• Title/Summary/Keyword: 자기포화도

Search Result 446, Processing Time 0.023 seconds

The Study on the Additives and Magnetic Property of YIG Ferrites for Circulator/Isolator (서큘레이터/아이솔레이터용 YIG 페라이트의 첨가제와 자기적 특성 연구)

  • 윤휘영;유승규;이수형;윤종남;김정식
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.12
    • /
    • pp.1155-1161
    • /
    • 2001
  • Yittrium Iron Garnet(YIG) has been used as an important material in the circulator/isolator which is used in RF communication system, mobile phone, adn satellite broadcasting, etc. In this study, we investigated the microstructural and magnetic properties of YIG ferrites with the sintering temperature and additives. We fabricated the YIG ferrites substituted with Ca, In, V by the traditional ceramic sintering method at 1250$\^{C}$, 1275$\^{C}$, 1300$\^{C}$ and 1325$\^{C}$. Powders were granulated by using a spray dryer. Crystallographic and microstructural properties were measured by using XRD and SEM. Magnetic properties were measured by using a VSM for saturation magnetization (4$\pi$M$\_$s/) and FMR (Ferromagnetic Resonance) experiment for ferromagnetic resonance line width (△H). The YIG ferrite, Y$\_$1.6/Ca$\_$1.4/Fe$_4$V$\_$0.7/In$\_$0.3/O$\_$12/, sintered at 1300$\^{C}$, showed higher saturation magnetization and lower ferromagnetic resonance line width than any other sintering temperatures.

  • PDF

Phase transformation and magnetic properties of NiFe thin films on Si(100) wafer and SiO2/Si(100) substrate by co-sputtering (Si(100) wafer와 SiO2/Si(100) 기판에 동시 스퍼터링법으로 증착된 NiFe 합금 박막의 상변화 및 자기적 특성)

  • Kang, Dae-Sik;Song, Jong-Han;Nam, Joong-Hee;Cho, Jeong-Ho;Chun, Myoung-Pyo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.20 no.5
    • /
    • pp.216-220
    • /
    • 2010
  • Ni-Fe alloys have various applications such as thin film inductor, thin film transformer, magnetic head's shield case, etc. Magnetic properties of Ni-Fe thin films depend on the process parameters such as thickness, contents, deposition rate, substrates, etc. In this study, NiFe films with a thickness of about 150nm were deposited on Si(100) wafer and $SiO_2$/Si(100) substrate at room temperature by a DC magnetron co-sputtering using Fe and Ni targets. Their phase formation and magnetic properties as a function of annealing temperature were investigated with XRD, FE-SEM and VSM. The assputtered films have BCC structure. With increasing annealing temperature, NiFe thin film for $SiO_2$/Si(100) substrate transformed completely from BCC to FCC phase above $500^{\circ}C$, but some BCC phase remained above $500^{\circ}C$ on Si(100) wafer. For samples annealed at $450^{\circ}C$, squareness ratio of NiFe thin film shows peak value and its saturation magnetization is around 0.0118 emu, which means that the optimum annealing temperature of NiFe thin film seems to be $450^{\circ}C$. The saturation magnetization of films decreased rapidly above the annealing temperature of $500^{\circ}C$ due to phase transformation from BCC to FCC phase.

Synthesis of Nanoscale Sn-Pb Alloy Powders by Electrical Explosion of Wire (전기선폭발법을 이용한 Sn-Pb 나노분말의 합성)

