Evaluation of Bending Strength for Ceramic Honeycomb Using Design of Experiments (실험계획법을 이용한 세라믹 허니컴의 굽힘강도평가)

  • Kim, Jong-Kyu;Baek, Seok-Heum;Cho, Seok-swoo;Shin, Soon-Ki;Joo, Won-Sik
    • Proceedings of the Korean Institute of Navigation and Port Research Conference
    • /
    • v.1
    • /
    • pp.379-384
    • /
    • 2006
  • Since the monolithic ceramic substrate was introduced for automotive catalytic converters, the durability of the substrate has been a continuing requirement to reduce the emission gas of vehicle. The substrate can occupy a volume as small as 82 $cm^3$ and as large as 8200 $cm^3$ to provide the required substrate for catalytic activity. The long-term durability varies with the size of the substrate from manufacture's point of view. Therefore This study presents that the response surface model using central composite design can explain size effect on the modulus of rupture in a cordierite ceramic monolithic substrate.

  • PDF

Acquirement of True Stress-strain Curve Using True Fracture Strain Obtained by Tensile Test and FE Analysis (인장시험과 유한요소해석으로 구한 파단 진변형률을 이용한 진응력-진변형률 선도 획득)

  • Lee, Kyoung-Yoon;Kim, Tae-Hyung;Lee, Hyung-Yil
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.33 no.10
    • /
    • pp.1054-1064
    • /
    • 2009
  • In this work, we predict a true fracture strain using load-displacement curves from tensile test and finite element analysis (FEA), and suggest a method for acquiring true stress-strain (SS) curves by predicted fracture strain. We first derived the true SS curve up to necking point from load-displacement curve. As the beginning, the posterior necking part of true SS curve is linearly extrapolated with the slope at necking point. The whole SS curve is then adopted for FE simulation of tensile test. The Bridgman factor or suitable plate correction factors are applied to pre and post FEA. In the load-true strain curve from FEA, the true fracture strain is determined as the matching point to test fracture load. The determined true strain is validated by comparing with test fracture strain. Finally, we complete the true SS curve by combining the prior necking part and linear part, the latter of which connects necking and predicted fracture points.

Block Shear Rupture and Shear Lag of Single angle in Tension Joint -Single angle with three or four bolt connection- (단일 ㄱ형강의 블록전단 파단 및 전단지체 현상 -고력볼트 3개 또는 4개로 접합된 단일 ㄱ형강-)

  • Lee, Hyang Ha;Shim, Hyun Ju;Lee, Eun Taik
    • Journal of Korean Society of Steel Construction
    • /
    • v.16 no.5 s.72
    • /
    • pp.565-574
    • /
    • 2004
  • The purpose of this paper was to investigate the block shear and the fracture in the net section, according to AISC Specifications, by analysing the shear lag effect in the block shear rupture of the single angle with three or four bolt connection. Specimen with three or four bolt connections showed that failure generally went from block shear with some net section failures to classic net section failures. From the test results, showed that the connection length, the thickness of angle, and reduction factor, which affect the block shear rupture, were investigated. According to the test results, it is suggested that the calculation of the net section rupture capacity by using the reduction factor of U, that was suggested by Kulak, is needed.

Effects of Cable Rupture on Dynamic Responses of a Concrete Cable-stayed Bridge (케이블 파단이 콘크리트사장교 동적거동에 미치는 영향)

  • Kim, Yu Hee;Go, Hyeong Gyu;Kim, Jae Cheon;Shin, Soobong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.16 no.3
    • /
    • pp.84-91
    • /
    • 2012
  • This paper aims to investigate the effects of cable rupture on the dynamic responses of concrete cable-stayed bridges in comparison with those of steel composite ones. It examines an adequate analysis method for simulating cable rupture using a time history function and evaluates the design guidelines for dynamic amplification factor (DAF). The computed DAFs from a concrete cable-stayed bridge are compared with those from a steel composite one based on the design guideline. As a conclusion, the current design guidelines for DAF may be reliable in overall but show some unstable cases despite satisfying the design guidelines, especially for concrete cable-stayed bridges.

An Experimental Study on the Block Shear Rupture of Angle Tension Members (인장력을 받는 ㄱ형강의 블록전단 파단에 관한 실험적 연구)

  • Kim, Bo Young;Lee, Kyu Kwong;Choi, Mun Sik
    • Journal of Korean Society of Steel Construction
    • /
    • v.10 no.4 s.37
    • /
    • pp.721-730
    • /
    • 1998
  • In this paper, an experimental study have been many studies on the joints of steel structure, for it has great influences on the safety of structures. Research on block shear rupture of the joint receiving pure tension have been done in foreign countries, but not in Korea. This study focuses on the propriety of block shear design code, according to limited state design criteria of steel structures recently established in Korea, by an experiment on the joint of angle tension members. The methods of this study were to compare other study results on block shear rupture mode and ultimate capacity, and to evaluate the propriety of the criteria design code. The result is that tension yield shear ruptures and shear yield tension ruptures happened at the joint, and the experimental rupture load was 15% higher than the capacity entered in the criteria design code. We conclude that it is necessary to revaluate the block shear design code presented by many studies on the limited state design criteria of steel structures.

