• Title/Summary/Keyword: 열적 산화

Search Result 279, Processing Time 0.039 seconds

Thermal behavior of $PrCl_3$ in an oxidizing condition (산화조건에서 $PrCl_3$의 열적거동)

  • Eun, Hee-Chul;Yang, Hee-Chul;Cho, Yong-Zun;Lee, Han-Soo;Kim, In-Tae
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.7 no.4
    • /
    • pp.207-212
    • /
    • 2009
  • In this study, a thermal behavior of $PrCl_3$ as one of the lanthanide chlorides in LiCl-KCl molten salts was investigated in an oxidizing condition. First, a thermo-gravimetric analysis (TGA) of $PrCl_3$ was carried out by an injection of $O_2$ gas. Based on the results, an oxidation of $PrCl_3$ in the molten salts was performed by sparging $O_2$ gas with changing temperatures. According to the TGA data of $PrCl_3$, a dissociation of $PrCl_3$ occurred rapidly by about $380^{\circ}C$ and a conversion of $PrCl_3$ to $PrCl_3$ was completed at about $600^{\circ}C$. The thermal behavior of $PrCl_3$ in LiCl-KCl molten salts by sparging $O_2$ gas was similar to that of $PrCl_3$ in the TGA test, and PrOCl as a insoluble compound in the molten salts was precipitated into the bottom of the molten salts. A conversion of $PrCl_3$ to PrOCl in the molten salts occurred actively at a higher temperature than $650^{\circ}C$. And it would be possible to estimate a conversion status of $PrCl_3$ to PrOCl by measuring a $Cl_2$ concentration in a flue gas generated from an oxidation test of $PrCl_3$ in LiCl-KCl molten salts.

  • PDF

Rare Earth Oxide Atomic Layer Deposition for Hydrophobic Coating (소수성 코팅을 위한 원자층 증착 희토류 금속산화물)

  • LeeHan, Bo-Ram
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2015.11a
    • /
    • pp.154-154
    • /
    • 2015
  • 소수성 코팅은 광범위하게 응용 가능하다. 희토류 금속 산화물(Rare earth oxides, REO)은 소수성 코팅 물질로써 우수한 열적 기계적 안정성으로 인해 전도유망하다. 본 연구는 원자층 증착법(Atomic layer deposition, ALD)을 이용한 나노 단위 두께의 희토류 금속 산화물 박막을 이용하여 소수성 코팅의 기초 연구이다. 미래 소수성 코팅 물질로써의 응용 가능성을 함께 다룬다.

  • PDF

Memory Characteristics of MNOS Devices (MNOS 소자의 기억특성)

  • 서광열;박영걸;김태만
    • Electrical & Electronic Materials
    • /
    • v.1 no.3
    • /
    • pp.243-250
    • /
    • 1988
  • 530A의 질화막과 23A의 엷은 산화막두께로 제작된 MNOS 소자의 기억트랩분포와 기억특성을 TSC방법과 C-V방법으로 조사하였다. 소자는 전기적으로 기억갱신이 가능하며 무전압유지가 반영구적임을 확인하였다. 기억트랩에 해당하는 TSC곡선을 분석하는데는 공간적, 에너지적인 트랩의 분포모형을 가정하고 best fitting법을 사용하였다. 그 결과 기억트랩은 질화막-산화막 계면에서 질화막안으로 10A 깊이로 분포되었으며 에너지준위는 질화막전도대 하단에서 2.35-2.38eV로 분포되어 있음을 밝혔다. 또한 방전기구는 산화막층을 통한 직접터널링과 열적여기를 함께 고려하여 설명할 수 있었다.

  • PDF

Research of Thermal Properties for Liquid Crystalline Epoxy Composites with Tin Oxide Filler (산화주석을 함유한 열경화성 액정 에폭시의 열적 특성에 관한 연구)

  • Hyun, Ha Nuel;Cho, Seung Hyun
    • Composites Research
    • /
    • v.33 no.1
    • /
    • pp.25-29
    • /
    • 2020
  • A liquid crystalline thermosetting-epoxy-based composite was fabricated using diglycidyl ether of 4,4'-biphenol, tin(IV) oxide as a filler, and sulfanilamide as a curing agent. To investigate the thermal behavior, Thermogravimetric Analysis and Laser Flash Apparatus were performed using 3.0-7.0 wt% Tin(IV) oxide. The result showed that the activation energy and thermal conductivity were proportional to the amount of added filler.

Effects of Oxidation Process on Thermal Properties of Petroleum-based Isotropic Pitch (산화 공정이 석유계 등방성 피치의 열거동 특성에 미치는 영향)

  • Lee, Namji;Seo, Sang Wan;Kwak, Cheol Hwan;Kim, Min Il;Im, Ji Sun
    • Applied Chemistry for Engineering
    • /
    • v.31 no.1
    • /
    • pp.36-42
    • /
    • 2020
  • In order to investigate the effect of the oxidation process on thermal properties of the pitch, the oxidized pitch was prepared by changing the oxidation temperature. Thermal properties of the pitch were analyzed using thermogravimetric analysis (TGA), and it divided into three sections as A (25~100 ℃), B (250~550 ℃) and C (550~800 ℃) by derivative thermogravimetry (DTG) graph behavior. In the A section, the was reduced because the moisture contained in the pitch was removed. In the B section, as the oxidation temperature increased, the thermal stability of the pitch is improved. Because the degree of aromaticity and molecular weight of the pitch increased with increasing oxidation temperature. In contrast, the results of the C section were shown opposite of B section. Because the introduced C-OH, C-O-C, and C=O bonds were decomposed, and the resulting oxygen compounds induced the combustion reaction of the pitch.

