• 제목/요약/키워드: 패각 잔골재

검색결과 22건 처리시간 0.015초

굴 패각 분말과 계란 껍데기 분말을 잔골재로 치환한 모르타르의 역학적 성능 (Mechanical Performance of Mortar Replacement of Oyster Shell Powder and Egg Shell Powder with Fine Aggregate)

  • 김해나;박준서;신종현;홍상훈;정의인;김봉주
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.33-34
    • /
    • 2022
  • The purpose of this study was to provide basic data for applying oyster shells and egg shells as fireproof cladding materials by substituting fine aggregates for oyster shell powder and egg shell powder, and comparing strength and fire resistance performance. The reason for the high strength was thought to be that the oyster shell had higher strength than the egg shell itself, and both ESP and OSP were measured at a backside temperature of less than 500℃, so it was judged that it could be used as a fireproof coating for steel structures.

  • PDF

탄산칼슘계 재료를 잔골재로 사용한 모르타르의 고온수열 후 중량변화 (Weight change after high-temperature hydrothermal heat of mortar using calcium carbonate-based material as fine aggregate)

  • 신종현;김해나;홍상훈;정의인;김봉주
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.75-76
    • /
    • 2022
  • In the event of a fire in the lower space, a high temperature of 1000℃ or more and an explosive fire may occur due to the closed structural features and combustible materials. On the other hand, more than 90% of oyster shells are made of CaCO3, and when heated to about 700℃ or higher, CaO and CO2 is generated due to decarboxylation reaction. In this study, we try to infer the amount generated by CO2 changing the weight of mortar using oyster shells as fine aggregates after heating. in conclusion It is considered that the smaller the particle, the greater the decarboxylation reaction and the greater the weight change.

  • PDF