• Title/Summary/Keyword: 초기시편

Search Result 341, Processing Time 0.032 seconds

A study of mixed-mode interlaminar fracture toughness of graphite/epoxy composite (炭素纖維强化 複合材料의 혼합모우드 層間破壞靭性値에 대한 硏究)

  • 윤성호;홍창선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.10 no.2
    • /
    • pp.198-207
    • /
    • 1986
  • This study investigates interlaminar fracture characteristics of Graphite/Epoxy composite (HFG Graphite/Epoxy) under mode I (opening mode), mode II (sliding mode) and mixed mode loading conditions. The effects on interlaminar fracture toughness due to different fiber orientations on the crack surface are also investigated. The antisymmetric test fixture proposed by M. Arcan is used for this test. Both critical stress intensity foctors and critical energy release rates were determined and several mixed mode fracture criteria were compared to the experimental data. Also fracture surfaces were investigaed to obtain informations on the fracture behaviors of Graphite/Epoxy composite by means of a scanning electron microscope(SEM).

A Study on the Variable Condition Debinding Process in Supercritical CO2 for Removing Binder from Thick Ceramic Injection Molded Parts (두꺼운 세라믹 사출성형체로부터 효율적인 결합제 제거를 위한 초임계 CO2 가변조건 탈지공정 연구)

  • Kim, Hyung-Kun;Yim, Joon-Hyuk;Kim, Hyung-Soo;Lim, Jong-Sung
    • Clean Technology
    • /
    • v.18 no.2
    • /
    • pp.155-161
    • /
    • 2012
  • The purpose of this study is to remove paraffin wax binder effectively from powder injection molded part using supercritical fluids in powder injection molding process. For a thin powder injection molded part about 1-2 mm thickness, paraffin wax binder can be removed rapidly without any defect by traditional supercritical extraction process which has fixed high temperature and pressure condition. But, for a thick powder injection molded part, there are limitations in removing paraffin wax binder by the fixed high process condition because crack occurs at the beginning step. Therefore, here we studied variable condition debinding process that starts with mild process condition at the beginning step and then increase the process conditions simultaneously at each step. To find out the initial process condition that has the highest extraction yield without any defect for each sample thickness, we investigated various supercritical debinding conditions using 1-4 mm thickness ceramic injection molded sample. By using the variable condition debinding process that starts with the initial process condition at the first step and then increasing process conditions simultaneously at each step (temperature from 333.15 to 343.15 K, pressure from 12 to 27 MPa, and $CO_2$ flow rate from 1.5 to 10 L/min), over 95% of paraffin wax binder was removed from the 4 mm thick (10 mm diameter) ceramic injection molded disk samples within 5 hours.

Fire-Retardation Properties of Silicone/Perlite Composites (실리콘/펄라이트 복합체의 난연 특성)

  • Lee, Byunggab;Won, Jongpil;Jang, Ilyoung;Bang, Daesuk
    • 한국방재학회:학술대회논문집
    • /
    • 2011.02a
    • /
    • pp.154-154
    • /
    • 2011
  • 최근 세계 각지에서 발생하는 대규모 터널 화재사고는 많은 사상자를 동반하고 이에 따른 경제적, 사회적 손실 또한 방대하게 진행되는 실정이다. 터널 구조물의 화재 특성상 외부에 쉽게 노출되지 않기 때문에 화재 발생 시 화재에 노출된 표층이 박리되거나 비산해서 단면결손이 생기는 폭렬 현상(explosive spalling)이 발생하게 된다. 이러한 폭렬 현상은 붕괴와 같은 대형 참사로 이어질 가능성이 크다. 따라서 본 연구에서는 터널 내 화재 발생 시 콘크리트 구조물의 폭렬에 의한 붕괴를 예방하기 위하여 이액형 상온경화 실리콘 고무와 인체에 무해한 친환경 첨가제인 펄라이트를 일정한 혼합비(5wt%, 10wt%, 15wt%, 20wt%)로 혼합하여 고성능 난연 복합체를 제조하고, 열적 특성과 난연 특성을 연구를 진행하였다. 열적 특성에 관한 시험으로 TGA를 측정하였으며, 난연 특성에 관한 시험으로는 화염 시험, 내화로 시험, 탄화로 시험을 진행하였다. 우선 TGA 시험은 $20^{\circ}C/min$ 승온 속도로 $800^{\circ}C$까지 실험을 하였고, 화염 시험은 제작한 시편과 gas torch($1200^{\circ}C$)의 화염 거리를 약 10cm로 하여 약 1시간 동안 시험을 하였다. 내화로 시험은 내화로 장치를 이용하여 RABT curve(5분만에 $1200^{\circ}C$도달 후 한 시간 동안 유지 후 냉각, 총 시험 시간 180분) 조건을 만족하는 환경에서 제작한 시편을 콘크리트에 부착하여 콘크리트의 내부온도를 측정하였다. 탄화로 시험은 탄화로 장치를 이용하여 $2^{\circ}C/min$ 승온속도로 $900^{\circ}C$까지 실험을 하여 외부 형태 변화를 관찰하였다. 각각의 시험 결과 TGA 열분해 결과 순수한 실리콘 고무보다 난연제인 펄라이트를 첨가했을 때 더 높은 온도에서 초기 분해 거동을 보였으며, 최종 잔류량은 80%를 보였고, 5 wt%의 펄라이트가 혼합된 시편의 최종 잔류량이 높은 것으로 보아 열분해에 가장 강한 조성임을 알 수 있었다. 화염 시험 결과 펄라이트가 혼합된 모든 시편에서 $300^{\circ}C$가 넘지 않은 결과를 보였다. 이는 제조된 복합체가 화염에 직접적으로 장시간 노출이 되어도 안전하다는 것을 알 수 있다. 내화로 및 탄화로 시험 결과 펄라이트가 15wt%와 20wt%가 첨가된 시편들보다 5wt%와 10wt% 첨가된 시편들이 고온에서 안정하다는 것을 보였다.

