Han, Woo Rim;Kim, So Jin;Lee, Eun Woo;Hwang, Jin Ju
Journal of Conservation Science
/
v.35
no.3
/
pp.187-196
/
2019
Bronzes excavated from a Gulsansa temple site in Gangneung were investigated in order to study the production of technology and provenance in this area. The bronze artifacts were discovered to consist of copper-tin or copper-tin-lead alloys using chemical analysis(EDS and EPMA). The excavated bronzes were manufactured using a casting or hammering process, and a bronze belt was gilded with gold foil. The provenance of 25 bronzes was studied using lead isotope analysis(TIMS and LA-MC-ICPMS). The results reveal the use of raw materials found near the excavated site. The object of this study was to investigate the manufacturing techniques and provenance in Gangneung without the need for a lot of data. Our results will contribute to the study of Gulsansa and bronze artifacts in Goryo(12-13th century).
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2000.07a
/
pp.671-674
/
2000
A children's electric shock accidents have broken out because children can easily insert sharp things in 220V receptacle holes. As the test result of pushing force, children's pushing force was about 2-4kg and the pushing force of sharp things was less than 2kg. Therefore, it is reason for electric shock that children's pushing force is large than pushing force of sharp things. We have measured insulation resistance for the receptacles of five companies during 50 weeks in humid condition. As these results, Insulation resistance for the receptacles of J. Co. had rapidly decreased with lapse of time. As the result for investigating the surface of receptacle by SEM and EDX, Al, Fe and Br, which weren't discovered at original form, were produced. Therefore, the receptacles of J. Co. should be the improved in the quality of insulating material because insulation resistance can be decreased in humid environment
We investigated the morphological characteristics of the pearlescent pigment by using scanning electron microscope, energy dispersive X-ray spectrometry and thermal analyzer. The result is that the shape of pigment is platy polygonal form through observing the pearlescent pigment by the scanning electron microscope. The size of pigment is various and not formed in standardized size or shape. The pigment flakes were measured about from $30{\mu}m$ to $300{\mu}m$. The tip of the piece of pigment is pointed shape or angled. The result of observing them by the scanning electron microscope in magnifying high power is that the edge and the lateral face of them is an round form and the measurement of thickness is about $9{\mu}m$. As well using the high magnification scanning electron microscope, the surface of the pigment flake observed like rugged as coating with the $TiO_2$ element, the diameter of the coating particle is around 60 nm, then the coating particle consists of granular substance. Analysis of the configuration elements of pearlescent pigment using by the energy dispersive X-ray spectrometry is that O, Si, C, Na, Ca, Ti, Zn detected in the surface of pigment and its lateral face identifies similar components. In thermal analysis, there are no contained quantity differences between them in beginning from $100^{\circ}C$ to $800^{\circ}C$ showing thermal analysis, 1.1% out of contained quantity reduced at $115^{\circ}C$, 1.7% dropped at $416^{\circ}C$, and 1.9% decreased at $797^{\circ}C$.
The physicochemical properties of damaged hair by irradiation of ultraviolet-B (UV-B) have been investigated by using transmission electron microscope and scanning electron microscope. The range of irradiation of hair irradiated for expectative 6 hours, 12 hours, 24 hours and 48 hours with stimulated ultraviolet ray. The treated hairs showed characteristic morphological damage pattern in the cornified cell of matrix and the cuticle following time past. The various sized vacuoles in the endocuticle of the cuticular cells was formed. The statistically significant differences in diameter of cuticular cell were observed in terms of tranverse swelling by formation of vacuoles. The hair cortex and matrix undergo long term exposure to UV-B radiation. The macrofibrils of cortex appeared to be affected most by UV-B, although the morphology and volume of melanin granule was not changed. The physicochemical destruction of hair matrix and cuticular cells is largely accelerated by long term irradiation of UV-B.
