Compressive Strength Correlation of Very-Early-Strength Dry-Mix Shotcrete on Test Method (측정방법에 따른 속경성 건식 숏크리트 압축강도의 상관관계)

  • Yun, Kyong-Ku;Choi, Sung-Yong;Kim, Jin-Woung;Kil, Yong-Su
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.11 no.10
    • /
    • pp.3988-3997
    • /
    • 2010
  • Shotcrete was a mortar or concrete that is pneumatically projected at high velocity onto a subject. It has been applied for tunneling, underground big-spaces, slope stabilization. Shotcrete is increasing use in structure repair. The dry-mix shotcrete require a smaller equipment, easy maintenance, possible of very-earlystrength materials than wet-mix shotcrete, which make this process attractive and economic for structural repairs. It is common practice core compressive strength to the dry-mix shotcrete quality control. This test is very difficult estimating eraly-strength of Very-Early-Strength Dry-Mix Shotcrete. The purpose of this research was to analyze the correlation of test results among cube test, core test, pullout test and maturity. The correlationship analysis of test results among cube test, core test, pullout test and maturity showed more than 90%.

Mock-up Test of Concrete Using AE Water Reducing Agent of Early-Strength Type in Construction Field (조기강도발현형 AE감수제를 사용한 콘크리트의 현장 Mock-up 실험)

  • 황인성;김기훈;김규동;이승훈;한천구
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2004.05a
    • /
    • pp.1-4
    • /
    • 2004
  • In this paper. applicability of high early strength type AE water reducing agent(HESAEWA) developed by the authors is discussed by applying Mock-up test. For fresh concrete properties, concrete using existing AE water reducing agent(EAEWRA) and HESAEW A meets the target slump and air content at jobsite. Setting time of concrete using HESAEWA is shorter than that using EAEWRA. Remarkable variance of bleeding and settlement is not observed with type of AE water reducing agent. For hardened concrete properties, use of HESAEW A results in higher strength development compared with that of EAEWRA at standard curing and in field curing condition. Reaching time to accomplish 5MPa of compressive strength. which is possible to remove side form. is taken using HESAEWA earlier than that of EAEWRA by 1day. Therefore, it is confirmed that use of HESAEWA can meet the requirements of general quality of concrete and achieve high early strength development as well as has a desirable field applicability.

  • PDF

An Experimental Study on the High Early Strength Development Properties of Concrete according to Batcher Plant Test and Mock-up Test (배쳐플랜트배합시험 및 실대부재시험을 통한 콘크리트의 조기강도 발현특성에 관한 실험적 연구)

  • Lee, Ji-Hwan;Lee, Jong-suk;Lee, Sang-Soo;Song, Ha-Young
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2008.11a
    • /
    • pp.1-5
    • /
    • 2008
  • In this study, batcher plant composition test and mock-up test were carried out to conduct comparison and analysis on flow behavior and strength properties of concrete at early age. As a result, it was found that slump and amount of air in batcher plant composition test reached the target range. As for compressive strength, composition using HESPC showed the most excellent strength development. In mock-up test which was carried out to find out the strength properties, two methods with specimen and core test body both revealed HESPC as the most excellent composition. However, strength estimation with ultrasonic survey presented less reliable data. As a result of the previously conducted indoor composition test and the mock-up test in this study, target performance of concrete at early age was 4day/cycle. It was found that the optimum conditions that meet the required strength, 5MPa/18hr and 14MPa/36hr in mullion and transom are; curing temperature above 15℃, W/B 45%, unit-water 165kg/㎥ and CHC cement.

  • PDF

Experimental Study on the Fire Resistance of Concrete Filled Steel Tubes according to Concrete Compressive Strengths (콘크리트 압축강도에 따른 강관기둥부재의 내화성능에 관한 실험적 연구)

  • Kwon, In-Kyu
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.11 no.2
    • /
    • pp.1-8
    • /
    • 2011
  • Concrete filled steel tubes(CFST) is considered as a column having better structural stability and better performance of fire resistance than that made with H-section and hollow section in itself. To get the fire resistance of the CFST, two kinds of concrete strength were used, 21 MPa, 40 MPa and 4 sorts of the applied loads were calculated and used to the specimens such as 3.5 m long, round and rectangular section. After various fire tests under 4 sorts of load ratios, the fire resistance of the CFST is not possible to get over 1 hour because of the rapid decrease of concrete strength. The below 50% of the applied load is recommended to obtain over 1 hour fire resistance of the CFST.