  • PDF

Size Effect on the Modulus of Rupture in Automotive Ceramic Monolithic Substrate using Optimization and Response Surface Method (반응표면법과 최적화방법을 이용한 자동차 세라믹 모노리스 담체의 파단계수에 미치는 치수효과)

  • Baek, Seok-Heum;Shin, Soon-Gi;Joo, Won-Sik;Cho, Seok-Swoo
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.30 no.11 s.254
    • /
    • pp.1392-1400
    • /
    • 2006
  • Since the monolithic ceramic substrate was in introduced for automotive catalytic converters, the durability of the substrate has been a continuing requirement to reduce the emission, gas of vehicle. The substrate can occupy a volume as small as 82 $cm^3$ and as large as 8200 $cm^3$ to provide the required substrate for catalytic activity. The long-term durability varies with the size of the substrate from manufacture's point of view. Therefore this study presents that the response surface model using central composite design can explain size effect on the modulus of rupture in a cordierite ceramic monolithic substrate.

Fracture Prediction in Concrete-Filled Square HSS Bracing Members (콘크리트충전 각형 강관 가새부재의 파단 예측)

  • Lee, Mi-Ji;Moon, Ki-Hoon;Han, Snag-Whan
    • Proceedings of the Computational Structural Engineering Institute Conference
    • /
    • 2011.04a
    • /
    • pp.583-586
    • /
    • 2011
  • 가새골조의 정확한 내진성능평가를 위해서는 실험과 유사한 이력거동과 파단 시점을 잘 예측할 수 있는 해석적 모델이 필요하다. 가새의 이력거동을 모사히기 위해 본 연구에서는 이전 연구자들에 의해 제안된 물리적 이론 모델을 사용하였다. 또한, 가새부재의 국부좌굴에 의한 파단 예측을 위해 피로변수의 보정계수를 도입한 손상 지표를 개선하였다. 결과적으로 실험과 해석 결과를 비교하여 콘크리트충전 각형 강관가새부재의 국부좌굴 효과를 반영한 피로 보정계수를 판폭두께비에 따라 회귀분석을 통해 결정하고, 본 연구에서 제안한 해석 모델의 결과와 이전 연구의 결과를 비교하여 검증하였다.

  • PDF

고리 1호기 가압열충격 해석을 위란 계통 열수력 해석 연구

  • 김용수;김재학;홍순준;박군철
    • Proceedings of the Korean Nuclear Society Conference
    • /
    • 1998.05a
    • /
    • pp.751-756
    • /
    • 1998
  • 고리 1호기 원전 수명 연장을 위한 가압열충격(Pressurized Thermal Shock : PTS) 해석은 확률론적 안전성 평가 방법에 따라 수행된다. 본 연구는 가압열충격 상세 해석 연구의 일환으로 가압열충격 해석을 위한 계통해석시 사용되는 최적 평가(Best Estimate) 방법과 기존의 PCT(Peak Cladding Temperature) 관점의 해석에 사용되는 결정론적 안전성 평가 방법간의 해석 방법론 차이에 의한 열수력 거동의 상이점을 평가하기 위함이다. 이를 위해 1998년 설치 예정인 고리 1호기 교체 증기발생기(Replacement Steam Generator ; RSG) 안전성 분석 보고서$^{[1]}$ 의 주증기관 파단사고 해석 결과와 동일한 파단 크기 및 운전 출력에 대해 최적 평가 방법론에 따라 해석된 본 연구의 해석 결과를 비교, 평가하였다. 해석 결과 전출력 소형 주증기관 파단 사고에서는 터빈 유량 모델링 및 반응도 계수, 고온 영출력 대형 파단 사고에서는 가압기 모델, 반응도 계수 및 정지여유도가 해석 방법론에 따른 열수력 거동의 차이에 영향이 큰 것으로 평가되었다

  • PDF

핵연료 건전성 관점에서의 증기관 파단사고 해석 방법에 대한 고찰

  • 김철우;이병일;백승수;서성기;김희철
    • Proceedings of the Korean Nuclear Society Conference
    • /
    • 1996.05b
    • /
    • pp.525-530
    • /
    • 1996
  • 1000 MWe 국내 표준발전소의 증기관 파단사고에 대한 초기 노심 유량의 영향과 감속재 반응도 값의 영향을 증기관 파단사고시의 핵연료 건전성 관점에서 고찰하였다. 최대 핵연료 손상은 원자로 정지 후 약 2.5초 정도에 발생하였으며, 초기 노심 유량이 클수록 더 많은 핵연료 손상이 예측되었다. 또한, 감속재 반응도 값에 대한 분석 결과, 최소 핵비등이탈률 발생 싯점에서의 감속 재 반응도 계수를 사용한 해석 방법이 타당한 것으로 나타났다.

  • PDF

Pressurized Thermal Shock Analyses of Reactor Pressure Vessel for Main Steam Line Break (주증기관 파단사고에 대한 원자로 용기의 가압열충격 해석)

  • 정명조;박윤원;장창희;정일석
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.12 no.3
    • /
    • pp.271-279
    • /
    • 1999
  • 본 연구에서는 국내에서 가장 취약할 것으로 예상되는 원자력 발전소에 가압열충격 사고를 유발할 수 있는 주증기관 파단사고를 가정하여 열수력 해석과 파괴역학 해석을 수행하였다. 원전수명관리연구의 일환으로 계통열수력 해석 및 혼합열유동 해석에 의하여 구한 냉각제의 온도와 압력의 이력 및 용기의 재질성분으로부터 용기의 응력확대계수와 파괴인성치를 계산하고 이들을 비교하여 균열의 진전여부를 판단하여 형상계수가 1/6인 표면균열이 견딜 수 있는 최대 기준무연성천이온도를 결정하였다.

  • PDF