Effect of Surfactant Type on the Particle Size and Yield in Semi-Continuous Emulsion Polymerization of n-Butyl Acrylate/Methyl Metacrylate (반연속식 노말브틸-아크릴레이트/메틸메타-아크릴레이트 유화중합(1) : 폴리머 라텍스의 수율과 입자크기에 관한 계면활성제 종류의 영향)

  • Ko, Ki-Young;Kim, Sung-il;Kim, Chul-Ung;Hyung, Gi-Woo
    • Clean Technology
    • /
    • v.11 no.1
    • /
    • pp.1-12
    • /
    • 2005
  • In these studies, semibatch emulsion copolymerization of n-butyl acrylate (n-BA) as adhesive component and methyl metacrylate (MMA) as coagulant component was carried out in order to investigate the role of surfactant in aqueous phase for polymer cement. It was found that the particle size and concentration of final polymer are affected by surfactant type used. The effect of nonionic surfactants was shown in the decrease of polymer emulsion concentration and small emulsion particle in order of LE-50, NP-50 > CE-50, Tween 20 > TX-405 > Brij 35. In LE and NP (n=7-50) as nonionic surfactant, it could be obtained the stable polymer emulsion of 40% in aqueous phase with average particle size of 250-320 nm using over n=30. On the other hand, the effect of surfactant type in initial reactor charge was shown that when SDS as ionic surfactant was used, the polymer emulsion concentration was constant irrespective of the amount used, whereas CTAB as cationic surfactant and HN-100 as reactive surfactant were shown a tendency to the decrease of that. The effect surfactant type on final polymer particle size was shown in decrease by the order of SDS > CTAB > HN-100.

  • PDF

Preparation and Properties of Cathode $(La{1-x}Sr_x)MnO_3$ Powder by GNP and Pechini Process (GNP and Pechini 법에 의한 Cathode용 $(La{1-x}Sr_x)MnO_3$ 분말 합성 및 특성)

  • 이미재;박상선;이경희;최병현
    • 한국전기화학회:학술대회논문집
    • /
    • 2002.07a
    • /
    • pp.117-122
    • /
    • 2002
  • 고체산화물 연료전지의 구성요소인 양극(공기극)을 GNP와 Pechini 법을 이용하여 $(La{1-x}Sr_x)MnO_3$ 양극을 합성하여 합성한 분말의 특성과 단위전지로 사용하기 위한 조건에서의 특성을 측정하였다. GNP로 합성한 분말의 경우 직접 $(LaSr)MnO_3$ 단일 결정상을 얻을 수 있었으나, Pechini 법으로 합성한 분말의 경우는 비정질이었다. 또한 각각의 방법으로 합성한 분말의 입자형태는 구형이었고 1차상 입자크기는 GNP가 40nm, Pechini, 법으로 합성한 경우 20nm 정도의 크기를 갖고 있었다. GNP로 합성한 분말의 입자크기와 비표면적의 경우 glycine의 첨가량이 증가함에 따라 입자크기는 감소하였으나 최적 glycine 첨가량은 2.0mole 였고, 이 때 평균2차상의 입자크기는 $13.24{\mu}m$로 agglomeration 되어있었다. 최적 cathode조성은 GNP법으로 합성한 $(La_{0.9}Sr_{0.1}MnO_3$로서 가능하였고, 이 조성에서의 열팽창계수는 $9.89\times10^{-6}/^{\circ}C$이고, 전기전도도($1200^{\circ}C$에서 2시간소결)는 110 S/cm을 나타내었다.

  • PDF

Preparation of Ultrafine Silica Particle by Pyrolysis in the Gas Phase (기상열분해법에 의한 초미립 실리카분말 제조)

  • Jang, Hee Dong;Yoon, Ho Sung
    • Applied Chemistry for Engineering
    • /
    • v.8 no.6
    • /
    • pp.901-906
    • /
    • 1997
  • Ultrafine silicon dioxide($SiO_2$) powder was prepared from tetraethylorthosilicate(TEOS) by the gas-phase reaction. The effects of reaction temperature, flow rate of gas, TEOS concentration, and preheating temperature of reactants on the particle size were investigated. As the reaction temperature increased, average particle size of the silicone dioxide powder became smaller. Smaller particles were also obtained with decreasing the residence time of reactants in the reaction zone. Larger particles having narrow size distribution were produced with the high concentrations of the reactants. The effect of the preheating temperature was not considerable on the average particle size. The range of average particle size was from 30 nm to 58 nm depending on experimental conditions.

