One of the most vulnerable properties in concrete is tensile cracking, which usually happens at early ages due to hydration heat and shrinkage. In order to accurately predict the early age cracking, it needs to find out how stress-crack opening relation is varying over time. In this study, inverse analyses were performed with the existing experimental data for wedge-splitting tests, and the parameters of the softening curve for the stress-crack opening relation were determined from the best fits of the measured load-CMOD curves. Based on the optimized softening curve, variation of fracture energy over time was first examined, and a model for the stress-crack opening relation at early ages was suggested considering the found feature of the fracture energy. The model was verified by comparisons of the peak loads, CMODs at peak loads, and fracture energies obtained from the experiments and the inverse analysis.
Journal of the Korea institute for structural maintenance and inspection
/
v.17
no.1
/
pp.46-54
/
2013
Two different UHPCCs having different fiber lengths and volume fractions are considered to be applied to bridge decks. The objective of this study is to estimate cracking resistance of the two UHPCCs. The notched beam tests were performed with the UHPCCs, and the relationships between load and CMOD(Crack Mouth Opening Displacement) were obtained from the tests. The tensile stress and crack opening relationships optimally fitting the measured load-CMOD curves were found through the inverse analyses. The UHPCC with 2% volume fraction of 13 mm long fiber has lower fracture energy than the UHPCC with 0.5% and 1.0% volume fractions of 16.3 mm and 19.5 mm long fibers, respectively. It indicates that the latter UHPCC is more effective in uniformly distributing crack formation and reducing crack width.
Transactions of the Korean Society of Mechanical Engineers
/
v.14
no.6
/
pp.1568-1575
/
1990
Fatigue crack growth behavior was investigated in the center cracked plate of KS SB41 steel and the relation between the crack growth rate and various mechanical parameters was studied at small scale yielding, large scale yielding and full scale yielding. The crack opening ratio U was about 0.6-0.8 and had the larger value in the case of load control than that of strain control. Effective stress intensity factor range, .DELTA.K$_{eff}$ and J integral range, .DELTA.J were obtained from the notion of crack opening, and the crack growth rate was expressed with these values. The value of J integral range increased rapidly at stress ratio, R=0 in full scale yielding of load control test. COD value also increased rapidly with the increase of ligament net stress at large scale yielding of load control test.t.
Journal of the Society of Naval Architects of Korea
/
v.39
no.2
/
pp.61-68
/
2002
From the viewpoint of linear fracture mechanics, the crack propagation behavior of two different structures having the same K-a relationship could be considered identical. In this study the stress distribution in an infinitely wide cracked plate with the same K-a relationship as in a real structure is defined as the equivalent stress distribution. Fatigue life of a real structural element can be predicted by applying the equivalent stress distribution to a simple structural element, and performing a fatigue crack propagation analysis. The K-a relationship for a structural member can be estimated by a finite element method or a simplified prediction method. The validity to obtain effective crack driving stresses by using the equivalent stress-distribution is examined.
콘크리트에 선형파괴역할의 적용가능성을 연구한 많은 논문이 발표되었다. 본 논문에서는 CLWL-DCB식편을 이용한 콘크리트의 개구형파괴를 연구하였다. 표면구열길이는 리프리카를 사용하여 직접적인 방법으로 측정하였고, 이 결과은 실험에서 얻은 측정가중과 구열개구변위의 관계곡선을 이용하여 분석하였다. 감계응력강도계수와 감계구열선단위는 Two Parameter 모델을 사용하여 유효구열선단에서 구하였다. LEFM 구열단면과 실험으로 구한 구열단면으로부터 폐쇄압력을 얻기 위하여 중첩법을 적용하여 5종의 균열모델을 평가하였다.
Kim, Yun-Yong;Lee, Bang-Yeon;Kwon, Seung-Hee;Kim, Jeong-Su
Proceedings of the Korea Concrete Institute Conference
/
2008.04a
/
pp.917-920
/
2008
ECC is a special kind of high performance cementititous composite which exhibits typically more than 2% tensile strain capacity by bridging microcracks at a crack section. Therefore, micromechanics should be adopted to obtain multiple cracking and strain hardening behavior. This paper propose a linear elastic analysis method to simulate the multiple cracking and strain hardening behavior of ECC. In an analysis, the stress-crack opening relation modified considering the orientation of fibers and the number of effective fibers is adopted. Furthermore, to account for uncertainty of materials and interface between materials, the randomness is assigned to the tensile strength(${\sigma}_{fci}$), elastic modulus($E_{ci}$), peak bridging stress(${\sigma}_{Bi}$) and crack opening at peak bridging stress(${\delta}_{Bi}$), initial stress at a crack section due to chemical bonding, (${\sigma}_{0i}$), and crack spacing(${\alpha}_cX_d$). Test results shows the number of cracking and stiffness of cracked section are important parameters and strain hardening behavior and maximum strain capacity can be simulated using the proposed method.
