• Title/Summary/Keyword: 혼합 섬유

Search Result 632, Processing Time 0.03 seconds

The study on the rheological properties the solution of polyvinyl alcohol(PVA) in dimethylsulfoxide(DMSO) and Ethanol(EtOH) mixed solvents (디메틸설폭사이드와 에탄을 혼합용매에 용해된 폴리비닐알코을올 용액의 유변학적 성질에 대한 연구)

  • 김학성;김병철
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2002.04a
    • /
    • pp.215-218
    • /
    • 2002
  • Poly(vinyl alcohol)(PVA)는 1924년 W. O. Herrmann과 W. Haehnel이 Poly(vinyl esters)를 caustic soda 용액에서 비누화하여 합성한 뒤 많은 연구 및 사용되어지고 있는 고분자이다. 환경친화적이고, 인체에 무해하여 인공관절, 콘택트 렌즈 등에 이용이 되고 있다. 특히 구조가 선형적이고 zig-zag구조를 가지기 때문에 고강도, 고탄성을 갖는 섬유의 제조가 가능한 소재이다[1]. PVA섬유의 제조는 용매를 이용한 습식방사 및 겔방사로 섬유를 제조한다. (중략)

  • PDF

Effect of Adsorption of Surfactant to the Particles on Dispersion Stability of Particulate Soil in Anionic-nonionic Surfactant Mixed Solution (음-비이온계 혼합계면활성제 용액에 있어 입자에의 계면활성제 흡착량이 고형오구의 분산안정성에 미치는 영향)

  • 정선영;강인숙
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2003.04a
    • /
    • pp.436-437
    • /
    • 2003
  • 고형오구의 분산안정화 작용은 고체 입자의 계면에 흡착한 계면활성제에 의한 전기적 반발력과 입체적 보호작용에 영향을 받게 된다. 특히 현재 시판세제의 조성에서 비이온계 계면활성제의 혼합이 점차 중요시되는 이때 입체적 보호작용에 의한 고형오구의 분산안정성은 의류제품의 세척성 제고에 좋은 정보가 되리라 생각된다. 따라서 본 연구는 시판되고 있는 세제 대부분이 음-비이온계 계면활성제의 혼합으로 되어 있는 점을 고려하여 음이온 계면활성제로서 D5S(sodium dodecyl benzene sulfonate), 비이온계 계면활성계 NPE(nonyl phenol polyoxyethylene ether, EO$_{10}$) 혼합용액에서 음이온과 비이온계 계면활성제의 입자에의 흡착과 고형오구의 안정성을 관련시켜 고찰하였다. (중략)

  • PDF

Mixed Mode Fracture of the Crack Inclined to the Grain Direction in Wood (목재(木材)의 섬유방향(纖維方向)에 경사(傾斜)진 균열의 혼합모-드파괴(破壞)에 관한 연구)

  • Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.17 no.4
    • /
    • pp.83-88
    • /
    • 1989
  • 목재의 섬유방향에 경사진 균열의 모-드I과 모-드II의 혼합모-드파괴시의 파괴거동을 조사하기 위하여 라왕(Shorea Spp.)의 LA시스템에 있어서 서로 다른 경사각도를 가진 SEN시험편(Single edge notch specimen)에 대하여 휨 시험을 행하였다. 얻이진 결과는 혼합모-드파괴시, 모-드I응력확대계수$K_I$과 모-드II응력확대계수$K_II$간에 일정한 상호작용이 존재한다는 것을 나타내었다. 또한, 모-드I과 모-드II의 임계응력확대계수(Critical stress intensity factor) $K_{IC}$$K_{IIC}$ 이용하여 혼합모-드파괴시의 $K_I$$K_II$간의 상호관계를 규정할 수 있었으며, 이미 보고된 여러 실험식과 본 실험결과를 비교하여 가장 적합한 관계로서 아래와 같은 관계를 얻을 수 있었다.

