질소와 진공 분위기에서 에이징 영향에 따른 불화유기박막의 나노트라이볼러지 특성 평가 (Nanotribological Characterization of Annealed Fluorocarbon Thin Film in N2 and Vacuum)

  • 김태곤;김남균;박진구;신형재
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2002년도 춘계 기술심포지움 논문집
    • /
    • pp.193-197
    • /
    • 2002
  • The tribological properties and van der Waals attractive forces and the thermal stability of films are very important characteristics of highly hydrophobic fluorocarbon (FC) films for the long-term reliability of nano system. The effect of thermal annealing on films and van der Waals attractive forces and friction coefficient of films have been investigate d in this study. It was coated Al wafer which was treated O2 and Ar that ocatfluorocyclobutane ($C_4_{8}$) and Ar were supplied to the CVD chamber in the ratio of 2:3 for deposition of FC Films. Static contact angle and dynamic contact angle were used to characterize FC films. Thickness of films was measured by variable angle spectroscopy ellipsometer (VASE). Nanotribological data was got by atomic force microscopy (AFM) to measure roughness, lateral force microscopy (LFM) to measure friction force, and force vs. distance (FD) curve to evaluate adhesion force. FC films were cured in N2 and vacuum. The film showed the slight changes in its properties after 3 hr annealing. FTIR ATR studies showed the decrease of C-F peak intensity in the spectra as the annealing time increased. A significant decrease of film thickness has been observed. The friction force of Al surface was at least thirty times higher than ones with FC films. The adhesive force of bare Al was greater than 100 nN. After deposit FC films adhesive force was decreased to 40 nN. The adhesive force of films was decreased down to 10 nN after 24 hr annealing. During 24 hr annealing in $N_2$and vacuum at $100^{\circ}C$ film properties were not changed so much.

  • PDF

레이저 유기 충격파를 이용한 나노 Trench 에서의 나노입자제거

  • 김진수;이승호;박진구
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 춘계학술발표대회
    • /
    • pp.25.1-25.1
    • /
    • 2009
  • Pattern 웨이퍼 상의 오염입자 제거는 반도체 산업의 주된 과제 중 하나이다. Pattern의 선폭이 좁아짐에 따라 Pattern에 손상을 가하지 않고 오염입자를 제거 하는 것은 더욱 어려워지고 있다. 그뿐만 아니라 기존 습식세정 공정에서의 화학액에 의한 환경오염 및 박막의 손실도 문제가 되기 시작했다. 이러한 문제를 해결하기 위해 기존 세정공정에서 화학액의 농도를 낮추고 Megasonic 등을 이용하여 세정력을 보완하는 방법들이 연구되고 있다. 하지만 습식세정의 경우 강한 화학작용으로 인한 표면 손상 및 물 반점의 문제는 여전히 이슈가 되고 있다. 이러한 단점을 극복하기 위하여 건식 세정법이 제시되고 있으며 이 중 레이저 충격파는 레이저를 집속시켜 발생된 충격파를 이용하여 입자를 제거하기 때문에 국부적인 세정이 가능하며 세정력 조절이 가능하여 손상이 세정을 할 수 있다. 그러나 Pattern의 구조에 의해 전되는 세정력의 차이가 발생하고 Trench 내부의 오염입자제거 문제점이 발생할 수 있다. 시편은 Si STI Pattern을 100 nm PSL Particle (Red Fluorescence, Duke Scientific, USA) 을 50ppm 농도로 희석시킨 IPA에 dipping 하여 오염시킨 후 N2 Gas를 이용하여 건조하여 준비하였다. 그리고 레이저 충격파 세정 시스템은 최대 에너지 1.8 J까지 가능한 레이저를 발생하는 1,064 nm Nd:YAG 레이저를 이용하여 실험하였다. 레이져 충격파 실험은 충격파와 시편사이의 거리, gap distance와 에너지를 변환하여 세정효율을 관찰하였다. 세정효율은 세정 전후의 입자 감소량을 현광현미경 (LV-150, Nikon, Japan)를 이용하여 측정하였다. 그 결과, Trench 내부의 오염입자의 경우 Trench 밖의 오염입자에 비해 세정효율이 떨어지는 것으로 나타났으나 시편과 레이저 초점과의 거리가 가까워짐에 따라 Trench 내부의 오염입자에 대한 세정 효율을 증가시킬 수 있었다.

