An Experimental Study on the Development of EMP Shielding Concrete Using Electric Furnace Oxidized Slag Aggregate (전기로산화슬래그 골재를 사용한 EMP차폐 콘크리트 개발에 관한 실험적 연구)

  • Min, Tae-Beom;Cho, Hyeong-Kyu
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.4
    • /
    • pp.514-520
    • /
    • 2021
  • In this study, EMP shielding performance was evaluated using electric furnace oxidized slag to give EMP shielding performance to concrete among the most used materials in construction sites. As a result of the evaluation, the component of the electric furnace oxidation slag was found to have an Fe2O3 content of 34%, and it was also found to contain an MgO component of about 4.8%. In addition, as a result of conducting an aggregate stability evaluation due to concerns about expansion due to MgO components, it is considered to be suitable for the KS standard. EMP shielding performance evaluation result showed that there was no correlation in EMP shielding performance according to compressive strength, and that general aggregates did not have EMP shielding. However, it was found that the aggregate using the furnace oxidized slag had excellent EMP shielding performance, and the shielding performance improved as the thickness increased. As a result of the durability evaluation, it was found that the EMP shielding concrete has the durability of abortion compared to the general concrete. Through this, it is thought that it will be good to improve the shielding rate if concrete is manufactured using electric furnace oxide slag when constructing EMP shielding structures in the future.

A Study on the Development of Light Emotion Friendly Concrete Block for Efficient Application of Titan-oxide Photocatalyst (이산화티탄 광촉매의 효율적 적용을 위한 LEFC 블록 제작에 관한 연구)

  • Kim, Byoung-Il;Oh, Sang-Keun;Seo, Seung-Hoon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.6
    • /
    • pp.120-131
    • /
    • 2019
  • Recently, the level of fine dust and ultrafine dust has reached its highest level, threatening the public's health. If the air purifier was not operated indoors, natural ventilation would not be possible. In this study, photocatalyst is applied to building materials to purify air in a passive manner. In order to use photocatalyst for LEFC(Light Emotion Friendly Concrete), it is necessary to secure self-consolidating capability. Therefore, self-consolidating performance was evaluated by slump test, J-ring test and L-box test with UHPC materials applied. Based on these results, the mixture proportion was determined, and the mechanical performance was evaluated by compressive and flexural tests. Concrete blocks were constructed with a fabrication method that improved the existing process of making LEFC. Also, the concrete block was emptied as a way to reduce the use of expensive photocatalyst. Finally, in order to identify the distribution of TiO2, an EDS analysis was performed.

An Experimental Study on the Characteristics of Fiber-Reinforced Concrete Beam Without Shear Reinforcement (전단보강근이 없는 섬유보강 철근콘크리트 보의 특성에 관한 실험적 연구)

  • Kim, Jeong-Sup;Go, Song-Kyoon;Choi, Jin-Seok
    • Journal of the Korea Institute of Building Construction
    • /
    • v.3 no.3
    • /
    • pp.83-90
    • /
    • 2003
  • This study examines the material characteristics of fibers and their influences on reinforced concrete through the tests of reinforced concrete by the types of fibers including non-reinforced, steel, polypropylene and cellulose fibers and the test of compressive strength and reinforced concrete beam without shear reinforcement and consequently it obtains the following conclusions. As a result of conducting compressive strength by the types of specimens, fiber reinforced specimen with the highest compressive strength value at 28 days of age was cellulose fiber reinforced specimen as 280.4kgf/$\textrm{cm}^2$ and steel fiber specimen had the highest compressive strength of 250.7kgf/$\textrm{cm}^2$ at 180 days of age. In case of non-reinforced specimen, its compressive strength was 277.4kgf/$\textrm{cm}^2$ at 28 days of age and 273.1kgf/$\textrm{cm}^2$ at 180 days of age. Comparing the compressive strength of non-reinforced specimen to that fiber reinforced specimen showed that the compressive strength of fiber reinforced specimen was lower in the passage of age and the results of this experiment showed no effects of fiber reinforcement. As a result of testing reinforced concrete beam without shear reinforcement, ductility factors of specimens were 4.67 for non-reinforced specimen, 8.18 for steel fiber reinforced specimen, 6.20 for polypropylene fiber reinforced specimen and 5.49 for cellulose reinforced specimen, and it is found that steel fiber reinforced specimen was highest. When non-reinforced specimen and steel fiber reinforced specimen were compared, steel fiber reinforced specimen had higher ductility factor of about 75.2% than that of non-reinforced specimen.