Behavior of Precast Concrete Shear Walls with C-Type Connections (C형 접합부를 이용한 프리캐스트 콘크리트 전단벽의 거동)

  • Lim, Woo-Young;Hong, Sung-Gul
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.4
    • /
    • pp.461-472
    • /
    • 2010
  • This paper investigates the behavior of precast concrete (PC) shear walls with a new vertical connections for a fast remodeling construction. The C-type vertical connections for the PC wall systems are proposed for transfer of bending moment between top and bottom walls in the vertical direction while a shear key in the center of wall is prepared to transfer shear forces by bearing action. The proposed vertical connections allows easy fabrication thanks to slots at the edges of wall in opposite directions. The plane PC wall systems subject to lateral load are compared with ordinary wall systems by investigating the effects of connection on the stiffness, strength, ductility, and failure modes of whole systems. The load-displacement relationship and influence of premature failure of connections are examined. The experimental test showed that the longitudinal reinforcing steel bars placed at the edges of walls yielded first and the ultimate deformation were terminated due to premature failure of connections. The diagonal reinforcements for efficient shear transfer in the walls were not effective. The strength and deformation obtained through the section analysis were generally in agreement with the experimental data, and indicated that. Gap opening contributed to the deformation behavior more than any other factors.

Evaluation on Workability and Compressive Strength Development of Concrete Using Modified Fly-Ash by Vibration Grinding (진동분쇄를 사용한 개질 플라이애시 콘크리트의 유동성 및 압축강도 발현 평가)

  • Ahn, Tae-Ho;Yang, Keun-Hyeok;Jeon, Young-Su
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.1
    • /
    • pp.66-74
    • /
    • 2021
  • The objective of this study is to evaluate the practical application potential and limitations of the modified fly ash(MFA) by vibration grinding as a partial replacement of ordinary portland cement(OPC). The test parameters investigated were the replacement level of fly ash(FA) and FA for OPC, varying from 10% to 40%, and curing temperatures of 5, 20, and 40℃. The various characteristics(including slump, air content, bleeding, setting time, compressive strength development, and hydration products) of MFA concrete were measured and then compared with those of the concrete with conventional FA. Test resul ts showed that the MFA prefers to FA in reducing the bl eeding of fresh concrete and enhancing the compressive strength gain at an early age. The compressive strength ratios between MFA and FA concrete specimens at an age of 1 day were 135%, 146%, and 111% at the curing temperatures of 5, 20, and 40℃, respectively. The corresponding ratios at an age of 28 days were approximately 110%, regardless of the curing temperatures. The X-ray diffraction analysis also revealed less calcium hydroxide products in MFA pastes than in FA pastes.

Properties of Early Strength Development according to the Replacing Method of Admixture of Concrete Using AE Water Reducing Agent of Early-Strength Type (조기강도 발현형 AE감수제를 사용한 콘크리트의 혼화재 치환방법 변화에 따른 초기 강도발현 특성)

  • 황인성;우종완;김규동;이승훈;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.11a
    • /
    • pp.269-272
    • /
    • 2003
  • This study is intended to investigate the properties of concrete using AE Water Reducing Agent of Early-Strength Type. According to the results, as for the replacing method of mineral admixture, setting time is shortened faster in order of replacement for fine aggregate, combination and replacement for cement, and when AE Water Reducing Agent of Early-Strength Type is used, it is shortened by about 4 hours, compared with normal AE Water Reducing Agent Compressive strength is lower in the case of replacement for fine aggregate, but higher in the other case than that of plain concrete. And When AE Water Reducing Agent of Early-Strength Type is used, early compressive strength is very high in comparison to normal AE Water Reducing Agent. Early strength development is very favorable by the use of AE Water Reducing Agent of Early-Strength Type regardless of the replacing method of mineral admixture at $20^{\circ}C$, but at $l0^{\circ}C$, it is effective for Early strength development that W/B is lowered to below 45%, BS of 20% is replaced for fine aggregate, and AE Water Reducing Agent of Early-Strength Type is used.