  • PDF

Diagnosis of Early Dental Caries with Dye-Enhancing Quantitative Light-Induced Fluorescence (QLF) (정량 광유도 형광법(QLF)과 광활성제를 이용한 초기 치아우식증의 진단)

  • Kim, Mihee;Lee, Sangho;Lee, Nanyoung
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.42 no.3
    • /
    • pp.218-225
    • /
    • 2015
  • This study used sodium fluorescein to improve imaging diagnostic ability by increasing the fluorescence difference between sound enamel and caries lesions. It also made it easier to discriminate between stain and caries lesions using quantitative light-induced fluorescence (QLF). Half of the specimen surface was covered with nail varnish as a control. Specimens were divided randomly in six decalcification groups and decalcified for different lengths of time. Then, ${\Delta}F$ was measured using QLF-D. After applying 0.075% sodium fluorescein, we measured ${\Delta}F$ again and compared it with the initial value. After cutting the central portion of the specimen, we measured the lesion depth using scanning electron microscopy. The lesion surfaces observed with QLF were darker than normal enamel, whereas they were lighter than normal enamel after applying fluorescein. Longer decalcification time was associated with greater fluorescent dye penetration. The ${\Delta}F$ measured after applying fluorescein was higher than the initial value (p < 0.05). Due to QLF measurement using fluorescein being more sensitive for diagnosing early decalcification, this approach will enable early diagnosis of dental caries before the cavity formation stage, allowing the treatment of early caries lesions. With QLF and sodium fluorescein, we can easily discriminate between stain and caries lesions.

A Proposal of Autogenous Deformation and Self-induced Restrained Stress Test Using Thermal Analysis Results to Predict Early-Age Cracks of Externally Restrained Concrete Members (외부구속 콘크리트 부재의 초기균열 예측을 위해 온도해석 결과를 이용한 자가변형 및 구속응력 측정 실험의 제안)

  • Byun, Jong-Kwan;Kang, Won Ho;Kang, Jeong-Kil;Bae, Seong-Jae
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.38 no.1
    • /
    • pp.1-10
    • /
    • 2018
  • It is difficult to predict the early-age cracks of strain restrained concrete members due to environmentally sensitive parameters. A new method is proposed to predict the cracks by test of autogenous deformation and self-induced restrained stress of specimens which simulates early-age crack state by hydration heat of the'Wall-On-Foundation'members. For this purpose, thermal analysis of entire structure considering the environmental condition is performed at first, and the specimens are set up where hydration heat was electronically controlled according to the analysis results. By measuring free deformation and force to compensate the autogenous strain including relaxation, feasibility of cracks can be estimated. The proposed method can predict the occurrence of cracks better than the material test of the early age concrete which has large variance. The method of this study is particularly useful when it is used as a preliminary experiments to predict the crack more precisely before full-scale concrete placement in construction of large structures.