Properties of High Volume Blast Furnace Slag Concrete using Recycled Aggregate with Incineration Waste Ash (소각장애시의 치환에 따른 고로슬래그 미분말 다량치환 순환골재 콘크리트의 특성)

  • Han, Cheon-Goo;Lee, Hyang-Jae;Kim, Jun-Ho
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.1 no.2
    • /
    • pp.107-113
    • /
    • 2013
  • This study is the study desiring to solve the problem by utilizing the kinds of recycled resources considered to be troubled complementarily. Namely the reaction of potential hydraulicity of Blast Furnace Slag Powder (BS) shall be reacted with the alkali of Recycled Fine Aggregates Coarse Aggregate, it has been experimented to obtain the optimum value with the replacement ratio of incineration plant ash (WA) treated with the slaked lime as the experiment variable by solving the alkali of shortage with the Ordinary Portland Cement (OPC). As a result, the liquidity and the air volume are declined slightly as the replacement ratio of incineration plant ash WA increases, the mixture of incineration plant ash WA 1% has been analyzed to be the most suitable considering the viewpoint of effective handling of waste as the compression and the tensile strength showed the maximum value before and after 1% even though it was disadvantageous with the increase of chloride content.

Evaluation on Strengthening Capacities and Rebound Rate of Structures with Sprayed FRP (분사식 FRP에 의한 구조물의 보강 성능 및 반발률 평가)

  • Han, Seung-Chul;Yang, Jun-Mo;Yoon, Young-Soo
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.12 no.1
    • /
    • pp.193-202
    • /
    • 2008
  • This paper investigates experimentally the confining effect, strengthening capacity and rebound rate of sprayed Fiber-Reinforced-Polymer (SFRP). From the method, resin and chopped fibers are sprayed separately from the nozzle with high pressure, and then they are attached to the concrete surface, so structure could be repaired. To evaluate the strengthening effect of sprayed FRP, cylindrical specimens and beam specimens were strengthening with SFRP. As main material of FRP, glass fiber and polyester resin are used. To investigate the optimum condition of sprayed FRP, the effects of fiber length, coating thickness, fiber volume ratio and concrete strength were examined. Capacities of sprayed FRP method were also compared to the FRP sheet method. In case of the sprayed FRP, rebound rate is important parameter considering economical efficiency and constructibility, so rebound rate of was discussed. From the test results, optimum conditions of sprayed FRP were determined. SFRP method showed superior strengthening capacities than FRP sheet method.

A Experimental Study on the Strength Improvement of Ground Granulated Blast Furnace Slag Concrete Using Recycled Aggregate Powder as Alkali-activator (순환골재 미분말을 알칼리 자극제로 활용한 고로슬래그 미분말 혼입 콘크리트의 강도증진에 관한 실험적 연구)

  • Jeon, Chan-Soo;Ryu, Dong-Wo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.6
    • /
    • pp.527-534
    • /
    • 2017
  • Accordingly, this study, in order to use powder of recycled aggregate from production of recycled aggregate as an activator of ground granulated blast furnace slag, the influence of added recycled aggregate powder on physical properties of concrete induced ground granulated blast furnace slag were analyzed by hydration stages. The results of the study are summarized as follows: Except for samples eluted powder of recycled aggregate 1%, all the samples were high alkali suspensions with higher than pH 12.0. In particular, when eluted time was 5 hours, the sample eluted powder of recycled aggregate 3% showed about 15 mg/l of calcium hydroxide that was not different from the amount of calcium hydroxide in the mixing water eluted powder of recycled aggregate 5%. Hence, from this results, it can be considered that optimal eluted powder of recycled aggregate was 3% in this study. When using mixing water eluted with powder of recycled aggregate, compared to use of ordinary mixing water, it showed greater compressive strength in the entire ages, and in the sample replaced with ground granulated blast furnace slag by 50%, its compressive strength was greater than that of the OPC. As use of mixing water eluted with powder of recycled aggregate in concrete used with large amount of ground granulated blast furnace slag was more effective for improving compressive strength than ordinary mixing water, it is verified that powder of recycled aggregate had an effect of activator.

Structural Performance of RC Slab-Wall Joints Reinforced by Welded Deformed Steel Bar Mats (철근격자망을 사용한 슬래브-벽체 접합부의 구조성능)

  • Park, Seong-Sik;Yoon, Young-Ho;Lee, Bum-Sik
    • Land and Housing Review
    • /
    • v.2 no.1
    • /
    • pp.61-68
    • /
    • 2011
  • In order to clarify the structural performances of Welded Deformed Steel Bar Mats (WDSBM), the research stated includes the tests for standard hook of top bars of slab in concrete slab-wall joints, the tests for embedment length of top bar of slab, and the development strength tests for standard hook. The test results are as follows; (1) For slab-wall joints using WDSBM as reinforcement in slab, if the top bars of WDSBM are spliced by ordinary bars with sufficient development length and size, it is enough for the strength and crack control. (2) When WDSBM of slab is spliced in joint, the strength is increased with the embedment of bars of this WDSBM into wall. Beyond peak strength, however, ductility is diminished to that as no splice due to pull-out failure. (3) For slab-wall system, ultimate strain of concrete for flexural compression zone in lower surface of slab seems much greater than that of normal concrete beam. The reason is that normal concrete beam has the joint with $180^{\circ}$, however slab-wall joint has the $90^{\circ}$ of which concrete can be confined.