Aging of Solid Fuels Composed of Zr and ZrNi Part 1: Thermal/Chemical/Spectroscopic Analysis (Zr과 ZrNi로 구성된 고체연료의 노화 연구 Part 1: 열/화학/분광학적 분석)

  • Han, Byungheon;Ryu, Jihoon;Yang, Junho;Oh, Juyoung;Gnanaprakash, K.;Yoh, Jai-ick
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.24 no.2
    • /
    • pp.1-13
    • /
    • 2020
  • The characterization of aging of the pyrotechnic device is conducted thermally, chemically, and spectroscopically. The device is comprised of two parts: (i) igniter composed of Zr and (ii) pyrotechnic delay composed of ZrNi alloy. The thermally induced chemical reaction is identified through Differential Scanning Calorimetry (DSC) and Thermogravimetry Analysis (TGA). The peak deconvolution of the themo-chemical data is used to estimate the enthalpy change of each metallic fuel component. Laser Induced Breakdown Spectroscopy (LIBS) and X-ray Photoelectron Spectroscopy (XPS) are used for chemical species analysis. The decomposition of oxidants by moisture significantly affected the fuel aging, and the formation of oxide film and metal oxide on the fuel surface gave rise to the thermal energy decrease.

Degradation Characteristics of Carbon Dioxide Absorbents with Different Chemical Structures (상이한 화학적 구조를 가진 이산화탄소 흡수제의 열화특성)

  • Kim, Jun-Han;Lee, Ji-Hyun;Jang, Kyung-Ryong;Shim, Jae-Goo
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.31 no.10
    • /
    • pp.883-892
    • /
    • 2009
  • We evaluated the degradation properties of various alkanolamine absorbents (MEA, AMP, DEA, and MDEA) having different chemical structures for $CO_2$ capture. The degradation of $CO_2$ absorbent in general was known to be caused by oxygen which is in flue gas and by heat source, respectively. To analyze the effect of $CO_2$ and $O_2$ on degree of degradation, we conducted a variety of experiments at $30^{\circ}C$ and $60^{\circ}C$ (oxidative degradation) and $130^{\circ}C$ and $150^{\circ}C$ (thermal degradation), respectively. DEA showed the worst property for oxidative degradation in the presence of oxygen among the alkanolamine absorbents. In the case of thermal degradation, the degradation of absorbent was occurred for most of absorbents at $150^{\circ}C$. Among these absorbents, MEA and DEA gave the worst results. As a result, AMP which is a primary amine and having a steric hindrance showed the best result through the degradation test. But, the degradation of absorbent proceeded easily in the case of DEA which is a secondary amine and having 2 OH groups in terminal position. Consequently, we have evaluated the degree of degradation of various absorbents having different chemical structures to give the basic data for the development of alkanolamine absorbent.

세륨산화물로 전처리된 다공성 니켈 지지체 위에 스퍼터 증착된 팔라듐-구리 합금 분리막 특성

  • An, Hyo-Seon;Gang, Seung-Min;Kim, Dong-Won;Lee, Sin-Geun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.196-196
    • /
    • 2011
  • 팔라듐-구리 합금 분리막은 세륨산화물로 전처리된 다공성 니켈 지지체 위에 마그네트론 스퍼터 공정과 구리리플로우 공정에 의해 제조되었다. 스퍼터 공정은 얇고 치밀한 팔라듐 합금 분리막 증착을 위해 아주 효과적이다. 본 연구에서는 고온 스퍼터 공정에 의해 증착된 팔라듐 상부에 유동성과 열적확산이 우수한 구리를 코팅한 후, 반도체 분야에서 기가 패턴 매립시 사용하는 구리리플로우 공정을 도입하였다. 구리리플로우 공정은 치밀하고 미세기공이 존재하지 않는 표면을 구현하고 무한대의 수소 투과도를 가능하게 한다. 이로써 마그네트론 스퍼터에 의해 $200^{\circ}C$에서 팔라듐과 구리를 순차적으로 코팅한 후, $700^{\circ}C$에서 2시간 구리리플로우 공정을 실시하여 $7.5{\mu}m$ 두께의 팔라듐-구리 합금 분리막이 제조되었다. 세륨산화물(CeO2)은 고온에서 장시간 운전하는 동안 다공성 니켈 지지체의 금속성분이 팔라듐 합금층으로 확산하는 금속의 확산 문제를 개선하고자 지지체와 코팅층 사이에 확산방지막으로 도입되었으며, 균일한 스퍼터 증착을 위해 평탄한 표면의 지지체를 구현하였다. 투과도 테스트는 100-400kPa 의 압력차, 673-773K 의 온도 조건에서 순수한 수소가스로 실시하였다. 표면 미세기공이 없는 치밀한 팔라듐-구리 합금 분리막은 혼합가스에서 질소의 투과 없이 수소만을 투과하는 무한대의 우수한 분리도를 나타내었으며, 상용온도 $500^{\circ}C$에서 12.6ml/$cm^2{\cdot}min{\cdot}atm$의 수소 투과 능력을 보였다. 본 연구에 의해 제조된 팔라듐-구리 합금 분리막은 표면 미세기공이 없는 치밀한 분리막 제조를 가능하게 하였으며 열팽창계수가 팔라듐과 매우 비슷한 세륨산화물($CeO_2$)로 인해 지지체층과 코팅층과의 접합력이 향상되고 수소취성에 강하고 높은 열적 안정성을 갖는다.

  • PDF