The purpose of this study was to observe the influences of the water fluoride concentration on the growth changes, the histologic characteristics of osteoblast in the tibia of growing newborn rats by using electron microscopy and on the composition changes of bone matrix in those by using energy dispersive x-ray system (EDX). The water fluoride concentration was respectively 0 ppm (contrast group), 100 ppm (100 ppm group), 200 ppm (200 ppm group) and 300 ppm (300 ppm group). The results of the investigation by using electron microscopy were as followed. In contrast group, the traditional cuboidal osteoblasts were observed. In 100 ppm group, several reversal line, the newly formed osteoid by the strongly activated osteoblast and the well developed rough endoplasmic reticulum, mitochondria in cytoplasm of osteoblast were observed. Also, many secretory vesicle around cell membrane were observed and some fused with cell membrane released secretory granule out of cell. In 200 ppm group, the depressed osteoblasts were observed, mitochondria in cytoplasm were expanded and cristae shape in mitochondria were destroyed. Also, the ribosome at the surface of rough endoplasmic reticulum were not observed. In 300 ppm group, the adjacent osteoblasts with endosteum were irregularly arranged, the cell membrane were destroyed and organelles were flowed out of cell. On the other hand, the results of the investigation by using energy dispersive x-ray system were as followed. P and Ca concentrations in 100 ppm group were increased more than those in contrast group. But, in 200 and 300 ppm group were not increased more than those in 100 ppm group. Therefore, the activities of the osteoblasts were increased, the bone matrix were actively synthesized by the supplied water fluoride. But, the osteoblasts were destroyed, inhibited by the higher water fluoride concentration.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.30
no.6
/
pp.271-276
/
2020
In this study, an amorphous SiC block was manufactured using polycarbosilane (PCS), an organosilicon polymer. The dense SiC blocks were easily fabricated in various shapes via pyrolysis at 1100℃, 1200℃, 1300℃, 1400℃ after manufacturing a PCS molded body using cured PCS powder. Physical and chemical properties were analyzed using a thermogravimetric analyzer (TGA), scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), and universal testing machine (UTM). The prepared SiC block was decomposed into SiO and CO gas as the temperature increased, and β-SiC crystal grains were grown in an amorphous structure. In addition, the density and flexural strength were the highest at 1.9038 g/㎤ and 6.189 MPa of SiC prepared at 1100℃. The manufactured amorphous silicon carbide block is expected to be applicable to other fields, such as the previously reported microwave assisted heating element.
Iron and nitrogen coordinated carbon catalyst (Fe-N-C) is the most promising non-precious metal catalyst (NPMC) studied to alternate the Pt-group oxygen reduction reaction (ORR) catalyst. In this work, Fe/N/C type catalysts are prepared by four different nitrogen precursors; N, N, N', N'-tetramethylethylenediamine (TMEDA), 1,2-ethylenediamine (EDA), m-dicyanobenzene (DCB), dicyandiamide (DCDA) which can chelate a transition metal; In addition, the catalysts conducted the pyrolysis process at four different temperatures of 700, 800, 900, 1000 ℃ to investigate the ORR activities depend on pyrolysis temperature and to find an appropriate temperature. The characterizations of catalysts were investigated by scanning electron microscope-energy dispersive X-ray spectrometer (SEM-EDS), X-ray diffraction (XRD), and element analysis (EA). The electrocatalytic activity was measured by ORR polarization, also the electron transfer number was calculated from the slope of the K-L plot. The FeNC-EDA-800 which were prepared at pyrolysis temperature of 800 ℃ with EDA showed better ORR activity than the other catalysts.