  • ;;;;A. P. Ilyin;D. V. Tichonov
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2003.04a
    • /
    • pp.35-35
    • /
    • 2003
  • )를 금속와이어에 인가하면 저항발열에 의해 와이어가 미세한 입자나 금속증기상태로 폭발하는 현상을 이용한 것으로 기상합성법에 속한다고 할 수 있다. 선폭법은 다른 제조법에 비해 공정이 간단하여 생산비용이 저렴하며, 원재료의 조성을 갖는 분말의 합성과 금속간화합물, 융점차이가 나는 재료의 합금화 등이 가능하다. 인가에너지의 크기와 폭발 시 분위기를 제어함으로써 분말의 평균크기와 분포 제어 또한 가능하다. 본 연구는 러시아의 우수한 기초기술을 바탕으로 Pb-Sn계 합금은 전기폭발법으로 극미세분말을 제조하였으며, 분말의 형상, 상 화학조성의 변화를 조사하였다. 본 실험에 사용된 Sn-Pb계(All-Union State Standard 1499-70, 0.53mm)합금와이어는 자동시스템(1-0.6Hz)에 의해 챔버안으로 공급되었다. 이 때 임계폭발 와이어 길이는 50-80nm으로 실험을 행하였다. 챔버 압력은 1.4~2.0atm으로 유지하였다. 제조된 분말의 특성은 XRD, XRPES, SEM등을 이용하여 분말의 형상과 상, 화학조성, 표면분석을 행하였으며 DSC, TGA, BET분석을 통하여 온도변화에 따른 금속분말의 열량변화, 질량변화, 비표면적을 측정하였다. 제조된 Sn-Pb계 분말은 모두 평균 입도 117nm~220nm의 구형형상이었다. 이때 합금분말의 조성은 51.17~63.21 at%Sn, 35.47~46.37 at%Pb로 나타났다. 와이어에 인가되는 비에너지(W/Wc)가 감소된에 EK라 표면층의 Pb함량이 증가함을 보였다. 이는 와이어 내부 저항의 감소로 인한 공정시간의 지연과 Sn, Pb의 확산계수 차이에 의한 것으로 사료된다. 열분석 결과, Sn~Pb계 화합물의 융점은 167~$169^{\circ}C$로 관찰되었으며, $10^{\circ}C$/min로 $920^{\circ}C$까지 승은 하였을 때 17.1~18 wt%의 질량증가를 보였다.TEX>계 나노복합분말이 얻어짐을 알 수 있었다. 이 때 X션 회절피크의 line broadening으로부터 복합분말의 Fe 명균 결정립 크기는 24nm로 초미세 결정럽의 분말합금이었다. 포화자화값은 볼밀처리에 따라 점점 증가하여 MA 30시간에는 20.3emu/g로 포화됨을 알 수 있었다. 또한 보자력 Hc는 MA초기단계에 350e로 매우 낮으나 30시간 후에는 Hc값이 2600e로 매우 큰 값을 나타내었다. 이것은 환원반응결과 초기에 생성된 Fe의 결정립이 비교적 크고 결정결함이 적으나 볼밀처리를 30시간까지 행하면 Fe 결정렵의 미세화 빛 strain 증가로 magnetic hardening이 일어나기 때문인 것으로 사료된다.길이가 50, 30cm인 압출재를 제조하였다. 열간압출한 후의 미세조직을 광학현미경으로 압출방향에 평행한 방향과 수직방향으로 관찰하였고, 열간 압출재 이방성을 검토하기 위하여 X선 회절분석을 실실하여 결정방위를 확인하였다. 전기 비저항 및 Seebeck 계수 측정을 위하여 각각 2$\times$2$\times$10$mm^3$ 그리고 5$\times$5$\times$10TEX>$mm^3$ 크기의 시편을 준비하였다.준비하였다.전류를 구성하는 주요 입자의 에너지 영역(75~l13keV)에서 가장 높은(0.80) 상관계수를 기록했다. 넷째, 회복기 중에 일어나는 입자들의 유입은 자기폭풍의 지속시간을 연장시키는 경향을 보이며 큰 자기폭풍일수록 현저했다. 주상에서 관측된 이러한 특성은 서브스톰 확장기 활동이 자기폭풍의 발달과 밀접한 관계가 있음을 시사한다.se that were all low in two aspects, named "the Nonsignificant group". And the issues were high risk perception in general setting and lo

  • PDF

Synthesis and Magnetic Characterization of Fe-nitride for Magnetic Recording (기록매체용 Iron-nitride의 합성 및 자기특성)

