• Title/Summary/Keyword: 합금층

Search Result 555, Processing Time 0.022 seconds

Estimation of Hardfacing Material and Thickness of STD61 Hot-Working Tool Steels Through Three-Dimensional Heat Transfer and Thermal Stress Analyses (3 차원 열전달/열응력 해석을 통한 STD61 열간 금형강의 하드페이싱 재료 및 두께 예측)

  • Park, Na-Ra;Ahn, Dong-Gyu
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.38 no.4
    • /
    • pp.427-436
    • /
    • 2014
  • The goal of this paper is to estimate proper hardfacing material and thickness of STD61 hot-working tool steel through three-dimensional heat transfer and thermal stress analyses. Stellite6, Stellite21 and 19-9DL superalloys are chosen as alternative hardfacing materials. The influence of hardfacing materials and thicknesses on temperature, thermal stress and thermal strain distributions of the hardfaced part are investigated using the results of the analyses. From the results of the investigation, it has been noted that a hardfacing material with a high conductivity and a thinner hardfaced layer are desired to create an effective hardfacing layer in terms of heat transfer characteristics. In addition, it has been revealed that the deviation of effective stress and principal strain in the vicinity of the joined region are minimized when the Stellite21 hardfaced layer with the thickness of 2 mm is created on the STD61. Based on the above results, a proper hardfacing material and thickness for STD61 tool steel have been estimated.

Improvement of Wear Resistance of Aluminum by Metal-Ceramic Particle Composite Layer (알루미늄표면에 금속-세라믹입자 복합첨가에 의한 내마모성개선)

  • ;;;中田一博;松田福久
    • Journal of Welding and Joining
    • /
    • v.15 no.6
    • /
    • pp.96-104
    • /
    • 1997
  • The present study was aimed to correlate the microstructure and the hardness as well as the wear resistance of the metal-ceramic particulated composite layer on the pure Al plate. The composite layers were constructed by the addition of TiC particles on the surface of Al-Cu alloyed layers by PTA overlaying process. Initially, the Al-Cu alloyed layers were achieved by the deposition of Al-(25 ~ 48%) Cu alloys on the pure Al plate by TIG process. It was revealed that TiC particles were uniformly dispersed without any reaction with matrix in the composite layer. The volume fraction of TiC particles (TiC V F) increased from 12% to 55% with increasing the number of pass of composite layer. Hardnesses of (Al-48%Cu + TiC (3&4layers)) composite layer were Hv450 and Hv560, respectively, due to the increase of TiC V/F. Hardnesses of (Al-Cu + TiC) composite layers decreased gradually with insreasing temperature from 100$^{\circ}$C to 400$^{\circ}$C, and hardnesses at 400$^{\circ}$C were then reached to 1/5 - 1/10 of room temperature hardness depending on the construction of composite layers. The Specific wear of (Al + Tic) layer and Al-48%Cu alloyed layer decreased to 1/10 of the of pure Al, while the specific wear of (Al-48%Cu + TiC (4 layers)) composite layer exhibited 1/15 of that of steel such as SS400 and STS304.

  • PDF

Influence of thickness ratio and substrate bias voltage on mechanical properties of AlCrN/AlCrSiN double-layer coating (두께 비율과 기판 바이어스 전압이 AlCrN/AlCrSiN 이중층 코팅의 기계적 특성에 미치는 영향)