  • PDF

Design and Characterization of Ascorbyl Glucoside loaded Solid Lipid Nanoparticles to improve skin penetration (피부 투과 개선을 위한 고형지질나노입자내 Ascorbyl glucoside 봉입 설계 및 특성화)

  • Yeo, Sooho
    • Journal of the Korean Applied Science and Technology
    • /
    • v.38 no.3
    • /
    • pp.662-668
    • /
    • 2021
  • The aim of the present study was to design ascorbyl glucoside (AG) loaded solid lipid nanoparticles (SLNs) to improve skin penetration of AG. AG loaded SLNs were prepared using double emulsion method. The prepared AG loaded SLNs investigated particle characteristics (particle size, polydispersity index, zeta potential, loading capacity). Skin penetration study was carried out using SkinEthic RHE as one of the reconstructed human epidermis models. The mean particle size and zeta potential of SLNs were 172.65 - 347.19 nm and -22.90 - -41.20 mV, respectively. The loading capacity of AG loaded SLNs demonstrated that loading efficiency and loading amount were ranged from 44.18% to 57.77% and 12.83% to 16.15%, respectively. The results of penetration showed that all SLNs enhanced the skin penetration of AG and the amount of AG from SLNs were approximately 3.7 - 7.4 times higher than that from AG solution. Therefore, AG loaded SLN might be a promising topical drug delivery system.

Controlled synthesis of silica nanoparticles by a two-fluid nozzle flame reactor (이류체 노즐형 화염 반응기에 의한 실리카 나노분말 제조)

  • Chang, Han-Kwon;Jang, Hee-Dong;Chang, Won-Chul
    • Proceedings of the Korean Institute of Resources Recycling Conference
    • /
    • 2005.10a
    • /
    • pp.308-313
    • /
    • 2005
  • 실리콘 잉고트의 절단공정에서 발생하는 폐실리콘 슬러지는 실리콘과 실리콘카바이드 등의 유가자원이 함유되어 있으며, 이 중 실리콘 분말은 실리콘 화합물인 알콕시실란 등을 제조하는데 원료로 사용이 가능하다. 본 연구에서는 폐실리콘 슬러지로부터 분리, 합성된 사에 톡시실란(TEOS)을 원료로 이용하여 실리카 나노분말을 합성하였다. TEOS 원료물질을 외부 혼합형 이류체 노즐을 이용하여 미세액적으로 분무하고 화염 속으로 도입시키고 화염열분해 반응을 진행시켜 실리카 나노분말을 합성하였다. 합성된 실리카 나노입자의 특성은 투과형 전자현미경 및 BET에 의하여 입자형상 및 평균 입자크기가 분석되었다. 주요 공정변수인 분산공기의 압력, 반응가스의 조성을 변화시켜 실험한 결과 평균크기가 $9{\sim}68nm$인 실리카 나노분말을 제조하였다.

  • PDF

Calibration of monodisperse polystylene spheres of size from 1 to 10 ${\mu}m$ by using optical array sizing method (광학적 입자열 측정법에 의한 폴리스티렌구의 평균지름 측정)

  • 강주식
    • Korean Journal of Optics and Photonics
    • /
    • v.10 no.1
    • /
    • pp.21-26
    • /
    • 1999
  • The technique for calibrating standard particles larger than 1 $\mu$m by using an optical array sizing method has been established. The system consists of an optical microscope with transmission light source, a CCD camera, and a computer equipped with a frame grabber. The center distance between two spheres located at both ends of a row which consists of N spheres is measured in terms of pixel numbers, and divided by (N-1) to obtain the average pixel numbers per particle. This value is multiplied by length conversion constant, which has been determined in advance, to obtain the mean diameter of polystylene spheres. The length conversion constant is found from the microscopic image of calibrated standard stage micrometer plate. In order to reduce error in finding center positions of the scale and particles in the image, a software filter which dilates bright (or dark) object has been used. Spheres having nominal size of 1, 2, 3, 5, and 10$\mu$m were measured, and the maximum deviation of the measured mean diameter valus from their certified values was 0.7%. Standard particles which is larger than 1 $\mu$m can be calibrated by this method with measuredment uncertainy (k=2) lees than 1.53%.