  • O, Yeong-U;Kim, Mun-Seop
    • Journal of the Korean Magnetics Society
    • /
    • v.2 no.3
    • /
    • pp.244-250
    • /
    • 1992
  • Iron nitride $Fe_4N$ by partial substitution of nitrogen by carbon was prepared by nitriding the iron oxalate whose thermal decomposition gives a carburating atmosphere. Iron oxalates, the precursors, were prepared by precipitation and co-precipitation. The size and shape of the carbonitride particles could be controlled by modifying the conditions of preparation of the oxalate precursor. From the results of electron micrographs, it is clear that the $Fe_4N$ pigment particle maintains the original shape(needle shape) of the starting materials and that it consists of fine unit particles which link together to form a stereo-network structure. An investigation of the $Fe^{II}_3\;Fe^I_{1-x}\;Sn_xN_{1-y}C_y$ solid solution has shown that Sn plays the role of a growth inhibitor of the elementary microcrystallites of the iron carbonitride. The coercive force and saturation magnetization of iron carbonitride obtained from co-precipitated iron oxalate were 500 Oe and 120 emu/g, respectively.

  • PDF

The Magnetic Properties of Fe-Hf-C Soft Magnetic Thin Films (Fe-Hf-C계 연자성 박막합금의 자기적 성질)

  • 최정옥;이정중;한석희;김희중;강일구
    • Journal of the Korean Magnetics Society
    • /
    • v.3 no.1
    • /
    • pp.23-28
    • /
    • 1993
  • Thin films of soft magnetic Fe-Hf-C alloys with nanoscale crystallites were investigated in this study. The films were fabricated by an RF diode magnetron sputtering apparatus and subsequently annealed in vacuum. The soft magnetic properties of the films were observed to differ depending on the different substrates such as Corning 7059, $CaTiO_3$ and $Al_2O_3-TiC$ with various underlayer(Cr, $SiO_2$) thickness. This results may be due to the interdiffusion between the substrate and the magnetic layer and/or between the underlayer and the magnetic layer, rather than the microstructural change such as grain size. The Fe-Hf-C films with high permeability up to 4000(at 1 MHz) and saturation magnetization up to 16 kG were obtained in the vicinity of phase boundary between the crystalline and amorphous state when the size of ${\alpha}-Fe$ grains is about 5 nm. And also the films were found to have thermal stability up to $600^{\circ}C$.

  • PDF

Numerical Analysis of Magnetic Flux Leakage Inspection (누설자속탐상의 수치해석)

  • Lee, Hyang-Beom;Kim, Sean
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.21 no.5
    • /
    • pp.485-492
    • /
    • 2001
  • In this paper, electro-magnetic numerical analysis of MFL(magnetic flux leakage) method is presented. For the electromagnetic numerical analysis, 2-D FEM(finite element method) is used. The magnetic vector potential is used as a variable. The analysis of the magnetic field considering the magnetic nonlinearity is performed for the effect of the magnetic salutation. For the verification of the validity of the numerical simulation results, by using the lab-made experimental setup, non-destructive inspection is performed. The SM 45C carbon steel is used as a specimen and the artificial defects are made on the specimen. The non-destructive testing for the detection of the defect is performed. The results according to the variation oi the defect depth and the defect shape are obtained. The experimental results are compared to the numerical ones, and we conclude that the numerical results are similar to the experimental ones. So the possibility of simulation of the MFL by using the numerical analysis is shown in this paper.

  • PDF

Influences of Oxygen Partial Pressure and Annealing Time on Microstructure and Magnetic Properties of Hexagonal Barium-Ferrite Thin Films (Hexagonal Barium-Ferrite 박막의 미세구조와 자기적 특성에 미치는 산소분압과 열처리 시간의 영향)

  • 김웅수;김동현;남인탁;홍양기
    • Journal of the Korean Magnetics Society
    • /
    • v.10 no.6
    • /
    • pp.285-290
    • /
    • 2000
  • BaM thin films were prepared by using RF magnetron sputtering system at room temperature, and then successively annealed to crystallize at 850$\^{C}$ using RTA. The structure and magnetic properties of post-annealed BaM films have been investigated using XRD and VSM, respectively. The dependences of partial oxygen gas pressure (Po2) on the characteristics of BaM films were investigated. Although mixing of spinel and BaM phase only was identified in 0.5 mTorr oxygen partial pressure, BaM phase only was identified in the range from 1 to 3 mTorr oxygen partial pressure. The saturation magnetization and perpendicular coercivity of BaM thin films decreases with increase of Po2 in the range of Pot between 0.5 and 3 mTorr.