Evaluation of Lateral Strength and Ductility of Velcro Reinforced RC Columns with Finite Element Analysis (유한요소해석을 통한 벨크로로 보강된 RC 기둥의 횡방향 강도 및 연성 능력 평가)

  • Kim, Sang-Woo;Kim, Kyeong-Min;Kim, Geon-Woo;Lee, Su-Young;Kim, Jin-Sup
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.4
    • /
    • pp.12-19
    • /
    • 2021
  • Recently, with frequent earthquakes around the world, research on seismic design and seismic reinforcement of reinforced concrete facilities has been actively conducted from earthquakes. In particular, columns, which are compressed members of reinforced concrete structures, are vulnerable to lateral forces caused by earthquakes, so an appropriate seismic reinforcement method is required. Therefore, this study intended to develop Velcro seismic reinforcement method that is quick and easy to construct. For the development of Velcro seismic reinforcement, the adhesion and tensile strength of the existing industrial velcro was improved. A direct tensile test was also conducted to compare the tensile performance of the newly-developed velcro seismic reinforcement to industrial one. In addition, numerical analysis was performed to predict the seismic performance of RC columns reinforced by industrial and newly-developed velcro. Based on the analysis results, the strength and ductility of the non-seismic and velcro-reinforced RC column were reviewed. The analysis confirmed that both the strength and ductility of non-seismic RC columns reinforced by industrial and newly-developed velcro increased, but the seismic performance of the newly-developed Velcro reinforcement is better than that of industrial velcro.

A Study on the Evaluating Method the most Favorable Mixture Proportion of Blended Fine Aggregate for Effective Application of Recycled Aggregate (재생골재의 효율적인 활용을 위한 혼합잔골재의 최적배합평가방법에 관한 연구)

  • Han, Cheon-Goo;Yoon, Gi-Won;Lee, Gun-Cheol;Park, Yong-Kyu
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.1
    • /
    • pp.113-119
    • /
    • 2006
  • It is now established that more than two types of blended aggregate have beneficial effects on quality and supply of concrete in the long run. However, studies on blended aggregate have not widely been progressive and the evaluation method of its most favorable mixture proportion is still needed. Therefore this study investigated the most favorable mixture proportion through the physical experiment of fresh and hardened state's cement mortar, in response to three types of composite ratio, natural fine aggregate(Ns), crushed fine aggregate(Cs) and recycled fine aggregate(Rs). Test showed that increase of blending ratio of Ns and Cs improved fluidity of mot1ar. For the properties of compressive and flexural strength, mortar blending Ns and Cs properly, exhibited similar value to one using only Cs, while mortar mixing Rs showed lower strength value as less as 6% of control one. Mortar using only Rs exhibited the largest drying shrinkage value. In addition, even thought it is not a clear quantitative analysis, technical-imaging-skill presenting the most favorable mixture proportion 3-dimensionally is proposed in this research, in order to notify the proportion easily.

  • PDF

Analyzing the Engineering Properties of Cement Mortar Using Mixed Aggregate with Reject Ash (혼합골재에 리젝트애시를 프리믹스하여 활용하는 시멘트 모르타르의 공학적 특성 분석)

  • Han, Cheon-Goo;Park, Byung-Moon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.3
    • /
    • pp.247-252
    • /
    • 2017
  • The aim of this research is the feasibility analysis of the reject ash premixed cement mortar with combined aggregate. Namely, for the combined aggregate with two different qualities of aggregates, a fundamental properties of cement mortar was evaluated depending on various replacing ratios of reject ash(Ri). According to the experimental results, the combined aggregate consisted with low-quality aggregate and sea sand did not change the flow value depending on the reject ash while the combined aggregates consisted with low quality aggregate and sea sand; and consisted exploded debris sand and sea sand the increasing reject ash increased the air content with increased replacing ratio of reject ash. In the case of compressive strength, as the replacing ratio of reject ash was increased, the compressive strength was increased. It is considered that when 5% of reject ash replacing ratio made similar quality of cement mortar with favorable quality aggregate, hence, it can be suggested that 5% replacement of reject ash for desirable fluidity and compressive strength of concrete.