  • Kinetic characteristics dependent on several factors such as iron mineral and organic solvents were investigated. When F $e^{0}$ , FeS and Fe $S_2$ were used as mediators, minerals affecting reaction rate were in the following order : $Fe_{0}$ 0/ > FeS > $FeS_2$ when in contact $C_2$C $l_{6}$ . The more chloride substituted, the higher reaction rate were observed. The reaction rates were dependent on pH, shaking rate, temperature and specific surface area. 1, 10-phenanthroline and EDTA degradation rates were fast, indicating that they adsorbed on the surface of the iron which makes the electron transfer reaction easy. Nitrate which has $\pi$* orbital of molecular can increase electron transfer rate because it is delocalized in its entity. The reaction rates were not affected by hydroquinone. Degradation rates were much enhanced with naturally occurring kaolinite because of the surface corrosion of Fe mineral. However, The reaction rate was not affected by F $e^{2+}$ or S $O_4$$^{2-}$ presented in solution.n.

Nitrate Reduction without Ammonium Release using Fe-loaded Zeolite

  • Lee Seunghak;Lee Kwanghun;Lee Sungsu;Park Junboum
    • Journal of Soil and Groundwater Environment
    • /
    • v.10 no.1
    • /
    • pp.1-5
    • /
    • 2005
  • Nitrate reduction with zero valent iron $(Fe^0)$ has been extensively studied, but the proper treatment for ammonium byproduct has not been reported yet. In groundwater, however, ammonium is regarded as contaminant species, and particularly, its acceptable level is regulated to 0.5 mg-N/L. for drinking water. This study is focused on developing new material to reduce nitrate and properly remove ammonium by-products. A new material, Fe-loaded zeolite, is derived from zeolite modified by Fe(II) chloride followed by reduction with sodium borohydride. Batch experiments were performed without buffer at two different pH to evaluate the removal efficiency of Fe-loaded zeolite. After 80 hr reaction time, Fe loaded zeolite showed about $60\%$ nitrate removal at initial pH of 3.3 and $40\%$ at pH of 6 with no ammonium release. Although iron filing showed higher removal efficiency than Fe-loaded zeolite at each pH, it released a considerable amount of ammonium stoichiometrically equivalent to that of reduced nitrate. In terms of nitrogen species including $NO_3-N$ and $NH_4^+-N$, Fe-loaded zeolite removed about $60\%\;and\;40\%$ of nitrogen in residual solution at initial pH of 3.3 and 6, respectively, while the removal efficiency of iron filing was negligible.

Active Material Crossover through Sulfonated Poly (Ether Ether Ketone) Membrane in Iron-Chrome Redox Flow Battery (철-크롬 산화환원흐름전지에서 Sulfonated Poly (Ether Ether Ketone)막의 활물질 Crossover)

  • Kim, Young-Sook;Oh, So-Hyeong;Kim, You-Jeong;Kim, Seong-ji;Chu, Cheun-Ho;Park, Kwonpil
    • Korean Chemical Engineering Research
    • /
    • v.57 no.1
    • /
    • pp.17-21
    • /
    • 2019
  • The redox flow battery (RFB) is a large-capacity energy storage equipment, and the vanadium redox flow cell is a typical RFB, but VRFB is expensive. Iron-chrome RFBs are economical because they use low-cost active materials, but their low performance is an urgent problem. One of the reasons for the low performance is the crossover of the active materials. In this study, the sulfonated Poly (ether ether ketone) (sPEEK) membrane, which is a hydrocarbon membrane, was used instead of the fluorine membrane to reduce the crossover of the active materials. The chromium ion permeability of the sPEEK membrane was $1.8{\times}10^{-6}cm^2/min$, which was about 1/33 of that of the Nafion membrane. Thus, it was shown that the use of the sPEEK membrane instead of the fluorine membrane could solve the high active material crossover problem. The activation energy of iron diffusion through the sPEEK membrane was 24.9 kJ/mol, which was about 66% of Nafion membrane. And that the e-PTFE support in the polymer membrane reduces the active material crossover through Iron-Chrome Redox Flow Battery (ICRFB).

Microbial Reduction of Iron(III) Oxides: Implication for Permeable Reactive Barriers. (철환원 미생물을 이용한 3가 철의 환원에 관한 연구)

  • 임현정;박재우
    • Proceedings of the Korean Society of Soil and Groundwater Environment Conference
    • /
    • 2002.04a
    • /
    • pp.250-253
    • /
    • 2002
  • Remediation of groundwater using zero valent iron filings has received considerable attention in recent years. However, zero valent iron is gradually transformed to iron(III) oxides at permeable reactive barriers, so the reduction of iron(III) oxides can enhance the longevity of the reactive barriers. In this study, microbial reduction of Fe(III) was performed in anaerobic condition. A medium contained nutrients similar to soil solution. The medium was autoclaved and deoxygenated by purging with 99.99% $N_2$ and pH was buffered to 6, while the temperature was regulated as 2$0^{\circ}C$. Activity of iron reducing bacteria were not affected by chlorinated organics but affected by iron(III) oxide. Although perchloroethylene(PCE) was not degraded with only ferric oxide, PCE was reduced to around 50% with ferric oxide and microorganism. It shows that reduced iron can dechlorinate PCE.

  • PDF

A Study on Reduction Treatment of EAF′s Dusts Mixed with Millscale (電氣爐製鋼粉塵과 millscale 混合펠릿의 還元擧動에 관한 硏究)

  • 윤기병
    • Resources Recycling
    • /
    • v.9 no.6
    • /
    • pp.45-52
    • /
    • 2000
  • Generally, the residues of EAF's dusts treated by reduction process at high temperature are disposed. If the residues can be recycled as iron sources of EAF by upgrading their iron contents, it can be expected to reduce the amounts of disposed wastes and the environmental impacts. Reduction of EAF's dusts mixed with millscale was carried out in rotary hearth furnace to upgrade iron contents of reduction residues. Dusts should be reduced rapidly to protect from reoxidation of reduced iron residue which can be reoxidized at high temperature. In our experimental conditions, optimum reduction time was about 40min. and iron contents of the residues were increased with increasing mixing ratio of millscale and upgrade to 85% at 50%wt mixing ratio. Zinc and lead contents in residues were about 3% and 0.5% respectively. The residues reduced rapidly must be recycled in EAF because heavy metal elements in the residues can be extracted easily and contaminate air and water.

  • PDF

Bioconversion of nitrogen oxides and reduction of ferric ions by probiotic lactic acid bacteria (프로바이오틱스 유산균에 의한 질소 산화물 전환 및 철 이온 환원활성)

  • Kim, Selim;Hong, Jungil
    • Korean Journal of Food Science and Technology
    • /
    • v.53 no.6
    • /
    • pp.785-791
    • /
    • 2021
  • Many lactic acid bacteria (LAB) have probiotic properties that exert various health benefits. In this study, the reduction potential of nitrogen oxide compounds and ferric ions by six LAB, including Lactobacillus kimchicus, L. lactis, L. casei, L. plantarum, L. rhamnosus GG, and Leuconostoc mesenteroides were evaluated. The L. kimchicus strain produced a substantial amount of nitrite reduced from nitrate added to the media, whereas the other five LAB strains did not. L. kimchicus also showed the most potent reducing activity of ferric to ferrous ions. However, the reduction potential of the autoclaved L. kimchicus was little pronounced. The scavenging activities of viable LAB or their cell lysates against different radicals were not consistent with the potency of the LAB's reducing ability. The present results indicate that L. kimchicus has a strong reduction potential for nitrogen oxides in viable status, and that this ability can be used as a probiotic property for various health benefits.