  • PDF

Effects of Seed Layers on Formation of Barium Ferrite Thin Films and Their Magnetic Properties (씨앗층이 바륨훼라이트 박막의 형성과 자기적 성질에 미치는 영향)

  • 나종갑;이택동;박순자
    • Journal of the Korean Magnetics Society
    • /
    • v.2 no.1
    • /
    • pp.22-28
    • /
    • 1992
  • Barium ferrite thin films were reactively deposited with Fe and BaO composite targets by a facing tergects sputtering unit. When thermally oxidized silicon wafers were used as substrates, minimum substrate heating of $750^{\circ}C$ was necessary for the perfect c-axis alignment in barium ferrite films. To lower the critical substrate temperature for the good c-axis alignment, such seed layers as ZnO, ${\alpha}-Fe_{2}O_{3}$ and ${\gamma}-Fe_{2}O_{3}$ were tested. The excellent c-axis algnment of BaM was obtained at a substrate temperature of $600^{\circ}C$ on ZnO seed layer whose (002) plane was parallel to the substrate surface. The magnetic properties of the BaM film showed saturation magnetization of 295 emu/cc, perpendicular coercivity of 1.7 kOe and squareness of 0.75. Optimum deposition rate of $230\;{\AA}/min$ was obtained with the composite target and this was 5 to 20 times higher than those of other investigators with oxide targets.

  • PDF

A First-principles Study on the Electronic Structures and Magnetism of Antiperovskite Ti0.96Co0.02Fe0.02O2 (페로브스카이트 구조를 가지는 Ti0.96Co0.02Fe0.02O2의 전자구조와 자성)

  • Song, Ki-Myung;Bialek, B.;Lee, Jae-Il
    • Journal of the Korean Magnetics Society
    • /
    • v.18 no.3
    • /
    • pp.85-88
    • /
    • 2008
  • We calculated the electronic structures of substituted cobalt nitrides, that is $FeCo_3N$ and $NiCo_3Ni$, by using the all electron fullpotential linearized augmented plane-wave (FLAPW) energy band method, and investigated the influence on the magnetic properties of $Co_4N$ due to the substitution of Co atom located at corner sites by iron and nickel atoms. We found that the magnetic moments of CoII atoms located at the face-center positions in these compounds are almost same to that of $Co_4N$. The magnetic moments of Fe and Ni atoms in $FeCo_3N$ and $NiCo_3Ni$ are 3.086 and $0.795\;{\mu}_B$, and they have the localized nature of magnetism.

Bias Field Effect of SmCo Films on Soft Magnetic Properties of CoZrNb Films (SmCo박막의 바이어스자계가 CoZrNb박막의 연자성특성에 미치는 효과)

  • Shin, K.H.;Kim, Y.H.
    • Journal of the Korean Magnetics Society
    • /
    • v.13 no.5
    • /
    • pp.198-203
    • /
    • 2003
  • To investigate whether the use of hard magnetic film is available to generate bias magnetic field for a magnetoimpedance sensor, the magnetic properties of SmCo hard magnetic films were investigated as a function of their compositions. The saturation magnetization decreased with Sm content increasing in SmCo films. And, the coercive force increased in the extent of Sm content of 28 at%, but decreased as Sm content increased moreover. The bias field effect of SmCo film to amorphous CoZrNb film was investigated with the magnetization corves, permeabilities, and magnetic domain structures of SmCo/CoZrNb multilayers. The bias field of about 60 Oe was observed in the film with 3 mm ${\times}$ 0.5 mm, which can be constructed as a MI sensor, and this result strongly indicates that the bias field generated from a hard magnetic film is adequate to enhance the sensitivity of a MI sensor with hard/soft magnetic multilayer structure.