  • Kim, Hoe-Geun;Ra, Jeong-Hyeon;Lee, Sang-Yul;Han, Hui-Deok
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.162-162
    • /
    • 2017
  • AlCrN 코팅은 높은 경도, 낮은 표면 조도 등의 상온에서의 우수한 기계적 특성 이외에 고온에서 안정한 합금상의 형성으로 인하여 우수한 내열성을 보이는 코팅이며, Si을 첨가하여 나노복합구조를 갖는 AlCrSiN 코팅은 고경도 특성을 나타내는 나노결정립과 고내열성을 나타내는 $Si_3N_4$ 비정질이 동시에 존재함으로써 뛰어난 고온 특성까지 보유하여 공구 코팅으로의 적용 가능성이 크다. 본 연구에서는, 가혹화된 공구사용 환경 대응 하는 더욱 우수한 내마모성 및 내열성을 보이는 코팅막을 개발하기 위해 AlCrN/AlCrSiN 이중층 코팅을 합성하였다. 합성된 코팅의 구조 및 물성을 분석하기 위해 field emission scanning electron microscopy(FE-SEM), nano-indentation, atomic force microscopy(AFM) 및 ball-on-disk wear tester를 사용하였다. 내열성을 확인하기 위하여 코팅을 furnace에 넣어 500, 600, 700, 800, 900도에서 30분 동안 annealing한 후에 nano-indentation을 사용하여 경도를 측정을 하였다. 5:5, 7:3, 9:1의 두께 비율로 AlCrN/AlCrSiN 이중층 코팅을 합성하였으며 모든 코팅의 두께는 $3{\mu}m$로 제어되었다. AlCrN 코팅층의 두께가 증가할수록, 이중층 코팅의 경도 및 내마모성은 점차 향상되었지만 코팅의 밀착력은 감소하였다. 일반적으로 AlCrN 코팅은 상대적으로 높은 잔류응력을 갖고 있으므로, AlCrN 층의 두께비율이 증가함에 따라 코팅내의 잔류응력이 높아져 코팅의 경도는 증가하고 밀착특성은 낮아진 것으로 판단된다. AlCrSiN 상부층 공정시 기판 바이어스 전압을 -50 ~ -200V 로 증가시키면서 이중층 코팅을 합성하였다. XRD 분석 결과, 공정 바이어스 전압이 증가함에 따라 AlCrSiN 상부층은 점차 비정질화 되었고, 코팅의 경도와 표면 특성이 향상되는 것을 확인하였다. 이러한 특성 향상은 높은 바이어스 인가가 이온 충돌효과의 증가를 야기시켰으, 이로 인해 치밀한 코팅층 합성에 의한 결과로 판단된다. AlCrN/AlCrSiN 이중층 코팅을 어닐링 한 후 경도 분석 결과, -150, -200V에서 합성한 코팅은 900도 이상에서 26GPa 이상의 높은 경도를 보인 것으로 보아 우수한 내열성을 갖는 것으로 확인 되었다. 이는 AlCrSiN 상부층의 높은 Si 함량 (11at.%) 으로 인한 충분한 $Si_3N_4$ 비정질상의 형성과, 고바이어스 인가로 인한 AlCrN 결정상과 $Si_3N_4$ 비정질상의 고른 분배가 코팅의 내열성을 향상시키는데 기여를 한 결과로 판단된다.

  • PDF

Effect of Nb, V and Cr on the High Temperature Oxidation of Ti-(42, 44)% Al Alloys (Ti-(42, 44)%Al 합금의 고온내산화성에 미치는 Nb, V 및 Cr의 영향)

  • Lee, Yeong-Chan;Kim, Mi-Hyeon;Kim, Seong-Hun;Lee, Won-Uk;Baek, Jong-Hyeon;Lee, Dong-Bok
    • Korean Journal of Materials Research
    • /
    • v.9 no.10
    • /
    • pp.1025-1031
    • /
    • 1999
  • Alloys of TiAl with six different compositions. i. e., Ti-(42, 44)Al-2Nb-4V. Ti-(42, 44)Al-4Nb-2V and Ti -(42, 44)Al-4Nb-2Cr, were manufactured by arc-melting. and their oxidation behavior was studied. Both isothermal and cyclic oxidation tests were performed at 700, 800 and $900^{\circ}C$ in air for 50hr. The oxidation resistance increased in the order of Ti-(42, 44)Al-2Nb-4V, Ti-(42, 44)Al-4Nb-ZV and Ti-(42, 44)Al-4Nb-2Cr. It was found that V was a deleterious element, while Cr was a beneficial element in terms of oxidation resistance. During oxidation, a simultaneous interdiffusion was observed. All the constituent elements in the base alloys diffused outward. whereas oxygen from the atmosphere diffused inward, to form triple oxide layers composed of an outermost $\textrm{TiO}_2$ layer. upper ($\textrm{TiO}_2+\textrm{Al}_2\textrm{O}_3$) mixed layer, and lower $\textrm{TiO}_2$-rich layer.