Estimation of Transient Creep C(t)-integrals for SE(B) Specimen Under Elastic-Plastic-Creep Conditions (탄성-소성-크리프 상태에서 SE(B) 시편의 천이크리프 C(t)-적분 평가)

  • Lee, Han-Sang;Je, Jin-Ho;Kim, Dong-Jun;Kim, Yun-Jae
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.39 no.9
    • /
    • pp.851-857
    • /
    • 2015
  • In this paper, we estimate the time-dependent C(t) integrals under elastic-plastic-creep conditions. Finite-element (FE) transient creep analyses have been performed for single-edge-notched-bend (SEB) specimens. We investigate the effect of the initial plasticity on the transient creep by systematically varying the magnitude of the initial step load. We consider both the same stress exponent and different stress exponents in the power-law creep and plasticity to elastic-plastic-creep behavior. To estimate the C(t) integrals, we compare the FE analysis results with those obtained using formulas. In this paper, we propose a modified equation to predict the C(t) integrals for the case of creep exponents that are different from the plastic exponent.

Estimation of Transient Creep Crack-tip Stress Fields for SE(B) specimen under Elastic-Plastic-Creep Conditions (탄성-소성-크리프 상태에서 SE(B) 시편의 천이크리프 균열 선단 응력장 평가)

  • Lee, Han-Sang;Je, Jin-Ho;Kim, Dong-Jun;Kim, Yun-Jae
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.39 no.10
    • /
    • pp.1001-1010
    • /
    • 2015
  • This paper estimates the time-dependent crack-tip stress fields under elastic-plastic-creep conditions. We perform Finite-Element (FE) transient creep analyses for a Single-Edge-notched-Bend (SEB) specimen. We investigate the effect of the initial plasticity on the transient creep by systematically varying the magnitude of the initial step-load. We consider both the same stress exponent and different stress exponent in the power-law creep and plasticity to determine the elastic-plastic-creep behaviour. To estimation of the crack-tip stress fields, we compare FE analysis results with those obtained numerically formulas. In addition, we propose a new equation to predict the crack-tip stress fields when the creep exponent is different from the plastic exponent.

Finite element analysis of unconstrained axisymmetric piercing (구속이 없는 축대칭 피어싱 공정의 유한요소해석)

  • 양동열;유요한;이종수
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.10 no.6
    • /
    • pp.876-888
    • /
    • 1986
  • The Study is concerned with the analysis of unconstrained axisymmetric piercing as a nonsteady forging process by the rigid-plastic finite element method. In the numerical analysis of axisymmetric piercing, the initial velocity field is generated by assuming the material as a linear viscous material to begin with in order to facilitate the input handling and to ensure better convergencey. The strain-hardening effect for nonsteady deformation and the friction of the die-material interial interface are considered in the formulation. Rigid body treatment is also incorporated in the developed program. The experiments are carried out for aluminum alloy specimens (A1204) with different specimen heights. It is shown that the experimental results are in excellent agreement with the finite element simulations is deformed configuration. For load prediction the theoretical prediction shows excellent agreement with th eexperimental laod in the initial stage of loading before fracture of the specimen is not initiated. Distribution of stresses, strains and strain rates has been found for the given cases in computation. On this basis several fracture criteria are introduced in order to check the fracture initiation. It is found that maximum shear criterion is capable of good fracture prediciton.

Finite Element Based Edge Crack Analysis of Silicon-Steel Sheet in Cold Rolling (실리콘 강판 압연시 에지크랙 발생에 관한 유한요소해석)

  • Byon, Sang-Min;Lee, Jae-Hyun;Kim, Sang-Rok;Jang, Yun-Chan;Na, Doo-Hyun;Lee, Jong-Bin;Lee, Gyu-Taek;Song, Gil-Ho;Lee, Sung-Jin
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.22 no.6
    • /
    • pp.511-517
    • /
    • 2009
  • In this paper an finite element approach for the edge crack analysis of silicon-steel sheet during cold rolling is presented. Based on the damage mechanics, the proposed approach follows the analysis steps which are composed of damage initiation, damage evolution and fracture. Through those steps, we can find out the initiation instant of crack and resulting propagated length and shape of the crack. The material constants related to fracture is experimentally obtained by tension tests using standard sheet-type specimen and notched sheet-type specimen. To evaluate the prediction accuracy, we performed a pilot rolling test with a initially notched sheets. It is shown that the results obtained by the approach converged to the experimental one concerning about the direction and length of propagated crack. The capability of the proposed one is demonstrated through the application to the actual silicon-steel rolling mill.