  • PDF

TCP-CVD법을 활용한 공정변수에 따른 산화막의 제작 (Fabrication of Oxidative Thin Film with Process Conditions by Transformer Coupled Plasma Chemical Vapor Deposition)

  • 김창조;최윤;신백균;박구범;신현용;이붕주
    • 한국진공학회지
    • /
    • 제19권2호
    • /
    • pp.148-154
    • /
    • 2010
  • 본 논문에서는 유기발광다이오드의 보호막 적용을 위하여 TCP-CVD를 이용한 실리콘 산화막 형성에서 산화막의 특성에 영향을 미치는 Power, 가스종류 및 유량, 소스와 기판거리 및 공정온도 등의 공정조건에 따른 증착된 산화막의 특성을 나타내는 증착률, 굴절률을 제어하고자 한다. 그 결과 $SiH_4$ : $O_2$ = 30 : 60 [sccm], 70 [mm]의 source와 기판 거리, Bias를 인가하지 않은 조건에서 80 [$^{\circ}C$] 이하의 공정온도를 보였으며 투과율 90% 이상, 높은 증착률 및 굴절률 1.4~1.5인 안정된 $SiO_2$ 산화박막을 제조할 수 있었다.

PECCP LB 박막을 발광층으로 사용한 유기 발광 다이오드의 특성 (Characteristics of Organic Light-Emitting Diodes using PECCP Langmuir-Blodgett(LB) Film as an Emissive Layer)

  • Lee, Ho-Sik;Lee, Won-Jae;Park, Jong-Wook;Kim, Tae-Wan;Dou--Yol Kang
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 추계학술대회 논문집
    • /
    • pp.111-114
    • /
    • 1999
  • Electroluminescence(EL) devices based on organic thin films have been attracted lots of interests in large-area light-emitting display. In this stuffy, an emissive layer was fabricated using Langmuir-Blodgett(LB) technique in organic light-emitting (OLEDs). This emissive organic material was synthesized and named PECCP[poly(3.6-N-2-ethylhexyl carbazolyl cyanoterephthalidene)] which has a strong electron donor group and an electron acceptor group in main chain repeated unit. This material has good solubility in common organic solvents such as chloroform. THF, etc, and has a good stability in air. The Langmuir-Blodgett(LB) technique has the advantage of precise control of the thickness down to the molecular scale, In particular, by varying the film thickness it is possible to investigate the metal/polymer interface. Optimum conditions for the LB film deposition are usually determined by investigating a relationship between a surface pressure $\pi$ and an effective are A occupied by one molecule on the subphase. The LB films were deposited on an indium-tin-oxide(ITO) glass at a surface pressure of 10 mN/m and dipping speed of 12 mm/min after spreading PECCP solution on distilled water surphase at room temperature, Cell structure was ITO/PECCP LB film/Alq$_3$/Al. We considered PECCP as a hole -transport layer inserted between the emissive layer and ITO. We also used Alq$_3$ as an emissive layer and an electron transport layer. We measured current-voltage(I-V) characteristics, UV/visible absorption, PL spectrum and EL spectrum of the OLEDs.

