in CrMoV rotor steel weldment experienced by the cyclic thermal aging heat treatment)

  • 김광수;고진현
    • 열처리공학회지
    • /
    • 제12권4호
    • /
    • pp.303-312
    • /
    • 1999
  • An investigation of the CrMoV rotor steel weldment which experienced by cyclic thermal aging heat treatment and as-received condition was performed. This evaluation was carried out to confirm whether this type of weldment is appropriate for the service environment in terms of microstructural examinations, microhardness measurements and tensile tests. The cyclic thermal aging heat treatment, containing continuous heating and cooling thermal cycle was programmed to simulate the real rotor service condition. The heat treatment was performed for 40 cycles(5920hrs). The results indicated that the weldment was composed of 4 different regions such as heat affected zone of the base metal, butter weld(initial weld), full thickness weld(final weld) and the base metal. The double welding process was applied to eliminate the susceptibility of reheat cracking at heat affected zone of base metal. The grain refinement at the HAZ due to the welding process could reduce the possibility of cracking susceptibility, but its tensile properties was appeared to be low due to the weld metal in as-received condition. The benefit effect, grain refinement was extended with carbides coarsening during the cyclic thermal aging heat treatment. However the poor mechanical properties of the weldment was more degraded as undergoing the heat treatment.

  • PDF

단상영역에서 압연된 API X80 라인파이프강의 인장 및 샤르피 충격 특성에 미치는 Mo, Cr, V의 영향 (Effect of Mo, Cr, and V on Tensile and Charpy Impact Properties of API X80 Linepipe Steels Rolled in Single Phase Region)

  • 한승엽;신상용;서창효;이학철;배진호;김기수;이성학;김낙준
    • 대한금속재료학회지
    • /
    • 제46권12호
    • /
    • pp.788-799
    • /
    • 2008
  • This study is concerned with the effects of Mo, Cr, and V addition on tensile and Charpy impact properties of API X80 linepipe steels. Four kinds of steels were processed by varying Mo, Cr, and V additions, and their microstructures and tensile and Charpy impact properties were investigated. Since the addition of Mo and V promoted to form fine acicular ferrite and granular bainite, while prohibiting the coarsening of granular bainite, it increased the strength and upper shelf energy, and decreased the energy transition temperature. The Cr addition promoted the formation of coarse granular bainite and secondary phases such as martensite-austenite constituents, thereby leading to the increased effective grain size, energy transition temperature, and strength and to the decreased upper shelf energy. The steel containing 0.3wt.% Mo and 0.06wt.% V without Cr had the highest upper shelf energy and the lowest energy transition temperature because its microstructure was composed of fine acicular ferrite and granular bainite, together with a small amount of hard secondary phases, while its tensile properties maintained excellent.

저압터빈용 로터강의 이축 피로수명예측법에 관한 연구 (Study of Axial and Torsional Fatigue Life Prediction Method for Low Pressure Turbine Rotor Steels)

  • 현중섭;송기욱;이영신
    • 한국정밀공학회지
    • /
    • 제22권12호
    • /
    • pp.149-155
    • /
    • 2005
  • The rotating components such as turbine rotors in service are generally subjected to multiaxial cyclic loading conditions. The prediction of fatigue lift for turbine rotor components under complex multiaxial loading conditions is very important to prevent the fatigue failures in service. In this paper, axial and torsional low cycle fatigue tests were preformed for 3.5NiCrMo steels serviced low pressure turbine rotor of nuclear power plant. Several methods to predict biaxial fatigue life such as Tresca, von Mises and Brown & Miller's critical plane approach were evaluated to correlate the experimental results for serviced NiCrMoV steel. The fracture mode and fatigue characteristics of NiCrMoV steel were discussed based on the results of fatigue tests performed under the axial and torsional test conditions. In particular, the Brown and Miller's critical plane approach was found to best correlate the experimental data with predictions being within a factor of 2.