콘크리트에 선형파괴역할의 적용가능성을 연구한 많은 논문이 발표되었다. 본 논문에서는 CLWL-DCB식편을 이용한 콘크리트의 개구형파괴를 연구하였다. 표면구열길이는 리프리카를 사용하여 직접적인 방법으로 측정하였고, 이 결과은 실험에서 얻은 측정가중과 구열개구변위의 관계곡선을 이용하여 분석하였다. 감계응력강도계수와 감계구열선단위는 Two Parameter 모델을 사용하여 유효구열선단에서 구하였다. LEFM 구열단면과 실험으로 구한 구열단면으로부터 폐쇄압력을 얻기 위하여 중첩법을 적용하여 5종의 균열모델을 평가하였다.
KSCE Journal of Civil and Environmental Engineering Research
/
v.5
no.2
/
pp.121-131
/
1985
The characteristic of fatigue crack growth in the homogeneous or the soft welded connections used SWS-53 steel and HT-80 steel as base metals is examined by fractographic analysis. As a result of this analysis, the fact that the characteristic of fatigue crack growth which is observed and measured at the surface has wide application to engineering practice is verified. Also, the fact that the welded parts of HT-80 steel have much danger of brittle fracture is prooved. Considering that the striations are observed at the welded parts of SWS-58 steel and the spacing of striations has higher numerical value than da/dN, we can prove that inner fatigue crack growth may develop in zig-zag directions.
Transactions of the Korean Society of Mechanical Engineers
/
v.14
no.3
/
pp.636-645
/
1990
Analytically induced wear mechanism of elastic body under Hertzian contact is applied in acutual wear test of ceramics. There are two types of wear in ceramics, a large scale wear and a small scale wear. The large scale wear is commensurable with Hertzian contact area and the small scale wear with real contact area. Nondimensional parameter, S$_{c}$, is introduced and fully examined to estimate or predict wear rate of ceramics. Ceramic wear for S$_{c}$.leq.0.8 is in small scale wear and for S$_{c}$;geq.1.6 in large scale wear. wear.
Journal of the korean Society of Automotive Engineers
/
v.14
no.2
/
pp.65-75
/
1992
An analytical scheme for predicting the crack aspect pattern of materials which contain twin surface cracks was developed. Fatigue tests were performed on twin surface cracked PMMA plate specimens to obtain the interaction factor accounting for the interference effect of adjacent cracks. Here, the interaction factor is defined as the ratio of the stress intensity factor for twin surface cracks to that for a single surface crack. From the analysis of the fatigue test result, the interaction factor was presented as the ninth-order polynomial expression having a function of dimensionless crack spacing ratio. Then the polynomial expression was incorporated into the prediction program of the crack aspect pattern for twin surface cracked materials. And, the interaction effect and the coalescence condition of adjacent cracks were simplified in the newly developed prediction scheme of the crack aspect pattern. The predicted crack growth pattern using the prediction scheme was compared with test data from PMMA specimen. The predicted pattern agreed well with the test data.
Transactions of the Korean Society of Mechanical Engineers
/
v.14
no.2
/
pp.492-501
/
1990
It was known that the fracture incidences of offshore structure were mostly originated from the surface defects. Especially, in the case of the welded structures, since the welded region has some defects and incomplete beads which are apt to behave like the surface cracks, it has been necessary to evaluate the environmental effects on crack growth at HAZ for the design crack growth behaviour at multi-pall HAZ for SWS41 steel under free corrosion and cathodic protection(-0.9V vs Ag/Agcl) conditions. The results are summarized as follows ; (1) Crack growth rate of the as weld in air was faster than that of the parent and PWHT specimens over all .DELTA.K rang. (2) In free corrosion test, surface crack growth rate of the as welded was decreased in comparison with that of the parents. (3) In fatigue test under cathodic protection, cathodic electric potential(-0.9V vs Ag/Agcl) for the SWS41 steel parent was effective, while for the as welded ineffective. (4) There was a tendency that the exponent(m) of the Paris' equation was decreased in order of microhardness magnititude in air and under cathodic protection conditions and vise versa in free corrosion. (5) Fracture surface has dimples and ductile striations in air test, but transgranular cracks and brittle striations under cathodic protection test.