  • PDF

에틸렌-아크릴산 공중합체/폴리에틸렌글리콜 블렌드의 상용성 연구: Ferric Chloride 첨가효과

  • 이준열;유희진
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 1998.04a
    • /
    • pp.58-62
    • /
    • 1998
  • 고분자 블렌드의 열역학적 상용성은 고분자 혼합물의 혼합 엔트로피가 무시할 수 있을 정도로 작기 때문에 성분 고분자 사이의 강한 분자간 인력에 의한 음의 값의 혼합 엔탈피에 의해서 유도되어진다. 상용성 고분자 블렌드를 얻기 위하여 도입되어질 수 있는 분자간 상호인력으로는 수소결합$^1$, 쌍극자-쌍극자 상호작용$^2$, 이온-쌍극자 상호작용$^3$, 산-염기 상호작용$^4$, 전이금속 복합체 형성$^{5}$ , 전하이동 복합체 형성$^{6}$ 등이다.(중략)

  • PDF

Rheological Properties During Mixing and Thermal Properties of Polypropylene/Natural Fiber Composites: II. Effects of A Compatibilizer (폴리프로필렌-천연섬유 복합재료의 혼합시 유변학적 및 열적 특성: II. 상용화제의 영향)

  • Kim, Sam-Jung;Yoo, Chong Sun;Ha, Chang-Sik
    • Journal of Adhesion and Interface
    • /
    • v.10 no.1
    • /
    • pp.23-29
    • /
    • 2009
  • We investigated effects of a compatibilizer on the rheological properties during mixing and thermal properties of polypropylene (PP)-natural fiber composites. Two types of natural fibers (cotton fiber and wood fiber) were compared. maleic anhydride grafted PP was used for a compatibilizer. On increasing the amounts of the compatibilizer, the torque values of composites were increased, regardless of the kind of fibers. X-ray diffraction (XRD) and differential scanning calorimetry (DSC) results showed a slight increase in the degree of crystallinity with adding the compaibilizing agent, while the effects of the kind of fibers were marginal. It may be considered, however, the cotton fiber exhibits better interaction with PP-g-MAH than the natural fiber based on the rheographs, DSC, and XRD results.

  • PDF

Evaluation of Dry Tribological Characteristics of Hybrid Metal Matrix Composites with Temperature Rising (온도 상승에 따른 혼합금속복합재료의 건식 마찰특성 평가)

  • Wang, Yi-Qi;Afsar, Ali-Md.;Song, Jung-Il
    • Composites Research
    • /
    • v.23 no.2
    • /
    • pp.10-16
    • /
    • 2010
  • $Al_2O_3$ fiber and SiC particle hybrid metal matrix composites (MMCs) were manufactured by squeeze casting method investigated for their tribological properties. The pin specimens had different ratios of fiber to particle content but their total weight fraction was constant at 20 wt. %. Tribological tests were performed with a pin-on-disk friction and wear tester. The investigation of the dry tribological characteristics of hybrid MMCs were carried out at room temperature and elevated temperature of$100^{\circ}C$ and$150^{\circ}C$. The morphologies of worn surfaces were examined by scanning electron microscope (SEM) to observe tribological characteristics and investigate wear behavior. The results revealed that the wear resistance improved with the content of SiCp increased of the planar random (PR) MMCs at room temperature. At the elevated temperature, it revealed that the wear resistance of normal (N) MMCs was superior to that of the PR-MMCs due to PR-fibers were easily pulled out holistically from the worn surface. Meanwhile, the coefficient of friction decreased with the temperature increasing.