  • PDF

A Study on Improvement of Durability for Run-out Table Roller with Hot Rolling by Porous Self-fluxing Alloy Coating (다공질 자용성 합금 피복에 의한 열간 압연용 런-아웃 테이블 롤러의 내구성 향상에 관한 연구)

  • Bae, Myung-Whan;Park, Byoung-Ho;Jung, Hwa
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.36 no.2
    • /
    • pp.276-285
    • /
    • 2012
  • The objective of this research is to develop the coating technique by a porous self-fluxing alloy for improving the mechanical properties of run-out table roller surface with the hot rolling. To enhance the durability of run-out table roller with the hot rolling, the high hardness of roller surface should be maintained at high temperatures, and the improvement of wear resistance, corrosion resistance, heat resistance, burn resistance and adhesion resistance should be maintained. In order to be able to transport reliably a hot rolled steel sheet, also, the appropriate friction coefficient on the roller surface should be maintained and the slip between roller and steel should not occur. In this study, the wear resistance of roller increases after the self-fluxing alloy is changed to a cermet by adding the tungsten carbide(WC), and the coefficient of friction increases and the ability of grip is improved because the porosities are made by coating with fine iron powder on the roller surface. As a result, it is found that the ability of grip between the steel and the roller coated by a porous self-fluxing alloy contained to 5 ~ 10 wt% of Fe in the coating layer is improved compared to the roller coated by Ni-Cr. This is because the porosities are made after Fe contained in the roller is partially alloyed by heating with a furnace in the fusing process and the rest is eliminated by oxidation and dissolution.

The Effects of Alloying Elements on the Formation of Interfacial Reaction Layer between Molten Aluminium Alloys and STD61 Tool Steel (알루미늄 합금 용탕/STD61 공구강의 계면 반응층 형성에 미치는 합금원소의 영향)

  • Park, Heung-Il;Park, Ho-Il
    • Journal of Korea Foundry Society
    • /
    • v.25 no.4
    • /
    • pp.161-167
    • /
    • 2005
  • The experiment of hot dip interaction tests was carried out in order to study the formation behavior of interfacial reaction layer between as-received STD61 hot work tool steel and a commercial pure aluminum melt, Al-xwt.%Fe(x=0.2, 0.5, 0.8 and 1.1) alloys melt and Al-xwt.%Si(x=1.0, 4.0, 7.0 and 10.0) alloys melt, respectively. The results show that the reaction layer, over 300 ${\mu}m$ in thickness, is easily formed by the dissolution of silicon from as-received tool steel. When the iron content in the aluminum alloy is higher than 1.1 wt.%, the thickness of reaction layer decreases below 180 ${\mu}m$ by preventing iron dissolution from the tool steel. The silicon dissolved from tool steel acts as a strong promoter on the formation of reaction layer, but the alloyed silicon in molten aluminum alloys acts as an inhibitor on the formation of reaction layer.

Attachment of Two-Way Shape Memory Alloy onto Fabric for Mass Production of Fire Fighters' Turnout Gear (지능형 소방복의 양산화를 위한 이방향 형상기억합금 부착 방법)

  • Park, Mi-Kyung;Lee, Ji-Yeon;Kim, Eun-Ae
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.36 no.4
    • /
    • pp.382-390
    • /
    • 2012
  • This study shows the optimum attachment of Two-Way Shape Memory Alloy (TWSMA) springs onto thermal liner and its sewing method for the mass production of fire fighter's intelligent turnout gear. SMA springs were attached to the fabric by four different methods and stitched by two different shapes (square and wave). The durability of the attached springs was tested by laundering up to 50 cycles. Examined were whether the springs would remain attached to the fabric after repeated laundering, the shape memory effect and reaction of the springs, and the anti-corrosiveness of the springs. A Human-Clothing-Environment simulator evaluated thermal insulation according to attachment methods, air layer volume, and stitch types. The findings showed that silicon attached springs remained intact after repeated laundering; in addition, repeated laundering did not influence the responsiveness and anti-corrosiveness of SMAs. Air volume had positive relations with the insulation. Attachment methods or stitch methods had limited impact on the thermal insulation. As a result, a wave type stitch with silicone attachment was suggested as the optimum method to attach the SMA springs onto the intelligent turnout gear for fire fighters.