파괴역할적으로 피로문제를 다룰 때는 언제나 crack의 존재를 전재로 한다. 재료가 피로하중을 받아 파괴에이르는 과정의 설명은, 일차적으로는 피로에의한 crack의 발생이고, 다음단계로는 발 생한 crack들의 상호연결 또는 성장을 거쳐 최종적으로 파단에 이른다는 순서로 이루어진다고 보 기 때문이다. 또한, crack의 존재를 전제로 하더래도 crack청단의 응력장이 탄성론적으로 해석될 수 있어야함도 절대적인 전제가 되고 있다. 모든 피로제엔 각경형태의 crack발생, 성장이 관찰되 고 있는데, 이들 모든 crack들이다. 파괴역학적으로 다루어 질 수 있는 것은 물론 아니고, 아직도 K해석이 도어있지 않은 crack들이 많이 남아 있는 것이다. 예컨대 회전굽힘 피로시험편에서 관찰 되는 각종 형태의 표면피로 crack들은 응력해석의 곤란 때문에 아직은 이들에 적용시킬 K의 표 식이 없는 실정이라 하겠다. 이들 crack에 대해서는 K해석 뿐만 아니고, 피로역학적인 다른 Factor 즉 $r_{p}$라든가 .phi.같은 것들도 이해색상태에 있어 이 분야에의 연구가 많이 기대되고 있는 실정이다. Crack에 대한 연구는, 그것이 파괴의 전제가 되기 때문에 큰 의의를 갖는다고 보 겠는데 표면 Crack이 연결 또는 성장해서 시편의 전주를 완전히 일주 했어도 그것만으로는 바로 재료의 파괴에 직결이 되지 않는 것도 이 시험편의 특색이라 하겠다. 물론 회전굽힘 피로시험편 외에도 K해석이 되어있지 않은 경우는 아직도 많으며, K가 해석되어 있는 경우에 대해서도 정확 한 경계조건 등을 잘 검토해 가면서 응용함이 옳을 것이다. 화전굽힘피로의 경우나 그밖의 예에 서와같이 정확한 K해석이 이루어져 있지 않드래도 연구자에 따라 "Effective Streess Intensity Factor"라는 것을 쓰는 예도 왕왕있는데, 이에는 상당한 검토와 타당성제가 요구되고 있으며, 그 사용가능성여부에 대해서는 논란이 많이 따르는데 상례이기도 하다. 몇가지의 피로구열해석예를 들어보기로 한다. 들어보기로 한다.
Transactions of the Korean Society of Mechanical Engineers
/
v.14
no.1
/
pp.87-95
/
1990
Rotating bending fatigue tests of an authentic steel 304 were performed at various temperatures such as room temperature, $538^{\circ}$ and $593^{\circ}C$. The plastic replica method was also applied in order to estimate the fatigue life on the basis of serial observation of small fatigue crack initiation and growth on the pit specimen surface. The fatigue crack growth behavior of 304 stainless steel was investigated within the frame work of elastic-plastic fracture mechanics within a narrow scatterband in spite of different stress levels at elevated temperature as at room temperature. The growth law of small surface crack is determined uniquely by the term. $\DELTA\sigma^{n}a$ where $\DELTA\sigma$ is the stress amplitude, a is the crack length, and n is a constant. It is found that the small crack growth behavior is basically equivalent to the S-$N_{f}$ relationship, where S and $N_{f}$ are stress and number of cycles to failure, and the fatigue life prediction is in good agreement with the experimental results.
The stone pagoda of the Bunhwangsa temple made by piling small brick-shaped stones. The major rock forming stone bricks are andesites with variable genesis. Rock properties of the pagoda roof stone suffer partly including multiple peel-offs, exfoliation, decomposition like onion peels, cracks forming round lines and falling off stone pieces. The stylobates and tabernacles in all the four directions the pagoda are mostly composed of granitic rocks. Those rock properties are heavily contaminated by lichens and mosses with the often marks of inorganic contamination by secondary hydrates that are dark black or yellowish brown. Within the four tabernacles and northern pagoda body situated to relatively high humidity. There are even light gray precipitate looking like stalactites between the northern and western rocks of the body Their major minerals are calcite, gypsum and clays. The stone lion standing in the southeast and northeast side are alkali granite, while that in the southwest and northwest lithic tuff. Total rock properties of the pagoda are 9,708 pieces, among the all properties, fractured blocks are 11.0%, fall out blocks are 6.7% and covered blocks by precipitates are 7.0%, respectively. The pagoda has highly deteriorated the functions of the rock properties due to physical, chemical and biological weathering, therefore, we suggest that this pagoda has need to do long term monitoring and synthetic conservation researches.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.