  • PDF

PC 기판위에 성막한 IZO/Ag/IZO 박막의 특성과 이를 이용하여 제작한 플렉시블 유기발광다이오드의 특성 분석 (Characteristics of flexible IZO/Ag/IZO anode on PC substrate for flexible organic light emitting diodes)

  • 조성우;정진아;배정혁;문종민;최광혁;김한기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.381-382
    • /
    • 2007
  • IZO/Ag/IZO (IAI) anode films for flexible organic light emitting diodes (OLEDs) were grown on PC (polycarbonate) substrate using DC sputter (IZO) and thermal evaporator (Ag) systems as a function of Ag thickness. To investigate electrical and optical properties of IAI stacked films, 4-point probe and UV/Vis spectrometer were used, respectively. From a IAI stacked film with 12nm-thick Ag, sheet resistance of $6.9\;{\Omega}/{\square}$ and transmittance of above 82 % at a range of 500-550 nm wavelength were obtained. In addition, structural and surface properties of IAI stacked films were analyzed by XRD (X-ray diffraction) and SEM (scanning electron microscopy), respectively. Moreover, IAI stacked films showed dramatically improved mechanical properties when subjected to bending both as a function of number of cycles to a fixed radius. Finally, OLEDs fabricated on both flexible IAI stacked anode and conventional ITO/Glass were fabricated and, J-V-L characteristics of those OLEDs were compared by Keithley 2400.

  • PDF

알킬기의 길이에 따른 지방산계 유기초박막의 유전 및 전기적 특성 비교 (Comparison to Dielectric and Electrical Characteristics of Fatty Acid Organic Thin Film for Length of Alkyl Group)

  • 강기호;이준호;김도균;권영수;장정수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 추계학술대회 논문집
    • /
    • pp.343-346
    • /
    • 1999
  • We have investigated the dielectric and electrical characteristics of palrnitic acid(PA), stearic acid(SA) and arachidic acid(AA) Langmuir-Blodgett(LB) films because these fatty acid systems have a same hydrophilic group and a different hydrophobic one(alky1 chain lqngth). The dielectric characteristics such as the capacitance-frequency(C-F) characteristics and the dielectric dispersion and absorption characteristics of PA, SA and AA through-plane were measured. In the result, the relative dielectric constants of PA, SA and AA LB films were about 3.0-4.6, 2.7-4.1 and 2.4-3.8, respectively. The relative dielectric constants were decreased in proportion to the chain length of alkyl group. Also, the dielectric dispersion and absorption of each fatty acid LB films have arisen from the dipole polarization in the range of $10^4~10^5[Hz]. And, the conductivity of PA, SA and AA LB films obtained from I-V characteristics were about $9{\times}10^{-14}, 3{\times}10^{-l4} and 5{\times}10^{-15}[S/cm], respectively. These results have shown the insulating materials and could control the conductivity by changing the length of alkyl group. Also, we have confirmed that the barrier height of fatty acid systems were about 1.32-1.40[eV] and the dielectric constant were about 3.0-4.2. These values were almost the same ones obtained from dielectric characteristics.

  • PDF

유/무기 복합 박막을 이용한 유기발광 소자의 보호층에 관한 연구 (Study on the Hybrid Passivation layer of OLEDs using the Organic/Inorganic Thin Film)

  • 배성진;이주원;이영훈;강남수;김동영;황성우;김재경;주병권
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 학술대회 및 기술세미나 논문집 디스플레이 광소자
    • /
    • pp.78-80
    • /
    • 2006
  • The hybrid thin-film (HTF) passivation layer composed of the Ultra Violet (UV) curable acrylate layer and MS-31 (MgO:$SiO_2$=3:1wt%) layer was adopted in organic light emitting device (OLEO) to protect organic light emitting materials from penetrations of oxygen and water vapors. The results showed that the HTF layer possessed a very low WVTR value of lower than $0.007gm/m^{2+}day$ at $37.8^{\circ}C$ and 100% RH. This value was within the limited range of the sensitivity of WVTR measurements. And the lifetime of the HTF passivated device became almost three times longer than that of the bare device. The HTF on the OLEO was found to be very effective in protect what from the penetrations of oxygen and moisture.