  • PDF

Characterization of CdS-quantum dot particles using sedimentation field-flow fractionation (SdFFF) (침강 장-흐름 분획법을 이용한 CdS 양자점 입자의 특성 분석)

  • Choi, Jaeyeong;Kim, Do-Gyun;Jung, Euo Chang;Kwen, HaiDoo;Lee, Seungho
    • Analytical Science and Technology
    • /
    • v.28 no.1
    • /
    • pp.33-39
    • /
    • 2015
  • CdS-QD particles are a nano-sized semiconducting crystal that emits light. Their optical properties show great potential in many areas of applications such as disease-diagnostic reagents, optical technologies, media industries and solar cells. The wavelength of emitting light depends on the particle size and thus the quality control of CdS-QD particle requires accurate determination of the size distribution. In this study, CdS-QD particles were synthesized by a simple ${\gamma}$-ray irradiation method. As a particle stabilizer polyvinyl pyrrolidone (PVP) were added. In order to determine the size and size distribution of the CdS-QD particles, sedimentation field-flow fractionation (SdFFF) was employed. Effects of carious parameters including the the flow rate, external field strength, and field programming conditions were investigated to optimize SdFFF for analysis of CdS-QD particles. The Transmission electron microscopy (TEM) analysis show the primary single particle size was ~4 nm, TEM images indicate that the primarty particles were aggregated to form secondary particles having the mean size of about 159 nm. As the concentration of the stabilizer increases, the particle size tends to decrease. Mean size determined by SdFFF, TEM, and dynamic light scattering (DLS) were 126, 159, and 152 nm, respectively. Results showed SdFFF may become a useful tool for determination of the size and its distribution of various types of inorganic particles.

Analysis of Beach Gravels, the Weaver Peninsula, King George Island, Antarctica (남극 킹 죠지섬의 위버 반도 해빈자갈에 관한 연구)

  • 박용안;최문영;고영이
    • The Korean Journal of Quaternary Research
    • /
    • v.5 no.1
    • /
    • pp.47-61
    • /
    • 1991
  • Textural analysis of gravels of raised beach (old beach) in the Weaver Peninsula, King George Island, Antarctica has been carried out as a first part study among 20 other sites surveyed in the Weaver Peninsula and Barton Peninsula, King George Island. The raised beach described as WP-5 in this paper is 3.95 m higher than the present beach in elevation. And it is described as old beach. The beach shows typical subenvironment, that is, beach berm and beach face. Mean size, mean roundness and mean sphericity of gravels from beach berm are -4.10ø, 0.44 and 0.66 respectively. However, mean size, mean roundness and mean sphericity from beach face are -4.23ø, 0.41 and 0.67 respectively. In particular, it seems to be worthy to note the differences of textural parameters between Antarctic glacio-marine beach gravels and temperate and normal marine beach gravels. Under such conception the present study wishes to show only textural parameters, i.e., size, roundness, sphericity and shape obtained from the analysis of Antarctic glacio-marine beach gravels.

  • PDF

Modeling of Size-Dependent Strengthening in Particle-Reinforced Aluminum Composites with Strain Gradient Plasticity (변형률 구배 소성을 고려한 입자 강화 알루미늄 복합재의 크기 종속 강화 모델링)

  • Suh, Yeong-Sung;Park, Moon-Shik;Song, Seung
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.35 no.7
    • /
    • pp.745-751
    • /
    • 2011
  • This study proposes finite element modeling of dislocation punching at cooling after consolidation in order to calculate the strength of particle-reinforced aluminum composites. The Taylor dislocation model combined with strain gradient plasticity around the reinforced particle is adopted to take into account the size-dependency of different volume fractions of the particle. The strain gradients were obtained from the equivalent plastic strain calculated during the cooling of the spherical unit cell, when the dislocation punching due to CTE (Coefficient of Thermal Expansion) mismatch is activated. The enhanced yield stress was observed by including the strain gradients, in an average sense, over the punched zone. The tensile strength of the SiCp/Al 356-T6 composite was predicted through the finite element analysis of an axisymmetric unit cell for various sizes and volume fractions of the particle. The predicted strengths were found to be in good agreement with the experimental data. Further, the particle-size dependency was clearly established.

Synthesis and characterization of $BaTiO_3$ fine particles by hydrothermal process (수열합성법에 의한 미립의 $BaTiO_3$ 분말합성 및 특성)

  • 배동식;주기태;한경섭;최상흘
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.8 no.4
    • /
    • pp.563-566
    • /
    • 1998
  • $BaTiO_3$ fine particles were prepared by hydrothermal process from titanium tetra-isoproproxide ($Ti(OiPr)_4$) and barium hexa-hydroxide ($Ba(OH)_2{cdot}8H_2O$) as raw materials. The fine particles were obtained at the temperature range of 160 to $185^{\circ}C$. The properties of $BaTiO_3$ particles were studied as a function of various parameters such as reaction temperature, reaction time and Ba/Ti ratio, etc. The average particle size of $BaTiO_3$ increased with increasing reaction temperature and time. After hydrothermal treatment at $170^{\circ}C$ for 8 h, the average particle size of $BaTiO_3$ was about 30 nm and the particle size distribution was narrow.

  • PDF