Ferroelectric Properties and DPT in the Perovskite PMT-PT System (Perovskite PMT-PT계의 강유전 특성 및 확산상전이)

  • Kim, Y.J.
    • Journal of the Korean Vacuum Society
    • /
    • v.17 no.2
    • /
    • pp.122-129
    • /
    • 2008
  • Ferroelectric properties of the PMT-PT were also studied from the temperature dependence of hysteresis loops using a method slightly modified from Sawyer-Tower's. Dielectric, pyroelectric and piezoelectric properties of the ceramics in the system PMT-PT were investigated. The resulted densities of the PMT-PT ceramics system were greater than 97 % of the theoretical value. As observed SEM micrograph of the fracture surfaces of the PMT-PT ceramics system, the average grain sizes were increased about 3-5 ${\mu}m$ to 6-8 ${\mu}m$ with increasing sintering temperature. The specimens with PT<0.30 for PMT-PT solid solution system exhibited the dielectric and pyroelectric properties of a typical relaxor ferroelectrics. The composition with the maximum dielectric constant exhibits relatively superior pyroelectric and piezoelectric properties.

TCC behavior of a shell phase in core/shell structure formed in Y-doped BaTiO3: an individual observation (Yttrium이 첨가된 BaTiO3에서 형성된 core/shell 구조에서 shell의 TCC 거동: 독립적 관찰)

  • Jeon, Sang-Chae
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.30 no.3
    • /
    • pp.110-116
    • /
    • 2020
  • Grains in the BaTiO3, which is used for a dielectric layer in MLCC(Multi-Layer Ceramic Capacitor) are necessary to form core/shell structure for a stable TCC(Temperature Coefficient of Capacitance) behavior. The shell property has been deduced from the whole TCC behavior of core/shell structure due to its tiny size, ~ few ㎛. This study demonstrates the individual TCC behavior of the shell phase measured by micro-contact measurement in a temperature range between 35 and 135℃. Pt electrode pairs deposited on an enlarged core/shell structure in a diffusion couple sample made the measurement possible. As a result, the DPT (Diffusion Phase Transition) behavior of the shell phase was revealed as a different TCC behavior from that of the core: a broad peak with Tm at 65℃. This would be also useful experimental data for a modelling that depicts dielectric-temperature behavior of core/shell structure.