Effect of Alloying Elements and Thermal Aging on the Contact Resistance of Electroplated Gold Alloy Layers (금 합금 도금층의 접촉저항에 미치는 합금원소의 종류 및 Thermal Aging의 영향)

  • Lee, Jiwoong;Son, Injoon
    • Journal of the Korean institute of surface engineering
    • /
    • v.46 no.6
    • /
    • pp.235-241
    • /
    • 2013
  • In this study, the effects of alloying elements and thermal aging on the contact resistance of electroplated gold alloy layers were investigated by surface analysis using X-ray photoelectron spectroscopy (XPS). The contact resistance of Au-Ag alloy was lower than that of Au-Ni or Au-Co alloy after thermal aging. The XPS results show that nickel and oxygen present as nickel oxides such as NiO and $Ni_2O_3$ on the surface of gold layers after thermal aging. The increase in the contact resistance after thermal aging is attributable to the nickel oxide layer formed on the surface of the gold layers. The content of nickel diffused from the underlayer during the thermal aging was high in the order of Au-Co, Au-Ni and Au-Ag alloy because the area of grain boundary was large in the order of Au-Ag, Au-Ni and Au-Co alloy.

The Effect of Current on Characteristics of Stellite 12 Alloy Overlayer by PTA Process (PTA법에 의한 스텔라이트 12 합금 육성층의 특성에 미치는 전류의 영향)

  • Jung, B.H.;Kim, M.K.;Ahan, Y.S.;Kim, M.Y.;Lee, S.Y.
    • Journal of Power System Engineering
    • /
    • v.5 no.3
    • /
    • pp.88-94
    • /
    • 2001
  • Stellite 12 alloy-powders were overlaid on 410 stainless steel valve seat using plasma transferred arc(PTA) process. Variation of the microstructure, hardness, wear and corrosion of overlaid deposit with current change was investigated. The deposit showed hypoeutectic microstructure, which was consisted of primary cobalt dendrite and networked $M_7C_3$ type eutectic carbides. As current increased, the amount of eutectic carbide decreased and its dendritic secondary arm spacing increased. Hardness of the deposit was decreased with increase of current. Stress relief heat treatment at $600^{\circ}C$ for two hours resulted in slight increase of hardness in the deposit and showed uniform hardness distribution in base metal without any hardened layer in HAZ. Specific wear decreased with increase of sliding distance. The deposit of high hardness with a lot of eutectic carbide showed relatively low specific wear. Initial corrosion current density of the deposit in 0.1N sulfuric acid was lower than those of 410 stainless steel, and showed a little variation with PTA current.

  • PDF

Estimations of the Adhesion Strength of Galvannealed Coatings on Coated Sheet Using Single Lap-Shear Test (단일겹치기이음시험을 이용한 합금화용융아연코팅강판의 코팅층 접합강도 평가)

  • Lee, Jung-Min;Lee, Chan-Joo;Ko, Dae-Cheol;Lee, Seon-Bong;Kim, Byung-Min
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.33 no.6
    • /
    • pp.560-567
    • /
    • 2009
  • This paper was designed to estimate the adhesion strength of galvannealed coatings on steel sheets. The adhesion strength were evaluated using single lap - shear tests where the lap joint was bonded by structural adhesive. Tests were performed for overlap length of 5mm, 10mm and 15 mm and three directions (0, 45, 90) of steel sheets used as the adherend of the overlap joint. After the tests, FE simulations of the single lap-shear test were also carried out to observe the stress distribution in the interface between the adhesive and the coated sheet. The results showed that the joint failure loads obtained from the tensile tests of bonded single lap-joints were the same, regardless of overlap lengths and directions of steel sheets. Also, the failure of galvannealed coatings greatly depended on shear stress distribution in the interface and the value was about 30MPa.