스테인레스강의 주요성능은 내식성이기 때문에 부식성의 환경에서 사용되는 일이 많다. 이 때문 에 스테인레스 강제강치에서는 부식에 관계되는 사고가 대단히 많다. 그림1(a)은 일본화학공학협 회가 1987년부터 1982년사이에 화학장치에 발생한 615건의 손상을 종류별로 분류한 것이다. 전면 부식, 공식, 동력부식균열등의 습성환경에서의 전기화학적 부식이 전체의 54%나 점하고 있 다. 이들 손상에 재료별로 보면 그림1(b)와 같이 스테인레스강이 차지하는 비율이 총 1/4에 달하 고 있다. 또한, 별도조사결과에 의하면 각종손상이 용접이음부에서 약 50% 발생하고 있어, 용접 이음부가 부식성환경에서 사용되는 경우에는 이를 부식현상과 그 방지대책을 세우지 않으면 안된다. 용접부에서 이들 부식현상이 발생하기 쉬운 것은 다음과 같은 요인으로 생각된다. (1) 용접내부는 모재와는 다른 금속조직을 가진다. (2) 용접잔류응력이 존재한다. (3) 용접결함이나 이음형식에 의한 형상불연속 놋치화하여 응력집중을 가져온다. 또한 이들이 표 면에 개구한 극간부식을 가질때에는 극간부식의 요인이 된다. 본고에서는 이들 부식현상중 가장 중요한 오-스테이나트계스테인레스강 용접부에서의 응력부식균열 현상에 대하여 설명한다.
Proceedings of the Korea Concrete Institute Conference
/
2008.04a
/
pp.433-436
/
2008
In order to estimate the mechanical properties of ultra high performance concrete, the most important is to evaluate its tensile behavior. The tensile behavior of concrete is generally characterized by the elastic behaviour before cracking and tensile stress-crack width relationship after cracking. We carried out the direct tensile and flexural tensile test and compared the tensile behaviors obtained by the direct tensile test and by inverse analysis of the flexural tensile test results. We compared the obtained tensile behavior with that of JSCE recommendations for ultra high performance concrete as well. we could see that the tensile stress-crack width relationship obtained from the flexural tensile test results using inverse analysis had good agreement with directly obtained tensile behaviour with direct tensile test and showed similar tensile softening behaviour introduced in JSCE recommendations for ultra high performance concrete.
In this study, the wedge splitting tcst (WST) was carried out for the fatigue wack growth behavior of concrete. Selected test variables were concrete compressive strength of 28, 60 and 118 MI%, and stress ratio with 2 levels (6. 13%). In oder to make the designed stress ratio, the maximum and thr minimum fatigue loading level were 75-85% and 5- 10% of ultimate static load, respectively. Fatigue testing was preceded by crack mout.h opening displacement (CMOI)) compliance calibration tcst, and then the fatigue crack growth was computed by crack lcngth vs. (lMOI) compliance relations acquisited by the CMOD compliance calibration technique. To evaluate thc validity of CMOD compliancc calibration techniquc, the crack length p~mlicted by this method was cornpard with the crack length by linear elastic fracture mechanics(LEFIbl) and dyeing test. On the basis of the experimental results, a LRFhl-based c.mpirica1 model for f'at,igue crack growth rate(da/dN-AKI relationships) was presented. The fat,igut. crack growth ratc increased with the strength of concwtc. It appcars that t.he da/tiN-AKI relationships was influenced by stress ratio, however, the effect is diminished with an increase of strength. The comparisons between CblOl) compliance calibration technique anti the other. methods gave the validity of' ('MOD compliance calibration technique for the LZXT.
콘크리트는 여러 구성 성분들이 불규칙적인 배열을 이루어 형성된 복합재료이지만, 과거에는 이 재료를 하나의 단종재료로 간주하여 해석하였기 때문에, LEFM에서 사용되는 파괴인성계수만으로는 콘크리트의 파괴역학적 접근이 어렵다는 것 이외에는 파괴인성계수들의 크기의존성에 대한 이유라든가, 실험을 통해서 관측된 구조물 두께 방향으로의 서로 다른 깊이의 균열 진행 현상에 대해서는 설명하기가 어려웠다. 따라서 본 연구는 콘크리트를 하나의 복합재료로써 각각의 구성요소들이 차지하고 있는 체적비 및 배열상의 효과를 고려하여 복합재료의 파괴거동을 해석하고, 구성재료의 수와 파괴인성계수와의 상관관계를 분석하였다. 각각의 구성요소들을 연립변형모드( SD mode)로 배열시킨 조건에서 복합재료역학개념에 입각하여 해석한 결과, 일반적으로 실험이나 비선형파괴역학 해석과 같이 하중-변위곡선 상단부에서 비선형 거동이 관측되었다. 또한 임계응력확대계수( $K_IC$)나 파괴에너지($G_r$)는 구성원의 수나 보의 크기에 대해서 거의 무관한 값을 나타내지만, 임계군열선단개구변위 ($CTOD_c$)는 크기에 영향을 받음을 보여 주었다. 균열의 진행속도는 균열이 진행될수록 감소하며, 파괴인성이 작은 구성원에서부터 균열이 발생되어 결과적으로 보의 두께 방향으로 서로 다른 크기의 균열길이가 생성됨이 관측되었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.