  • PDF

The influence of dynamic force balance on the estimation of dynamic uniaxial compression strength (암석시료 내 동적하중 분배특성이 동적일축압축강도에 미치는 영향성에 관한 연구)

  • Oh, Se-Wook;Min, Gyeong-Jo;Park, Se-Woong;Park, Hoon;Suk, Chul-Gi;Cho, Sang-Ho
    • Explosives and Blasting
    • /
    • v.37 no.1
    • /
    • pp.14-23
    • /
    • 2019
  • It has been an always issue for the blasting or the impact analysis to consider the strength characteristics of the rock materials associate with loading rate dependency. Due to the nature of transient loading, the dynamic rock test requires a careful technique to achieve the stress equilibrium state of the specimen. In this study, to investigate the relationship between the rock dynamic strength and the stress equilibrium state, a series of dynamic uniaxial compression tests for Pocheon granite were performed. As a result, the unbalanced stress state on the specimen can lead to the premature failure on the specimen and the less estimation of dynamic strength characteristic as well as the overestimation of strain rate. Consequently, a careful consideration of rock fracture process to achieve the dynamic force balance on the specimen should be required to make an reasonable evaluation of rock dynamic strength.

Characteristics of Ternary Blended Cement Concrete Using Fly Ash and Silica Fume for Post-Tensioned Concrete Pavement Application (포스트텐션 콘크리트 포장 적용을 위한 실리카흄과 플라이 애시를 사용한 삼성분계 콘크리트의 특성)

  • Choi, Pan-Gil;Shim, Do-Sick;Lee, Bong-Hak
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.9 no.3
    • /
    • pp.41-47
    • /
    • 2009
  • Post-tensioned concrete pavement(PTCP) was developed to built long-span concrete pavement(120 m span) and to maintain long-term service life(over 40 years) of concrete pavement. In the present study, research for high-durable concrete was conducted to utilize the advantage of PTCP construction method efficiently. First of all, 20% of fly ash(by binder weight) was replaced to control alkali silica reaction. Second, silica fume was applied to improve the water-permeability and early-age strength. Results of tests for mechanical properties, water-permeability resistance, and surface-scaling resistance of ternary blended cement concrete showed that the early-age strength was improved significantly with addition of silica fume. The water-permeability resistance was improved from "Low" to "Very Low"(ASTM C 1202). However, surface-scaling resistance was decreased with an increase of silica fume, therefore, content of silica fume should be kept in less than 5%(by binder weight) to assure field application considering durability. The results of air-void analysis showed that durability factors were improved since spacing factors were estimated as 250$\pm$15 micron in adjusted mixtures.

A Study on Preventive Methods Against Concrete Corrosion by Sea Water of the of West Sea (서해조수에 의한 콘크리트의 부식 방지법에 관한 연구)

  • 고재군
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.14 no.2
    • /
    • pp.2622-2633
    • /
    • 1972
  • This study was attempted in order to search for phyosical properties on various mix designs of concrete as ne of studies relating top revention against corrosion by action of sea water in the West Sea. In this study, as concerete mix design, fly ash, pozzolith and vinsolresin were used as admixtures for normal portland cement respectively, and pozzolan cement and normal cement were also used for each plain concrete. Concrete specimens were made and cured in accordance with the Korean Standard Specifications for concrete. In thetest, compressive strengths of the specimens were measured at the following ages; 7-day, 28-days and 3-months. Absorption test was made by immersing the specimens in water kept at boiling temperature for 5 hours. The results obtained from the tests are summarized as follows; 1. The use of fly ash as an admixture in mix design of concrete, has an effect on compressive strength at each age. But it is actually not effective on absorption by concrete, as the result of the fly ash concrete is almost the same at that of ordinary plain concrete. 2. The use of pozzolith as an admixture in mix design of concrete, has an effect on both of compressive strength at each age and absorption rate. The pozzolith is more effective than vinsol resin, relating to improvement for physical proreties of concrete. 3. The use of vinsol resin as an admixture in mix design of concrete, has also an effect on both of compressive strength at each age and absorption rate. As the above fact, effectiveness of the vinsol resin is some what lower than pozzolith, as far as physical properties of the concrete are concerned. 4. Plain concrete used pozzolan cement only is the most effective on both of strength at each age and absorption rate in this study. The pozzolan cement is characteristic of higher strenth as the age is later. 5. Relationship between compreessive strengths and absorption rates of the concrete is shown by a different regression line dependingon ages. The gradient of the regression line is steeper as the age is later. 6. Throught physical test, it may be expected that the use of pozzolith and vinsol resinas asan admixture respectively will be better resistant than fly ash or ordinary plain concrete and that plain pozzolan concrete will also be the best resistant to action of sea water due to improvement of theirphysical properties.