Carbon monoxide (CO) intoxication, arising from CO from an ignited charcoal briquette (ICB), is a popular means of committing suicide in Korea. Most CO intoxications are related to suicide attempts; however, the possibility of a homicide disguised as a suicide cannot be ruled out. Therefore, forensic investigation of the deceased and the crime scene is crucial to confirm that the deceased committed suicide. Detection of the components of an ICB on the objects suspected of being contacted by the deceased, such as the hands, nostrils, and doorknobs, is essential for linking the crime scene to the victim in the case of suicides by ignited ICBs. The traces from an ICB were analyzed by investigating the morphological characteristics and obtaining elemental compositions. The ICBs were completely different from blackened wood, as detected by discriminant analysis with the elements of carbon and oxygen. We analyzed one case of CO intoxication to demonstrate an excellent procedure for verifying whether a suicide occurred with an ICB. We employed SEM-EDX for the analysis of an ICB, microscope-FT/IR and pyrolysis-GC/MS for a partly burnt resin-type substance, GC/MS for diphenhydramine (a sleeping drug), and GC/TCD for the CO-Hb level. We detected traces of an ICB on the hands, nostrils, and doorknobs, which were all discriminated into an ICB group. Detection of ICB traces from the nostrils could indicate that the deceased started the fire themselves to commit suicide. The partially burnt black material was analyzed as an acrylronitrilestyrene polymer, which is normally used to make bags for carrying or wrapping and could be assumed to have been used to transport the ICB. Diphenhydramine, a sleeping drug, was detected at a level of 2.3 mg/L in the blood, which was lower than that in fatal cases (8-31 mg/L; mean 16 mg/L). A CO-Hb level of 79% was found in the blood, which means that the cause of death was CO intoxication. The steps shown here could represent an ideal method for reaching a verdict of suicide by CO intoxication produced by burning an ICB in a sealed room or a car.
Research was conducted to characterize the copper production and smelting process with 11 copper smelting by-products (copper slag and copper crucible) excavated from the NA and LA areas at the Gwanbuk-ri archeological site in Buyeo. Scanning electron microscopy-energy dispersive spectroscopy, wavelength dispersive X-ray fluorescence, X-ray diffraction, and Raman microspectroscopy were employed in the analysis. The research results reveal that the copper slag from Gwanbuk-ri contained silicate oxide, magnetite, fayalite, and delafossite, which are typical characteristics of crucible slag and refined slag. The outward appearance and microstructure of the slag were grouped as follows: 1. glassy matrix + Cu prill, 2. glassy matrix + Cu prill + magnetite, 3. silicate mineral matrix + Cu prill, 4. crystalline (delafossite and magnetite) + amorphous (Cu prill), 5. magnetite + fayalite, and 6. slag from slag. The copper slags from Guanbuk-ri were found to contain residues of impurities such as SiO2, Al2O3, CaO, SO4, P2O5, Ag2O, and Sb2O3 in their microstructure, and, in some cases, it was confirmed that copper, tin and lead are alloys. These results indicate that refining of intermediate copper(including impurities) and refining of alloys of copper(including impurities) - tin and refining of copper(including impurities) - tin - lead took place during the copper production process at Gwanbuk-ri, Buyeo.
Nitrogen ion implantation and ion plating techniques were applied for improvement of the wear resistance of metallic implant materials. In this work, the wear dissolution behaviour of a nitrogen ion implanted super stainless steel (S.S.S, 22Cr-20Ni-6Mo-0.25N) was compared with those of S.S.S, 316L SS and TiN coated 316L SS. The amounts of Cr and Ni ions worn-out from the specimens were Investigated using an electrothermal atomic absorption spectrometry. Furthermore, the Ti(Grade 2) disks were coated with TiN, ZrN and TiCN by use of low temperature arc vapor deposition and the wear resistance of the coating layers was compared with that of titanium. The chemical compositions of the nitrogen ion implanted and nitride coated layers were examined with a scanting auger electron spectroscopy. It wat observed that the metal ions released from the nitrogen ion implanted S.S.S surface were significantly reduced. From the results obtained, it was shown that the nitrogen ion implanted zone obtained with 100 KeV ion energy was easily removed within 200,000 revolutions from a wear dissolution testing under a similar load condition when applied to artificial hip joint. The remarkable improvement in wear resistance weir confirmed by the nitrides coated Ti materials and the wear properties differ greatly according to the chemical composition of the coating layers. for specimens with the same coating thickness of about 3$\mu\textrm{m}$, TiCN coated Ti showed the highest wear resistance. However, after removing the coating layers, the wear rates of all nitrides coated Ti reverted to their normal rates of below 10,000 revolutions from Ti-disk-on-disk wear testing under the same load condition. From the results obtained, it is suggested that the insufficient depth of the 100 Kel N$\^$+/ ion implanted zone and of the nitrides coated layers of 3$\mu\textrm{m}$ are subject to restriction when used as frictional parts of load bearing implants.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.