  • PDF

고분자 기판위에 유기 용매를 사용하지 않은 다층 박막 Encapsulation 기술 개발 (Improvement of Permeation of Solvent-free Multi-Layer Encapsulation of thin films on Ethylene Terephthalate(PET))

  • 강희진;한진우;김종연;문현찬;최성호;박광범;김태하;김휘운;서대식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 학술대회 및 기술세미나 논문집 디스플레이 광소자
    • /
    • pp.56-57
    • /
    • 2006
  • In this paper, the inorganic multi-layer thin film encapsulation was newly adopted to protect the organic layer from moisture and oxygen. Using the electron beam, Sputter, inorganic multi-layer thin-film encapsulation was deposited onto the Ethylene Terephthalate(PET) and their interface properties between inorganic and organic layer were investigated. In this investigation, the SiON SiO2 and parylene layer showed the most suitable properties. Under these conditions, the WVTR for PET can be reduced from a level of $0.57\;g/m^2/day$ (bare subtrate) to 1*10-5 g/$m^2$/day after application of a SiON and SiO2 layer. These results indicates that the PET/SiO2/SiON/Parylene barrier coatings have high potential for flexible organic light-emitting diode(OLED) applications.

  • PDF

P3HT(poly-3-hexylthiophene)를 이용한 고분자 유기 TFT 제작을 위한 Ink-jet printing 기술 응용 (Application of Ink-jet Printing Technology for Fabrication of Polymer Organic TFT using P3HT(poly-3-hexylthiophene))

  • 김준영;송대호;이용균;박태진;권순갑;강문효;이선희;한승훈;조상미;김준희;장진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 춘계학술대회 논문집 디스플레이 광소자 분야
    • /
    • pp.84-87
    • /
    • 2005
  • 본 논문에서는 p-type 고분자 물질인 P3HT (Poly-3-hexylthiophene)를 잉크젯 프린팅 방식으로 활성화층을 적층함으로써 Organic thin film transistor를 제작하여 이에 대한 특성을 연구하였다. Piezoelectric 방식의 잉크젯 프린팅을 이용하여 P3HT single drop jetting 시 두께 $150{\sim}200{\AA}$, 직경 약 70 ~ 80 um정도의 drop profile을 얻을 수 있었다. P3HT의 solvent로서 Chlorobenzene을 사용하여 농도 약 0.5 wt.%의 Ink-jet용 ink를 제작하여 이를 Channel Width 37, 236 um 크기의 Au 전극 위에 jetting 하여 각각의 특성을 측정하였다. 상기 실험은 상온의 외부환경에서 실시되었으며 실험 결과 최대 ${\mu}=1{\times}10^{-2}\;cm^2/Vsec$, $I_{on}/I_{off}=10^3{\sim}10^4$ 정도로서 off current가 높은 편이나 이동도 측면에서는 다른 방법의 박막 증착 실험결과와 비교할 때 동등 수준의 결과를 얻을 수 있었다.

  • PDF

유기 발광소자의 효율 향상을 위한 광학박막 및 마이크로렌즈 설계 (Optical Thin Film and Micro Lens Design for Efficiency Improvement of Organic Light Emitting Diode)

  • 기현철;김두근;김선훈;김상기;박아름;구할본
    • 한국전기전자재료학회논문지
    • /
    • 제24권10호
    • /
    • pp.817-821
    • /
    • 2011
  • We have proposed an optical thin film and micro lens to improve the luminance of organic light emitting device. The first method, optical thin film was calculated refractive index of dielectric layer material that was modulated refractive index of organic material, ITO (indium tin oxide)and glass. The second method, microlens was applied with lenses on the organic device. Optical thin films were designed with Macleod Simulator and Micro Lenses were calculated by FDTD (finite-difference time-domain) solution. The structure of thin film was designed in organic material/ITO/dielectric layer/glass. The lenses size, height and distance were 5 ${\mu}m$, 1 ${\mu}m$, 1 ${\mu}m$, respectively. The material of micro lenses used silicon dioxide. Result, The highest luminance of OLED which applied with microlens was 11,185 $cd/m^2$, when approval voltage was 14.5 V, applied thin film was 5,857 $cd/m^2$. The device efficiency applying microlens increased 3 times than the device which does not apply microlens.