Utilization of Wood by-product and Development of Horticultural Growing Media (임산부산물을 이용한 원예용 혼합상토 개발)

  • Jung, Ji Young;Lim, Ki-Byung;Kim, Ji Su;Park, Han Min;Yang, Jae-Kyung
    • Horticultural Science & Technology
    • /
    • v.33 no.3
    • /
    • pp.435-442
    • /
    • 2015
  • The main objective of this work was to identify and evaluate possible substrate alternatives or amendments to peat moss. This study involves the physical and chemical characterization and growth test of wood sawdust and wood fiber in order to evaluate their use as components of horticultural media. The carbohydrate content, C/N ratio, pH, phenolic compound, total porosity and water holding capacity were 58.9%, 425.1, 4.8, 181.8 ($mg{\cdot}g^{-1}$), 82.5% and 47.1% in wood sawdust and 41.1%, 240.8, 5.9, 29.8 ($mg{\cdot}g^{-1}$), 90.6% and 56.2% in wood fiber, respectively. Wood sawdust (K, $998.0mg{\cdot}100g^{-1}$ ; Ca, $1196.0mg{\cdot}100g^{-1}$; Mg, $105.6mg{\cdot}100g^{-1}$) and wood fiber (K, $1250.1mg{\cdot}100g^{-1}$; Ca, $1982.6mg{\cdot}100g^{-1}$; Mg, $173.1mg{\cdot}100g^{-1}$) showed adequate mineral elements properties compared to peat moss (K, $0.02mg{\cdot}100g^{-1}$; Ca, $0.57mg{\cdot}100g^{-1}$; Mg, $0.13mg{\cdot}100g^{-1}$) for their use as growing media. The mixtures of the horticultural media were prepared using different substrate as wood sawdust and wood fiber to grow Chinese cabbage (Brassica campestris L.) in a greenhouse. The seed germination, leaf area and stem height were 75%, $0.50cm^2$ and 2.8 cm in PS substrate (containing 30% peat moss, 10% perlite and 60% wood sawdust) and 95%, $0.65cm^2$ and 3.3 cm in PF substrate (containing 30% peat moss, 10% perlite and 60% wood fiber), respectively. The seed germination and stem height of the PF substrate (containing 30% peat moss, 10% perlite and 60% wood fiber) was higher than those in peat moss (control). Utilization of wood by-product can be considered as an alternative media component to substitute the widely using expensive peat moss.

Tensile Properties of Hybrid Fiber Reinforced Cement Composite according to the Hooked & Smooth Steel Fiber Blending Ratio and Strain Rate (후크형 및 스무스형 강섬유의 혼합 비율과 변형속도에 따른 하이브리드 섬유보강 시멘트복합체의 인장특성)

  • Son, Min-Jae;Kim, Gyu-Yong;Lee, Sang-Kyu;Kim, Hong-Seop;Nam, Jeong-Soo
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.3
    • /
    • pp.31-39
    • /
    • 2021
  • In this study, the fiber blending ratio and strain rate effect on the tensile properties synergy effect of hybrid fiber reinforced cement composite was evaluated. Hooked steel fiber(HSF) and smooth steel fiber(SSF) were used for reinforcing fiber. The fiber blending ratio of HSF+SSF were 1.5+0.5, 1.0+1.0 and 0.5+1.5vol.%. As a results, in the cement composite(HSF2.0) reinforced with HSF, as the strain rate increases, the tensile stress sharply decreased after the peak stress because of the decrease in the number of straightened pull-out fibers by increase of micro cracks in the matrix around HSF. When 0.5 vol.% of SSF was mixed, the micro cracks was effectively controlled at the static rate, but it was not effective in controlling micro cracks and improving the pull-out resistance of HSF at the high rate. On the other hand, the specimen(HSF1.0SSF1.0) in which 1.0vol.% HSF and 1.0vol.% SSF were mixed, each fibers controls against micro and macro cracks, and SSF improves the pull-out resistance of HSF effectively. Thus, the fiber blending effect of the strain capacity and energy absorption capacity was significantly increased at the high rate, and it showed the highest dynamic increase factor of the tensile strength, strain capacity and peak toughness. On the other hand, the incorporation of 1.5 vol.% SSF increases the number of fibers in the matrix and improves the pull-out resistance of HSF, resulting in the highest fiber blending effect of tensile strength and softening toughness. But as a low volume fraction of HSF which controlling macro crack, it was not effective for synergy of strain capacity and peak toughness.