  • Dispersion and electrical resistance (ER) properties of polyurethane (PU) type topcoat were evaluated using carbon nanotube (CNT) with different CNT weight fraction. CNT was dispersed in PU type topcoat using ultra sonication dispersion method. CNT/PU topcoat was coated on carbon fiber reinforced epoxy composite (CFRC) surface using gravity feed spraying method. Static contact angles of CFRC and CNT/PU topcoat were performed using 4 types of solvents to calculate the work of adhesion between CNT/PU topcoat and CFRC surface. Surface resistance of CNT added PU topcoat was measured to determine CNT dispersion. Adhesion property between CNT/PU topcoat and CFRC was determined via cross hatch cutting test based on ASTM D3359. The optimized condition of CNT weight fraction was found.

Hydrophobicity and Adhesion of SiO2/Polyurethane Nanocomposites Topcoat for Aircraft De-icing with Different Pre-curing Time (선경화 시간에 따른 항공기 De-icing용 나노실리카/폴리우레탄 복합재료 탑코트의 소수성 및 접착특성 평가)

  • Kim, Jong-Hyun;Shin, Pyeong-Su;Kwon, Dong-Jun;Park, Joung-Man
    • Composites Research
    • /
    • v.33 no.6
    • /
    • pp.365-370
    • /
    • 2020
  • The icing formation at aircraft occur problems such as increasing weight of the body, fuel efficiency reduction, drag reduction, the error of sensor, and etc. The viscosity of polyurethane (PU) topcoat was measured at 60℃ in real time to set the pre-curing time. SiO2 nanoparticles were dispersed in ethanol using ultra-sonication method. The SiO2/ethanol solution was sprayed on PU topcoat that was not cured fully with different pre-curing conditions. Surface roughness of SiO2/PU nanocomposites were measured using surface roughness tester and the surface roughness data was visualized using 3D mapping. The adhesion property between SiO2 and PU topcoat was evaluated using adhesion pull-off test. The static contact angle was measured using distilled water to evaluate the hydrophobicity. Finally, the pre-curing time of PU topcoat was optimized to exhibit the hydrophobicity of SiO2/PU topcoat.

Hydrophobicity and Adhesion Evaluation of MWCNT/Teflon-polyurethane Topcoat for Aircraft with Different MWCNT Coating Times (탄소나노튜브 코팅횟수에 따른 항공기용 탄소나노튜브/테프론-폴리우레탄 탑코트의 표면소수성 및 부착력 평가)

  • Lee, Jae-Hyuk;Kim, Jong-Hyun;Park, Joung-Man
    • Composites Research
    • /
    • v.35 no.2
    • /
    • pp.80-85
    • /
    • 2022
  • This work presents an experiment study to evaluate the nanoparticle adhesion and surface hydrophobicity characteristics of Teflon-polyurethane top coat depending on the number of multi-wall carbon nanotube (MWCNT) coatings, which is a carbon-based hydrophobic particle. In order to measure the adhesion between the nanoparticles and the top coat, adhesion pull-off test was performed with different MWCNT oxidation times. Static contact angle and roughness measurements were carried out to characterize the surface hydrophobic behavior. Through the roughness evaluation, it was confirmed that the carbon nanotubes were wetted in the Teflon-polyurethane top coat, and the degree carbon nanotube wetting was confirmed through a USB-microscope. As a result, it was found that the larger the degree of wetting, the better the adhesion. From the experimental results, as the hydrophobicity of Teflon-polyurethane increased, the adhesive propertydecreased with the number of coatings. It was possible to improve the adhesive force and determine the number of coatings of carbon nanotubes with optimized hydrophobicity.

Investigation of Damage to Polyurethane Topcoat Based on De-icing Cycles (De-icing 횟수에 따른 폴리우레탄 탑코트의 손상 조사)

  • Donghyeon Lee;Joung-Man Park;Hyung Mi Lim;Dong-Jun Kwon
    • Composites Research
    • /
    • v.37 no.3
    • /
    • pp.204-208
    • /
    • 2024
  • De-icing/anti-icing fluid is essential for removing ice formation on aircraft. It chemically removes ice using organic solvents, which can cause damage to the topcoat surface in the process. In this study, glycol-based deicing/anti-icing fluid was used to remove ice, and the resulting damage to the topcoat was examined. USB microscope was used to observe the formation and growth of ice, while a confocal microscope was employed to observe the surface morphology after treatment with de-icing/anti-icing fluid. Additionally, coating thickness measurements and Fourier transform infrared (FT-IR) analysis were conducted to investigate the physical and chemical changes on the surface. The repeated application of de-icing/anti-icing fluid showed a reduction in the ice formation rate and an increase in the growth rate. Damage during the pressurization process and surface damage to the polyurethane topcoat caused by ethylene glycol were observed during the de-icing process. Although no chemical changes were detected, the analysis revealed that surface uniformity decreased, with physical damage such as cracks and undulations forming on the surface. It was confirmed that while de-icing/anti-icing fluid is effective in removing ice, it also causes surface damage.

Evaluation of Adhesion, Hydrophobicity and Color Gamut of Nanoparticle embedded Polyurethane Topcoat for Aircraft with 3 Different Nanoparticles (항공기용 3종류 나노입자들로 함침된 폴리우레탄 탑코트의 접착성, 소수성 및 색재현성 특성평가)

  • Kim, Jong-Hyun;Kwon, Dong-Jun;Park, Joung-Man
    • Journal of Adhesion and Interface
    • /
    • v.22 no.1
    • /
    • pp.16-21
    • /
    • 2021
  • In the aircraft industry, anti- and de-icing are one of very important techniques for the safety. The anti-icing technique had not been studied while de-icing technique had been not only researched enough but applied to aircraft industry. In this work, surface roughness and energies of polyurethane (PU) topcoat were controlled with 3 different nanoparticles which was coated to PU topcoat. It was evaluated via static contact angle using distilled water. The adhesion property of 3 nanoparticles was evaluated directly using adhesion pull-off test. The color gamut of nanoparticle coated PU topcoat was also evaluated with 3 different nanoparticles. It was determined using RGB color degree variation between neat PU topcoat and coated nanoparticle. Finally, the optimized nanoparticle was determined to manufacture hydrophobic surface and to maintain color of neat PU topcoat for the aircraft.